Q355NC steel plate GB/T 1591 high-strength low-alloy plate stock at SHH STEEL supplier yard

Q355NC Steel Plate GB/T 1591 Supplier

GB/T 1591 Q355NC is normalized high-strength low-alloy plate with 355 MPa minimum yield and 0°C impact. SHH STEEL supplies Q355NC plate mill-direct for buildings, bridges and fabrication that names the N condition. This is not hot-rolled Q355C and not TMCP Q355MC.
Keywords
Q355NC, Q355NC steel plate, GB/T 1591 Q355NC, Q355NC plate, Q355NC supplier, EN 10025-3 S355N, EN 10025-2 S355J0, Q355C, Q355MC
Equivalent Grades:
EN 10025-3 S355N / ASTM A633 Gr.C
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q355NC Steel Plate GB/T 1591?

Q355NC, also searched as GB/T 1591 Q355NC, Q355NC steel plate, Q355NC plate and Q355 NC, is the 355 MPa quality-grade-C grade delivered normalized or normalizing-rolled in GB/T 1591-2018. Q is the yield symbol, 355 is the thin-plate minimum yield in MPa, N is the delivery letter, and C is the quality letter for Charpy impact at 0°C.

The N is the point of this page. Hot-rolled GB/T 1591 Q355C has no N. Thermomechanical Q355MC has an M. A hot-rolled certificate cannot be stamped NC. A TMCP certificate cannot be stamped NC. Grade B is +20°C and is GB/T 1591 Q355NB. D is −20°C. E is −40°C. The 2018 edition replaced Q345 with Q355, so an old Q345NC drawing is reviewed against Q355NC, not silently swapped. Hot-rolled GB/T 1591 Q355B is the warmer sister without the N.

The closest process comparison is EN 10025-3 S355N, a normalized fine-grain grade, but that letter is tested at −20°C. EN 10025-2 S355J0 is 0°C and is closer in impact temperature, but it is not an N grade. EN 10025-3 S355NL is colder. On the US side, ASTM A572 Gr.50 is 50 ksi / 345 MPa and is not an NC twin. JIS G3106 SM490B is the usual Japanese comparison. Dual mark only when both books are fully met. See EN 10025-3 and high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q355NC from first-line structural mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q355NC Confirmed
Other search names Q355NC steel plate, Q355 NC Covered
Delivery condition Normalized or normalizing rolled Confirmed
Yield, ≤ 16 mm 355 MPa min Confirmed
Quality grade C, impact at 0°C Confirmed
Not this page Hot-rolled GB/T 1591 Q355C Different condition
Not this page TMCP Q355MC Different condition
EN comparison EN 10025-3 S355N Process comparison, not a swap
US comparison ASTM A572 Gr.50 is 345 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include EN 10025-3 S355N, EN 10025-2 S355J0 and ASTM A572 Gr.50.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for normalized Q355. Product analysis, when ordered, follows GB/T 222. Q355NC is a carbon-manganese HSLA plate. Grade C is tighter on phosphorus and sulfur than grade B, because the impact test is at 0°C. Mills may add Nb, V or Ti. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 1591 Q355NC, normalized

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.50 0.55
Manganese (Mn), max 1.60 1.70
Phosphorus (P), max 0.030 0.035
Sulfur (S), max 0.030 0.035
Niobium (Nb), max 0.05 0.06
Vanadium (V), max 0.15 0.16
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.30 0.35
Nickel (Ni), max 0.50 0.55
Copper (Cu), max 0.40 0.45
Molybdenum (Mo), max 0.10 0.11
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The N route often has a different CEV window from hot-rolled GB/T 1591 Q355C. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as quenched-and-tempered GB/T 16270 Q460C. A 420 MPa file is GB/T 1591 Q420B, not this grade.

Mechanical Properties

Buyers search Q355NC mechanical properties, Q355NC yield strength, GB/T 1591 Q355NC tensile and Q355NC impact 0°C.

Tensile and impact — GB/T 1591 Q355NC, normalized

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 355 MPa 470–630 MPa 22% 0°C, grade C
> 16–40 mm 345 MPa 470–630 MPa 21% 0°C, grade C
> 40–63 mm 335 MPa 470–630 MPa 20% 0°C, grade C
> 63–80 mm 325 MPa 470–630 MPa 19% 0°C, grade C
> 80–100 mm 315 MPa 470–630 MPa 19% 0°C, grade C
> 100–150 mm 295 MPa 450–600 MPa 18% 0°C, grade C
> 150–200 mm 285 MPa 450–600 MPa 17% 0°C, grade C

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at 0°C. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 355 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 355 MPa is about 51.5 ksi. ASTM A572 Gr.50 is 50 ksi and is not this book. SHH STEEL quotes the thickness band and the N condition on the offer.

Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the C letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 1591 Q355B GB/T 1591-2018 Hot rolled 355 MPa +20°C Different process
GB/T 1591 Q355C GB/T 1591-2018 Hot rolled 355 MPa 0°C Different process
GB/T 1591 Q355NB GB/T 1591-2018 Normalized 355 MPa +20°C Warmer N sister
Q355NC GB/T 1591-2018 Normalized 355 MPa 0°C This page
Q355MC GB/T 1591-2018 TMCP 355 MPa 0°C Different process
GB/T 1591 Q355D GB/T 1591-2018 Hot rolled 355 MPa −20°C Colder, not N
EN 10025-3 S355N EN 10025-3 Normalized 355 MPa −20°C Colder comparison
ASTM A572 Gr.50 ASTM A572 As rolled 345 MPa Different Lower yield

A 420 MPa hot-rolled file is GB/T 1591 Q420D or GB/T 1591 Q420E, not Q355NC. A 460 MPa file is GB/T 1591 Q460C.

Equivalent Material Grades

There is no official one-to-one substitute for Q355NC. What buyers compare is a 355 MPa normalized plate tested at 0°C.

EN 10025-3 S355N is the process comparison, but it is tested at −20°C. EN 10025-3 S355NL is colder. EN 10025-2 S355J0 matches the 0°C letter and does not match the N route. EN 10025-4 S355M is TMCP and closer to Q355MC. In the United States, ASTM A572 Gr.50 is 50 ksi / 345 MPa. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM490B is the usual comparison. SHH STEEL will not stamp EN 10025-3 S355N or ASTM A572 Gr.50 on a Q355NC certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q355NC China GB/T 1591-2018 Name on this page
GB/T 1591 Q355C China GB/T 1591-2018 Hot rolled, not this page
GB/T 1591 Q355NB China GB/T 1591-2018 Normalized, +20°C
Q355MC China GB/T 1591-2018 TMCP, not this page
GB/T 1591 Q355E China GB/T 1591-2018 Hot rolled, −40°C
EN 10025-3 S355N Europe EN 10025-3 Normalized, −20°C
EN 10025-2 S355J0 Europe EN 10025-2 0°C, not normalized
ASTM A572 Gr.50 USA ASTM A572 50 ksi, lower yield

Structural Service

Buyers pick Q355NC when a building, bridge member or welded fabrication wants about 355 MPa yield, a normalized or normalizing-rolled condition, and impact at 0°C. Search phrases such as Q355NC steel plate and GB/T 1591 Q355NC all point here.

It is the wrong plate when the drawing says hot rolled only. That work is GB/T 1591 Q355C. It is the wrong plate when the drawing says TMCP. That work is Q355MC. It is the wrong plate for a +20°C file. That work is GB/T 1591 Q355NB. It is the wrong plate for a −20°C file. That work is Q355ND, and the hot-rolled sister is GB/T 1591 Q355D. It is the wrong plate for a 420 MPa file. That work is GB/T 1591 Q420B or GB/T 1591 Q420E. It is the wrong plate for a 460 MPa file. That work is GB/T 1591 Q460D or GB/T 1591 Q460E. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade C, and the N condition at 355 MPa.

Weldability

Q355NC is a weldable normalized HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 can be a starting point on thin plate, but it is not a finished WPS for thick Q355NC. Carbon equivalent on the N route is not the same window as hot-rolled GB/T 1591 Q355C. A procedure qualified only at +20°C may miss the 0°C coupon.

Typical consumables are matching 50 ksi / 355 MPa low-hydrogen electrodes or wires. E7018-class electrodes are common on shop joints that do not need full plate strength in the weld metal. A procedure written for EN 10025-3 S355N is a useful process reference after the impact temperature is checked. Preheat follows thickness, hydrogen and the approved WPS. Thick plate and restrained joints need more preheat than a 10 mm web.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q355NC procedure on Q355MC without checking the TMCP carbon equivalent.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q355NC is normalized or normalizing rolled. The plate is not hot rolled as GB/T 1591 Q355C and not thermomechanical rolled as Q355MC.

Normalizing is typically about 880–920°C, followed by air cooling, unless the mill uses a normalizing-rolling route that the standard accepts for the N letter. Do not order Q355NC as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting.

The certificate lists GB/T 1591 Q355NC, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and 0°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-3 S355N is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q355NC steel plate:

  • Thickness: commonly 8 mm – 100 mm, heavier plate to 150 mm by enquiry
  • Width: 1500 mm – 3000 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q355NC follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q355NC plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 60 −0.6 +1.3
60 – 100 −0.7 +1.5

Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q355NC unless the order says so.

Supplementary Requirements

Q355NC already defines 355 MPa yield, normalized delivery and 0°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q355NC. Do not write only Q355, and do not write Q355C if the mill must stamp N.

Impact. Grade C is 0°C. Write a higher energy if the owner requires it. Do not expect a −20°C result unless the grade is changed to Q355ND.

Delivery condition. Write normalized or normalizing rolled. Write GB/T 1591 Q355C if hot rolled is enough. Write Q355MC if TMCP is required.

EN or US comparison. Write EN 10025-3 S355N or ASTM A572 Gr.50 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q355NC, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Buildings and workshops Q355NC columns, beams and base plates
Bridges and towers Q355NC webs and flanges from SHH STEEL
Construction machinery Q355NC frames where the drawing names N and 0°C
General fabrication Q355NC gussets and connection plates
Comparison vs EN 10025-3 Q355NC next to EN 10025-3 S355N
Comparison vs EN 10025-2 Q355NC next to EN 10025-2 S355J0
Higher yield option GB/T 1591 Q460C when 460 MPa is named

Q355NC is the plate for a 355 MPa normalized file tested at 0°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270.

Supply Capability

SHH STEEL sources Q355NC from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an N heat is in yard; standard normalizing about 30–45 days; 3.2 inspection about 40–50 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q355NC that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually normalize or normalizing-roll the heat, so the N is on the certificate and not only in the enquiry.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard N heat about 30–45 days, 3.2 inspection about 40–50 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q355NC, keep the normalized route, and do not ship GB/T 1591 Q355C or Q355MC as NC. We will not drop the N to save a furnace cycle, and we will not treat Q355NC as ASTM A36. If the drawing only needs hot-rolled plate, we will move the inquiry to Q355C and keep the price on the right condition.

FAQ

What is Q355NC steel plate?
Q355NC in GB/T 1591-2018 is normalized or normalizing-rolled high-strength low-alloy plate with 355 MPa minimum yield on thin plate and Charpy impact at 0°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q355NC the same as Q355C?
No. Both yield at 355 MPa and both are tested at 0°C. Q355C is hot rolled. Q355NC is normalized or normalizing rolled.
Is Q355NC the same as Q355NB?
No. Both are normalized. Q355NB is tested at +20°C. Q355NC is tested at 0°C.
Is Q355NC the same as Q355MC?
No. Q355NC is normalized. Q355MC is thermomechanical rolled. Impact letter C is the same temperature. The process is not.
What is the European equivalent of Q355NC?
The nearest process comparison is EN 10025-3 S355N, which is normalized but tested at −20°C. EN 10025-2 S355J0 is 0°C and is not an N grade. Dual mark only when both books are fully met.
What is the US equivalent of Q355NC?
There is no official ASTM twin. ASTM A572 Grade 50 is 50 ksi / 345 MPa, slightly lower, and it does not carry an NC letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
What thickness can SHH STEEL supply?
Common supply is 8 mm to 100 mm. Plate to 150 mm is quoted by enquiry. Yield on plate over 16 mm is lower than the 355 MPa thin-plate number.

Conclusion

Q355NC steel plate to GB/T 1591 is 355 MPa normalized structural plate with impact at 0°C. It is not hot-rolled GB/T 1591 Q355C and not TMCP Q355MC. The nearest European process comparison is EN 10025-3 S355N, and that grade is tested at −20°C. ASTM A572 Grade 50 is 345 MPa and is not a substitute. Whether the inquiry says Q355NC, GB/T 1591 Q355NC or Q355NC steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q355NC chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q355NC Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the N condition.

Contact SHH STEEL for mill rolling, normalized Q355NC, cutting, UT, 3.2 inspection or a worldwide quotation.

Q355NC, Q355NC steel plate, GB/T 1591 Q355NC, Q355NC plate, Q355NC supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *