JIS G3103 SB410 carbon steel boiler and pressure vessel plate, tensile 410–550 MPa, SHH STEEL

JIS G3103 SB410 Steel Plate | SB410 Boiler Vessel Plate supplier

JIS G3103 SB410 is Japanese carbon boiler and pressure-vessel plate. Tensile is 410–550 MPa and yield is 225 MPa min. Thickness is 6–200 mm. SHH STEEL supplies SB410 worldwide as a global steel mill sourcing partner.
Keywords
JIS G3103 SB410, SB410, SB410 steel plate, SB410 boiler plate, JIS G3103 SB410 equivalent, SB410 supplier, SB410 vessel plate
Equivalent Grades:
JIS G3103 SB410 / EN 10028-2 P235GH (near) / ASTM A285 Gr C / ASME SA285 Gr C / GB Q245R — Material Specification: JIS G3103 — Delivery: Normalized (N) or As-rolled (AR; thin section)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Boiler and Intermediate-Temperature Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is JIS G3103 SB410 Steel?

SB410 is the lowest carbon grade in JIS G3103. Buyers search JIS G3103 SB410, SB410 steel plate, SB410 boiler plate, SB410 vessel plate and SB410 supplier. The letters SB mean boiler plate. 410 is the tensile class in N/mm². This page is not SB450. SB450 is 450–590 MPa. This page is not SB480. SB480 is 480–620 MPa. This page is not SB450M or SB480M. Those two grades carry 0.45–0.60% Mo. This page is not JIS G3115 SPV315. G3115 is a different Japanese vessel book.

Tensile is 410–550 MPa. Yield is 225 MPa min. Thickness is 6–200 mm. Delivery is as-rolled up to 50 mm and normalized above 50 mm unless the order names another route. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against JIS G3103, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

If a drawing says SB450, we will not ship SB410 and call 410 close. If a drawing says ASME SA515 Grade 60, we will not stamp both names unless chemistry, tensile and delivery all fit.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade JIS G3103 SB410 Confirmed
Product specification JIS G3103 Applied
Steel type Killed carbon boiler / vessel plate Confirmed
Usual delivery As-rolled ≤50 mm; normalized >50 mm Confirmed
Tensile 410–550 MPa Confirmed
Yield 225 MPa min Confirmed
Thickness 6–200 mm Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and carbon steel plates. Japanese vessel sisters belong on JIS G3115. High-temp European carbon sisters belong on EN 10028-2. ASME high-temp carbon sisters belong on ASME SA515.

Chemical Composition

Cast analysis follows JIS G3103. Product analysis is supplied when ordered.

Cast Analysis and Product Analysis — JIS G3103 SB410

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), t ≤ 25 mm, max 0.24 0.26
Carbon (C), 25 < t ≤ 50 mm, max 0.27 0.29
Carbon (C), t > 50 mm, max 0.30 0.32
Silicon (Si) 0.15 – 0.40 0.13 – 0.45
Manganese (Mn), max 0.90 0.98
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.020 0.025
Copper (Cu), max 0.40 0.43
Nickel (Ni), max 0.40 0.43
Chromium (Cr), max 0.30 0.34
Molybdenum (Mo), max 0.12 0.15

JIS G3103 allows Mn to rise 0.06% for every 0.01% C drop, with Mn still capped at 1.50%. Cu + Ni + Cr + Mo is 1.00% max. Cr + Mo is 0.32% max. SB410 is carbon steel. It is not a molybdenum grade. If the file wants 0.45–0.60% Mo, the grade name is SB450M or SB480M. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search SB410 mechanical properties, SB410 yield strength and SB410 tensile strength.

Tensile and Yield — JIS G3103 SB410

Item Requirement
Yield / proof, min 225 MPa
Tensile 410 – 550 MPa
Elongation, 1A, t ≤ 40 mm, min 21%
Elongation, No.10, thicker plate, min 25%
Density 7.85 g/cm³

Bend test is 180°. Inside radius is 0.5t up to 25 mm and 0.75t from 25 to 50 mm. Do not quote 245 MPa yield on SB410. That number belongs to SB450. Do not treat 410–550 MPa as permission to stamp EN 10028-2 P235GH or Q245R steel plate without checking both books.

Material Comparison

Grade Book What buyers search Swap?
JIS G3103 SB410 JIS G3103 SB410 steel plate This page
JIS G3103 SB450 JIS G3103 SB450 No
JIS G3103 SB480 JIS G3103 SB480 No
JIS G3103 SB450M JIS G3103 SB450M No
JIS G3115 SPV315 JIS G3115 SPV315 No
EN 10028-2 P235GH EN 10028-2 P235GH No auto swap
ASME SA515 Grade 60 SA-515 SA515 Gr.60 No auto swap
ASTM A515 Grade 60 A515 A515 Gr.60 No auto swap
Q245R steel plate GB/T 713 Q245R No auto swap

Equivalent Material Grades

Designation Standard / region Notes
JIS G3103 SB410 JIS G3103 Name on this page
SB450 / SB480 JIS G3103 Higher carbon sisters
JIS G3115 SPV315 JIS G3115 Japanese vessel sister
EN 10028-2 P235GH EN 10028-2 High-temp carbon comparison
ASME SA515 Grade 60 SA-515 ASME high-temp carbon
ASTM A515 Grade 60 A515 ASTM high-temp carbon
ASME SA285 Grade C SA-285 Intermediate-tensile carbon
Q245R steel plate GB/T 713 Chinese vessel carbon
DIN 17102 StE255 DIN 17102 Fine-grain comparison

Boiler and Intermediate-Temperature Vessel Service

Buyers pick SB410 when a Japanese boiler or intermediate-temperature vessel file wants 410 MPa carbon plate. Search phrases such as SB410 boiler plate, JIS G3103 SB410 and SB410 vessel plate all point here.

It is not a substitute for EN 10028-2 16Mo3. That grade is 0.3Mo. It is not a substitute for ASME SA204 Grade A. That grade is molybdenum vessel steel. It is not a low-temperature plate. Low-temperature Japanese work belongs on other JIS books or on GB/T 713.3 16MnDR. Dual marking is possible only when both books are met.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

SB410 is killed carbon boiler plate. Treat welding as production welding, and as boiler / PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. Consumables must match the 410–550 MPa band. A procedure written for ASME SA516 Grade 70 may be heavy on strength. A Cr-Mo procedure written for ASME SA387 Grade 11 Class 1 is the wrong family. Preheat is usually light on thin plate and must follow the qualified WPS on thicker normalized plate. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL follows JIS G3103:

  • Thickness ≤ 50 mm: as-rolled. Normalizing or stress-relief may be added when ordered.
  • Thickness > 50 mm up to 200 mm: normalized, or heated uniformly during hot forming to give the same effect as normalizing.

This is not QT from EN 10028-6 P355Q. This is not TMCP from EN 10028-5.

If the vessel will see PWHT, say so. Simulated PWHT on test coupons is worth naming. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists JIS G3103 SB410; heat number; cast analysis; product analysis when ordered; tensile; bend; delivery condition. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for SB410 boiler vessel plate:

  • Thickness: 6 mm – 200 mm
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Mo boiler plate belongs on SB450M / SB480M. Japanese SPV plate belongs on JIS G3115 SPV315.

Tolerances

Dimensional limits for JIS G3103 SB410 follow JIS G3193 unless the purchase order names another table. Do not apply ASTM A36 structural tolerances to a boiler plate without writing them. When dual-named against ASME SA515 Grade 60, write whether JIS G3193 or SA-20 governs the minus on thickness.

Typical thickness tolerance idea for SB410 (JIS G3193 reference)

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
6 – 16 −0.4 +0.8
16 – 25 −0.5 +0.9
25 – 40 −0.6 +1.0
40 – 80 −0.8 +1.2
80 – 200 −1.0 +1.6

Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless the mill quote names a tighter extra. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows JIS G3193 unless a tighter class is written. Edge condition is mill edge or cut edge as ordered. If the vessel calculation used minimum thickness after corrosion, write the allowed minus on the RFQ. SHH STEEL will not assume a zero-minus extra on SB410 unless the order says so.

Supplementary Requirements

JIS G3103 SB410 already defines tensile, bend and the as-rolled / normalized split. Extra items still have to be written on the purchase order. SHH STEEL will not assume them from the grade name alone.

Elevated-temperature proof. JIS G3103 is a mid-to-high temperature boiler book. Write the test temperatures if the design needs Rp0.2 at 200–400 °C.

Charpy details. SB410 does not assume −20 °C or −40 °C. Write temperature, joules, location and orientation if impact is required.

Impact after simulated PWHT. When the boiler will be stress-relieved, name hold temperature, hold time and cooling rate on the coupon.

Product analysis. Especially C by thickness band, P, S, Mn, Cu, Ni, Cr and Mo.

Through-thickness / Z-test. Name Z15, Z25 or Z35 when the plate will be welded in the thickness direction.

NDE. JIS ultrasonic practice, EN 10160, ASTM A435 or ASTM A578 as named. Write scanning extent and acceptance class.

Hardness. If the destination file caps hardness after rolling or after simulated PWHT, write the max HB and the test location.

HIC / SSC / NACE. Only when the equipment is sour service. SB410 is not automatically NACE MR0175 / ISO 15156.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV, NK, KR or the inspector named. Hold points for normalizing, tensile, bend and UT should be listed on the ITP.

Identification and stamping. Heat number, grade SB410, JIS G3103, thickness and mill logo on each plate. Transfer marks after cutting if the plate will be cut before shipment.

Applications

Industry Typical components
Japanese boilers JIS G3103 SB410 drums and shells
Intermediate-temp vessels SB410 courses from SHH STEEL
Dual-certified export SB410 / ASME SA515 Grade 60 when both books fit
Comparison vs EN carbon SB410 next to EN 10028-2 P235GH

SB410 is the plate for a Japanese boiler file that wants 410 MPa carbon steel. It is the wrong plate for 0.5Mo service. That work is SB450M or SB480M. It is the wrong plate for high-strength QT. That work is EN 10028-6 P355Q.

Supply Capability

SHH STEEL sources JIS G3103 SB410 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement up to 200 mm.

Processing: CNC or flame cutting, bevel, flattening, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard rolling / normalizing about 45–60 days; simulated PWHT / 3.2 about 2 months.

Why Choose SHH STEEL

Experience on this grade is simple: keep the number after SB. 410, 450 and 480 are three different purchase orders, and none of them is SB450M. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices SB410 from first-line mills, reports JIS G3103 chemistry, records as-rolled or normalized by thickness, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. SB410 is not SB450. SB410 is not JIS G3115 SPV315. SB410 is not Q345R steel plate. If the drawing says SB480M, we will not ship SB410 and call carbon close.

FAQ

What is SB410 steel plate?
SB410 is a JIS G3103 carbon boiler and pressure-vessel plate. Tensile is 410–550 MPa and yield is 225 MPa min. Thickness is 6–200 mm. As-rolled is usual up to 50 mm. Normalizing is required above 50 mm. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of SB410?
Related comparisons are P235GH, SA-515 Grade 60, A515 Grade 60, SA-285 Grade C and Q245R. Dual marking is possible only when both books are fully met.
How is SB410 different from SB450 and SB480?
SB450 is 450–590 MPa with 245 MPa yield. SB480 is 480–620 MPa with 265 MPa yield. Same book, higher tensile class.
How is SB410 different from SB450M?
SB450M is a molybdenum boiler plate. SB410 is carbon steel. Do not ship SB410 against an Mo drawing.
How is SB410 different from SPV315?
SPV315 is JIS G3115. SB410 is JIS G3103. Same country, different vessel book.
Can SHH STEEL issue EN 10204 3.2 for SB410?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS, CCS, DNV, NK, KR or the inspector named on the order.

Conclusion

JIS G3103 SB410 Steel Plate is Japanese carbon boiler and pressure-vessel plate at 410–550 MPa tensile and 225 MPa yield. Whether the inquiry says JIS G3103 SB410, SB410 boiler plate, SB410 vessel plate or SB410 supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with SB410 chemistry, recorded as-rolled or normalized delivery, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies JIS G3103 SB410 Boiler Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

JIS G3103 SB410 Steel Plate, SB410 boiler vessel plate, SB410 supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response