EN 10217-7 1.4563 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4563 Welded Stainless Steel Tube

EN 10217-7 1.4563 / X1NiCrMoCu31-27-4 welded stainless pressure tube (Alloy 28 / N08028), austenitic, cast analysis per EN table, ambient Rp0.2 min 215 MPa, Rm 500–750, solution annealed 1070–1150 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4563 / X1NiCrMoCu31-27-4 (Alloy 28 / N08028 — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4563 Welded Stainless Steel Tube

Ordering welded pressure stainless under EN 10217-7 means choosing a steel number from the austenitic or duplex tables, a test category, and a delivery-condition path — not pasting a shop alias onto random mill stock. 1.4563 is the EN designation for X1NiCrMoCu31-27-4 (Alloy 28 / N08028 in commercial speech) in the austenitic family. Part 7 of EN 10217 defines the welded circular product for pressure plus corrosion-resisting service; the order text must carry EN 10217-7, 1.4563, TC1 or TC2, and options so the mill runs the right strip/plate route and inspection. Use case: high-alloy Ni-Cr-Mo-Cu austenitic (Alloy 28-type) welded pressure tube for reducing acids and severe chemical PED service.

SHH STEEL can produce and supply EN 10217-7 1.4563 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover specialty welded OD with longer lead times than commodity 1.4404. Browse the series hub at EN 10217-7.

When the process book says Alloy 28 / N08028 welded tube for pressure duty under EN rules, EN 10217-7 1.4563 is the steel number on the PO. Typical welded pressure duties include sulphuric and phosphoric acid lines, fertiliser and mining-chemical PED piping, and mixed-acid duties that outgrow 904L. Design caution: fabrication and filler selection are alloy-specific; do not weld with generic 316L procedures. PREN marketing numbers are not EN acceptance limits Commercially the grade is often called Alloy 28 / N08028; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4563 / X1NiCrMoCu31-27-4 on the MTC. Sister numbers on this hub include EN 10217-7 1.4539, EN 10217-7 1.4547, EN 10217-7 1.4529.4539, 1.4547, 1.4529.

Scope check before release: Part 7 = welded X1NiCrMoCu31-27-4 tube; Part 5 = seamless. Preferred OD × wall language follows EN ISO 1127. Listed manufacture is longitudinal automatic arc or laser welding — helical seam stays outside the public Table 1 routes referenced here. Live seamless sister: EN 10216-5 1.4563.

Chemical Composition of EN 10217-7 1.4563

EN 10217-7 requires the cast analysis of 1.4563 to meet X1NiCrMoCu31-27-4 limits in the austenitic listing. Product analysis is the Option 6 path. On the certificate SHH STEEL shows actual cast chemistry for this Alloy 28 / N08028 welded pressure grade — not a marketing typical.

Chemical limits for 1.4563 / X1NiCrMoCu31-27-4 come from the public BSSA EN 10217-7 article, cross-checked to the 2021 grade list. Unless a range is stated, treat values as maxima. Secondary catalogues are not the purchase contract.

Element 1.4563 cast analysis (mass %)
Carbon (C) ≤0.020
Silicon (Si) ≤0.70
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.030
Sulfur (S) ≤0.010
Nitrogen (N) ≤0.10
Chromium (Cr) 26.0–28.0
Nickel (Ni) 30.0–32.0
Molybdenum (Mo) 3.00–4.00
Copper (Cu) 0.70–1.50

The X1NiCrMoCu31-27-4 composition window shown for 1.4563 is taken from the BSSA EN 10217-7 chemistry article. Public standard cross-check applies. Unlisted elements stay off the intentional-addition list unless the purchaser agrees, with the usual finishing-addition / scrap exceptions for austenitic melts.

Mechanical Properties of EN 10217-7 1.4563

Mechanical floors for welded 1.4563 tube in X1NiCrMoCu31-27-4 are the EN 10217-7 austenitic ambient (+AT) figures for walls inside the public characterisation window (about 60 mm unless Options say otherwise). Rp0.2, Rp1.0, Rm, and elongation are the everyday acceptance set; cryogenic impact stays optional until selected.

Ambient mechanical values shown for X1NiCrMoCu31-27-4 track BSSA BS EN 10217-7 (2021 framing). Public EN solution-annealing ranges are used with an UNCERTAIN tag relative to paid EN 10217-7 footnotes. Acceptance for steel number 1.4563 stays on the Part 7 table SHH STEEL cites — not on a borrowed sister datasheet.

Property 1.4563 ambient (solution annealed +AT)
Rp0.2 min (MPa) 215
Rp1.0 min (MPa) 245
Rm (MPa) 500–750
A min % long / trans 40 / 35
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1070–1150 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 60 at -196 °C (Option to verify)

Public sources for the X1NiCrMoCu31-27-4 ambient table: BSSA EN 10217-7 mechanical article; annealing windows from public EN stainless documents (UNCERTAIN vs paid 2021 Part 7). Select impact Options on 1.4563 when certified joules are mandatory.

Welded Tube Manufacture for EN 10217-7 1.4563

Building 1.4563 under EN 10217-7 means committing to a welded circular tube: longitudinal automatic arc or laser weld from X1NiCrMoCu31-27-4 strip or plate, following Table 1. As-welded, outside-ground, and bead-worked-before-heat-treatment variants are the listed paths; spiral seam is not among them in the public text used for this series. Continuous strip forming and plate forming cover the size map. SHH STEEL will not treat a helical-weld drawing as automatic Part 7 acceptance. Seamless pressure tube belongs on the EN 10216-5 sister conversation.

High-alloy austenitic 1.4563 (X1NiCrMoCu31-27-4) is welded longitudinally under Table 1 with procedures that respect the Mo-Cu (and nitrogen where present) balance — heat input and cleanliness matter more than on commodity 18-8. Options 3/4 dress the ID weld when required; Table 2 symbols set surface/heat-treatment path with Option 5 to lock. SHH STEEL can produce and supply 1.4563 as heat-treated descaled or cold-finished product when strip chemistry and weld slots align. Filler guidance for this page: matching Alloy 28-type fillers; strict heat-input and cleanliness controls; often Option 13 corrosion tests

Call TC1 or TC2 when releasing 1.4563 to production. Marking will carry it; weld-seam NDT and tensile sampling follow it; leak-tightness still hits every tube with Option 15 available. SHH STEEL documents the executed weld route and delivery-condition symbol for X1NiCrMoCu31-27-4.

Dimensions and Tolerances for EN 10217-7 1.4563

EN 10217-7 1.4563 is sized by D × T. Start from EN ISO 1127 preferred sizes for X1NiCrMoCu31-27-4; apply stainless density for mass. Tolerance classes follow the Part 7 framework — Option 20 selects D4 when instrumentation fit-up needs it. Out-of-roundness, eccentricity, and weld-edge radial offset rules in the dimensional clauses still apply.

Options 19 (exact length) and 18 (bevel, wall ≥ 3.2 mm) sit on top of the D × T order for 1.4563. Cold-finished WCA/WCR is the common upgrade path when OD tolerance and weld recrystallization matter. SHH STEEL confirms those choices with the delivery symbol before production release.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

SHH STEEL’s dimensional report on 1.4563 / X1NiCrMoCu31-27-4 cites the ordered tolerance class, not a generic “per EN” line. Straightness and end-finish checks remain part of release under EN 10217-7 dimensional clauses. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4563 / X1NiCrMoCu31-27-4 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4563

EN 10217-7 identifies this welded product as 1.4563 / X1NiCrMoCu31-27-4. Keep Alloy 28 / N08028 in body text and enquiry notes, not as the sole MTC identity. ASTM/ASME standards that share the alias differ in scope; EN 10216-5 is seamless, not an alternate welded acceptance path.

Cross-standard shopping for Alloy 28 / N08028 chemistry is common; acceptance is not. EN 10217-7 1.4563 remains the welded pressure-tube contract for X1NiCrMoCu31-27-4 on this page. Seamless sisters and ASTM/ASME pages are references until the order explicitly dual-certifies under each standard’s clauses.

Reference Designation Note
EN 10217-7 1.4563 / X1NiCrMoCu31-27-4 This product standard (welded pressure tube)
EN steel name X1NiCrMoCu31-27-4 EN 10027-1 designation used in body and marking
Commercial alias (body only) Alloy 28 / N08028 Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4563 Related live page — different product form (seamless)

Inside this welded series, compare EN 10217-7 1.4539, EN 10217-7 1.4547, EN 10217-7 1.4529. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4563.

Heat Treatment and Delivery Condition for EN 10217-7 1.4563

EN 10217-7 1.4563 is supplied to a Table 2 delivery condition. Where that symbol requires heat treatment, solution annealing (+AT) is the reference path behind the X1NiCrMoCu31-27-4 ambient properties: soak in the solution band, cool rapidly, and document what was done. For X1NiCrMoCu31-27-4 under steel number 1.4563, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

X1NiCrMoCu31-27-4 solution annealing on public tables: 1070–1150 °C, cooled by water or air. Treat as UNCERTAIN relative to paid EN 10217-7:2021 footnotes. Delivery-condition symbol (Option 5) then selects the surface path for 1.4563. For X1NiCrMoCu31-27-4 under steel number 1.4563, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Item 1.4563
Solution annealing band (public) 1070–1150 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

Ordered heat treatment on X1NiCrMoCu31-27-4 is verified before dispatch. SHH STEEL’s paperwork for EN 10217-7 1.4563 ties ambient tensile results to the Table 2 delivery symbol and notes weld-seam treatment on cold-finished product, so the certificate matches the tube that arrives. For X1NiCrMoCu31-27-4 under steel number 1.4563, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Corrosion Resistance of EN 10217-7 1.4563

Choose 1.4563 (X1NiCrMoCu31-27-4) when welded PED tubing must carry this corrosion story: high Ni-Cr-Mo-Cu balance for reducing and oxidising acid mixtures; strong general corrosion resistance in many strong-acid media. Delivery-condition IGC resistance is characterised to EN ISO 3651-2 methods in the Part 7 tables, but a tested IGC result still requires Option 13 on the order.

Final corrosion discipline for EN 10217-7 1.4563: order the steel number that matches the medium, use Option 13 when tested IGC is mandatory for X1NiCrMoCu31-27-4, and treat guideline sensitisation temperatures as warnings — never as PREN/CPT acceptance floors. Sisters on this hub: EN 10217-7 1.4539, EN 10217-7 1.4547, EN 10217-7 1.4529.

Applications of EN 10217-7 1.4563 Tube

Applications for steel number 1.4563 / X1NiCrMoCu31-27-4 cluster around welded PED service that tolerates a mill seam: sulphuric and phosphoric acid lines, fertiliser and mining-chemical PED piping, and mixed-acid duties that outgrow 904L. Delivery condition and test category on the order decide how that tube is finished and inspected before it reaches the spool.

Skip 1.4563 when the specification locks seamless product (EN 10216-5 — see EN 10216-5 1.4563), when ASTM A269/A312 text is the only acceptance language, or when corrosion/strength clearly points at another family. SHH STEEL can produce and supply X1NiCrMoCu31-27-4 welded tube in the enquiry band and will redirect to a sister or live ASTM/ASME page when that is wiser.

Weldability of EN 10217-7 1.4563

Mill welding of EN 10217-7 1.4563 is the longitudinal arc/laser seam on the ordered Table 1 route; field or shop welding is a separate PED joint design. Filler and procedure choices track the austenitic chemistry of X1NiCrMoCu31-27-4. Practical note: matching Alloy 28-type fillers; strict heat-input and cleanliness controls; often Option 13 corrosion tests

Once X1NiCrMoCu31-27-4 tube leaves the mill as EN 10217-7 1.4563, spool welding is a separate engineering act. SHH STEEL does not own the fabricator’s as-welded corrosion or PWHT choices; we own the mill certificate package — chemistry, seam route, heat treatment symbol, tensile, and leak/NDT.

Surface Finishes for EN 10217-7 1.4563

Ordered surface on EN 10217-7 1.4563 / X1NiCrMoCu31-27-4 follows the delivery-condition letter the purchaser locks (Option 5) or the manufacturer selects. Pickle/descaled suits lagged utility; bright anneal suits cleaner OD; grind/polish needs grit or Ra on the PO. Protect Alloy 28 / N08028 from carbon-steel contact in every pack design so free-iron transfer never becomes a site cleanup project after ocean freight.

Electropolish and ID Ra belong in the PO alongside steel number 1.4563. SHH STEEL can produce and supply the common descaled and bright-annealed routes for X1NiCrMoCu31-27-4, plus polished OD when grit is agreed and checked — no catalogue fiction, no unverified “mirror” claims for Alloy 28 / N08028.

Buyers sometimes request “same as last Alloy 28 / N08028 lot” without a symbol. For 1.4563 / X1NiCrMoCu31-27-4, SHH STEEL restates the Table 2 finish on the order acknowledgement so there is no silent drift between descaled utility and bright-annealed instrumentation product across releases.

Inspection and Testing for EN 10217-7 1.4563

TC1/TC2 define tensile intensity on 1.4563, but leak-tightness is per tube either way. Cast analysis, technological tests, dimensions, visuals, and material ID complete the baseline for X1NiCrMoCu31-27-4. Option 15 selects the leak-test method when the purchaser refuses manufacturer choice. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4563 purchase order so X1NiCrMoCu31-27-4 inspection planning matches the PED file before weld slots are locked.

Weld-seam NDT intensity and optional laminar/edge tests rise with TC2 for X1NiCrMoCu31-27-4. IGC (Option 13) and Charpy Options remain opt-in. SHH STEEL reports the ordered package on EN 10204 3.1 for 1.4563 and keeps mandatory Part 7 tests on the schedule. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4563 purchase order so X1NiCrMoCu31-27-4 inspection planning matches the PED file before weld slots are locked.

Final inspection release for 1.4563 is a signed package: chemistry, delivery condition, tensile, leak/NDT, dimensions, marking. SHH STEEL will not ship X1NiCrMoCu31-27-4 on a partial document set to meet an artificial packing date.

Packaging and Shipping for EN 10217-7 1.4563

When 1.4563 (X1NiCrMoCu31-27-4) leaves the mill as EN 10217-7 welded tube, packing protects both the weld-seam region and the ordered surface condition. End protection, sorted bundles or crates, and ocean-freight wrap are baseline. High-alloy Alloy 28 / N08028 bright-annealed or polished OD is sleeved against transit galling; descaled chemical-service tube still ships on non-contaminating supports with capped ends. Carbon-steel banding against stainless is not used — free-iron staining on Alloy 28 / N08028 tube is a packing defect SHH STEEL designs out before dispatch.

Goods-in should read EN 10217-7, 1.4563, dimensions, cast, and test category without decoding gymnastics. Delivery condition may be marked; it is required in spirit when Option 5 applied. SHH STEEL sets stencil and tags for X1NiCrMoCu31-27-4 before the pack line closes. SHH STEEL treats packing and marking for EN 10217-7 1.4563 / X1NiCrMoCu31-27-4 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Traceable packing lists link X1NiCrMoCu31-27-4 heats to physical bundles. Option 19/18 pieces get their own capped packs. Dispatch waits until packing and marking match the 1.4563 purchase order. SHH STEEL treats packing and marking for EN 10217-7 1.4563 / X1NiCrMoCu31-27-4 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and supply welded EN 10217-7 1.4563 / X1NiCrMoCu31-27-4 against the delivery symbol and inspection package on your enquiry. We will not sell anonymous Alloy 28 / N08028 footage as Part 7, and we keep seamless EN 10216-5 and ASTM A269/A213/A312 off this MTC path.

Compare LINKPLACE1.4539, LINKPLACE1.4547, LINKPLACE1.4529 before freezing 1.4563. Caution: fabrication and filler selection are alloy-specific; do not weld with generic 316L procedures. PREN marketing numbers are not EN acceptance limits SHH STEEL will say no to a mismatched grade rather than force-fit X1NiCrMoCu31-27-4 into the wrong medium Linked sisters on this hub: EN 10217-7 1.4539, EN 10217-7 1.4547, EN 10217-7 1.4529.

Supply Capability

SHH STEEL’s supply offer on 1.4563 is welded Part 7 tube made and tested to your stated options. The tables that follow — including Stock / Available sizes — help buyers sketch OD × wall before a firm mill answer. Specialty welded od with longer lead times than commodity 1.4404.

Item SHH STEEL capability for 1.4563
Standard EN 10217-7
Grade 1.4563 / X1NiCrMoCu31-27-4
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Available-size talk for 1.4563 follows mill strip/plate and finishing reality for X1NiCrMoCu31-27-4. Use the table to draft the enquiry; SHH STEEL confirms against current heats and slots — not against a static warehouse spreadsheet.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Ask for cut length, bevel, IGC, or sister numbers (1.4539, 1.4547, 1.4529) in the same RFQ. The size table is a starting grid under EN 10217-7 / EN ISO 1127. SHH STEEL can produce and supply 1.4563 when the finishing route is available.

FAQ

What is EN 10217-7 1.4563 welded stainless steel tube used for?
EN 10217-7 1.4563 (X1NiCrMoCu31-27-4) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is sulphuric and phosphoric acid lines, fertiliser and mining-chemical PED piping, and mixed-acid duties that outgrow 904L. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4563 the same as Alloy 28 / N08028 under ASTM A269 or A312?
No. Commercial alias Alloy 28 / N08028 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing.
Does EN 10217-7 1.4563 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4563. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4563?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 215 MPa, Rp1.0 min 245 MPa, Rm 500–750 MPa, and elongation 40% longitudinal / 35% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4563 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4563 when the enquiry names this steel number or the duty matches high-alloy Ni-Cr-Mo-Cu austenitic (Alloy 28-type) welded pressure tube for reducing acids and severe chemical PED service. Compare EN 10217-7 1.4539, EN 10217-7 1.4547, EN 10217-7 1.4529 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: fabrication and filler selection are alloy-specific; do not weld with generic 316L procedures. PREN marketing numbers are not EN acceptance limits
What delivery conditions are available for EN 10217-7 1.4563?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4563?
SHH STEEL can produce and supply EN 10217-7 1.4563 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Specialty welded od with longer lead times than commodity 1.4404.
TC1 or TC2 for EN 10217-7 1.4563?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4563?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4563.
What documents come with SHH STEEL EN 10217-7 1.4563?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4563, size, cast, and test category.
How do I enquire for EN 10217-7 1.4563 with SHH STEEL?
Send EN 10217-7, steel number 1.4563 / X1NiCrMoCu31-27-4, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4563 (X1NiCrMoCu31-27-4) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4563 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X