EN 10028-2 12CrMoV12-10 Steel Plate | 12CrMoV12-10 3Cr-1Mo-V Vessel Plate
What is EN 10028-2 12CrMoV12-10 Steel?
12CrMoV12-10 is the 3Cr-1Mo-V grade in EN 10028-2. Buyers search EN 10028-2 12CrMoV12-10, 12CrMoV12-10 steel plate, 1.7767, 12CrMoV12-10 equivalent and 12CrMoV12-10 3Cr-1Mo-V vessel plate. Steel number is 1.7767. Chromium is about 2.70–3.30%. Molybdenum is about 0.90–1.20%. Vanadium is about 0.25–0.35%. That vanadium is why this page is not 10CrMo9-10 and not 11CrMo9-10.
Yield is in the 400 MPa class at ≤16 mm. Tensile is 580–760 MPa. Delivery is usually normalized and tempered (+NT). Some mill routes use quench and temper when thickness or the order requires it. Write the route. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplying this grade to the USA, Europe, Middle East, Southeast Asia, Africa and South America.
Do not ship 10CrMo9-10 against a 12CrMoV12-10 drawing. 10CrMo9-10 is 2.25Cr-1Mo without this vanadium band. Do not ship 13CrMo4-5 and call 1.25Cr close to 3Cr. The closest ASME talk grades are SA387 Grade 21 Class 2 and SA832 Grade 21V. SA387 Grade 21 Class 1 is the lower class in that 3Cr family. Dual marking is possible only when chemistry, tensile, hardness, impact and delivery all fit.
Company scope: global exporter SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | EN 10028-2 12CrMoV12-10 | Confirmed |
| Steel number | 1.7767 | Confirmed |
| Product specification | EN 10028-2 + EN 10028-1 | Applied |
| Steel type | Alloy special steel, 3Cr-1Mo-V | Confirmed |
| Usual delivery | +NT, QT by agreement | Confirmed |
| Yield idea | 400 MPa class at ≤16 mm | Confirmed |
| Tensile | 580–760 MPa | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | USA, Europe, Middle East, SE Asia, Africa, South America | As ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. Cr-Mo comparisons belong on ASME SA387. Cr-Mo-V vessel comparisons belong on ASME SA832 and ASME SA542.
Chemical Composition
Cast analysis follows EN 10028-2 Table 1. Product analysis follows EN 10028-1 when ordered. People who type 12CrMoV12-10 chemical composition or 1.7767 chemistry into Google want chromium near 3%, molybdenum near 1% and vanadium on the same line. A 10CrMo9-10 table does not answer that.
Cast Analysis and Product Analysis — EN 10028-2 12CrMoV12-10 (1.7767)
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C) | 0.10 – 0.15 | 0.08 – 0.17 |
| Silicon (Si), max | 0.30 | 0.35 |
| Manganese (Mn) | 0.30 – 0.80 | 0.25 – 0.88 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.013 |
| Nitrogen (N), max | 0.012 | 0.014 |
| Chromium (Cr) | 2.70 – 3.30 | 2.60 – 3.40 |
| Copper (Cu), max | 0.30 | 0.35 |
| Molybdenum (Mo) | 0.90 – 1.20 | 0.85 – 1.25 |
| Nickel (Ni), max | 0.30 | 0.35 |
| Vanadium (V) | 0.25 – 0.35 | 0.22 – 0.38 |
Vanadium is not an optional extra. It is the letter in the grade name. Chromium at 2.70–3.30% is the 3Cr step above 10CrMo9-10. Molybdenum stays near 1%. This is not P91 9Cr plate and not 1.25Cr-0.5Mo plate. SHH STEEL reports cast analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search 12CrMoV12-10 mechanical properties, 12CrMoV12-10 yield strength and 12CrMoV12-10 tensile strength. Room-temperature values fall with thickness. Use the thickness column on the mill certificate.
Tensile and Yield — EN 10028-2 12CrMoV12-10
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| ≤ 16 | 400 | 580 – 760 |
| 16 – 40 | 390 | 580 – 760 |
| 40 – 60 | 380 | 570 – 750 |
| 60 – 100 | 360 | 560 – 740 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is typically 18% min on thinner plate. Impact at 0 °C, 27 J, is the usual option when the order names it. Some files ask hardness after heat treatment because vanadium-bearing Cr-Mo can run hard if tempering is short. Write hardness if the vessel specification uses it. Elevated-temperature proof strength is part of EN 10028-2. Ask for that table when the calculation uses design temperature.
Do not quote 400 MPa yield on an 80 mm plate. Do not treat 580–760 MPa tensile as permission to stamp SA387 Grade 21 Class 2 without checking vanadium, class and PWHT.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| EN 10028-2 13CrMo4-5 | EN 10028-2 | 13CrMo4-5 steel plate | No |
| EN 10028-2 10CrMo9-10 | EN 10028-2 | 10CrMo9-10 steel plate | No |
| EN 10028-2 11CrMo9-10 | EN 10028-2 | 11CrMo9-10 steel plate | No |
| EN 10028-2 12CrMoV12-10 | EN 10028-2 | 12CrMoV12-10 steel plate | This page |
| EN 10028-2 X10CrMoVNb9-1 | EN 10028-2 | P91 steel plate | No |
| SA387 Grade 21 Class 2 | SA-387 | SA387 Gr.21 Cl.2 | No auto swap |
| SA387 Grade 22 Class 2 | SA-387 | SA387 Gr.22 Cl.2 | No |
| SA832 Grade 21V | SA-832 | SA832 21V | No auto swap |
| 12Cr2Mo1VR steel plate | GB/T 713.2 | 12Cr2Mo1VR | No |
| Q345R steel plate | GB/T 713.2 | Q345R | No |
Equivalent Material Grades
People type 12CrMoV12-10 equivalent, 1.7767 equivalent and 12CrMoV12-10 vs SA387 Grade 21 because there is no one-line twin. Give the talk list. Keep the EN name on the order.
| Designation | Standard / region | Notes |
|---|---|---|
| EN 10028-2 12CrMoV12-10 / 1.7767 | EN 10028-2 | Name on this page |
| 10CrMo9-10 / 1.7380 | EN 10028-2 | 2.25Cr-1Mo, no this V band |
| SA387 Grade 21 Class 1 | SA-387 | 3Cr-1Mo Class 1 |
| SA387 Grade 21 Class 2 | SA-387 | 3Cr-1Mo Class 2 |
| SA387 Grade 21L Class 1 | SA-387 | Lower carbon 3Cr |
| SA832 Grade 21V | SA-832 | Cr-Mo-V vessel |
| SA832 Grade 22V | SA-832 | 2.25Cr-1Mo-V |
| SA542 Type C Class 4 | SA-542 | QT Cr-Mo-V |
| 12Cr1MoVR steel plate | GB/T 713.2 | Chinese Cr-Mo-V |
| SA516 Grade 70 | SA-516 | Carbon |
3Cr-1Mo-V Pressure-Vessel Service
Buyers pick 12CrMoV12-10 when the PED file wants 3% chromium, about 1% molybdenum and vanadium together. That combination is used on high-temperature pressure equipment that has already left 2.25Cr-1Mo behind and has not jumped to 9Cr P91. Search phrases such as 12CrMoV12-10 boiler plate, 1.7767 steel plate and 12CrMoV12-10 pressure vessel plate all point here.
Do not ship SA387 Grade 22 Class 2 against 12CrMoV12-10. Grade 22 is 2.25Cr-1Mo. Do not ship SA387 Grade 91 Class 2. That grade is 9Cr-1Mo-V-Nb. An ASME file that wants 3Cr-1Mo should name SA-387 Grade 21 on ASME SA387 and then write class and vanadium extras. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. The purchase is not limited to China, Hong Kong or Singapore.
Weldability
12CrMoV12-10 is 3Cr-1Mo-V vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.
Qualify to the applicable code. ASME dual-name work uses ASME Section IX. Consumables must match 3Cr-1Mo-V practice. A carbon procedure written for SA516 Grade 70 is not valid. A 2.25Cr-1Mo procedure written for SA387 Grade 22 Class 2 is the previous family, not this one. A P91 procedure written for SA387 Grade 91 Class 2 is the next family. Preheat, interpass, hydrogen control and PWHT window all belong in the WPS. Vanadium-bearing weld metal does not like a copied Grade 22 temper. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized and tempered EN 10028-2 12CrMoV12-10 (+NT). Quench and temper is used when the mill route and the order require it. Buyers who search 12CrMoV12-10 heat treatment, 12CrMoV12-10 PWHT or 12CrMoV12-10 NT are asking for this control.
If the vessel will see PWHT, write the temperature window. Test coupons then follow a simulated cycle. Hardness after simulated PWHT is worth naming on vanadium-bearing plate. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists EN 10028-2 12CrMoV12-10; 1.7767; heat number; cast analysis including chromium, molybdenum and vanadium; product analysis when ordered; tensile to the correct thickness column; +NT or QT; hardness when ordered; impact when ordered; elevated-temperature values when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for 12CrMoV12-10 3Cr-1Mo-V vessel plate:
- Thickness: commonly 8 mm – 120 mm, thicker by mill agreement
- Width: 1500 mm – 3500 mm
- Length: 3000 mm – 12000 mm
2.25Cr-1Mo plate belongs on 12Cr2Mo1R steel plate. 1Cr-0.5Mo plate belongs on 15CrMoR steel plate. Carbon vessel plate belongs on Q345R steel plate.
Tolerances
Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another tolerance table. Do not apply ASTM A36 structural tolerances to a PED 3Cr-1Mo-V vessel plate without writing them.
Supplementary Requirements
Charpy details. Temperature, energy, location and orientation. Do not assume 0 °C.
Hardness. After heat treatment and after simulated PWHT when written.
Product analysis. Add this when the destination file wants finished-plate chemistry, especially V, Cr and Mo.
Elevated-temperature proof strength. Add this when the calculation uses design temperature.
Simulated PWHT. Almost always relevant on this grade.
NDE. EN 10160 or the named UT class.
Third-party. EN 10204 3.2 when written.
Applications
| Industry | Typical components |
|---|---|
| PED high-temp boilers | EN 10028-2 12CrMoV12-10 shells |
| 3Cr-1Mo-V heat exchangers | 12CrMoV12-10 channels |
| Alloy high-temp vessels | 12CrMoV12-10 plate from SHH STEEL |
| Dual-certified export | 12CrMoV12-10 / SA387 Grade 21 Class 2 when both books fit |
Supply Capability
SHH STEEL sources EN 10028-2 12CrMoV12-10 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or heat-treatment route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness for this family: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, with thicker plate by mill agreement. Width and length follow the mill table above.
Processing available with the plate: CNC or flame cutting to drawing, bevel preparation, flattening, and ultrasonic testing to EN 10160 or the named class. Extra NDE is written on the order, not assumed.
Trade terms: FOB Shanghai is the usual main term. CIF to the buyer’s destination port can be quoted. Payment is TT, LC, or TT + LC, as agreed on the contract.
Destination ports and typical ocean time from Shanghai, subject to sailing and customs:
- US West Coast (Los Angeles / Long Beach / Oakland): about 14–18 days
- US Gulf (Houston / New Orleans): about 28–35 days
- Rotterdam / Antwerp: about 28–35 days
- Jebel Ali: about 18–25 days
- Singapore: about 7–12 days
- Other major ports in Mexico, South America, the Mediterranean, India, Africa, Japan and Korea: quoted case by case
Third-party inspection can be SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector the buyer names. The hold point is booked before rolling or before shipment, depending on the 3.2 scope.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin. The commercial offer is not limited to one region.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time:
- Ex-stock: about 5–7 days when 3Cr-1Mo-V plate is in yard
- Mill rolling, standard +NT: about 45 days
- Simulated PWHT, hardness, 3.2 or extra NDE: about 2 months
Company scope: worldwide delivery SHH STEEL.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). On EN 10028-2 12CrMoV12-10 that means mill pricing from Wuyang, Angang, Baosteel and other first-line mills, 1.7767 chemistry reported as cast analysis and as product analysis when ordered, vanadium shown on the certificate, recorded +NT or QT, tensile results to the correct thickness column, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. 12CrMoV12-10 is not 10CrMo9-10. 12CrMoV12-10 is not SA387 Grade 22 Class 2. 12CrMoV12-10 is not P91. 12CrMoV12-10 is not Q345R steel plate. If the drawing says Grade 22, we will not ship 3Cr-1Mo-V and call chromium close.
Company scope: global exporter SHH STEEL.
FAQ
- What is 12CrMoV12-10 steel plate?
- 12CrMoV12-10 is an EN 10028-2 3Cr-1Mo-V high-temperature pressure-vessel plate, steel number 1.7767. Yield is in the 400 MPa class at ≤16 mm and tensile is 580–760 MPa. Delivery is usually +NT. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
- What is the equivalent of 12CrMoV12-10?
- Related comparisons are SA-387 Grade 21 and SA-832 Grade 21V. There is no automatic substitute. Dual marking is possible only when both books are fully met.
- What is the difference between 12CrMoV12-10 and 10CrMo9-10?
- 10CrMo9-10 is 2.25Cr-1Mo. 12CrMoV12-10 is 3Cr-1Mo with 0.25–0.35% vanadium. Welding and PWHT are not copied from Grade 22 practice.
- What is the chemical composition of 12CrMoV12-10?
- ypical cast analysis is C 0.10–0.15, Cr 2.70–3.30, Mo 0.90–1.20 and V 0.25–0.35, with tight P and S. SHH STEEL prints heat analysis on every certificate and product analysis when ordered.
- Can 12CrMoV12-10 be welded?
- Yes, with a qualified 3Cr-1Mo-V procedure. Preheat, hydrogen control and a written PWHT window are part of production welding, not optional workshop habit.
- What PWHT is used for 12CrMoV12-10?
- Follow the vessel code and the WPS. Do not copy a Grade 22 or P91 cycle without review. SHH STEEL can run simulated PWHT on test coupons when the order names the cycle.
- Is 12CrMoV12-10 the same as SA387 Grade 21?
- They sit in the same 3Cr-1Mo family. SA-387 Grade 21 does not automatically carry the same vanadium band. Keep both names only when both books are met.
- Who supplies 12CrMoV12-10 steel plate for export?
- HH STEEL supplies 12CrMoV12-10 from first-line Chinese mills to the USA, Europe, Middle East, Southeast Asia, Africa and South America, with EN 10204 3.1 or 3.2.
- What is the lead time for 12CrMoV12-10?
- Ex-stock about 5–7 days when plate is in yard. Standard +NT mill rolling about 45 days. Simulated PWHT, hardness or 3.2 inspection about 2 months.
Conclusion
EN 10028-2 12CrMoV12-10 Steel Plate is European 3Cr-1Mo-V high-temperature pressure-vessel plate, steel number 1.7767, at the 400 MPa yield class and 580–760 MPa tensile at ≤16 mm, usually +NT. Whether the inquiry says EN 10028-2 12CrMoV12-10, 1.7767 or 12CrMoV12-10 3Cr-1Mo-V Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 12CrMoV12-10 chemistry, heat and product analysis when ordered, recorded heat treatment, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies EN 10028-2 12CrMoV12-10 3Cr-1Mo-V Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
EN 10028-2 12CrMoV12-10 Steel Plate, 12CrMoV12-10 3Cr-1Mo-V vessel plate, 1.7767, 12CrMoV12-10 supplier, global exporter SHH STEEL