EN 10217-7 1.4529 Welded Stainless Steel Tube
What is EN 10217-7 1.4529 Welded Stainless Steel Tube
Inside the EN 10217-7:2021 welded stainless pressure-tube list, 1.4529 / X1NiCrMoCuN25-20-7 is the austenitic grade purchasers pick when the duty matches this chemistry story. The standard covers circular welded tubes for pressure and corrosion-resisting purposes; it does not accept a bare “6Mo / N08926” stamp as a substitute for steel number, delivery-condition symbol, or test category. Name EN 10217-7, 1.4529, TC1/TC2, and the options list on the purchase order so cast analysis, longitudinal weld manufacture, solution treatment where required, mechanical verification, and leak-tightness are unambiguous. Practical role: 6Mo high-Ni super-austenitic (N08926-type) welded pressure tube for severe chloride PED service with a higher Ni window than 1.4547.
SHH STEEL can produce and supply EN 10217-7 1.4529 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover specialty welded OD; agree route and delivery symbol at enquiry. Browse the series hub at EN 10217-7.
1.4529 is the EN welded-pressure designation for the N08926 chemistry idea — order the steel number, test category, and delivery condition, not only the UNS alias. Typical welded pressure duties include offshore, desalination-adjacent, and aggressive chloride chemical PED piping that names N08926 / 1.4529. Design caution: UNCERTAIN elevated-temperature HTML labelling on one BSSA row — rely on ambient Tables 6/7 and the purchased edition for elevated design data Commercially the grade is often called 6Mo / N08926; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4529 / X1NiCrMoCuN25-20-7 on the MTC. Sister numbers on this hub include EN 10217-7 1.4547, EN 10217-7 1.4563, EN 10217-7 1.4410.4547, 1.4563, 1.4410.
Product-form discipline: order EN 10217-7 for welded 1.4529, EN 10216-5 for seamless. Dimensions lean on EN ISO 1127. Manufacture is longitudinal arc or laser from strip or plate per Table 1; spiral/helical is not invented as a listed Part 7 route in this series. Live seamless sister: EN 10216-5 1.4529.
Chemical Composition of EN 10217-7 1.4529
Heat acceptance for 1.4529 starts with cast analysis to X1NiCrMoCuN25-20-7. Option 6 product analysis uses the standard’s permissible deviations. SHH STEEL documents real ladle results on EN 10204 3.1 and treats private catalogue windows as non-EN unless the purchaser agrees them separately.
The following cast analysis for X1NiCrMoCuN25-20-7 is taken from public BSSA EN 10217-7 data for steel number 1.4529. Maxima apply except where a range is shown. Verify against the ordered EN 10217-7:2021 text before release.
| Element | 1.4529 cast analysis (mass %) |
|---|---|
| Carbon (C) | ≤0.020 |
| Silicon (Si) | ≤0.50 |
| Manganese (Mn) | ≤1.00 |
| Phosphorus (P) | ≤0.030 |
| Sulfur (S) | ≤0.010 |
| Nitrogen (N) | 0.15–0.25 |
| Chromium (Cr) | 19.0–21.0 |
| Nickel (Ni) | 24.0–26.0 |
| Molybdenum (Mo) | 6.00–7.00 |
| Copper (Cu) | 0.50–1.50 |
Public BSSA EN 10217-7 chemistry underpins the 1.4529 / X1NiCrMoCuN25-20-7 table below. Cross-check is against the 2021 grade list framing. Scrap and finishing practice must still protect the austenitic property set — unlisted deliberate additions require agreement.
Mechanical Properties of EN 10217-7 1.4529
EN 10217-7 lists ambient tensile and ductility requirements for solution-annealed X1NiCrMoCuN25-20-7 (steel number 1.4529) in the austenitic table, covering walls up to about 60 mm by default. Both 0.2% and 1.0% proof stresses are specified. −196 °C impact data are available as characterisation; verification is an Option-driven act.
For 1.4529, the tensile and ductility floors below are BSSA EN 10217-7 ambient figures. Solution temperatures for X1NiCrMoCuN25-20-7 come from public EN stainless tables (UNCERTAIN against paid Part 7 footnotes). SHH STEEL will not inflate or swap those floors using another product standard’s numbers. UNCERTAIN: BSSA elevated-temperature HTML row for 1.4529 appears mislabelled with 1.4501 steel name — ambient values used as primary
| Property | 1.4529 ambient (solution annealed +AT) |
|---|---|
| Rp0.2 min (MPa) | 300 |
| Rp1.0 min (MPa) | 340 |
| Rm (MPa) | 600–800 |
| A min % long / trans | 40 / 40 |
| IGC resistance (delivery) | Yes (method A) |
| Solution annealing (public EN band) | 1120–1180 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges |
| Cooling | water or air |
| Charpy sub-zero (transverse min J) | 60 at -196 °C (Option to verify) |
Mechanical source stack for 1.4529: BSSA EN 10217-7 ambient properties; public EN solution-anneal bands with UNCERTAIN paid-edition flag. Characterisation impact energies for X1NiCrMoCuN25-20-7 become certificate entries only through the relevant Options.
Welded Tube Manufacture for EN 10217-7 1.4529
Part 7 production of 1.4529 / X1NiCrMoCuN25-20-7 is a longitudinal weld story. Strip or plate is formed and closed by automatic arc or laser welding on a Table 1 route, with or without filler and with optional outside grind or bead work ahead of heat treatment. Everyday sizes run on strip; heavier walls use plate. Finished tubes exclude pre-forming strip-join welds. Helical manufacture is outside the listed routes — settle any non-standard seam in writing. Seamless pressure stainless is ordered under EN 10216-5, not under this welded page.
High-alloy austenitic 1.4529 (X1NiCrMoCuN25-20-7) is welded longitudinally under Table 1 with procedures that respect the Mo-Cu (and nitrogen where present) balance — heat input and cleanliness matter more than on commodity 18-8. Options 3/4 dress the ID weld when required; Table 2 symbols set surface/heat-treatment path with Option 5 to lock. SHH STEEL can produce and supply 1.4529 as heat-treated descaled or cold-finished product when strip chemistry and weld slots align. Filler guidance for this page: matching 6Mo/high-Ni fillers; rigorous cleanliness; corrosion testing frequently mandatory on the project spec
Specify TC1 or TC2 with the 1.4529 size list. Inspection intensity and marking content depend on it; leak-tightness applies to each length, and Option 15 can freeze the technique. SHH STEEL’s documents name the weld manufacture route and delivery-condition symbol used for X1NiCrMoCuN25-20-7.
Dimensions and Tolerances for EN 10217-7 1.4529
Buyers order 1.4529 (X1NiCrMoCuN25-20-7) on outside diameter and wall thickness. EN ISO 1127 preferred sizes and stainless densities apply. EN 10217-7 tolerance classes (Option 20 → D4) govern diameter and wall; ovality and eccentricity remain inside those envelopes, and abutting-edge radial offset at the weld is limited per public text.
Exact-length Option 19 and bevel Option 18 (wall ≥ 3.2 mm) are standard extras. For 6Mo / N08926-class welded pressure tube needing tighter OD, WCA/WCR is usually discussed alongside W1A/W2A. SHH STEEL locks OD × wall, class, and symbol on the 1.4529 order prior to welding.
| Route / condition | Typical use | Notes |
|---|---|---|
| W1 / W1A / W1R | Hot-rolled starting flat product | Descaled or bright-annealed per symbol |
| W2 / W2A / W2R | Cold-rolled starting flat product | Smoother OD than W1 family except at weld |
| WCA / WCR | Cold finished ≥20% after weld | Recrystallized weld metal; OD often ≤168.3 mm |
| WG / WP | Ground / polished | Agree ID/OD scope and grit at enquiry |
Release of EN 10217-7 1.4529 includes confirmation that OD × wall sit inside the purchased class for X1NiCrMoCuN25-20-7. Straightness and end condition are inspected to the standard; cold-finished routes are recommended when D4 is specified. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4529 / X1NiCrMoCuN25-20-7 on the inspection document rather than assuming mid-tolerance catalogue values.
Equivalent Grades for EN 10217-7 1.4529
Steel number 1.4529 with name X1NiCrMoCuN25-20-7 is what EN 10217-7 stamps on welded pressure tube of this analysis. Alias 6Mo / N08926 is commercial language. Treat ASTM/ASME lookalikes and EN 10216-5 seamless pages as related references — verify before dual-marking or substituting.
Bill-of-materials writers sometimes list 6Mo / N08926 next to EN and ASTM numbers interchangeably. For this product, steel number 1.4529 with name X1NiCrMoCuN25-20-7 under EN 10217-7 is the welded acceptance path; confirm any dual mark against both mechanical tables before release to fabrication.
| Reference | Designation | Note |
|---|---|---|
| EN 10217-7 | 1.4529 / X1NiCrMoCuN25-20-7 | This product standard (welded pressure tube) |
| EN steel name | X1NiCrMoCuN25-20-7 | EN 10027-1 designation used in body and marking |
| Commercial alias (body only) | 6Mo / N08926 | Not a substitute for the steel number on the MTC |
| EN 10216-5 (seamless sister) | 1.4529 | Related live page — different product form (seamless) |
Inside this welded series, compare EN 10217-7 1.4547, EN 10217-7 1.4563, EN 10217-7 1.4410. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4529.
Heat Treatment and Delivery Condition for EN 10217-7 1.4529
Choose the Table 2 symbol for 1.4529 with heat treatment in mind. W1A/W2A, cold-finished WCA/WCR, and bright-annealed W1R/W2R all imply treated routes; mechanical acceptance for X1NiCrMoCuN25-20-7 is written for solution-annealed (+AT) tube. For X1NiCrMoCuN25-20-7 under steel number 1.4529, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
Reference solution window for 1.4529: 1120–1180 °C with water or air cooling, drawn from public EN stainless tables and flagged UNCERTAIN vs paid Part 7 notes. Surface finish remains a Table 2 / Option 5 decision after heat treatment of X1NiCrMoCuN25-20-7. For X1NiCrMoCuN25-20-7 under steel number 1.4529, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
| Item | 1.4529 |
|---|---|
| Solution annealing band (public) | 1120–1180 °C (UNCERTAIN vs paid Part 7 footnote) |
| Cooling | water or air |
| Delivery condition symbols | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify) |
| Inspection document | EN 10204 3.1 default; 3.2 under Option 21 |
Delivery-condition control for 1.4529 means more than a furnace ticket: SHH STEEL records the symbol, the heat treatment implied for X1NiCrMoCuN25-20-7, and cold-finished weld recrystallization status when WCA/WCR applies, then ships only material that matches that record. For X1NiCrMoCuN25-20-7 under steel number 1.4529, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
Corrosion Resistance of EN 10217-7 1.4529
Corrosion-resisting austenitic 1.4529 / X1NiCrMoCuN25-20-7 is selected for welded pressure duty where the medium and temperature need 6Mo + Cu + N with higher Ni for stability in severe chloride and many chemical media. EN 10217-7 marks intergranular-corrosion behaviour in the delivery condition against EN ISO 3651-2 methods in the mechanical tables; verification of IGC remains Option 13 even when the table says the grade resists IGC as delivered.
Elevated-temperature service of X1NiCrMoCuN25-20-7 still needs proper design data; IGC guideline temperatures only address sensitisation susceptibility. For 1.4529, SHH STEEL keeps those notes distinct from tensile floors and from any PREN marketing the enquiry may quote. Sisters: EN 10217-7 1.4547, EN 10217-7 1.4563, EN 10217-7 1.4410.
Applications of EN 10217-7 1.4529 Tube
EN 10217-7 1.4529 welded tube is used where PED-oriented pressure tubing must also resist corrosion and a longitudinal weld seam is accepted on the drawing. For X1NiCrMoCuN25-20-7 the practical band is offshore, desalination-adjacent, and aggressive chloride chemical PED piping that names N08926 / 1.4529, supplied as welded tube in the ordered delivery condition with TC1 or TC2 testing.
It is the wrong first choice when a seamless product is mandatory (use EN 10216-5 — see EN 10216-5 1.4529), when the drawing is ASTM A269 instrumentation tubing or A312 pipe without an EN dual mark, or when the medium clearly needs a different family. SHH STEEL can produce and supply 1.4529 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit.
Weldability of EN 10217-7 1.4529
1.4529 / X1NiCrMoCuN25-20-7 is welded both as a mill seam under EN 10217-7 manufacturing routes and later as a fabricator joint on the PED spool. Mill seams follow the qualified longitudinal arc or laser procedures for the ordered route; shop welds use processes and fillers chosen for the EN chemistry family. For this grade: matching 6Mo/high-Ni fillers; rigorous cleanliness; corrosion testing frequently mandatory on the project spec
Mill weldability of 1.4529 is proven on the Table 1 route; fabricator weldability is proven on the WPS. Keep those scopes apart. SHH STEEL certifies X1NiCrMoCuN25-20-7 mill tube to the ordered delivery condition and inspection Options, and leaves joint design — including as-welded service limits — with the PED responsible party.
Surface Finishes for EN 10217-7 1.4529
W1A/W2A descaled, W1R/W2R/WCR bright-annealed, and WG/WP ground or polished are the finish vocabulary for 1.4529. Write roughness when WP/WG is wanted; do not assume a grit from a brochure photo of X1NiCrMoCuN25-20-7. Carbon-steel banding on stainless is rejected in SHH STEEL packing rules because free-iron stains on 6Mo / N08926 are expensive to remove and easy to prevent at the dock.
Anything beyond Table 2 surface language needs writing: Ra, EP, films, capped cleanliness. SHH STEEL can produce and supply finishes it can report for EN 10217-7 1.4529; unmeasured grit marketing is not offered for X1NiCrMoCuN25-20-7, and commercial 6Mo / N08926 habits do not override that discipline.
If the drawing shows a hygienic OD note without EN delivery language, translate it into W1R/W2R, WCR, or WP with criteria before releasing 1.4529. SHH STEEL will help map that note onto a measurable finish for X1NiCrMoCuN25-20-7 instead of guessing what the last fabricator accepted on unlabeled 6Mo / N08926 tube.
Inspection and Testing for EN 10217-7 1.4529
Baseline Part 7 inspection for 1.4529: cast analysis, room-temperature tensile at the ordered test-category rate, technological tests, full leak-tightness coverage, plus dimensional/visual/ID work on X1NiCrMoCuN25-20-7. Hydrostatic or eddy-current leak testing may be locked with Option 15. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4529 purchase order so X1NiCrMoCuN25-20-7 inspection planning matches the PED file before weld slots are locked.
TC2, Option 13 IGC, and impact Options are how purchasers thicken the 1.4529 inspection story beyond baseline leak-tightness and tensile. SHH STEEL documents chemistry, heat treatment, tensile, and NDT/leak results for X1NiCrMoCuN25-20-7 and will not delete mandatory tests to chase a shorter promise date.
Leak-tightness failures on 1.4529 are dispositioned per procedure — not silently downgraded to a non-pressure grade. SHH STEEL keeps failed X1NiCrMoCuN25-20-7 lengths out of EN 10217-7 shipments.
Packaging and Shipping for EN 10217-7 1.4529
Dispatch packing on EN 10217-7 1.4529 covers mechanical protection and stainless hygiene. Caps or plugs close the ends, bundles are size-sorted, and waterproof wrap covers long sea legs. High-alloy 6Mo / N08926 bright-annealed or polished OD is sleeved against transit galling; descaled chemical-service tube still ships on non-contaminating supports with capped ends. Contact materials exclude bare carbon steel so X1NiCrMoCuN25-20-7 OD — commercially still discussed as 6Mo / N08926 — does not pick up rust blooms in transit that complicate PED receiving inspection.
Marking discipline for 1.4529: standard, steel number or X1NiCrMoCuN25-20-7, size, cast, TC1/TC2, inspection marks. Delivery symbols follow manufacturer practice unless Option 5 demands them. SHH STEEL verifies the marking clause on the 6Mo / N08926 order prior to shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4529 / X1NiCrMoCuN25-20-7 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Ocean and road packs for 1.4529 keep heat identity visible at bundle level. Bevelled and exact-length tube is capped and segregated. SHH STEEL closes packaging only after the order’s packing and marking lines are satisfied for this 6Mo / N08926 grade. SHH STEEL treats packing and marking for EN 10217-7 1.4529 / X1NiCrMoCuN25-20-7 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Why Choose SHH STEEL
SHH STEEL can produce and supply 1.4529 welded stainless pressure tube with matching heat treatment and TC1/TC2 documentation for X1NiCrMoCuN25-20-7. The commercial alias 6Mo / N08926 may appear in body text; it does not replace the steel number on the certificate, and sister-standard tensile floors stay off this Part 7 document.
Use LINKPLACE1.4547, LINKPLACE1.4563, LINKPLACE1.4410 as the short-list when 1.4529 is borderline. Remember: UNCERTAIN elevated-temperature HTML labelling on one BSSA row — rely on ambient Tables 6/7 and the purchased edition for elevated design data The PED file needs the right steel number more than it needs a fast yes Linked sisters on this hub: EN 10217-7 1.4547, EN 10217-7 1.4563, EN 10217-7 1.4410.
Supply Capability
SHH STEEL can produce and supply 1.4529 welded stainless pressure tube under EN 10217-7 with the documents and tests your enquiry lists. Capability plus Stock / Available sizes below are the sizing scratchpad for X1NiCrMoCuN25-20-7. Specialty welded od; agree route and delivery symbol at enquiry.
| Item | SHH STEEL capability for 1.4529 |
|---|---|
| Standard | EN 10217-7 |
| Grade | 1.4529 / X1NiCrMoCuN25-20-7 |
| Product form | Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition |
| Delivery condition | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock) |
| Typical size band | ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement |
| Testing | TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options |
| Documents | EN 10204 3.1 (3.2 Option 21); third-party inspection on request |
Stock / Available sizes
The Stock / Available sizes block for 1.4529 is a planning aid. Actual commitment waits on X1NiCrMoCuN25-20-7 melt/strip position and the ordered W-symbol finishing path. Send sizes, TC1/TC2, and delivery condition to firm it up.
| OD (mm) | Typical walls (mm) | Notes |
|---|---|---|
| 12 / 14 / 16 / 19 / 21.3 / 25 | 1.0 / 1.5 / 2.0 / 2.5 | Instrument / hygienic; often WCA/WCR or W2R |
| 26.9 / 33.7 / 38 / 42.4 / 48.3 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Process and utility welded pressure tube |
| 60.3 / 76.1 / 88.9 / 114.3 | 2.0 / 3.0 / 4.0 / 5.0 / 6.0 | Utility and process; lock W1A/W2A vs WCA |
| 141.3 / 168.3 / 219.1 | 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 | Larger welded pressure tube; watch family wall ceiling |
Option-driven extras and sister comparisons (1.4547, 1.4563, 1.4410) belong on the enquiry. Size rows are typical, not promised stock. SHH STEEL can produce and supply EN 10217-7 1.4529 across this map when X1NiCrMoCuN25-20-7 feedstock and weld capacity agree.
FAQ
-
What is EN 10217-7 1.4529 welded stainless steel tube used for?
- EN 10217-7 1.4529 (X1NiCrMoCuN25-20-7) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is offshore, desalination-adjacent, and aggressive chloride chemical PED piping that names N08926 / 1.4529. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
-
Is EN 10217-7 1.4529 the same as 6Mo / N08926 under ASTM A269 or A312?
- No. Commercial alias 6Mo / N08926 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing.
-
Does EN 10217-7 1.4529 include seamless tube?
- No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4529. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
-
What mechanical properties does EN 10217-7 require for 1.4529?
- In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 300 MPa, Rp1.0 min 340 MPa, Rm 600–800 MPa, and elongation 40% longitudinal / 40% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
-
1.4529 vs sister grades — which EN 10217-7 number should I buy?
- Buy 1.4529 when the enquiry names this steel number or the duty matches 6Mo high-Ni super-austenitic (N08926-type) welded pressure tube for severe chloride PED service with a higher Ni window than 1.4547. Compare EN 10217-7 1.4547, EN 10217-7 1.4563, EN 10217-7 1.4410 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: UNCERTAIN elevated-temperature HTML labelling on one BSSA row — rely on ambient Tables 6/7 and the purchased edition for elevated design data
-
What delivery conditions are available for EN 10217-7 1.4529?
- Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
-
What size range can SHH STEEL supply for EN 10217-7 1.4529?
- SHH STEEL can produce and supply EN 10217-7 1.4529 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Specialty welded od; agree route and delivery symbol at enquiry.
-
TC1 or TC2 for EN 10217-7 1.4529?
- Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
-
Is the intergranular corrosion test mandatory for 1.4529?
- No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4529.
-
What documents come with SHH STEEL EN 10217-7 1.4529?
- EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4529, size, cast, and test category.
-
How do I enquire for EN 10217-7 1.4529 with SHH STEEL?
- Send EN 10217-7, steel number 1.4529 / X1NiCrMoCuN25-20-7, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.
Conclusion
EN 10217-7 1.4529 (X1NiCrMoCuN25-20-7) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4529 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.