ASTM A387 Grade 22 Class 2 / A387 Gr.22 Cl.2 is 2.25Cr-1Mo pressure-vessel plate. Tensile is 515–690 MPa and yield is 310 MPa min. SHH STEEL supplies A387GR22CL2 worldwide as a global steel mill sourcing partner. SEO Title
Keywords
ASTM A387 Grade 22 Class 2, A387 Gr.22 Cl.2, A387GR22CL2, A387GR22 CL2, SA387 Grade 22 Class 2, 2.25Cr-1Mo vessel plate, A387 Gr.22 Cl.2 supplier
Equivalent Grades:
EN 10028-2 10CrMo9-10 / JIS SCMV4 Cl2 / GB 12Cr2Mo1R — Material Specification: ASTM A387 / ASME SA-387 — Delivery: Normalized + Tempered (N+T); hydrogen-service workhorse, max ~75 mm
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
2.25Cr-1Mo Elevated-Temperature Service
Weldability
Heat Treatment and Delivery Conditio
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is ASTM A387 Grade 22 Class 2 Steel?

ASTM A387 Grade 22 Class 2, also searched as A387 Gr.22 Cl.2, A387GR22CL2, A387GR22 CL2, A387GR.22 Class 2, A387-22 Cl.2 and SA387 Grade 22 Class 2, is the higher-strength class of Grade 22 in ASTM A387/A387M. The book is chromium-molybdenum plate for welded boilers and elevated-temperature vessels. Nominal alloy is 2.25Cr-1.00Mo. This page is not Class 1. Class 1 is 415–585 MPa. This page is not ASME SA387 Grade 22L Class 1. Grade 22L is the low-carbon sister and Class 1 only. This page is not ASME SA387 Grade 11 Class 2. Grade 11 is 1.25Cr-0.5Mo. This page is not ASME SA542 Type B Class 2. SA-542 is quenched and tempered Cr-Mo.

Tensile is 75–100 ksi / 515–690 MPa. Yield is 45 ksi / 310 MPa min. Class 2 values are not used on annealed plate. Usual delivery is normalized and tempered, or accelerated cooling plus temper. Minimum temper for Grade 22 is 1250 °F / 675 °C. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against A387 / SA-387 and A20 / SA-20, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

If a drawing says A387 Gr.22 Cl.1, we will not ship Class 2 and call stronger automatically acceptable. For ASME Code work the name on the certificate should be SA-387 Grade 22 Class 2. Related category pages: ASTM A387 and ASME SA387.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade / class ASTM A387/A387M Grade 22 Class 2 Confirmed
Code counterpart ASME SA-387 Grade 22 Class 2 Available
Other search names A387 Gr.22 Cl.2, A387GR22CL2, A387GR22 CL2 Covered
Steel type Killed 2.25Cr-1Mo vessel plate Confirmed
Usual delivery N+T; not annealed Class 2 Confirmed
Tensile 515–690 MPa (75–100 ksi) Confirmed
Yield 310 MPa (45 ksi) min Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and ASTM A387. European 2.25Cr-1Mo sisters belong on EN 10028-2. Chinese 2.25Cr-1Mo sisters belong on GB/T 713.

Chemical Composition

Heat analysis and product analysis follow ASTM A387 Table 1 for Grade 22. Class 1 and Class 2 share the same chemistry.

Heat Analysis and Product Analysis — ASTM A387 Grade 22

Element Heat Analysis (%) Product Analysis (%)
Carbon (C) 0.05 – 0.15 0.04 – 0.15
Manganese (Mn) 0.30 – 0.60 0.25 – 0.66
Phosphorus (P), max 0.025 0.025
Sulfur (S), max 0.025 0.025
Silicon (Si), max 0.50 0.50
Chromium (Cr) 2.00 – 2.50 1.88 – 2.62
Molybdenum (Mo) 0.90 – 1.10 0.85 – 1.15

Grade 22L limits carbon lower and is Class 1 only. Do not treat EN 10028-2 13CrMo4-5 as Grade 22. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search A387 Gr.22 Cl.2 mechanical properties, A387GR22CL2 yield and A387 Grade 22 Class 2 tensile.

Tensile and Yield — ASTM A387 Grade 22 Class 2

Item Requirement
Tensile strength 75–100 ksi / 515–690 MPa
Yield strength, min 45 ksi / 310 MPa
Elongation in 2 in. [50 mm], min 18%
Reduction of area, min 40%
Density 7.85 g/cm³

Class 1 on the same grade is 60–85 ksi / 415–585 MPa with 30 ksi / 205 MPa yield. Do not quote Class 1 numbers on a Class 2 order. Class 2 tensile is not applicable to annealed plate.

Material Comparison

Grade Book What buyers search Swap?
ASTM A387 Grade 22 Class 1 A387 A387 Gr.22 Cl.1 / A387GR22CL1 No
ASTM A387 Grade 22 Class 2 A387 A387 Gr.22 Cl.2 / A387GR22CL2 This page
ASME SA387 Grade 22 Class 2 SA-387 SA387 Gr.22 Cl.2 Code name
ASME SA387 Grade 22L Class 1 SA-387 SA387 Gr.22L Cl.1 No
ASME SA387 Grade 11 Class 2 SA-387 SA387 Gr.11 Cl.2 No
EN 10028-2 10CrMo9-10 EN 10028-2 10CrMo9-10 No auto swap
GB/T 713 12Cr2Mo1R GB/T 713 12Cr2Mo1R No auto swap
ASME SA542 Type B Class 2 SA-542 SA542 Type B Cl.2 No

Equivalent Material Grades

There is no official one-to-one worldwide swap for A387 Gr.22 Cl.2. What buyers compare is the 2.25Cr-1Mo idea in other books, not an automatic substitute.

In the United States the Code name is ASME SA-387 Grade 22 Class 2. That is the same chemistry and the same Class 2 tensile table. ASTM A387 Grade 22 Class 1 is the same chemistry at the lower strength class. ASME SA387 Grade 22L Class 1 is the low-carbon sister, Class 1 only. Quenched-and-tempered 2.25Cr-1Mo belongs on ASME SA542 Type B Class 2.

In Europe the nearest comparison is EN 10028-2 10CrMo9-10. EN 10028-2 11CrMo9-10 is a related 2.25Cr-1Mo grade. Both sit on EN 10028-2.

In China the usual vessel comparison is GB/T 713 12Cr2Mo1R. See 12Cr2Mo1R.

Designation Country / region Standard Notes
ASTM A387 Gr.22 Cl.2 / A387GR22CL2 USA ASTM A387 Name on this page
ASME SA-387 Grade 22 Class 2 USA SA-387 Code counterpart
ASTM A387 Grade 22 Class 1 USA A387 Same chemistry, lower class
ASME SA387 Grade 22L Class 1 USA SA-387 Low-carbon sister
EN 10028-2 10CrMo9-10 Europe EN 10028-2 2.25Cr-1Mo comparison
EN 10028-2 11CrMo9-10 Europe EN 10028-2 Related 2.25Cr-1Mo
GB/T 713 12Cr2Mo1R China GB/T 713 2.25Cr-1Mo vessel
ASME SA542 Type B Class 2 USA SA-542 QT Cr-Mo, not A387 N+T

Dual marking is possible only when both books are fully met.

2.25Cr-1Mo Elevated-Temperature Service

Buyers pick A387 Gr.22 Cl.2 when a file wants 2.25Cr-1Mo at the Class 2 strength band. This is the usual stock class for Grade 22. Search phrases such as A387GR22CL2, A387 Grade 22 Class 2 and SA387 Grade 22 Class 2 all point here.

It is not a substitute for ASME SA387 Grade 11 Class 2. That grade is 1.25Cr-0.5Mo. It is not a substitute for ASME SA387 Grade 21 Class 2. That grade is 3Cr-1Mo. Dual marking with SA-387 Grade 22 Class 2 is the normal Code route.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

A387 Grade 22 Class 2 is killed 2.25Cr-1Mo vessel plate at 515–690 MPa. Treat welding as production welding, and as ASME Section VIII / PED welding when the equipment is a vessel.

Qualify to the applicable code. Consumables must match a 2.25Cr-1Mo family. A procedure written for ASME SA516 Grade 70 is the wrong alloy. A procedure written for ASME SA387 Grade 11 Class 2 is too lean in Cr and Mo. A procedure written for EN 10028-2 10CrMo9-10 is the usual European comparison. Preheat, interpass and PWHT must stay inside the qualified WPS. Minimum temper on the plate is 675 °C. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Conditio

Usual delivery from SHH STEEL for A387 Gr.22 Cl.2 is normalized and tempered, or accelerated cooling plus temper. Minimum tempering temperature for Grade 22 is 1250 °F / 675 °C.

Class 2 tensile values are not applicable to annealed plate. If the mill only annealed the heat, it cannot be certified Class 2.

If the vessel will see PWHT, say so. Simulated PWHT on test coupons is worth naming on 2.25Cr-1Mo work. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists ASTM A387 Grade 22 Class 2 and, when ordered, ASME SA-387 Grade 22 Class 2; heat number; heat analysis; product analysis when ordered; tensile to the Class 2 table; heat-treatment route. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for A387 Gr.22 Cl.2 2.25Cr-1Mo vessel plate:

  • Thickness: commonly 6 mm – 200 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Maximum thickness is limited by the ability of the composition to meet Class 2 tensile. QT 2.25Cr-1Mo belongs on ASME SA542 Type B Class 2. 3Cr-1Mo plate belongs on ASME SA387 Grade 21 Class 2.

Tolerances

Dimensional limits for ASTM A387 Grade 22 Class 2 follow ASTM A20 / ASME SA-20 unless the purchase order names another table. Do not apply ASTM A36 structural tolerances to a Cr-Mo vessel plate without writing them.

Typical thickness tolerance idea for A387 Gr.22 Cl.2 (A20 / SA-20 reference)

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
6 – 16 −0.3 +0.8
16 – 25 −0.4 +0.9
25 – 40 −0.5 +1.0
40 – 80 −0.8 +1.2
80 – 150 −1.0 +1.6
150 – 200 −1.2 +2.0

Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless the mill quote names a tighter extra. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows A20 / SA-20 unless a tighter class is written. Edge condition is mill edge or cut edge as ordered. If the vessel calculation used minimum thickness after corrosion, write the allowed minus on the RFQ. SHH STEEL will not assume a zero-minus extra on A387GR22CL2 unless the order says so.

Supplementary Requirements

ASTM A387 Grade 22 Class 2 already defines chemistry, Class 2 tensile and the 675 °C minimum temper. Extra items still have to be written on the purchase order. SHH STEEL will not assume them from the grade name alone.

Code name. Write SA-387 Grade 22 Class 2 when the equipment is ASME Code work.

Heat-treatment route. Write normalized and tempered, or accelerated cooling plus temper. Do not accept annealed plate as Class 2.

Charpy details. Class 2 does not assume a default impact temperature. Write temperature, joules, location and orientation if impact is required.

Simulated PWHT. When the vessel will be stress-relieved, name hold temperature, hold time and cooling rate on the coupon.

Product analysis. Especially C, Cr, Mo, P and S.

Through-thickness / Z-test. Name Z15, Z25 or Z35 when the plate will be welded in the thickness direction.

NDE. A20 / SA-20 ultrasonic extras, ASTM A435 or ASTM A578 as named. Write scanning extent and acceptance class.

Hardness. If the destination file caps hardness after heat treatment or after simulated PWHT, write the max HB and the test location.

HIC / SSC / NACE. Only when the equipment is sour service. A387 Gr.22 Cl.2 is not automatically NACE MR0175 / ISO 15156.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named. Hold points for heat treatment, chemistry, tensile and UT should be listed on the ITP.

Identification and stamping. Heat number, grade A387 Grade 22 Class 2 / A387 Gr.22 Cl.2, SA-387 Grade 22 Class 2 when ordered, thickness and mill logo on each plate.

Applications

Industry Typical components
2.25Cr-1Mo boilers A387 Gr.22 Cl.2 / A387GR22CL2 shells
Hydrogen / refinery vessels A387 Grade 22 Class 2 courses from SHH STEEL
ASME Code dual-name A387 Gr.22 Cl.2 / SA-387 Grade 22 Class 2
Comparison vs QT Cr-Mo A387GR22CL2 next to ASME SA542 Type B Class 2

A387 Grade 22 Class 2 is the plate for a file that wants 2.25Cr-1Mo at the higher strength class. It is the wrong plate for Class 1 tensile. That work is A387 Grade 22 Class 1. It is the wrong plate for 9Cr-1Mo-V. That work is ASME SA387 Grade 91 Class 2.

Supply Capability

worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or heat-treatment route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, 120 mm, 150 mm, thicker by mill agreement.

Processing: CNC or flame cutting, bevel, flattening, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard rolling / N+T about 45–60 days; simulated PWHT / 3.2 about 2 months.

Why Choose SHH STEEL

Experience on this grade is simple: keep Grade 22 away from Grade 11 and Grade 21, keep Class 2 away from annealed Class 1, and keep A387 away from SA-542 QT. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices A387 Gr.22 Cl.2 from first-line mills, reports 2.25Cr-1Mo chemistry, records N+T delivery, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. A387GR22CL2 is not A387 Gr.22 Cl.1. A387 Grade 22 Class 2 is not ASME SA387 Grade 22L Class 1. A387 Gr.22 Cl.2 is not ASME SA542 Type B Class 2. If the drawing says Class 1, we will not ship Class 2 and call stronger automatically acceptable.

FAQ

What is A387 Grade 22 Class 2 steel plate?
ASTM A387 Grade 22 Class 2, also searched as A387 Gr.22 Cl.2, A387GR22CL2 and SA387 Grade 22 Class 2, is 2.25Cr-1Mo pressure-vessel plate. Tensile is 515–690 MPa and yield is 310 MPa min. Delivery is normalized and tempered, not annealed. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of A387 Gr.22 Cl.2?
The Code counterpart is SA-387 Grade 22 Class 2. Related comparisons are 10CrMo9-10 in Europe and 12Cr2Mo1R in China. Dual marking is possible only when both books are fully met.
How is Class 2 different from Class 1 on Grade 22?
Class 2 is 515–690 MPa with 310 MPa yield. Class 1 is 415–585 MPa with 205 MPa yield. Chemistry is the same. Annealed plate cannot be Class 2.
How is A387GR22CL2 different from Grade 22L?
Grade 22L is the low-carbon version and Class 1 only. Grade 22 Class 2 is the higher-strength class of the standard carbon window.
Can SHH STEEL issue EN 10204 3.2 for A387GR22CL2?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named on the order.

Conclusion

ASTM A387 Grade 22 Class 2 Steel Plate is 2.25Cr-1Mo pressure-vessel plate at 515–690 MPa tensile and 310 MPa yield. Whether the inquiry says ASTM A387 Grade 22 Class 2, A387 Gr.22 Cl.2, A387GR22CL2, A387GR22 CL2 or SA387 Grade 22 Class 2, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with Grade 22 chemistry, Class 2 tensile, recorded N+T delivery, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies ASTM A387 Grade 22 Class 2 / A387 Gr.22 Cl.2 2.25Cr-1Mo Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade and class.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

ASTM A387 Grade 22 Class 2 Steel Plate, A387 Gr.22 Cl.2, A387GR22CL2, 2.25Cr-1Mo vessel plate, A387 Gr.22 Cl.2 supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X