EN 10217-7 1.4550 Welded Stainless Steel Tube
What is EN 10217-7 1.4550 Welded Stainless Steel Tube
Steel name X6CrNiNb18-10 under steel number 1.4550 is the austenitic chemistry EN 10217-7 uses when a welded pressure-tube order must carry that analysis into the PED file. The product standard is EN 10217-7:2021 — welded stainless circular tubes for pressure and corrosion-resisting service at room, low, or elevated temperature. Writing only “347 welded tube” on a bill of materials leaves cast limits, weld route, delivery condition, and test category unspecified. Order EN 10217-7, 1.4550, TC1 or TC2, and the delivery-condition / options list so mill documentation matches the drawing. Role in practice: niobium-stabilised 18-8 austenitic welded pressure tube for as-welded corrosive and elevated-temperature PED duties parallel to the Ti-stabilised sister.
SHH STEEL can produce and supply EN 10217-7 1.4550 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover process welded tube bands with descaled or bright-annealed delivery symbols. Browse the series hub at EN 10217-7.
1.4550 is the welded EN pressure twin of commercial 347 thinking — order the steel number, not only the shop alias, when TC1/TC2 and leak-tightness must sit on the certificate. Typical welded pressure duties include process heaters, exhaust gas lines, and chemical transfer where Nb stabilisation is named on the material list. Design caution: Nb stabilisation is not a chloride upgrade; for Mo-bearing stabilised duty look at 1.4571 rather than forcing 1.4550 into a brine Commercially the grade is often called 347; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4550 / X6CrNiNb18-10 on the MTC. Sister numbers on this hub include EN 10217-7 1.4541, EN 10217-7 1.4301, EN 10217-7 1.4571.4541, 1.4301, 1.4571.
Remember the product-form split: this page is welded EN 10217-7 1.4550; seamless pressure stainless in the same chemistry idea belongs under EN 10216-5. Dimension preference is EN ISO 1127. Manufacturing routes stay longitudinal arc or laser per Table 1 — helical seam is outside the listed Part 7 paths used for this series. Live seamless sister: EN 10216-5 1.4550. Related live ASTM/ASME anchors: A269 TP347, A213 TP347.
Chemical Composition of EN 10217-7 1.4550
Cast chemistry for 1.4550 / X6CrNiNb18-10 is the acceptance gate on every EN 10217-7 heat. Option 6 opens product analysis with the standard’s deviation table. SHH STEEL prints the measured cast figures on the inspection document and will not market private melt windows as EN 10217-7 limits for this austenitic grade.
Public BSSA EN 10217-7 chemistry for 1.4550 / X6CrNiNb18-10 is tabulated below after cross-check to the 2021 framing. Figures are maxima unless shown as ranges. Always reconcile secondary datasheets to the purchased Part 7 edition.
| Element | 1.4550 cast analysis (mass %) |
|---|---|
| Carbon (C) | ≤0.08 |
| Silicon (Si) | ≤1.00 |
| Manganese (Mn) | ≤2.00 |
| Phosphorus (P) | ≤0.045 |
| Sulfur (S) | ≤0.015 |
| Chromium (Cr) | 17.0–19.0 |
| Nickel (Ni) | 9.0–12.0 |
| Niobium (Nb) | 10×C to 1.00 |
Reference for X6CrNiNb18-10: public BSSA EN 10217-7 chemical compositions article, cross-checked to the 2021 grade list framing. Unlisted elements are not intentional additions without agreement, aside from finishing additions under scrap discipline that protects 1.4550 properties.
Mechanical Properties of EN 10217-7 1.4550
Solution-annealed (+AT) ambient data for steel number 1.4550 (X6CrNiNb18-10) are taken from the EN 10217-7 austenitic table that characterises walls up to roughly 60 mm unless the order agrees values beyond that band. Both Rp0.2 and Rp1.0 appear for austenitics. Sub-zero impact figures at −196 °C are characterisation data until Options make them certified.
The ambient numbers for X6CrNiNb18-10 are taken from BSSA’s BS EN 10217-7 mechanical article (2021 framing). Solution annealing temperatures are public EN cross-checks and stay UNCERTAIN versus paid Part 7 footnotes. SHH STEEL keeps 1.4550 tensile acceptance on the EN 10217-7 table — foreign standard floors are not mixed onto the MTC.
| Property | 1.4550 ambient (solution annealed +AT) |
|---|---|
| Rp0.2 min (MPa) | 205 |
| Rp1.0 min (MPa) | 240 |
| Rm (MPa) | 510–740 |
| A min % long / trans | 35 / 30 |
| IGC resistance (delivery) | Yes (method A) |
| Solution annealing (public EN band) | 1020–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges |
| Cooling | water or air |
| Charpy sub-zero (transverse min J) | 60 at -196 °C (Option to verify) |
Reference trail for X6CrNiNb18-10: BSSA EN 10217-7 ambient mechanical article; public EN solution bands with UNCERTAIN vs paid Part 7 footnotes. Charpy values are characterisation data — verify by Option when joules must appear on the 1.4550 MTC.
Welded Tube Manufacture for EN 10217-7 1.4550
Manufacture of EN 10217-7 1.4550 (X6CrNiNb18-10) is longitudinal welded only: automatic arc or laser along the abutting edges of formed strip or plate. Public Table 1 sets the allowed weld-preparation and bead-work combinations; continuous forming from strip is the everyday path, while single forming from plate handles the heavier end of the band. The finished product must not include welds used only to join strip lengths prior to forming. Helical seam manufacture is outside the listed routes for this series. If the drawing demands seamless tube, change the standard to EN 10216-5.
Niobium-stabilised austenitic 1.4550 (X6CrNiNb18-10) follows the same Table 1 longitudinal arc/laser routes as other austenitics, with Options 3/4 available for ID weld dressing. Table 2 delivery symbols carry surface and heat-treatment path; Option 5 freezes the choice. Nb stabilisation supports as-welded corrosive and elevated temperature stories, but the ordered delivery-condition heat treatment still applies. SHH STEEL can produce and supply 1.4550 on descaled and cold-finished routes when the symbol is named. Shop practice: Nb-bearing or 347-class fillers; keep procedures aligned with the stabilised base metal
Part 7 forces an explicit TC1 or TC2 decision on 1.4550. That decision changes how hard the seam is interrogated and how tensile units are drawn; it does not waive leak-tightness. Option 15 can freeze the leak-test method. SHH STEEL reports the real weld manufacture path and delivery symbol for each X6CrNiNb18-10 lot.
Dimensions and Tolerances for EN 10217-7 1.4550
Dimensional ordering for 1.4550 / X6CrNiNb18-10 is OD × wall under EN ISO 1127 preferences. Stainless density, not carbon-steel 7.85, drives mass. EN 10217-7 tolerance classes apply, with Option 20 available for D4. Ovality stays within diameter tolerance; eccentricity within wall tolerance; abutting-edge radial offset at the longitudinal weld is capped by the standard’s dimensional clauses.
Option 19 covers exact lengths; Option 18 covers bevels when wall is at least 3.2 mm. For precision OD on 1.4550, WCA/WCR cold-finished delivery is often the first finish talk after descaled W1A/W2A. SHH STEEL freezes size, tolerance class, and Table 2 symbol against the order before the weld line is scheduled.
| Route / condition | Typical use | Notes |
|---|---|---|
| W1 / W1A / W1R | Hot-rolled starting flat product | Descaled or bright-annealed per symbol |
| W2 / W2A / W2R | Cold-rolled starting flat product | Smoother OD than W1 family except at weld |
| WCA / WCR | Cold finished ≥20% after weld | Recrystallized weld metal; OD often ≤168.3 mm |
| WG / WP | Ground / polished | Agree ID/OD scope and grit at enquiry |
Dimensional conformity on 1.4550 is checked against the ordered EN ISO 1127 / Part 7 class before release. Straightness and end condition for X6CrNiNb18-10 follow the standard’s clauses; SHH STEEL records measured OD × wall on the inspection document rather than assuming catalogue mid-tolerance. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4550 / X6CrNiNb18-10 on the inspection document rather than assuming mid-tolerance catalogue values.
Equivalent Grades for EN 10217-7 1.4550
The welded pressure-tube nameplate for this chemistry is EN 10217-7 1.4550 with steel name X6CrNiNb18-10. Commercial alias 347 may appear on ASTM/ASME tubing or pipe pages, but those standards are not automatic substitutes. Seamless EN 10216-5 is a sister product form, not a second way to accept a welded Part 7 seam.
Cross-standard shopping for 347 chemistry is common; acceptance is not. EN 10217-7 1.4550 remains the welded pressure-tube contract for X6CrNiNb18-10 on this page. Seamless sisters and ASTM/ASME pages are references until the order explicitly dual-certifies under each standard’s clauses.
| Reference | Designation | Note |
|---|---|---|
| EN 10217-7 | 1.4550 / X6CrNiNb18-10 | This product standard (welded pressure tube) |
| EN steel name | X6CrNiNb18-10 | EN 10027-1 designation used in body and marking |
| Commercial alias (body only) | 347 | Not a substitute for the steel number on the MTC |
| EN 10216-5 (seamless sister) | 1.4550 | Related live page — different product form (seamless) |
| A269 TP347 | A269 TP347 | Related live page — different product standard |
| A213 TP347 | A213 TP347 | Related live page — different product standard |
Inside this welded series, compare EN 10217-7 1.4541, EN 10217-7 1.4301, EN 10217-7 1.4571. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4550. Live cross-standard anchors: A269 TP347, A213 TP347.
Heat Treatment and Delivery Condition for EN 10217-7 1.4550
Delivery condition and heat treatment travel together on EN 10217-7 1.4550. Symbols such as W1A/W2A, WCA/WCR, and W1R/W2R imply the heat-treatment path; mechanical data assume solution-annealed (+AT) X6CrNiNb18-10. Uniform heating into the solution band and rapid cooling are the reference story. For X6CrNiNb18-10 under steel number 1.4550, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
Public solution-annealing guidance for X6CrNiNb18-10 sits at 1020–1120 °C with water or air cooling. Cross-check source is public EN 10216-5 / EN 10028-7 framing — labelled UNCERTAIN versus paid Part 7:2021 footnotes. Surface (pickle, bright anneal, grind, polish) rides on Option 5 / the chosen Table 2 symbol for 1.4550.
| Item | 1.4550 |
|---|---|
| Solution annealing band (public) | 1020–1120 °C (UNCERTAIN vs paid Part 7 footnote) |
| Cooling | water or air |
| Delivery condition symbols | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify) |
| Inspection document | EN 10204 3.1 default; 3.2 under Option 21 |
No 1.4550 length leaves SHH STEEL outside the ordered delivery-condition story. Certificates for X6CrNiNb18-10 list the Table 2 symbol, confirm heat treatment when the symbol demands it, and call out recrystallized-weld status on WCA/WCR product so goods-in inspectors are not left reading between the lines.
Corrosion Resistance of EN 10217-7 1.4550
Corrosion-resisting austenitic 1.4550 / X6CrNiNb18-10 is selected for welded pressure duty where the medium and temperature need niobium stabilisation protects against sensitisation in many as-welded aqueous and mildly oxidising services. EN 10217-7 marks intergranular-corrosion behaviour in the delivery condition against EN ISO 3651-2 methods in the mechanical tables; verification of IGC remains Option 13 even when the table says the grade resists IGC as delivered.
As-welded IGC risk on 1.4550 is managed by chemistry choice, heat input, and delivery condition — not by quoting a brochure PREN. Compare EN 10217-7 1.4541, EN 10217-7 1.4301, EN 10217-7 1.4571 for X6CrNiNb18-10 before accepting a borderline medium. Guideline sensitisation temperatures remain warnings inside long service times.
Applications of EN 10217-7 1.4550 Tube
EN 10217-7 1.4550 welded tube is used where PED-oriented pressure tubing must also resist corrosion and a longitudinal weld seam is accepted on the drawing. For X6CrNiNb18-10 the practical band is process heaters, exhaust gas lines, and chemical transfer where Nb stabilisation is named on the material list, supplied as welded tube in the ordered delivery condition with TC1 or TC2 testing.
It is the wrong first choice when a seamless product is mandatory (use EN 10216-5 — see EN 10216-5 1.4550), when the drawing is ASTM A269 instrumentation tubing or A312 pipe without an EN dual mark, or when the medium clearly needs a different family. SHH STEEL can produce and supply 1.4550 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit. Related live pages: A269 TP347, A213 TP347.
Weldability of EN 10217-7 1.4550
1.4550 / X6CrNiNb18-10 is welded both as a mill seam under EN 10217-7 manufacturing routes and later as a fabricator joint on the PED spool. Mill seams follow the qualified longitudinal arc or laser procedures for the ordered route; shop welds use processes and fillers chosen for the EN chemistry family. For this grade: Nb-bearing or 347-class fillers; keep procedures aligned with the stabilised base metal
Fabricator responsibility covers as-welded corrosion risk, duplex phase balance where relevant, and any PWHT the joint calculation demands on 1.4550. SHH STEEL supplies the mill product: ordered chemistry, seam route, heat treatment/delivery symbol, tensile floors, leak-tightness, and listed Options for X6CrNiNb18-10.
Surface Finishes for EN 10217-7 1.4550
Read the finish for steel number 1.4550 from the delivery symbol first. W1A/W2A descaled X6CrNiNb18-10 is the everyday pressure-tube look; W1R/W2R and WCR bright anneal serve buyers who need a cleaner outside diameter; WG/WP are written scopes, not implied catalogue grades. Packing instructions for this austenitic grade keep bare carbon steel off the tube. Free iron from foreign banding creates receiving NCRs that a PED spool does not have time to argue about on 347 material.
ID cleanliness beyond the Table 2 story — Ra caps, electropolish, solvent wipe — must be written on the 1.4550 purchase order. SHH STEEL can produce and supply descaled, bright-annealed, and polished routes for X6CrNiNb18-10 with measurable results, and refuses phantom surface grades that cannot be shown on the EN 10204 document for this 347 tube.
Finish upgrades on X6CrNiNb18-10 consume furnace and polishing capacity that descaled 1.4550 does not — schedule them explicitly. SHH STEEL confirms the Table 2 symbol against finishing slots and will say when a requested WP grit cannot be measured on the ordered OD × wall rather than shipping hopeful 347 tube.
Inspection and Testing for EN 10217-7 1.4550
Inspection on 1.4550 is specific, not statistical sampling theatre. One cast analysis per heat; tensile once per test unit under TC1 and twice from different tubes under TC2; technological tests per the D/T matrix; leak-tightness on every length (hydro or ET, Option 15 to choose); plus dimensions, visuals, and ID of X6CrNiNb18-10.
Under TC2 the longitudinal seam sees a tougher NDT package; laminar and edge Options appear for starting product. Order Option 13 when IGC must be tested; order impact Options when joules must appear on the certificate. SHH STEEL 3.1 documents for 1.4550 state chemistry, heat-treatment/delivery status, tensile, and leak/NDT — mandatory tests stay.
When TC2 is selected for 1.4550, plan NDT capacity on the longitudinal seam before promising a short mill date. SHH STEEL will not drop mandatory seam examination on X6CrNiNb18-10 to protect an aggressive schedule.
Packaging and Shipping for EN 10217-7 1.4550
Outbound packing for 1.4550 / X6CrNiNb18-10 welded pressure tube starts with protected ends, size segregation, and moisture barrier wrap on export loads. Stabilised 347 finishes that were bright-annealed or polished take sleeve wrap against galling; descaled utility lengths still travel on clean timber or plastic-lined supports. Bundle contact with carbon steel is forbidden in SHH STEEL packing instructions for this grade: rust blooms from foreign iron are visible defects on 347 OD and are treated as packing failures, not cosmetic footnotes.
Stencil content for 1.4550 normally shows maker, OD × wall, EN 10217-7, 1.4550 or X6CrNiNb18-10, cast, TC1/TC2, inspection mark, and correlation number. Delivery-condition letters appear when useful or when Option 5 made them contractual. SHH STEEL reconciles tags to the purchase-order marking clause before trucks leave.
Bundle IDs on the packing list point back to heats on the 1.4550 certificate. Exact-length and bevelled pieces are kept separate and end-protected. Packaging clauses in the PO are implemented before X6CrNiNb18-10 leaves the yard. SHH STEEL treats packing and marking for EN 10217-7 1.4550 / X6CrNiNb18-10 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Why Choose SHH STEEL
SHH STEEL can produce and supply X6CrNiNb18-10 under EN 10217-7 1.4550 with the heat treatment, TC1/TC2 tests, and EN 10204 3.1 paperwork the order names — not a relabelled 347 remnant. Part 7 stays separate from seamless Part 5 and from ASTM tubing/pipe standards on the certificate; wrong-table tensile paste-ups are refused.
Practical selection beats wishful stamping. Sisters worth comparing: LINKPLACE1.4541, LINKPLACE1.4301, LINKPLACE1.4571. Caution on 1.4550: Nb stabilisation is not a chloride upgrade; for Mo-bearing stabilised duty look at LINKPLACE1.4571 rather than forcing 1.4550 into a brine We would rather redirect the enquiry than ship the wrong EN number Linked sisters on this hub: EN 10217-7 1.4541, EN 10217-7 1.4301, EN 10217-7 1.4571. Live ASTM/ASME anchors: A269 TP347, A213 TP347.
Supply Capability
Enquiry intake for 1.4550 / X6CrNiNb18-10: SHH STEEL can produce and make EN 10217-7 welded tube to the edition, TC1/TC2, delivery symbol, and options you name. Use the capability table and Stock / Available sizes map as a starting size conversation. Process welded tube bands with descaled or bright-annealed delivery symbols.
| Item | SHH STEEL capability for 1.4550 |
|---|---|
| Standard | EN 10217-7 |
| Grade | 1.4550 / X6CrNiNb18-10 |
| Product form | Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition |
| Delivery condition | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock) |
| Typical size band | ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement |
| Testing | TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options |
| Documents | EN 10204 3.1 (3.2 Option 21); third-party inspection on request |
Stock / Available sizes
Stock / Available sizes for 1.4550 is an enquiry map. Heats of X6CrNiNb18-10, forming/weld capacity, and finish route decide what can ship when. Provide OD × wall, test category, and delivery symbol rather than assuming shelf SKUs.
| OD (mm) | Typical walls (mm) | Notes |
|---|---|---|
| 12 / 14 / 16 / 19 / 21.3 / 25 | 1.0 / 1.5 / 2.0 / 2.5 | Instrument / hygienic; often WCA/WCR or W2R |
| 26.9 / 33.7 / 38 / 42.4 / 48.3 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Process and utility welded pressure tube |
| 60.3 / 76.1 / 88.9 / 114.3 | 2.0 / 3.0 / 4.0 / 5.0 / 6.0 | Utility and process; lock W1A/W2A vs WCA |
| 141.3 / 168.3 / 219.1 | 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 | Larger welded pressure tube; watch family wall ceiling |
Options 19/18/13 and dual quotes with 1.4541, 1.4301, 1.4571 are normal add-ons. Size bands were sense-checked against peer catalogues; contractual acceptance is still EN 10217-7 with EN ISO 1127. SHH STEEL can produce and supply 1.4550 when capacity matches the order.
FAQ
-
What is EN 10217-7 1.4550 welded stainless steel tube used for?
- EN 10217-7 1.4550 (X6CrNiNb18-10) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is process heaters, exhaust gas lines, and chemical transfer where Nb stabilisation is named on the material list. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
-
Is EN 10217-7 1.4550 the same as 347 under ASTM A269 or A312?
- No. Commercial alias 347 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP347, A213 TP347.
-
Does EN 10217-7 1.4550 include seamless tube?
- No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4550. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
-
What mechanical properties does EN 10217-7 require for 1.4550?
- In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm 510–740 MPa, and elongation 35% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
-
1.4550 vs sister grades — which EN 10217-7 number should I buy?
- Buy 1.4550 when the enquiry names this steel number or the duty matches niobium-stabilised 18-8 austenitic welded pressure tube for as-welded corrosive and elevated-temperature PED duties parallel to the Ti-stabilised sister. Compare EN 10217-7 1.4541, EN 10217-7 1.4301, EN 10217-7 1.4571 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: Nb stabilisation is not a chloride upgrade; for Mo-bearing stabilised duty look at 1.4571 rather than forcing 1.4550 into a brine
-
What delivery conditions are available for EN 10217-7 1.4550?
- Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
-
What size range can SHH STEEL supply for EN 10217-7 1.4550?
- SHH STEEL can produce and supply EN 10217-7 1.4550 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Process welded tube bands with descaled or bright-annealed delivery symbols.
-
TC1 or TC2 for EN 10217-7 1.4550?
- Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
-
Is the intergranular corrosion test mandatory for 1.4550?
- No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4550.
-
What documents come with SHH STEEL EN 10217-7 1.4550?
- EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4550, size, cast, and test category.
-
How do I enquire for EN 10217-7 1.4550 with SHH STEEL?
- Send EN 10217-7, steel number 1.4550 / X6CrNiNb18-10, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.
Conclusion
EN 10217-7 1.4550 (X6CrNiNb18-10) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4550 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.