EN 10025-3 S460NL Steel Plate | S460NL Fine Grain Structural Steel - SHH STEEL

EN 10025-3 S460NL Steel Plate | S460NL Fine Grain Structural Steel

EN 10025-3 S460NL is a normalized fine-grain structural steel plate with a minimum yield strength of 460 MPa and impact tested at –50°C. It offers high strength, excellent low-temperature toughness and good weldability. SHH STEEL is a China Mill-Direct Exporter supplying S460NL steel plate worldwide.
Equivalent material:
ASTM A572 Gr 65 (with -50℃ CVN) / JIS SM570 (L ref) / GB Q460E / ISO E460NL
Material Specification:
EN 10025-3 — Delivery: Normalized (N) or Normalized Rolled
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-3 S460NL Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-3 S460NL Steel Plate (Material Number: 1.8903).

S460NL is a normalized (or normalized rolled) weldable fine-grain structural steel under the European standard EN 10025-3. It provides a minimum yield strength of 460 MPa (for thickness ≤ 16 mm) and is impact tested at –50°C with a minimum energy of 27 J. This is one of the highest strength low-temperature grades in the EN 10025-3 series, combining high load-bearing capacity with excellent toughness in cold environments. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S460NL steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-3 S460NL steel plate is produced in accordance with EN 10025-3.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-3 Full compliance
Steel Grade S460NL (1.8903) Confirmed
Delivery Condition Normalized (+N) Confirmed
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-3, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Max. / Range (%)
Carbon (C) ≤ 0.20
Silicon (Si) ≤ 0.60
Manganese (Mn) 1.00 – 1.70
Phosphorus (P) ≤ 0.025
Sulfur (S) ≤ 0.020
Niobium (Nb) ≤ 0.05
Vanadium (V) ≤ 0.20
Aluminium (Al total) ≥ 0.020
Titanium (Ti) ≤ 0.05
Chromium (Cr) ≤ 0.30
Nickel (Ni) ≤ 0.80
Molybdenum (Mo) ≤ 0.10
Copper (Cu) ≤ 0.55
Nitrogen (N) ≤ 0.025

Product Analysis

Element Max. / Range (%)
Carbon (C) ≤ 0.22
Silicon (Si) ≤ 0.65
Manganese (Mn) 0.95 – 1.80
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.025
Niobium (Nb) ≤ 0.06
Vanadium (V) ≤ 0.22
Aluminium (Al total) ≥ 0.015
Titanium (Ti) ≤ 0.06
Chromium (Cr) ≤ 0.35
Nickel (Ni) ≤ 0.85
Molybdenum (Mo) ≤ 0.13
Copper (Cu) ≤ 0.60
Nitrogen (N) ≤ 0.027

Note:

  • V + Nb + Ti ≤ 0.22%
  • Mo + Cr ≤ 0.30%
  • The minimum Al content does not apply if sufficient other nitrogen-binding elements are present.

Mechanical Properties

Mechanical properties of EN 10025-3 S460NL (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 460 MPa 540 – 720 MPa 17% 27 J at –50°C
> 16 ≤ 40 440 MPa 540 – 720 MPa 17% 27 J at –50°C
> 40 ≤ 63 430 MPa 540 – 720 MPa 17% 27 J at –50°C
> 63 ≤ 80 410 MPa 540 – 720 MPa 17% 27 J at –50°C
> 80 ≤ 100 400 MPa 540 – 720 MPa 17% 27 J at –50°C
> 100 ≤ 150 380 MPa 530 – 710 MPa 17% 27 J at –50°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-3 S460NL steel plate in the normalized (+N) condition.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S460NL steel plate follow EN 10029 (for plates).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S460NL has moderate-to-good weldability for a high-strength fine-grain structural steel. It can be welded by conventional methods (SMAW, GMAW, FCAW, SAW).

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E8018, E7018
GMAW (MIG/MAG) ER80S-D2, ER70S-6
FCAW E81T1, E71T-1
SAW EH14 / EM12K + suitable flux

Preheating is generally required for thicker plates. Low-hydrogen consumables and strict control of heat input are strongly recommended, especially for low-temperature service.

Equivalent Material Grades

Grade Standard Notes
S460NL EN 10025-3 —
1.8903 EN Material number
Q460NL / Q460E GB/T 1591 Closest Chinese equivalents
A633 / high-strength low-temp ASTM Approximate
TStE 460 DIN (old) Former designation

Applications

EN 10025-3 S460NL is used in structural applications requiring very high strength and excellent low-temperature toughness. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Heavy beams, columns in cold regions – S460NL Structural Steel
Bridges Bridge components – S460NL Bridge
Offshore & Marine Heavy structural components – S460NL Offshore
Machinery Heavy equipment frames – S460NL Machinery
Low-Temperature Construction High-strength structures requiring –50°C toughness – S460NL Construction
General Fabrication Critical high-strength fine-grain structures – S460NL Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-3 S460NL Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for high-strength fine-grain low-temperature structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “NL” in S460NL mean?
“NL” indicates that the steel is supplied in the normalized condition and meets impact requirements of minimum 27 J at –50°C.
What is the difference between S460N and S460NL?
Both have the same strength level (460 MPa yield). S460N is impact tested at –20°C (40 J), while S460NL is impact tested at –50°C (27 J), providing better low-temperature toughness.
Is S460NL suitable for low-temperature high-strength applications?
Yes. With a minimum yield strength of 460 MPa and guaranteed impact toughness at –50°C, S460NL is ideal for demanding structural applications in cold environments.
What is the material number of S460NL?
1.8903

Conclusion

EN 10025-3 S460NL (1.8903) Steel Plate from SHH STEEL is a high-strength normalized fine-grain structural steel offering 460 MPa yield strength and excellent toughness at –50°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S460NL fine grain structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-3 S460NL Steel Plate, S460NL steel plate, S460NL fine grain structural steel, EN 10025 S460NL, S460NL equivalent, S460NL supplier, 1.8903

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X