JIS G3103 SB480 Steel Plate | SB480 Boiler Vessel Plate supplier
What is JIS G3103 SB480 Steel ?
SB480 is the highest carbon grade in JIS G3103. Buyers search JIS G3103 SB480, SB480 steel plate, SB480 boiler plate, SB480 vessel plate and SB480 supplier. The letters SB mean boiler plate. 480 is the tensile class in N/mm². This page is not SB410. SB410 is 410–550 MPa. This page is not SB450. SB450 is 450–590 MPa. This page is not SB480M. SB480M carries 0.45–0.60% Mo. This page is not JIS G3115 SPV410. G3115 is a different Japanese vessel book.
Tensile is 480–620 MPa. Yield is 265 MPa min. Thickness is 6–200 mm. Delivery is as-rolled up to 50 mm and normalized above 50 mm unless the order names another route. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against JIS G3103, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
If a drawing says SB450, we will not ship SB480 and call stronger automatically acceptable. If a drawing says SB480M, we will not ship SB480 and call 480 enough. Dual marking with ASME SA515 Grade 70 is possible only when both books are fully met.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | JIS G3103 SB480 | Confirmed |
| Product specification | JIS G3103 | Applied |
| Steel type | Killed carbon boiler / vessel plate | Confirmed |
| Usual delivery | As-rolled ≤50 mm; normalized >50 mm | Confirmed |
| Tensile | 480–620 MPa | Confirmed |
| Yield | 265 MPa min | Confirmed |
| Thickness | 6–200 mm | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and carbon steel plates. Japanese vessel sisters belong on JIS G3115. High-temp European carbon sisters belong on EN 10028-2. ASME high-temp carbon sisters belong on ASME SA515.
Chemical Composition
Cast analysis follows JIS G3103. Product analysis is supplied when ordered.
Cast Analysis and Product Analysis — JIS G3103 SB480
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), t ≤ 25 mm, max | 0.31 | 0.33 |
| Carbon (C), 25 < t ≤ 50 mm, max | 0.33 | 0.35 |
| Carbon (C), t > 50 mm, max | 0.35 | 0.37 |
| Silicon (Si) | 0.15 – 0.40 | 0.13 – 0.45 |
| Manganese (Mn), max | 1.20 | 1.28 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.020 | 0.025 |
| Copper (Cu), max | 0.40 | 0.43 |
| Nickel (Ni), max | 0.40 | 0.43 |
| Chromium (Cr), max | 0.30 | 0.34 |
| Molybdenum (Mo), max | 0.12 | 0.15 |
JIS G3103 allows Mn to rise 0.06% for every 0.01% C drop, with Mn still capped at 1.50%. Cu + Ni + Cr + Mo is 1.00% max. Cr + Mo is 0.32% max. SB480 is carbon steel. It is not a molybdenum grade. If the file wants 0.45–0.60% Mo, the grade name is SB480M. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search SB480 mechanical properties, SB480 yield strength and SB480 tensile strength.
Tensile and Yield — JIS G3103 SB480
| Item | Requirement |
|---|---|
| Yield / proof, min | 265 MPa |
| Tensile | 480 – 620 MPa |
| Elongation, 1A, t ≤ 40 mm, min | 17% |
| Elongation, No.10, thicker plate, min | 21% |
| Density | 7.85 g/cm³ |
Bend test is 180°. Inside radius is 1.00t up to 50 mm on the usual thin-plate class. Do not quote 245 MPa yield on SB480. That number belongs to SB450. Do not treat 480–620 MPa as permission to stamp EN 10028-2 P295GH or Q345R steel plate without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| JIS G3103 SB410 | JIS G3103 | SB410 steel plate | No |
| JIS G3103 SB450 | JIS G3103 | SB450 steel plate | No |
| JIS G3103 SB480 | JIS G3103 | SB480 steel plate | This page |
| JIS G3103 SB480M | JIS G3103 | SB480M | No |
| JIS G3115 SPV410 | JIS G3115 | SPV410 | No |
| EN 10028-2 P295GH | EN 10028-2 | P295GH | No auto swap |
| ASME SA515 Grade 70 | SA-515 | SA515 Gr.70 | No auto swap |
| ASTM A515 Grade 70 | A515 | A515 Gr.70 | No auto swap |
| Q345R steel plate | GB/T 713 | Q345R | No auto swap |
Equivalent Material Grades
| Designation | Standard / region | Notes |
|---|---|---|
| JIS G3103 SB480 | JIS G3103 | Name on this page |
| SB410 / SB450 | JIS G3103 | Lower carbon sisters |
| SB480M | JIS G3103 | 0.5Mo sister, not this page |
| JIS G3115 SPV410 | JIS G3115 | Japanese vessel sister |
| EN 10028-2 P295GH | EN 10028-2 | High-temp carbon comparison |
| ASME SA515 Grade 70 | SA-515 | ASME high-temp carbon |
| ASTM A515 Grade 70 | A515 | ASTM high-temp carbon |
| Q345R steel plate | GB/T 713 | Chinese vessel carbon |
| DIN 17102 StE315 | DIN 17102 | Fine-grain comparison |
Boiler and Intermediate-Temperature Vessel Service
Buyers pick SB480 when a Japanese boiler or intermediate-temperature vessel file wants 480 MPa carbon plate. Search phrases such as SB480 boiler plate, JIS G3103 SB480 and SB480 vessel plate all point here.
It is not a substitute for EN 10028-2 16Mo3. That grade is 0.3Mo. It is not a substitute for ASME SA204 Grade B. That grade is molybdenum vessel steel. It is not a low-temperature plate. Low-temperature work belongs on GB/T 713.3 16MnDR. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
SB480 Weldability
SB480 is killed carbon boiler plate at the top of the JIS G3103 carbon family. Treat welding as production welding, and as boiler / PED / ASME Code welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must match the 480–620 MPa band. A procedure written for ASME SA516 Grade 70 is a comparison only. A Cr-Mo procedure written for ASME SA387 Grade 11 Class 2 is the wrong family. Preheat must follow the qualified WPS, especially on thicker normalized plate. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL follows JIS G3103:
- Thickness ≤ 50 mm: as-rolled. Normalizing or stress-relief may be added when ordered.
- Thickness > 50 mm up to 200 mm: normalized, or heated uniformly during hot forming to give the same effect as normalizing.
This is not QT from EN 10028-6 P355Q. This is not TMCP from EN 10028-5.
If the vessel will see PWHT, say so. Simulated PWHT on test coupons is worth naming. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists JIS G3103 SB480; heat number; cast analysis; product analysis when ordered; tensile; bend; delivery condition. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for SB480 boiler vessel plate:
- Thickness: 6 mm – 200 mm
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Mo boiler plate belongs on SB450M / SB480M. Japanese SPV plate belongs on JIS G3115 SPV410.
Tolerances
Dimensional limits for JIS G3103 SB480 follow JIS G3193 unless the purchase order names another table. Do not apply ASTM A36 structural tolerances to a boiler plate without writing them. When dual-named against ASME SA515 Grade 70, write whether JIS G3193 or SA-20 governs the minus on thickness.
Typical thickness tolerance idea for SB480 (JIS G3193 reference)
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 6 – 16 | −0.4 | +0.8 |
| 16 – 25 | −0.5 | +0.9 |
| 25 – 40 | −0.6 | +1.0 |
| 40 – 80 | −0.8 | +1.2 |
| 80 – 200 | −1.0 | +1.6 |
Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless the mill quote names a tighter extra. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows JIS G3193 unless a tighter class is written. Edge condition is mill edge or cut edge as ordered. If the vessel calculation used minimum thickness after corrosion, write the allowed minus on the RFQ. SHH STEEL will not assume a zero-minus extra on SB480 unless the order says so.
Supplementary Requirements
JIS G3103 SB480 already defines tensile, bend and the as-rolled / normalized split. Extra items still have to be written on the purchase order. SHH STEEL will not assume them from the grade name alone.
Elevated-temperature proof. JIS G3103 is a mid-to-high temperature boiler book. Write the test temperatures if the design needs Rp0.2 at 200–400 °C.
Charpy details. SB480 does not assume −20 °C or −40 °C. Write temperature, joules, location and orientation if impact is required.
Impact after simulated PWHT. When the boiler will be stress-relieved, name hold temperature, hold time and cooling rate on the coupon.
Product analysis. Especially C by thickness band, P, S, Mn, Cu, Ni, Cr and Mo.
Through-thickness / Z-test. Name Z15, Z25 or Z35 when the plate will be welded in the thickness direction.
NDE. JIS ultrasonic practice, EN 10160, ASTM A435 or ASTM A578 as named. Write scanning extent and acceptance class.
Hardness. If the destination file caps hardness after rolling or after simulated PWHT, write the max HB and the test location.
HIC / SSC / NACE. Only when the equipment is sour service. SB480 is not automatically NACE MR0175 / ISO 15156.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV, NK, KR or the inspector named. Hold points for normalizing, tensile, bend and UT should be listed on the ITP.
Identification and stamping. Heat number, grade SB480, JIS G3103, thickness and mill logo on each plate. Transfer marks after cutting if the plate will be cut before shipment.
Applications
| Industry | Typical components |
|---|---|
| Japanese boilers | JIS G3103 SB480 drums and shells |
| Intermediate-temp vessels | SB480 courses from SHH STEEL |
| Dual-certified export | SB480 / ASME SA515 Grade 70 when both books fit |
| Comparison vs EN carbon | SB480 next to EN 10028-2 P295GH |
SB480 is the plate for a Japanese boiler file that wants 480 MPa carbon steel. It is the wrong plate for 0.5Mo service. That work is SB480M. It is the wrong plate for high-strength QT. That work is EN 10028-6 P355Q.
Supply Capability
SHH STEEL sources JIS G3103 SB480 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement up to 200 mm.
Processing: CNC or flame cutting, bevel, flattening, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days; standard rolling / normalizing about 45–60 days; simulated PWHT / 3.2 about 2 months.
Why Choose SHH STEEL
Experience on this grade is simple: keep the number after SB. 410, 450 and 480 are three different purchase orders, and none of them is SB480M. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices SB480 from first-line mills, reports JIS G3103 chemistry, records as-rolled or normalized by thickness, and issues 3.1 as standard or 3.2 when specified.
We keep the grade on the order. SB480 is not SB450. SB480 is not SB480M. SB480 is not JIS G3115 SPV410. SB480 is not Q245R steel plate. If the drawing says SB450M, we will not ship SB480 and call carbon close.
FAQ
-
What is SB480 steel plate?
- SB480 is a JIS G3103 carbon boiler and pressure-vessel plate. Tensile is 480–620 MPa and yield is 265 MPa min. Thickness is 6–200 mm. As-rolled is usual up to 50 mm. Normalizing is required above 50 mm. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
What is the equivalent of SB480?
- Related comparisons are P295GH, SA-515 Grade 70, A515 Grade 70 and Q345R. Dual marking is possible only when both books are fully met.
-
How is SB480 different from SB410 and SB450?
- SB410 is 410–550 MPa with 225 MPa yield. SB450 is 450–590 MPa with 245 MPa yield. Same book, lower tensile class.
-
How is SB480 different from SB480M?
- SB480M is a molybdenum boiler plate. SB480 is carbon steel. Do not ship SB480 against an Mo drawing.
-
How is SB480 different from SPV410?
- SPV410 is JIS G3115. SB480 is JIS G3103. Same country, different vessel book.
-
Can SHH STEEL ship SB480 to the USA, Europe or the Middle East?
- Yes. SHH STEEL quotes FOB Shanghai and CIF to US West, US Gulf, Rotterdam, Jebel Ali, Singapore and other major ports.
-
What is the delivery time for SB480?
- Ex-stock about 5–7 days when plate is in yard. Standard mill rolling about 45–60 days. Simulated PWHT or 3.2 inspection about 2 months.
Conclusion
JIS G3103 SB480 Steel Plate is Japanese carbon boiler and pressure-vessel plate at 480–620 MPa tensile and 265 MPa yield. Whether the inquiry says JIS G3103 SB480, SB480 boiler plate, SB480 vessel plate or SB480 supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with SB480 chemistry, recorded as-rolled or normalized delivery, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies JIS G3103 SB480 Boiler Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
JIS G3103 SB480 Steel Plate, SB480 boiler vessel plate, SB480 supplier, SHH STEEL