Q460NC steel plate GB/T 1591 high-strength low-alloy plate stock at SHH STEEL supplier yard

Q460NC Steel Plate GB/T 1591 Supplier

GB/T 1591 Q460NC is normalized high-strength low-alloy plate with 460 MPa minimum yield and 0°C impact. SHH STEEL supplies Q460NC plate mill-direct for bridges, buildings and fabrication that names the N condition. This is not hot-rolled Q460C, not TMCP Q460MC, and not GB/T 16270 QT plate.
Keywords
Q460NC, Q460NC steel plate, GB/T 1591 Q460NC, Q460NC plate, Q460NC supplier, EN 10025-3 S460N, ASTM A572 Gr.65, Q460C, Q460MC
Equivalent Grades:
EN 10025-3 S460N
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q460NC Steel Plate GB/T 1591?

Q460NC, also searched as GB/T 1591 Q460NC, Q460NC steel plate, Q460NC plate and Q460 NC, is the 460 MPa quality-grade-C grade delivered normalized or normalizing-rolled in GB/T 1591-2018. Q is the yield symbol, 460 is the thin-plate minimum yield in MPa, N is the delivery letter, and C is the quality letter for Charpy impact at 0°C.

The N is the point of this page. Hot-rolled GB/T 1591 Q460C has no N. Thermomechanical Q460MC has an M. A hot-rolled certificate cannot be stamped NC. A TMCP certificate cannot be stamped NC. Grade D is −20°C. E is −40°C. Hot-rolled Q460 starts at C. There is no Q460B in that delivery condition. Q460 sits above GB/T 1591 Q420NC. Do not drop a 460 MPa drawing onto a 420 MPa plate.

Do not confuse this page with GB/T 16270 Q460C. That grade is quenched and tempered. Same yield number, different book, different process and different weld procedure. A GB/T 1591 certificate cannot be used as a GB/T 16270 certificate.

The closest process comparison is EN 10025-3 S460N, a normalized fine-grain grade, but that letter is tested at −20°C. EN 10025-3 S460NL is colder. EN 10025-4 S460M is TMCP and closer to Q460MC. On the US side, ASTM A572 Gr.65 is 65 ksi / 450 MPa, one step lower, and it is not an NC twin. JIS G3106 SM570 is a lower Japanese comparison. Dual mark only when both books are fully met. See EN 10025-3 and high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q460NC from first-line structural mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q460NC Confirmed
Other search names Q460NC steel plate, Q460 NC Covered
Delivery condition Normalized or normalizing rolled Confirmed
Yield, ≤ 16 mm 460 MPa min Confirmed
Quality grade C, impact at 0°C Confirmed
Not this page Hot-rolled GB/T 1591 Q460C Different condition
Not this page GB/T 16270 Q460C Different book
EN comparison EN 10025-3 S460N Process comparison, not a swap
US comparison ASTM A572 Gr.65 is 450 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include EN 10025-3 S460N, ASTM A572 Gr.65 and GB/T 1591 Q460C.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for normalized Q460. Product analysis, when ordered, follows GB/T 222. Q460NC is a microalloyed HSLA plate. Grade C is the warmest impact letter on normalized Q460. Mills may add Nb, V, Ti, Cr or Ni. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 1591 Q460NC, normalized

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.60 0.65
Manganese (Mn), max 1.80 1.90
Phosphorus (P), max 0.030 0.035
Sulfur (S), max 0.030 0.035
Niobium (Nb), max 0.11 0.12
Vanadium (V), max 0.20 0.22
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.80 0.85
Nickel (Ni), max 0.80 0.85
Copper (Cu), max 0.55 0.60
Molybdenum (Mo), max 0.20 0.22
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The N route often has a different CEV window from hot-rolled GB/T 1591 Q460C. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as the QT chemistry on GB/T 16270 Q460C. A 420 MPa file is GB/T 1591 Q420NC, not this grade.

Mechanical Properties

Buyers search Q460NC mechanical properties, Q460NC yield strength, GB/T 1591 Q460NC tensile and Q460NC impact 0°C.

Tensile and impact — GB/T 1591 Q460NC, normalized

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 460 MPa 550–720 MPa 17% 0°C, grade C
> 16–40 mm 440 MPa 550–720 MPa 17% 0°C, grade C
> 40–63 mm 420 MPa 550–720 MPa 16% 0°C, grade C
> 63–80 mm 400 MPa 550–720 MPa 16% 0°C, grade C
> 80–100 mm 400 MPa 550–720 MPa 16% 0°C, grade C
> 100–150 mm 380 MPa 530–700 MPa 16% 0°C, grade C

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at 0°C. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 460 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 460 MPa is about 67 ksi. ASTM A572 Gr.65 is 65 ksi and is not this book. SHH STEEL quotes the thickness band and the N condition on the offer.

Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the C letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 1591 Q460C GB/T 1591-2018 Hot rolled 460 MPa 0°C Different process
Q460NC GB/T 1591-2018 Normalized 460 MPa 0°C This page
Q460MC GB/T 1591-2018 TMCP 460 MPa 0°C Different process
Q460ND GB/T 1591-2018 Normalized 460 MPa −20°C Colder sister
GB/T 16270 Q460C GB/T 16270 QT 460 MPa 0°C Different book
GB/T 1591 Q420NC GB/T 1591-2018 Normalized 420 MPa 0°C Lower yield
EN 10025-3 S460N EN 10025-3 Normalized 460 MPa −20°C Colder comparison
ASTM A572 Gr.65 ASTM A572 As rolled 450 MPa Different Lower yield

A colder hot-rolled file is GB/T 1591 Q460D. A warmer 420 MPa file is GB/T 1591 Q420B.

Equivalent Material Grades

There is no official one-to-one substitute for Q460NC. What buyers compare is a 460 MPa normalized plate tested at 0°C.

EN 10025-3 S460N is the process comparison, but it is tested at −20°C. EN 10025-3 S460NL is colder. EN 10025-4 S460M is TMCP and closer to Q460MC. GB/T 16270 Q460C is quenched and tempered. In the United States, ASTM A572 Gr.65 is 65 ksi / 450 MPa. ASTM A572 Gr.60 is 60 ksi and is one step lower. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM570 is lower. SHH STEEL will not stamp EN 10025-3 S460N or ASTM A572 Gr.65 on a Q460NC certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q460NC China GB/T 1591-2018 Name on this page
GB/T 1591 Q460C China GB/T 1591-2018 Hot rolled, not this page
Q460MC China GB/T 1591-2018 TMCP, not this page
GB/T 16270 Q460C China GB/T 16270 QT, different book
GB/T 1591 Q420NC China GB/T 1591-2018 420 MPa, normalized
EN 10025-3 S460N Europe EN 10025-3 Normalized, −20°C
ASTM A572 Gr.65 USA ASTM A572 65 ksi, lower yield
JIS G3106 SM570 Japan JIS G3106 Lower yield

Structural Service

Buyers pick Q460NC when a bridge, building member or welded fabrication wants about 460 MPa yield, a normalized or normalizing-rolled condition, and impact at 0°C. Search phrases such as Q460NC steel plate and GB/T 1591 Q460NC all point here.

It is the wrong plate when the drawing says hot rolled only. That work is GB/T 1591 Q460C. It is the wrong plate when the drawing says TMCP. That work is Q460MC. It is the wrong plate for a −20°C file. That work is Q460ND, and the hot-rolled sister is GB/T 1591 Q460D. It is the wrong plate for a −40°C file. That work is Q460NE, and the hot-rolled sister is GB/T 1591 Q460E. It is the wrong plate for a 420 MPa file. That work is GB/T 1591 Q420NC or GB/T 1591 Q420D. It is the wrong plate when the drawing says quenched and tempered. That work is GB/T 16270 Q460C. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade C, and the N condition at 460 MPa.

Weldability

Q460NC is a weldable normalized HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q460NC. Carbon equivalent on the N route is not the same window as hot-rolled GB/T 1591 Q460C. A procedure written for GB/T 16270 Q460C is a QT procedure and is not this page.

Typical consumables are matching 65 ksi / 460 MPa low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.65 is a useful strength reference after chemistry is checked. Preheat follows thickness, hydrogen and the approved WPS. Thick plate and restrained joints need more preheat than a 10 mm web.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q460NC procedure on Q460MC without checking the TMCP carbon equivalent.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q460NC is normalized or normalizing rolled. The plate is not hot rolled as GB/T 1591 Q460C and not thermomechanical rolled as Q460MC. It is not quenched and tempered unless the order moves to GB/T 16270.

Normalizing is typically about 880–920°C, followed by air cooling, unless the mill uses a normalizing-rolling route that the standard accepts for the N letter. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move yield on a controlled heat.

The certificate lists GB/T 1591 Q460NC, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and 0°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-3 S460N is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q460NC steel plate:

  • Thickness: commonly 8 mm – 60 mm, heavier plate to 80 mm by enquiry
  • Width: 1500 mm – 2800 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q460NC follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q460NC plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 60 −0.6 +1.3
60 – 80 −0.7 +1.5

Width on 1500–2800 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q460NC unless the order says so.

Supplementary Requirements

Q460NC already defines 460 MPa yield, normalized delivery and 0°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q460NC. Do not write only Q460, and do not write Q460C if the mill must stamp N. If the file needs QT, write GB/T 16270 Q460C.

Impact. Grade C is 0°C. Write a higher energy if the owner requires it. Do not expect a −20°C result unless the grade is changed to Q460ND.

Delivery condition. Write normalized or normalizing rolled. Write GB/T 1591 Q460C if hot rolled is enough. Write Q460MC if TMCP is required.

EN or US comparison. Write EN 10025-3 S460N or ASTM A572 Gr.65 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q460NC, GB/T 1591, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Bridges and towers Q460NC webs and flanges from SHH STEEL
Buildings Q460NC columns, beams and base plates
Construction machinery Q460NC frames where the drawing names N and 0°C
General fabrication Q460NC gussets and connection plates
Comparison vs EN 10025-3 Q460NC next to EN 10025-3 S460N
Comparison vs ASTM A572 Q460NC next to ASTM A572 Gr.65
Not the QT grade Different book: GB/T 16270 Q460C

Q460NC is the plate for a 460 MPa normalized file tested at 0°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a QT boom under GB/T 16270.

Supply Capability

SHH STEEL sources Q460NC from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm, 60 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an N heat is in yard; standard normalizing about 30–45 days; 3.2 inspection about 40–50 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q460NC that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually normalize or normalizing-roll the heat, so the N is on the certificate and not only in the enquiry.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard N heat about 30–45 days, 3.2 inspection about 40–50 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q460NC, keep the normalized route, and do not ship GB/T 1591 Q460C or GB/T 16270 Q460C as NC. We will not drop the N to save a furnace cycle, and we will not treat Q460NC as ASTM A36. If the drawing needs QT plate, we will move the inquiry to GB/T 16270 and keep the price on the right book.

FAQ

What is Q460NC steel plate?
Q460NC in GB/T 1591-2018 is normalized or normalizing-rolled high-strength low-alloy plate with 460 MPa minimum yield on thin plate and Charpy impact at 0°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q460NC the same as Q460C?
No. Both yield at 460 MPa and both are tested at 0°C under GB/T 1591. Q460C is hot rolled. Q460NC is normalized or normalizing rolled.
Is GB/T 1591 Q460NC the same as GB/T 16270 Q460C?
No. GB/T 1591 Q460NC is normalized. GB/T 16270 Q460C is quenched and tempered. Same yield number, different book and different weld procedure.
Is Q460NC the same as Q460MC?
No. Q460NC is normalized. Q460MC is thermomechanical rolled. Impact letter C is the same temperature. The process is not.
What is the European equivalent of Q460NC?
The nearest process comparison is EN 10025-3 S460N, which is normalized but tested at −20°C. EN 10025-4 S460M is the TMCP comparison. Dual mark only when both books are fully met.
What is the US equivalent of Q460NC?
There is no official ASTM twin. ASTM A572 Grade 65 is 65 ksi / 450 MPa, slightly lower, and it does not carry an NC letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.

Conclusion

Q460NC steel plate to GB/T 1591 is 460 MPa normalized structural plate with impact at 0°C. It is not hot-rolled GB/T 1591 Q460C and not GB/T 16270 Q460C. The nearest European process comparison is EN 10025-3 S460N, and that grade is tested at −20°C. ASTM A572 Grade 65 is 450 MPa and is not a substitute. Whether the inquiry says Q460NC, GB/T 1591 Q460NC or Q460NC steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q460NC chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q460NC Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the N condition.

Contact SHH STEEL for mill rolling, normalized Q460NC, cutting, UT, 3.2 inspection or a worldwide quotation.

Q460NC, Q460NC steel plate, GB/T 1591 Q460NC, Q460NC plate, Q460NC supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X