Q460NB Steel Plate GB/T 1591 Supplier
What is Q460NB Steel Plate GB/T 1591?
Q460NB, also searched as GB/T 1591 Q460NB, Q460NB steel plate, Q460 NB and Q460NB normalized plate, is the 460 MPa quality-grade-B grade delivered by normalizing or normalizing rolling in GB/T 1591-2018. Q is the yield symbol, 460 is the thin-plate minimum yield in MPa, N is the delivery letter, and B is the quality letter for Charpy impact at +20°C.
The N is the point of this page. A hot-rolled certificate cannot be stamped NB. Hot-rolled Q460 on letter C is GB/T 1591 Q460C; that page is not the N route. Grade C on the normalized route is GB/T 1591 Q460NC, tested at 0°C. Grade D is GB/T 1591 Q460ND. Grade E is GB/T 1591 Q460NE. The TMCP sister at the same yield is GB/T 1591 Q460MC (0°C); do not treat TMCP as normalized. The 420 MPa normalized sister at +20°C is GB/T 1591 Q420NB. The 390 MPa normalized sister is GB/T 1591 Q390NB. The full family sits on GB/T 1591. Do not drop a 460 MPa drawing onto a 420 MPa plate, and do not upgrade it to GB/T 16270 Q460C without a price and WPS check.
EN 10025-3 has no +20°C quality letter on S460N. The closest normalized comparison is EN 10025-3 S460N, tested at −20°C. That is colder than this B letter. EN 10025-4 S460M is TMCP. On the US side, ASTM A572 Grade 65 is 65 ksi / 450 MPa, one step lower, and it is not an NB twin. ASTM A572 Gr.60 is 60 ksi. JIS G3106 SM570 is the usual Japanese comparison. Dual mark only when both books are fully met. See EN 10025-3 and high strength low alloy plates.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q460NB from first-line structural mills that can actually run the normalizing or normalizing-rolling schedule and hold +20°C impact, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.
Buyers also search Q460NB equivalent, Q460NB material, Q460NB vs Q460NC and Q460NB vs Q460C when they compare normalized B to colder N letters or to hot-rolled Q460C.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 1591-2018 Q460NB | Confirmed |
| Other search names | Q460NB steel plate, Q460 NB, Q460NB normalized | Covered |
| Delivery condition | Normalized or normalizing rolled | Confirmed |
| Yield, ≤ 16 mm | 460 MPa min | Confirmed |
| Quality grade | B, impact at +20°C | Confirmed |
| Not this page | GB/T 1591 Q460C | Hot rolled, not N |
| Not this page | GB/T 1591 Q460NC | 0°C, not B |
| Not this page | GB/T 16270 Q460C | Different book (QT) |
| EN comparison | EN 10025-3 S460N is −20°C | Not a twin |
| US comparison | ASTM A572 Gr.65 is 450 MPa | Not a twin |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q460NC, GB/T 1591 Q420NB and ASTM A572 Gr.65.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 1591-2018 for normalized Q460. Product analysis, when ordered, follows GB/T 222. Q460NB is a microalloyed HSLA plate. Grade B allows the widest phosphorus and sulfur window on the N route for this yield. Mills may add Nb, V or Ti. The certificate shows the elements actually used. Normalized chemistry is often richer than a TMCP heat of the same yield, because the rolling schedule does less of the grain refinement.
Heat Analysis and Product Analysis — GB/T 1591 Q460NB, normalized
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.20 | 0.22 |
| Silicon (Si), max | 0.60 | 0.65 |
| Manganese (Mn), max | 1.80 | 1.90 |
| Phosphorus (P), max | 0.035 | 0.040 |
| Sulfur (S), max | 0.035 | 0.040 |
| Niobium (Nb), max | 0.11 | 0.12 |
| Vanadium (V), max | 0.20 | 0.22 |
| Titanium (Ti), max | 0.20 | 0.21 |
| Chromium (Cr), max | 0.80 | 0.85 |
| Nickel (Ni), max | 0.80 | 0.85 |
| Copper (Cu), max | 0.55 | 0.60 |
| Molybdenum (Mo), max | 0.20 | 0.22 |
| Nitrogen (N), max | 0.015 | 0.017 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
Carbon equivalent is limited by thickness in the standard. The N route often has a higher CEV window than TMCP GB/T 1591 Q460MC. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as quenched-and-tempered GB/T 16270 Q460C. A colder normalized file is GB/T 1591 Q460NC, not this grade.
Mechanical Properties
Buyers search Q460NB mechanical properties, Q460NB yield strength, GB/T 1591 Q460NB tensile and Q460NB impact +20°C.
Tensile and impact — GB/T 1591 Q460NB, normalized
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 16 mm | 460 MPa | 550–720 MPa | 17% | +20°C, grade B |
| > 16–40 mm | 440 MPa | 550–720 MPa | 17% | +20°C, grade B |
| > 40–63 mm | 420 MPa | 550–720 MPa | 16% | +20°C, grade B |
| > 63–80 mm | 400 MPa | 550–720 MPa | 16% | +20°C, grade B |
| > 80–100 mm | 400 MPa | 550–720 MPa | 16% | +20°C, grade B |
| > 100–150 mm | 380 MPa | 530–700 MPa | 16% | +20°C, grade B |
Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at +20°C, depending on the ordered edition and thickness. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it. Not every normalized heat will hold B on thick plate. SHH STEEL confirms the thickness before promising the letter.
Yield steps down with thickness. A 460 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 460 MPa is about 67 ksi. ASTM A572 Grade 65 is 65 ksi and is not this book. Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the B letter.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| GB/T 1591 Q460C | GB/T 1591-2018 | Hot rolled | 460 MPa | 0°C | Different process |
| Q460NB | GB/T 1591-2018 | Normalized | 460 MPa | +20°C | This page |
| GB/T 1591 Q460NC | GB/T 1591-2018 | Normalized | 460 MPa | 0°C | Colder sister |
| GB/T 1591 Q460MC | GB/T 1591-2018 | TMCP | 460 MPa | 0°C | Different process |
| GB/T 1591 Q420NB | GB/T 1591-2018 | Normalized | 420 MPa | +20°C | Lower yield |
| GB/T 16270 Q460C | GB/T 16270 | QT | 460 MPa | 0°C | Different book |
| EN 10025-3 S460N | EN 10025-3 | Normalized | 460 MPa | −20°C | Closest, not a twin |
| ASTM A572 Gr.65 | ASTM A572 | As rolled | 450 MPa | Different | Lower yield |
A colder normalized file is GB/T 1591 Q460ND. A 420 MPa file is GB/T 1591 Q420NB.
Equivalent Material Grades
There is no official one-to-one substitute for Q460NB. What buyers compare is a 460 MPa normalized plate tested at +20°C.
EN 10025-3 S460N is the closest process comparison, but it stops at −20°C. EN 10025-4 S460M is TMCP. EN 10025-3 S460NL is colder still. In the United States, ASTM A572 Grade 65 is 65 ksi / 450 MPa. ASTM A572 Gr.60 is 60 ksi. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM570 is the usual comparison. SHH STEEL will not stamp EN 10025-3 S460N or ASTM A572 Gr.65 on a Q460NB certificate unless the purchase order names both books and both tables are met.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q460NB | China | GB/T 1591-2018 | Name on this page |
| GB/T 1591 Q460C | China | GB/T 1591-2018 | Hot rolled, not this page |
| GB/T 1591 Q460NC | China | GB/T 1591-2018 | Normalized, 0°C |
| GB/T 1591 Q460MC | China | GB/T 1591-2018 | TMCP, not this page |
| GB/T 1591 Q420NB | China | GB/T 1591-2018 | 420 MPa, normalized |
| GB/T 16270 Q460C | China | GB/T 16270 | QT, different book |
| EN 10025-3 S460N | Europe | EN 10025-3 | Normalized, −20°C, not a twin |
| ASTM A572 Gr.65 | USA | ASTM A572 | 65 ksi, lower yield |
| JIS G3106 SM570 | Japan | JIS G3106 | Usual Japanese comparison |
Structural Service
Buyers pick Q460NB when a building member, bridge accessory or welded fabrication wants about 460 MPa yield, a normalized condition, and impact at +20°C. Search phrases such as Q460NB steel plate and GB/T 1591 Q460NB all point here. The family index is GB/T 1591.
It is the wrong plate when the drawing says hot rolled only. That work is GB/T 1591 Q460C if 0°C is enough on the AR route. It is the wrong plate for a 0°C normalized file. That work is GB/T 1591 Q460NC. It is the wrong plate for a −20°C file. That work is GB/T 1591 Q460ND, and the −40°C sister is GB/T 1591 Q460NE. It is the wrong plate for a TMCP file. That work is GB/T 1591 Q460MC. It is the wrong plate for a 420 MPa file. That work is GB/T 1591 Q420NB or GB/T 1591 Q420NC. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.
SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade B, and the N condition at 460 MPa.
Weldability
Q460NB is a weldable normalized HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q460NB. Carbon equivalent on the N route is often higher than TMCP GB/T 1591 Q460MC, so the root pass needs a qualified procedure. A procedure qualified only at 0°C may still cover +20°C, but the certificate letter must match the drawing.
Typical consumables are matching 70 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.65 is a useful strength reference after chemistry and the +20°C coupon are checked, but it does not cover 460 MPa by itself. Preheat follows thickness, hydrogen and the approved WPS.
The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q460NB procedure on GB/T 1591 Q420NB without checking the lower-yield carbon equivalent. Do not use it on GB/T 16270 Q460C either.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q460NB is normalized or normalizing rolled. The plate is not hot rolled as GB/T 1591 Q460C and not TMCP as GB/T 1591 Q460MC.
Normalizing refines the as-rolled grain. Normalizing rolling finishes in the normalizing temperature range and may replace a separate furnace cycle when the mill procedure allows it. Do not order Q460NB as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting.
The certificate lists GB/T 1591 Q460NB, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and +20°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-3 S460N is available only when both books are fully met. S460N does not cover +20°C by itself as an NB twin.
Dimensions
Usual supply range from SHH STEEL for Q460NB steel plate:
- Thickness: commonly 8 mm – 80 mm, heavier plate to 100–150 mm by mill confirmation
- Width: 1500 mm – 3000 mm, wider by enquiry
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.
Tolerances
Dimensional limits for Q460NB follow GB/T 709 unless the purchase order names EN 10029 or another table.
Typical thickness tolerance idea for Q460NB plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 15 | −0.3 | +0.8 |
| 15 – 25 | −0.4 | +0.9 |
| 25 – 40 | −0.5 | +1.1 |
| 40 – 60 | −0.6 | +1.3 |
| 60 – 80 | −0.7 | +1.5 |
| 80 – 100 | −0.8 | +1.6 |
Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q460NB unless the order says so.
Supplementary Requirements
Q460NB already defines 460 MPa yield, normalized delivery and +20°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 1591 Q460NB. Do not write only Q460, and do not write Q460NC if the mill must stamp B. The family page is GB/T 1591.
Impact. Grade B is +20°C. Write a higher energy if the owner requires it. Do not expect a colder result from this letter — move to GB/T 1591 Q460NC or GB/T 1591 Q460ND.
Delivery condition. Write normalized or normalizing rolled. Write GB/T 1591 Q460C if hot rolled and 0°C are enough.
EN or US comparison. Write EN 10025-3 S460N or ASTM A572 Gr.65 only if dual mark is required and both tables are met. S460N is −20°C, not +20°C.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Identification. Heat number, Q460NB, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Building structures | Q460NB columns and base plates from SHH STEEL |
| Bridges and infrastructure | Q460NB webs and flanges where +20°C impact is enough |
| Construction machinery | Q460NB frames where the drawing names N and B |
| General fabrication | Q460NB gussets and connection plates |
| Comparison vs EN 10025-3 | Q460NB next to EN 10025-3 S460N |
| Comparison vs ASTM A572 | Q460NB next to ASTM A572 Gr.65 |
| Lower yield option | GB/T 1591 Q420NB when 420 MPa is enough |
Q460NB is the plate for a 460 MPa normalized file tested at +20°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A colder 460 MPa normalized file is GB/T 1591 Q460ND.
Supply Capability
SHH STEEL sources Q460NB from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm, 60 mm, 80 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when a B heat is in yard; standard normalize with +20°C test about 30–45 days; 3.2 inspection about 40–55 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q460NB that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the normalizing schedule and test at +20°C, so the N and the B are both on the certificate.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard NB heat about 30–45 days, 3.2 inspection about 40–55 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 1591 Q460NB, keep the N route, and do not ship GB/T 1591 Q460C or GB/T 1591 Q460NC as NB. We will not drop the N to save a furnace cycle, and we will not change B to C to save a colder test unless the drawing asks for it. If the drawing only needs 0°C normalized, we will move the inquiry to GB/T 1591 Q460NC. If the drawing needs QT, we will move it to GB/T 16270 Q460C.
FAQ
-
What is Q460NB steel plate?
- Q460NB in GB/T 1591-2018 is normalized or normalizing-rolled high-strength low-alloy plate with 460 MPa minimum yield on thin plate and Charpy impact at +20°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q460NB the same as Q460C?
- No. Both can yield at 460 MPa under GB/T 1591, but Q460C is hot rolled (typically tested at 0°C for letter C). Q460NB is normalized or normalizing rolled and tested at +20°C.
-
Is Q460NB the same as Q460NC?
- No. Both are normalized. Q460NC is tested at 0°C. Q460NB is tested at +20°C.
-
Is GB/T 1591 Q460NB the same as GB/T 16270 Q460C?
- No. GB/T 1591 Q460NB is normalized. GB/T 16270 Q460C is quenched and tempered. Same yield number, different book and different weld procedure.
-
What is the European equivalent of Q460NB?
- There is no official twin. EN 10025-3 S460N is the closest normalized comparison, and it is tested at −20°C, not +20°C. Dual mark only when both books are fully met.
-
What is the US equivalent of Q460NB?
- There is no official ASTM twin. ASTM A572 Grade 65 is 65 ksi / 450 MPa, slightly lower, and it does not carry an NB letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
Conclusion
Q460NB steel plate to GB/T 1591 is 460 MPa normalized structural plate with impact at +20°C. It is not hot-rolled GB/T 1591 Q460C and not 0°C GB/T 1591 Q460NC. EN 10025-3 S460N is the closest normalized comparison, tested at −20°C. ASTM A572 Grade 65 is 450 MPa and is not a substitute. Whether the inquiry says Q460NB, GB/T 1591 Q460NB or Q460NB normalized plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q460NB chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q460NB Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the N condition and the B letter. The grade family is listed on GB/T 1591.
Contact SHH STEEL for mill rolling, +20°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.
Q460NB, Q460NB steel plate, GB/T 1591 Q460NB, Q460NB normalized, Q460NB supplier, SHH STEEL