EN 10217-7 1.4306 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4306 Welded Stainless Steel Tube

EN 10217-7 1.4306 / X2CrNi19-11 welded stainless pressure tube (304L (high-Ni)), austenitic, cast analysis per EN table, ambient Rp0.2 min 180 MPa, Rm 460–680, solution annealed 1000–1100 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4306 / X2CrNi19-11 (304L (high-Ni) — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4306 Welded Stainless Steel Tube

Ordering welded pressure stainless under EN 10217-7 means choosing a steel number from the austenitic or duplex tables, a test category, and a delivery-condition path — not pasting a shop alias onto random mill stock. 1.4306 is the EN designation for X2CrNi19-11 (304L (high-Ni) in commercial speech) in the austenitic family. Part 7 of EN 10217 defines the welded circular product for pressure plus corrosion-resisting service; the order text must carry EN 10217-7, 1.4306, TC1 or TC2, and options so the mill runs the right strip/plate route and inspection. Use case: high-nickel low-carbon 18-8 austenitic welded pressure tube when ferrite control and forming behaviour matter more than the lower-Ni 1.4307 window.

SHH STEEL can produce and supply EN 10217-7 1.4306 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover precision and mid-OD welded tube where cold finishing after welding is common. Browse the series hub at EN 10217-7.

1.4306 is the EN welded-pressure answer when the enquiry literally names X2CrNi19-11 or a high-Ni 304L cast analysis — not a catalogue synonym for every 1.4307 quote. Typical welded pressure duties include cryogenic and cold-service PED lines, deep-drawing-adjacent fabrications, and process utilities where the purchaser specifies the higher-Ni 1.4306 analysis. Design caution: the high-Ni window costs more than 1.4307 for little chloride benefit — do not upgrade on habit; upgrade when the order or welding procedure actually needs it Commercially the grade is often called 304L (high-Ni); keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4306 / X2CrNi19-11 on the MTC. Sister numbers on this hub include EN 10217-7 1.4307, EN 10217-7 1.4311, EN 10217-7 1.4301.4307, 1.4311, 1.4301.

Scope check before release: Part 7 = welded X2CrNi19-11 tube; Part 5 = seamless. Preferred OD × wall language follows EN ISO 1127. Listed manufacture is longitudinal automatic arc or laser welding — helical seam stays outside the public Table 1 routes referenced here. Live seamless sister: EN 10216-5 1.4306. Related live ASTM/ASME anchors: A269 TP304L, A213 TP304L.

Chemical Composition of EN 10217-7 1.4306

EN 10217-7 requires the cast analysis of 1.4306 to meet X2CrNi19-11 limits in the austenitic listing. Product analysis is the Option 6 path. On the certificate SHH STEEL shows actual cast chemistry for this 304L (high-Ni) welded pressure grade — not a marketing typical.

Chemical limits for 1.4306 / X2CrNi19-11 come from the public BSSA EN 10217-7 article, cross-checked to the 2021 grade list. Unless a range is stated, treat values as maxima. Secondary catalogues are not the purchase contract.

Element 1.4306 cast analysis (mass %)
Carbon (C) ≤0.030
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.045
Sulfur (S) ≤0.015
Nitrogen (N) ≤0.10
Chromium (Cr) 18.0–20.0
Nickel (Ni) 10.0–12.0

The X2CrNi19-11 composition window shown for 1.4306 is taken from the BSSA EN 10217-7 chemistry article. Public standard cross-check applies. Unlisted elements stay off the intentional-addition list unless the purchaser agrees, with the usual finishing-addition / scrap exceptions for austenitic melts.

Mechanical Properties of EN 10217-7 1.4306

Mechanical floors for welded 1.4306 tube in X2CrNi19-11 are the EN 10217-7 austenitic ambient (+AT) figures for walls inside the public characterisation window (about 60 mm unless Options say otherwise). Rp0.2, Rp1.0, Rm, and elongation are the everyday acceptance set; cryogenic impact stays optional until selected.

Ambient mechanical values shown for X2CrNi19-11 track BSSA BS EN 10217-7 (2021 framing). Public EN solution-annealing ranges are used with an UNCERTAIN tag relative to paid EN 10217-7 footnotes. Acceptance for steel number 1.4306 stays on the Part 7 table SHH STEEL cites — not on a borrowed sister datasheet.

Property 1.4306 ambient (solution annealed +AT)
Rp0.2 min (MPa) 180
Rp1.0 min (MPa) 215
Rm (MPa) 460–680
A min % long / trans 40 / 35
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1000–1100 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 60 at -196 °C (Option to verify)

Public sources for the X2CrNi19-11 ambient table: BSSA EN 10217-7 mechanical article; annealing windows from public EN stainless documents (UNCERTAIN vs paid 2021 Part 7). Select impact Options on 1.4306 when certified joules are mandatory.

Welded Tube Manufacture for EN 10217-7 1.4306

Building 1.4306 under EN 10217-7 means committing to a welded circular tube: longitudinal automatic arc or laser weld from X2CrNi19-11 strip or plate, following Table 1. As-welded, outside-ground, and bead-worked-before-heat-treatment variants are the listed paths; spiral seam is not among them in the public text used for this series. Continuous strip forming and plate forming cover the size map. SHH STEEL will not treat a helical-weld drawing as automatic Part 7 acceptance. Seamless pressure tube belongs on the EN 10216-5 sister conversation.

For austenitic 1.4306 (X2CrNi19-11), mill seams are typically made without filler or with matching filler depending on route and wall; Options 3 and 4 cover inside-weld remelt or bead working when the purchaser wants a smoothed ID weld. Delivery condition symbols (Table 2) include W0, W1/W1A/W1R, W2/W2A/W2R, cold-finished WCA/WCR with recrystallized weld metal, and WG/WP ground or polished. Unless Option 5 is specified, selection is at the manufacturer’s discretion. SHH STEEL can produce and supply 1.4306 as W1A/W2A descaled or WCA/WCR cold-finished in the common pressure-tube band, and as WG/WP when roughness is agreed. low-carbon austenitic fillers; ferrite balance is often easier to keep in the desired band than with the leaner-Ni L grades

EN 10217-7 expects TC1 or TC2 on the 1.4306 purchase order and on the tube. Seam NDT and tensile sampling follow; leak testing remains length-by-length with Option 15 as the method lock. Manufacturing route plus delivery-condition symbol for X2CrNi19-11 are stated by SHH STEEL as run.

Dimensions and Tolerances for EN 10217-7 1.4306

EN 10217-7 1.4306 is sized by D × T. Start from EN ISO 1127 preferred sizes for X2CrNi19-11; apply stainless density for mass. Tolerance classes follow the Part 7 framework — Option 20 selects D4 when instrumentation fit-up needs it. Out-of-roundness, eccentricity, and weld-edge radial offset rules in the dimensional clauses still apply.

Options 19 (exact length) and 18 (bevel, wall ≥ 3.2 mm) sit on top of the D × T order for 1.4306. Cold-finished WCA/WCR is the common upgrade path when OD tolerance and weld recrystallization matter. SHH STEEL confirms those choices with the delivery symbol before production release.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

SHH STEEL’s dimensional report on 1.4306 / X2CrNi19-11 cites the ordered tolerance class, not a generic “per EN” line. Straightness and end-finish checks remain part of release under EN 10217-7 dimensional clauses. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4306 / X2CrNi19-11 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4306

EN 10217-7 identifies this welded product as 1.4306 / X2CrNi19-11. Keep 304L (high-Ni) in body text and enquiry notes, not as the sole MTC identity. ASTM/ASME standards that share the alias differ in scope; EN 10216-5 is seamless, not an alternate welded acceptance path.

Cross-standard shopping for 304L (high-Ni) chemistry is common; acceptance is not. EN 10217-7 1.4306 remains the welded pressure-tube contract for X2CrNi19-11 on this page. Seamless sisters and ASTM/ASME pages are references until the order explicitly dual-certifies under each standard’s clauses.

Reference Designation Note
EN 10217-7 1.4306 / X2CrNi19-11 This product standard (welded pressure tube)
EN steel name X2CrNi19-11 EN 10027-1 designation used in body and marking
Commercial alias (body only) 304L (high-Ni) Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4306 Related live page — different product form (seamless)
A269 TP304L A269 TP304L Related live page — different product standard
A213 TP304L A213 TP304L Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4307, EN 10217-7 1.4311, EN 10217-7 1.4301. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4306. Live cross-standard anchors: A269 TP304L, A213 TP304L.

Heat Treatment and Delivery Condition for EN 10217-7 1.4306

EN 10217-7 1.4306 is supplied to a Table 2 delivery condition. Where that symbol requires heat treatment, solution annealing (+AT) is the reference path behind the X2CrNi19-11 ambient properties: soak in the solution band, cool rapidly, and document what was done. For X2CrNi19-11 under steel number 1.4306, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

X2CrNi19-11 solution annealing on public tables: 1000–1100 °C, cooled by water or air. Treat as UNCERTAIN relative to paid EN 10217-7:2021 footnotes. Delivery-condition symbol (Option 5) then selects the surface path for 1.4306. For X2CrNi19-11 under steel number 1.4306, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Item 1.4306
Solution annealing band (public) 1000–1100 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

Ordered heat treatment on X2CrNi19-11 is verified before dispatch. SHH STEEL’s paperwork for EN 10217-7 1.4306 ties ambient tensile results to the Table 2 delivery symbol and notes weld-seam treatment on cold-finished product, so the certificate matches the tube that arrives. For X2CrNi19-11 under steel number 1.4306, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Corrosion Resistance of EN 10217-7 1.4306

For 304L (high-Ni)-class welded pressure tube under steel number 1.4306, corrosion performance rests on same Mo-free family story as 1.4307 with a higher nickel floor that stabilises austenite during weld thermal cycles. Tables may indicate IGC resistance as delivered for X2CrNi19-11; ordering Option 13 is what puts a tested EN ISO 3651-2 result onto the certificate.

Chloride and acid selection for welded 1.4306 should start from the corrosion paragraph on this page, then move among EN 10217-7 1.4307, EN 10217-7 1.4311, EN 10217-7 1.4301 if needed. SHH STEEL will not convert marketing PREN/CPT figures into EN certificate limits for X2CrNi19-11, and will not treat IGC guideline temperatures as strength ceilings.

Applications of EN 10217-7 1.4306 Tube

Specify EN 10217-7 1.4306 when the line list wants 304L (high-Ni)-class welded pressure tube for duties such as cryogenic and cold-service PED lines, deep-drawing-adjacent fabrications, and process utilities where the purchaser specifies the higher-Ni 1.4306 analysis. The steel name X2CrNi19-11 belongs on the MTC with TC1 or TC2 and the chosen Table 2 symbol.

Do not force 1.4306 into seamless-only drawings (switch to EN 10216-5 — see EN 10216-5 1.4306), pure ASTM tubing/pipe scopes without EN dual marking, or media that outclass this chemistry. SHH STEEL can produce and supply EN 10217-7 1.4306 and will recommend EN 10217-7 1.4307, EN 10217-7 1.4311, EN 10217-7 1.4301 or a live cross-standard page when selection is still open. Related live pages: A269 TP304L, A213 TP304L.

Weldability of EN 10217-7 1.4306

Weldability talk for 304L (high-Ni) under steel number 1.4306 splits mill seam versus fabricator joint. The mill follows Part 7 longitudinal routes for X2CrNi19-11; the fabricator picks process and filler for the spool. Shop guidance on this page: low-carbon austenitic fillers; ferrite balance is often easier to keep in the desired band than with the leaner-Ni L grades

Once X2CrNi19-11 tube leaves the mill as EN 10217-7 1.4306, spool welding is a separate engineering act. SHH STEEL does not own the fabricator’s as-welded corrosion or PWHT choices; we own the mill certificate package — chemistry, seam route, heat treatment symbol, tensile, and leak/NDT.

Surface Finishes for EN 10217-7 1.4306

Ordered surface on EN 10217-7 1.4306 / X2CrNi19-11 follows the delivery-condition letter the purchaser locks (Option 5) or the manufacturer selects. Pickle/descaled suits lagged utility; bright anneal suits cleaner OD; grind/polish needs grit or Ra on the PO. Protect 304L (high-Ni) from carbon-steel contact in every pack design so free-iron transfer never becomes a site cleanup project after ocean freight.

Electropolish and ID Ra belong in the PO alongside steel number 1.4306. SHH STEEL can produce and supply the common descaled and bright-annealed routes for X2CrNi19-11, plus polished OD when grit is agreed and checked — no catalogue fiction, no unverified “mirror” claims for 304L (high-Ni).

Buyers sometimes request “same as last 304L (high-Ni) lot” without a symbol. For 1.4306 / X2CrNi19-11, SHH STEEL restates the Table 2 finish on the order acknowledgement so there is no silent drift between descaled utility and bright-annealed instrumentation product across releases.

Inspection and Testing for EN 10217-7 1.4306

TC1/TC2 define tensile intensity on 1.4306, but leak-tightness is per tube either way. Cast analysis, technological tests, dimensions, visuals, and material ID complete the baseline for X2CrNi19-11. Option 15 selects the leak-test method when the purchaser refuses manufacturer choice. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4306 purchase order so X2CrNi19-11 inspection planning matches the PED file before weld slots are locked.

Weld-seam NDT intensity and optional laminar/edge tests rise with TC2 for X2CrNi19-11. IGC (Option 13) and Charpy Options remain opt-in. SHH STEEL reports the ordered package on EN 10204 3.1 for 1.4306 and keeps mandatory Part 7 tests on the schedule. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4306 purchase order so X2CrNi19-11 inspection planning matches the PED file before weld slots are locked.

Dimensional and visual release on 1.4306 still matters after NDT and tensile pass — ovality, weld bead, and end condition can fail a spool fit-up. SHH STEEL includes those checks in the X2CrNi19-11 inspection release gate.

Packaging and Shipping for EN 10217-7 1.4306

When 1.4306 (X2CrNi19-11) leaves the mill as EN 10217-7 welded tube, packing protects both the weld-seam region and the ordered surface condition. End protection, sorted bundles or crates, and ocean-freight wrap are baseline. Bright-annealed and polished OD (W1R/W2R, WCR, WP) take sleeve or paper wrap against transit galling; descaled W1A/W2A utility tube still needs clean supports under the longitudinal seam. Carbon-steel banding against stainless is not used — free-iron staining on 304L (high-Ni) tube is a packing defect SHH STEEL designs out before dispatch.

Goods-in should read EN 10217-7, 1.4306, dimensions, cast, and test category without decoding gymnastics. Delivery condition may be marked; it is required in spirit when Option 5 applied. SHH STEEL sets stencil and tags for X2CrNi19-11 before the pack line closes. SHH STEEL treats packing and marking for EN 10217-7 1.4306 / X2CrNi19-11 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Traceable packing lists link X2CrNi19-11 heats to physical bundles. Option 19/18 pieces get their own capped packs. Dispatch waits until packing and marking match the 1.4306 purchase order. SHH STEEL treats packing and marking for EN 10217-7 1.4306 / X2CrNi19-11 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and supply welded EN 10217-7 1.4306 / X2CrNi19-11 against the delivery symbol and inspection package on your enquiry. We will not sell anonymous 304L (high-Ni) footage as Part 7, and we keep seamless EN 10216-5 and ASTM A269/A213/A312 off this MTC path.

Compare LINKPLACE1.4307, LINKPLACE1.4311, LINKPLACE1.4301 before freezing 1.4306. Caution: the high-Ni window costs more than LINKPLACE1.4307 for little chloride benefit — do not upgrade on habit; upgrade when the order or welding procedure actually needs it SHH STEEL will say no to a mismatched grade rather than force-fit X2CrNi19-11 into the wrong medium Linked sisters on this hub: EN 10217-7 1.4307, EN 10217-7 1.4311, EN 10217-7 1.4301. Live ASTM/ASME anchors: A269 TP304L, A213 TP304L.

Supply Capability

SHH STEEL’s supply offer on 1.4306 is welded Part 7 tube made and tested to your stated options. The tables that follow — including Stock / Available sizes — help buyers sketch OD × wall before a firm mill answer. Precision and mid-od welded tube where cold finishing after welding is common.

Item SHH STEEL capability for 1.4306
Standard EN 10217-7
Grade 1.4306 / X2CrNi19-11
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Available-size talk for 1.4306 follows mill strip/plate and finishing reality for X2CrNi19-11. Use the table to draft the enquiry; SHH STEEL confirms against current heats and slots — not against a static warehouse spreadsheet.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Ask for cut length, bevel, IGC, or sister numbers (1.4307, 1.4311, 1.4301) in the same RFQ. The size table is a starting grid under EN 10217-7 / EN ISO 1127. SHH STEEL can produce and supply 1.4306 when the finishing route is available.

FAQ

What is EN 10217-7 1.4306 welded stainless steel tube used for?
EN 10217-7 1.4306 (X2CrNi19-11) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is cryogenic and cold-service PED lines, deep-drawing-adjacent fabrications, and process utilities where the purchaser specifies the higher-Ni 1.4306 analysis. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4306 the same as 304L (high-Ni) under ASTM A269 or A312?
No. Commercial alias 304L (high-Ni) may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP304L, A213 TP304L.
Does EN 10217-7 1.4306 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4306. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4306?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 180 MPa, Rp1.0 min 215 MPa, Rm 460–680 MPa, and elongation 40% longitudinal / 35% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4306 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4306 when the enquiry names this steel number or the duty matches high-nickel low-carbon 18-8 austenitic welded pressure tube when ferrite control and forming behaviour matter more than the lower-Ni 1.4307 window. Compare EN 10217-7 1.4307, EN 10217-7 1.4311, EN 10217-7 1.4301 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: the high-Ni window costs more than 1.4307 for little chloride benefit — do not upgrade on habit; upgrade when the order or welding procedure actually needs it
What delivery conditions are available for EN 10217-7 1.4306?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4306?
SHH STEEL can produce and supply EN 10217-7 1.4306 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Precision and mid-od welded tube where cold finishing after welding is common.
TC1 or TC2 for EN 10217-7 1.4306?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4306?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4306.
What documents come with SHH STEEL EN 10217-7 1.4306?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4306, size, cast, and test category.
How do I enquire for EN 10217-7 1.4306 with SHH STEEL?
Send EN 10217-7, steel number 1.4306 / X2CrNi19-11, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4306 (X2CrNi19-11) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4306 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X