EN 10025-3 S420N Steel Plate | S420N Fine Grain Structural Steel - SHH STEEL

EN 10025-3 S460N Steel Plate | S460N Fine Grain Structural Steel

EN 10025-3 S460N is a normalized fine-grain structural steel plate with a minimum yield strength of 460 MPa and impact tested at –20°C. It offers high strength, good weldability and toughness for heavy structural applications. SHH STEEL is a China Mill-Direct Exporter supplying S460N steel plate worldwide.
Equivalent material:
ASTM A572 Gr 65 / JIS SM520C / GB Q460D / ISO E460N
Material Specification:
EN 10025-3 — Delivery: Normalized (N) or Normalized Rolled
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-3 S460N Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-3 S460N Steel Plate (Material Number: 1.8901).

S460N is a normalized (or normalized rolled) weldable fine-grain structural steel under the European standard EN 10025-3. It provides a minimum yield strength of 460 MPa (for thickness ≤ 16 mm) and is impact tested at –20°C with a minimum energy of 40 J. This is one of the highest strength grades in the EN 10025-3 normalized series, suitable for heavily loaded structural applications while maintaining good toughness and weldability. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S460N steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-3 S460N steel plate is produced in accordance with EN 10025-3.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-3 Full compliance
Steel Grade S460N (1.8901) Confirmed
Delivery Condition Normalized (+N) Confirmed
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-3, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Max. / Range (%)
Carbon (C) ≤ 0.20
Silicon (Si) ≤ 0.60
Manganese (Mn) 1.00 – 1.70
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.025
Niobium (Nb) ≤ 0.05
Vanadium (V) ≤ 0.20
Aluminium (Al total) ≥ 0.020
Titanium (Ti) ≤ 0.05
Chromium (Cr) ≤ 0.30
Nickel (Ni) ≤ 0.80
Molybdenum (Mo) ≤ 0.10
Copper (Cu) ≤ 0.55
Nitrogen (N) ≤ 0.025

Product Analysis

Element Max. / Range (%)
Carbon (C) ≤ 0.22
Silicon (Si) ≤ 0.65
Manganese (Mn) 0.95 – 1.80
Phosphorus (P) ≤ 0.035
Sulfur (S) ≤ 0.030
Niobium (Nb) ≤ 0.06
Vanadium (V) ≤ 0.22
Aluminium (Al total) ≥ 0.015
Titanium (Ti) ≤ 0.06
Chromium (Cr) ≤ 0.35
Nickel (Ni) ≤ 0.85
Molybdenum (Mo) ≤ 0.13
Copper (Cu) ≤ 0.60
Nitrogen (N) ≤ 0.027

Note:

  • V + Nb + Ti ≤ 0.22%
  • Mo + Cr ≤ 0.30%
  • The minimum Al content does not apply if sufficient other nitrogen-binding elements are present.

Mechanical Properties

Mechanical properties of EN 10025-3 S460N (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 460 MPa 540 – 720 MPa 17% 40 J at –20°C
> 16 ≤ 40 440 MPa 540 – 720 MPa 17% 40 J at –20°C
> 40 ≤ 63 430 MPa 540 – 720 MPa 17% 40 J at –20°C
> 63 ≤ 80 410 MPa 540 – 720 MPa 17% 40 J at –20°C
> 80 ≤ 100 400 MPa 540 – 720 MPa 17% 40 J at –20°C
> 100 ≤ 150 380 MPa 530 – 710 MPa 17% 40 J at –20°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-3 S460N steel plate in the normalized (+N) condition.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S460N steel plate follow EN 10029 (for plates).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S460N has moderate-to-good weldability for a high-strength fine-grain structural steel. It can be welded by conventional methods (SMAW, GMAW, FCAW, SAW).

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E8018, E7018
GMAW (MIG/MAG) ER80S-D2, ER70S-6
FCAW E81T1, E71T-1
SAW EH14 / EM12K + suitable flux

Preheating is generally required for thicker plates. Low-hydrogen consumables and strict control of heat input are strongly recommended.

Equivalent Material Grades

Grade Standard Notes
S460N EN 10025-3 —
1.8901 EN Material number
Q460N / Q460D GB/T 1591 Closest Chinese equivalents
A633 / A572 (high strength) ASTM Approximate
StE 460 DIN (old) Former designation

Applications

EN 10025-3 S460N is used in structural applications requiring very high strength. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Heavy beams, columns, high-load frames – S460N Structural Steel
Bridges Bridge components – S460N Bridge
Machinery Heavy equipment frames – S460N Machinery
Construction High-strength construction – S460N Construction
Offshore & Industrial Heavy structural components – S460N Industrial
General Fabrication High-strength fine-grain structures – S460N Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-3 S460N Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for high-strength fine-grain structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “N” in S460N mean?
“N” indicates that the steel is supplied in the normalized condition and meets impact requirements of minimum 40 J at –20°C.
What is the difference between S460N and S460NL?
Both have the same strength level. S460N is impact tested at –20°C (40 J), while S460NL is impact tested at –50°C (27 J), offering better low-temperature toughness.
Is S460N suitable for heavily loaded structures?
Yes. With a minimum yield strength of 460 MPa, S460N is one of the highest strength normalized fine-grain grades under EN 10025-3.
What is the material number of S460N?
1.8901

Conclusion

EN 10025-3 S460N (1.8901) Steel Plate from SHH STEEL is a high-strength normalized fine-grain structural steel offering 460 MPa yield strength and reliable toughness at –20°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S460N fine grain structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-3 S460N Steel Plate, S460N steel plate, S460N fine grain structural steel, EN 10025 S460N, S460N equivalent, S460N supplier, 1.8901

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X