Q420B steel plate GB/T 1591 high-strength low-alloy plate stock at SHH STEEL supplier yard

Q420B Steel Plate GB/T 1591 Supplier

GB/T 1591 Q420B is hot-rolled high-strength low-alloy plate with 420 MPa minimum yield and +20°C impact. SHH STEEL supplies Q420B plate mill-direct for buildings, bridges, equipment frames and general fabrication.
Keywords
Q420B, Q420B steel plate, GB/T 1591 Q420B, Q420B plate, Q420B supplier, EN 10025-3 S420N, ASTM A572 Gr.60, Q420NB, Q420MB
Equivalent Grades:
EN 10025-3 S420N / ASTM A572 Gr.60
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q420B Steel Plate GB/T 1591?

Q420B, also searched as GB/T 1591 Q420B, Q420B steel plate, Q420B plate and Q420 B, is the 420 MPa quality-grade-B grade in GB/T 1591-2018. That standard covers high-strength low-alloy structural steels. Q is the yield symbol, 420 is the thin-plate minimum yield in MPa, and B is the quality letter for Charpy impact at +20°C.

Q420B on this page is the hot-rolled grade. It has no N and no M suffix. Q420NB is normalized or normalizing-rolled. Q420MB is thermomechanical rolled. Those are different delivery conditions, different carbon-equivalent windows and different thickness limits. A hot-rolled Q420B certificate cannot be stamped NB or MB. Grade C is 0°C. D is −20°C. E is −40°C. F exists on some M grades, not on hot-rolled Q420B.

The closest European comparison is EN 10025-3 S420N, a normalized fine-grain grade, not a hot-rolled twin. EN 10025-4 S420M is the TMCP comparison and lines up more closely with Q420MB. On the US side, ASTM A572 Gr.60 is 60 ksi / 415 MPa, one step lower, and it is not a B-letter twin. JIS G3106 SM570 is higher yield and is not a swap. Dual mark only when both books are fully met. See EN 10025-3 and high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q420B from first-line structural mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q420B Confirmed
Other search names Q420B steel plate, Q420 B Covered
Delivery condition Hot rolled Confirmed
Yield, ≤ 16 mm 420 MPa min Confirmed
Quality grade B, impact at +20°C Confirmed
EN comparison EN 10025-3 S420N Comparison, not a swap
US comparison ASTM A572 Gr.60 is 415 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Not the same condition Q420NB or Q420MB Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include EN 10025-3 S420N, ASTM A572 Gr.60 and ASTM A36.

Chemical Composition

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for hot-rolled Q420. Product analysis, when ordered, follows GB/T 222. Q420B is a microalloyed HSLA plate. Grade B allows a wider phosphorus and sulfur window than grade D or E. That is acceptable at +20°C. It is not a reason to use Q420B on a −20°C drawing. Mills may add Nb, V or Ti. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 1591 Q420B, hot rolled

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.50 0.55
Manganese (Mn), max 1.70 1.80
Phosphorus (P), max 0.035 0.040
Sulfur (S), max 0.035 0.040
Niobium (Nb), max 0.07 0.08
Vanadium (V), max 0.20 0.22
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.40 0.45
Nickel (Ni), max 0.70 0.75
Copper (Cu), max 0.40 0.45
Molybdenum (Mo), max 0.20 0.22
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. A thick flange can have a lower CEV cap than a 12 mm web. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as quenched-and-tempered GB/T 16270 Q460C.

Mechanical Properties

Buyers search Q420B mechanical properties, Q420B yield strength, GB/T 1591 Q420B tensile and Q420B impact 20°C.

Tensile and impact — GB/T 1591 Q420B, hot rolled

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 420 MPa 520–680 MPa 19% +20°C, grade B
> 16–40 mm 400 MPa 520–680 MPa 19% +20°C, grade B
> 40–63 mm 390 MPa 520–680 MPa 18% +20°C, grade B
> 63–80 mm 380 MPa 520–680 MPa 18% +20°C, grade B
> 80–100 mm 370 MPa 520–680 MPa 18% +20°C, grade B
> 100–150 mm 360 MPa 500–650 MPa 17% +20°C, grade B

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at +20°C. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 420 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 420 MPa is about 61 ksi. ASTM A572 Gr.60 is 60 ksi and is not this book. SHH STEEL quotes the thickness band on the offer.

Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the B letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q420B GB/T 1591-2018 Hot rolled 420 MPa +20°C This page
Q420C GB/T 1591-2018 Hot rolled 420 MPa 0°C Colder sister
Q420D GB/T 1591-2018 Hot rolled 420 MPa −20°C Colder sister
Q420NB GB/T 1591-2018 Normalized 420 MPa +20°C Different process
Q420MB GB/T 1591-2018 TMCP 420 MPa +20°C Different process
EN 10025-3 S420N EN 10025-3 Normalized 420 MPa −20°C Different process
EN 10025-4 S420M EN 10025-4 TMCP 420 MPa −20°C Different process
ASTM A572 Gr.60 ASTM A572 As rolled 415 MPa Different Lower yield

Equivalent Material Grades

There is no official one-to-one substitute for Q420B. What buyers compare is a 420 MPa plate tested at +20°C.

EN 10025-3 S420N is normalized. EN 10025-3 S420NL is colder. EN 10025-4 S420M is TMCP and closer to Q420M than to this hot-rolled page. In the United States, ASTM A572 Gr.60 is 60 ksi / 415 MPa. ASTM A572 Gr.65 is 65 ksi / 450 MPa and is one step higher. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM570 is higher. SHH STEEL will not stamp EN 10025-3 S420N or ASTM A572 Gr.60 on a Q420B certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q420B China GB/T 1591-2018 Name on this page
Q420C / Q420D / Q420E China GB/T 1591-2018 Colder quality letters
Q420NB / Q420MB China GB/T 1591-2018 Normalized / TMCP, not this page
EN 10025-3 S420N Europe EN 10025-3 Normalized comparison
EN 10025-4 S420M Europe EN 10025-4 TMCP comparison
ASTM A572 Gr.60 USA ASTM A572 60 ksi, lower yield
JIS G3106 SM570 Japan JIS G3106 Higher yield

Structural Service

Buyers pick Q420B when a building, bridge member, equipment frame or welded fabrication wants about 420 MPa yield, hot-rolled delivery and impact at +20°C. Search phrases such as Q420B steel plate and GB/T 1591 Q420B all point here.

It is the wrong plate for a 0°C file. That work is Q420C. It is the wrong plate for a −20°C file. That work is Q420D. It is the wrong plate when the drawing says normalized. That work is Q420NB, and the European file is often EN 10025-3 S420N. It is the wrong plate when the drawing says TMCP. That work is Q420MB, and the European file is often EN 10025-4 S420M. It is the wrong plate for a quenched-and-tempered 460 MPa boom. That work is GB/T 16270 Q460C. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591 and quality grade B at 420 MPa, hot rolled.

Weldability

Q420B is a weldable HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q420B. Carbon equivalent rises with thickness, and the standard caps CEV by band.

Typical consumables are matching 60 ksi / 420 MPa low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.60 is a useful strength reference after chemistry is checked. Preheat follows thickness, hydrogen and the approved WPS. Thick plate and restrained joints need more preheat than a 10 mm web.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q420B procedure on Q420MB without checking the TMCP carbon equivalent.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q420B is hot rolled. The plate is not normalized and not thermomechanical rolled unless the order changes the grade to Q420NB or Q420MB.

Do not order Q420B as quenched and tempered. That route belongs to GB/T 16270, not to this page. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move yield on a controlled-rolled heat.

The certificate lists GB/T 1591 Q420B, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and +20°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-3 S420N is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q420B steel plate:

  • Thickness: commonly 8 mm – 80 mm, heavier plate to 100 mm by enquiry
  • Width: 1500 mm – 3000 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q420B follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q420B plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 60 −0.6 +1.3
60 – 80 −0.7 +1.5
80 – 100 −0.8 +1.6

Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q420B unless the order says so.

Supplementary Requirements

Q420B already defines 420 MPa yield, hot-rolled delivery and +20°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q420B. Do not write only Q420.

Impact. Grade B is +20°C. Write a higher energy if the owner requires it. Do not expect a −20°C result unless the grade is changed to D.

Delivery condition. Write hot rolled. Write Q420NB or Q420MB if normalized or TMCP is required.

EN or US comparison. Write EN 10025-3 S420N or ASTM A572 Gr.60 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q420B, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Buildings and workshops Q420B columns, beams and base plates
Bridges and towers Q420B webs and flanges from SHH STEEL
Construction machinery Q420B frames where +20°C is enough
General fabrication Q420B gussets and connection plates
Comparison vs EN 10025-3 Q420B next to EN 10025-3 S420N
Comparison vs ASTM A572 Q420B next to ASTM A572 Gr.60
Comparison vs ASTM A36 Q420B next to ASTM A36

Q420B is the plate for a 420 MPa hot-rolled file tested at +20°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270.

Supply Capability

SHH STEEL sources Q420B from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm, 60 mm, 80 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when plate is in yard; standard rolling about 25–40 days; 3.2 inspection about 35–45 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q420B that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that already roll GB/T 1591, so the heat carries the +20°C impact without a second upgrade charge.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 25–40 days, 3.2 inspection about 35–45 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q420B, keep the hot-rolled route, and do not ship Q420C or Q420MB as B. We will not change B to D on the certificate to win an order, and we will not treat Q420B as ASTM A36. If the drawing needs normalized plate, we will move the inquiry to Q420NB and keep the price on the right grade.

FAQ

What is Q420B steel plate?
Q420B in GB/T 1591-2018 is hot-rolled high-strength low-alloy plate with 420 MPa minimum yield on thin plate and Charpy impact at +20°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q420B the same as Q420NB or Q420MB?
No. Q420B is hot rolled. Q420NB is normalized. Q420MB is thermomechanical rolled. Impact letter B is the same temperature. The process is not.
What is the European equivalent of Q420B?
The nearest comparison is EN 10025-3 S420N, which is normalized, not hot rolled. EN 10025-4 S420M is the TMCP comparison. Dual mark only when both books are fully met.
What is the US equivalent of Q420B?
There is no official ASTM twin. ASTM A572 Grade 60 is 60 ksi / 415 MPa, slightly lower, and it does not carry a B letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
What thickness can SHH STEEL supply?
Common rolling is 8 mm to 80 mm. Plate to 100 mm is quoted by enquiry. Yield on plate over 16 mm is lower than the 420 MPa thin-plate number.
What is the delivery time for Q420B?
Ex-stock about 5–7 days when plate is in yard. Standard rolling about 25–40 days. 3.2 inspection about 35–45 days.

Conclusion

Q420B steel plate to GB/T 1591 is 420 MPa hot-rolled structural plate with impact at +20°C. The nearest European comparison is EN 10025-3 S420N, and that grade is normalized. ASTM A572 Grade 60 is 415 MPa and is not a substitute. Q420NB and Q420MB are different processes. Whether the inquiry says Q420B, GB/T 1591 Q420B or Q420B steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q420B chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q420B Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, hot-rolled Q420B, cutting, UT, 3.2 inspection or a worldwide quotation.

Q420B, Q420B steel plate, GB/T 1591 Q420B, Q420B plate, Q420B supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X