GB/T 1591 Q550MD thermomechanically rolled high-strength low-alloy structural steel plate, 550 MPa yield, −20 °C impact, SHH STEEL

Q550MD TMCP Steel Plate GB/T 1591 Supplier

GB/T 1591 Q550MD is thermomechanical controlled process plate with 550 MPa minimum yield and −20°C impact. SHH STEEL supplies Q550MD plate mill-direct for bridges, buildings and cold-weather frames that name the M condition. This is not quenched-and-tempered GB/T 16270 Q550D.
Keywords
Q550MD, Q550MD steel plate, GB/T 1591 Q550MD, Q550MD TMCP, Q550MD supplier, EN 10025-6 S550Q, ASTM A514, Q550MC, Q550D
Equivalent Grades
GB/T 1591 Q550MD / EN 10025-4 S550ML (near) / JIS G3128 SHY685 (lower) — Material Specification: GB/T 1591 — Delivery: TMCP; -20℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q550MD TMCP Steel Plate GB/T 1591?

Q550MD, also searched as GB/T 1591 Q550MD, Q550MD steel plate, Q550MD TMCP plate and Q550 MD, is the 550 MPa quality-grade-D grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 550 is the thin-plate minimum yield in MPa, M is the delivery letter, and D is the quality letter for Charpy impact at −20°C.

The M is the point of this page. A quenched-and-tempered certificate cannot be stamped MD. That route is GB/T 16270 Q550D. Grade C on the TMCP route is GB/T 1591 Q550MC. The 500 MPa TMCP sister at the same temperature is GB/T 1591 Q500MD. The 460 MPa TMCP sister is GB/T 1591 Q460MD. The full family sits on GB/T 1591. Do not drop a 550 MPa drawing onto a 500 MPa plate, and do not upgrade it to GB/T 16270 Q620D without a price check.

EN 10025-4 stops at S460M and S460ML. There is no S550M. The usual European comparison is EN 10025-6 S550Q, which is quenched and tempered, not TMCP, and is also tested at −20°C. EN 10025-4 S460M is one yield step lower. EN 10025-6 is the QT book. On the US side, ASTM A514 is about 100 ksi / 690 MPa and is quenched and tempered, so it is not an MD twin. ASTM A572 Gr.55 is 55 ksi. Dual mark only when both books are fully met. See high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q550MD from first-line structural mills that can actually run the TMCP schedule at 550 MPa and test at −20°C, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q550MD Confirmed
Other search names Q550MD steel plate, Q550 MD, Q550MD TMCP Covered
Delivery condition Thermomechanical controlled process Confirmed
Yield, ≤ 16 mm 550 MPa min Confirmed
Quality grade D, impact at −20°C Confirmed
Not this page GB/T 16270 Q550D QT, different book
Warmer TMCP sister GB/T 1591 Q550MC 0°C
EN comparison EN 10025-6 S550Q is QT Not a swap
US comparison ASTM A514 is QT, about 690 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q500MD, GB/T 16270 Q550E and ASTM A572 Gr.55.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q550. Product analysis, when ordered, follows GB/T 222. Q550MD is a microalloyed HSLA plate. Grade D is tighter on phosphorus and sulfur than grade B or C, because the impact test is at −20°C. Mills may add Nb, V or Ti, and some heats use nickel, chromium or molybdenum to hold the 550 MPa window. The certificate shows the elements actually used. TMCP chemistry is often leaner than a QT heat of the same yield, because the rolling schedule does part of the strengthening.

Heat Analysis and Product Analysis — GB/T 1591 Q550MD, TMCP

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.60 0.65
Manganese (Mn), max 2.00 2.10
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.020 0.025
Niobium (Nb), max 0.11 0.12
Vanadium (V), max 0.12 0.13
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.80 0.85
Nickel (Ni), max 1.00 1.05
Copper (Cu), max 0.80 0.85
Molybdenum (Mo), max 0.30 0.35
Boron (B), max 0.004 0.005
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than quenched-and-tempered GB/T 16270 Q550D. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. A 500 MPa file is GB/T 1591 Q500MD, not this grade.

Mechanical Properties

Buyers search Q550MD mechanical properties, Q550MD yield strength, GB/T 1591 Q550MD tensile and Q550MD impact −20°C.

Tensile and impact — GB/T 1591 Q550MD, TMCP

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 550 MPa 670–830 MPa 16% −20°C, grade D
> 16–40 mm 530 MPa 620–800 MPa 16% −20°C, grade D
> 40–63 mm 520 MPa 600–790 MPa 16% −20°C, grade D
> 63–80 mm 500 MPa 590–780 MPa 15% −20°C, grade D
> 80–100 mm 490 MPa 570–770 MPa 15% −20°C, grade D

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at −20°C. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 550 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 550 MPa is about 80 ksi. ASTM A514 is about 100 ksi and is not this book. SHH STEEL quotes the thickness band and the M condition on the offer.

Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the D letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 16270 Q550D GB/T 16270 QT 550 MPa −20°C Different process
GB/T 1591 Q550MC GB/T 1591-2018 TMCP 550 MPa 0°C Warmer M sister
Q550MD GB/T 1591-2018 TMCP 550 MPa −20°C This page
Q550ME GB/T 1591-2018 TMCP 550 MPa −40°C Colder M sister
GB/T 1591 Q500MD GB/T 1591-2018 TMCP 500 MPa −20°C Lower yield
GB/T 16270 Q620D GB/T 16270 QT 620 MPa −20°C Higher yield
EN 10025-6 S550Q EN 10025-6 QT 550 MPa −20°C Different process
ASTM A572 Gr.55 ASTM A572 As rolled 380 MPa Different Lower yield

A colder QT file is GB/T 16270 Q550E. A 460 MPa file is GB/T 1591 Q460MD.

Equivalent Material Grades

There is no official one-to-one substitute for Q550MD. What buyers compare is a 550 MPa TMCP plate tested at −20°C.

EN 10025-4 has no S550M. EN 10025-6 S550Q is the strength comparison at the same impact temperature, but it is quenched and tempered. EN 10025-4 S460M is the nearest TMCP book grade and is one step lower. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A514 is about 100 ksi and is quenched and tempered. ASTM A572 Gr.55 is 55 ksi. ASTM A36 is 36 ksi and is well below this yield. SHH STEEL will not stamp EN 10025-6 S550Q or ASTM A514 on a Q550MD certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q550MD China GB/T 1591-2018 Name on this page
GB/T 16270 Q550D China GB/T 16270 QT, not this page
GB/T 1591 Q550MC China GB/T 1591-2018 TMCP, 0°C
GB/T 1591 Q500MD China GB/T 1591-2018 500 MPa, TMCP
EN 10025-6 S550Q Europe EN 10025-6 QT, −20°C
EN 10025-4 S460M Europe EN 10025-4 TMCP, lower yield
ASTM A514 USA ASTM A514 QT, about 690 MPa
JIS G3106 SM570 Japan JIS G3106 Lower yield comparison

Structural Service

Buyers pick Q550MD when a bridge, building member or welded fabrication wants about 550 MPa yield, a TMCP condition, and impact at −20°C. Search phrases such as Q550MD steel plate and GB/T 1591 Q550MD all point here. The family index is GB/T 1591.

It is the wrong plate when the drawing says quenched and tempered. That work is GB/T 16270 Q550D. It is the wrong plate for a 0°C file. That work is GB/T 1591 Q550MC, and the QT sister is GB/T 16270 Q550C. It is the wrong plate for a −40°C file. That work is Q550ME, and the QT sister is GB/T 16270 Q550E. It is the wrong plate for a 500 MPa file. That work is GB/T 1591 Q500MD or GB/T 1591 Q500ME. It is the wrong plate for a 620 MPa file. That work is GB/T 16270 Q620D. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade D, and the M condition at 550 MPa.

Weldability

Q550MD is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q550MD. Carbon equivalent on the M route is often lower than quenched-and-tempered GB/T 16270 Q550D, which helps the root pass, but the TMCP microstructure still needs a qualified procedure. A procedure qualified only at 0°C may miss the −20°C coupon.

Typical consumables are matching 80–90 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 does not cover 550 MPa. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q550MD procedure on GB/T 1591 Q420MB without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q500MC either if the joint must develop 550 MPa.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q550MD is thermomechanical controlled process. The plate is not quenched and tempered as GB/T 16270 Q550D.

TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q550MD as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.

The certificate lists GB/T 1591 Q550MD, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and −20°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-6 S550Q is available only when both books are fully met. S550Q is not a TMCP grade.

Dimensions

Usual supply range from SHH STEEL for Q550MD steel plate:

  • Thickness: commonly 8 mm – 40 mm, heavier plate to 50 mm by mill confirmation
  • Width: 1500 mm – 3000 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q550MD follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q550MD plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 50 −0.6 +1.3

Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q550MD unless the order says so.

Supplementary Requirements

Q550MD already defines 550 MPa yield, TMCP delivery and −20°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q550MD. Do not write only Q550, and do not write GB/T 16270 if the mill must stamp M. The family page is GB/T 1591.

Impact. Grade D is −20°C. Write a higher energy if the owner requires it. Do not expect a −40°C result unless the grade is changed to Q550ME.

Delivery condition. Write thermomechanical controlled process. Write GB/T 16270 Q550D if quenched and tempered is required.

EN or US comparison. Write EN 10025-6 S550Q or ASTM A514 only if dual mark is required and both tables are met. S550Q is QT, not TMCP.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q550MD, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Bridges and towers Q550MD webs and flanges from SHH STEEL
Buildings in cold regions Q550MD columns, beams and base plates
Construction machinery Q550MD frames where the drawing names M and −20°C
General fabrication Q550MD gussets and connection plates
Comparison vs EN 10025-4 Q550MD next to EN 10025-4 S460M
Comparison vs ASTM A572 Q550MD next to ASTM A572 Gr.55
Lower yield option GB/T 1591 Q500ME when 500 MPa is enough

Q550MD is the plate for a 550 MPa TMCP file tested at −20°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A colder QT file is GB/T 16270 Q550E.

Supply Capability

SHH STEEL sources Q550MD from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an M heat is in yard; standard TMCP about 35–50 days; 3.2 inspection about 45–55 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q550MD that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule at 550 MPa and test at −20°C, so the M and the D are both on the certificate.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard M heat about 35–50 days, 3.2 inspection about 45–55 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q550MD, keep the TMCP route, and do not ship GB/T 16270 Q550D as MD. We will not drop the M to save a cooling cycle, and we will not change D to C to save a cold test. If the drawing needs quenched and tempered plate, we will move the inquiry to Q550D under GB/T 16270. If the drawing needs 500 MPa, we will move it to GB/T 1591 Q500ME or GB/T 1591 Q500MF.

FAQ

What is Q550MD steel plate?
Q550MD in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 550 MPa minimum yield on thin plate and Charpy impact at −20°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q550MD the same as GB/T 16270 Q550D?
No. Both can yield at 550 MPa and both can be tested at −20°C. GB/T 16270 Q550D is quenched and tempered. Q550MD is TMCP.
Is Q550MD the same as Q550MC?
No. Both are TMCP. Q550MC is tested at 0°C. Q550MD is tested at −20°C.
Is Q550MD the same as Q500MD?
No. Both are TMCP and both are tested at −20°C. Q500MD is 500 MPa. Q550MD is 550 MPa.
What is the European equivalent of Q550MD?
There is no S550M in EN 10025-4. The strength comparison is EN 10025-6 S550Q, which is quenched and tempered and tested at −20°C. Dual mark only when both books are fully met.
What is the US equivalent of Q550MD?
There is no official ASTM twin. ASTM A514 is about 100 ksi and is quenched and tempered. SHH STEEL does not dual-mark ASTM A514 unless both books are met.

Conclusion

Q550MD steel plate to GB/T 1591 is 550 MPa TMCP structural plate with impact at −20°C. It is not quenched-and-tempered GB/T 16270 Q550D. EN 10025-4 has no S550M. EN 10025-6 S550Q is the strength comparison and is QT. ASTM A514 is about 690 MPa and is not a substitute. Whether the inquiry says Q550MD, GB/T 1591 Q550MD or Q550MD TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q550MD chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q550MD Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition. The grade family is listed on GB/T 1591.

Contact SHH STEEL for mill rolling, TMCP Q550MD, cutting, UT, 3.2 inspection or a worldwide quotation.

Q550MD, Q550MD steel plate, GB/T 1591 Q550MD, Q550MD TMCP, Q550MD supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X