GOST 22178 VT6S Titanium Sheet | Ti-6Al-4V Variant (BT6S)
What is GOST 22178 VT6S titanium sheet?
GOST 22178 VT6S titanium sheet is made to GOST 22178, the interstate standard for sheets of titanium and titanium alloys. VT6S (BT6S) is a Ti-6Al-4V variant with tighter aluminium and vanadium ranges and lower oxygen (0.15% max). It is more ductile and better suited to welding and forming than VT6, with somewhat lower annealed strength.
This is an alpha-beta titanium alloy. Aluminium strengthens the alpha phase and vanadium or molybdenum stabilises the beta phase, so the structure and properties depend on hot working and heat treatment. Plate is normally supplied mill annealed, giving high strength, good fatigue performance and a strength-to-weight ratio well above that of steels.
Its typical density of about 4.43 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Russian designations follow the original VT (BT in Cyrillic) and OT naming. VT1-00 and VT1-0 are unalloyed titanium, OT4 grades are Ti-Al-Mn alloys, and VT5-1, VT6, VT14 and VT20 are structural alloys used widely in aerospace sheet work.
SHH STEEL handles VT6S sheet enquiries within its range of titanium alloy plates and sheets, checking the ordered GOST 22178 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 23, ASME SB-265 Grade 23, JIS H4600 Class 60E TAP6400E.
Material specification for GOST 22178 VT6S
GOST 22178 is the interstate standard for sheets of titanium and titanium alloys. It covers sheets from 0.3 to 10.5 mm thick, sets sizes, tolerances, surface quality groups and mechanical properties, and refers chemical composition to GOST 19807 or OST 1 90013. Because the standard covers sheet, this page uses the term titanium sheet.
| Ordering item | GOST 22178 basis |
|---|---|
| Standard | GOST 22178-76 with its amendments; state the revision required |
| Grade | VT6S (Ti-6Al-4V Variant (BT6S)) |
| Size range for this grade | 1.0–10.5 mm thick |
| Condition | Annealed; quenched-and-aged test samples on request |
| Surface finish | Ordinary or high surface finish; improved flatness on request |
| Designation example | Sheet VT6S 5 × 1000 × 1500 GOST 22178-76 |
| Certificate | Quality document with chemistry and test results |
Width and length tolerances are plus-only: up to +10 mm on width for sheets up to 1500 mm long and up to +20 mm on length for sheets up to 2000 mm long. Order the grade, thickness, width, length, surface finish group and flatness class.
Many Russian aerospace orders cite OST 1 90013 for chemistry or add supplementary technical conditions to GOST 22178. If the drawing names such documents, list them on the order, because they can change impurity limits, test frequency and acceptance criteria. When sheet is bought for use outside the CIS, agree in advance whether a GOST certificate alone is acceptable or a cross-reference to another standard is required.
Chemical composition of GOST 22178 VT6S
Composition follows GOST 19807 for the grade. Single values are maximums; titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.04 max |
| Carbon (C) | 0.10 max |
| Hydrogen (H) | 0.015 max |
| Iron (Fe) | 0.25 max |
| Oxygen (O) | 0.15 max |
| Aluminium (Al) | 5.3–6.5 |
| Vanadium (V) | 3.5–4.5 |
| Zirconium (Zr) | 0.30 max |
| Silicon (Si) | 0.15 max |
| Other impurities, total | 0.30 max |
| Titanium (Ti) | Balance |
Alloying ranges are wider than in some Western specifications, so a sheet can meet GOST 19807 and still fall outside another standard’s range. Where an order cites both GOST and another standard, both sets of limits must be satisfied.
Mechanical properties of GOST 22178 VT6S
The values below are the requirements for VT6S sheet in the annealed condition.
| Sheet thickness, mm (condition) | Tensile strength, MPa | Elongation, min, % |
|---|---|---|
| 1.0–6.0 (annealed) | 835 min | 12 |
| >6.0–10.5 (annealed) | 835 min | 10 |
| 1.0–10.5 (quenched and aged samples) | 980 min | 8 |
GOST 22178 sets minimum tensile strength and elongation; yield strength is not specified and can be agreed separately. Tests are made on transverse specimens. The bend test is made around a mandrel, and the sheet must reach the minimum angle below without cracks.
| Sheet thickness, mm | Bend angle, min |
|---|---|
| 1.0–1.8 | 30° |
| >1.8–6.5 | 40° |
| >6.5–10.5 | 50° |
Where sheets are quenched and aged, the properties of heat-treated samples are agreed when ordering.
Delivery condition, finish and marking
GOST 22178 sheets are supplied with an ordinary or high surface finish. Light dressing of surface defects is allowed within the depth limits of the standard, and the angles of the sheet must stay within the flatness requirement for the ordered class.
- Condition: Annealed; quenched-and-aged test samples on request
- Surface: ordinary or high surface finish group, as ordered
- Flatness: normal or improved, as ordered
- Marking and packing: grade, heat, sheet size and standard number, with protection for transport
Plate is supplied annealed. Solution treating and ageing, where wanted, is normally done on the part and its properties are agreed separately. Mechanical tests are made on 10% of the sheets in a lot, but not fewer than one sheet, and the lot is accepted or retested on the results.
Welding and fabrication of VT6S titanium sheet
VT6S can be welded by gas tungsten arc, plasma arc, electron beam and laser processes, but it needs more control than CP titanium.
- Shield the weld, heat-affected zone and root with inert gas until below about 400 °C
- Use qualified procedures and matching or engineer-approved filler metal
- Expect lower weld-zone ductility than in the base plate; stress relief after welding is common
- Clean joints thoroughly and avoid iron contamination
Cold formability is limited. Most forming of alpha-beta plate is done hot or by creep forming, and machining needs sharp tools, rigid set-ups and generous coolant.
Plan machining around the low thermal conductivity of the alloy: heat stays at the tool edge, so cutting speeds are low and coolant flow is high. Avoid interrupted light cuts that work-harden the surface, and keep fine chips away from ignition sources.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
GOST 22178 sets thickness tolerances in Table 1 by thickness and width, and flatness and corner-gap limits in Table 5 by grade and flatness class. Width tolerance is up to +10 mm for sheets up to 1500 mm long and +15 mm above that; length tolerance is +20 mm up to 2000 mm and +25 mm above.
Order the thickness, width, length, surface finish group and flatness class. Theoretical sheet mass is based on 4.50 g/cm³ for VT1-00 and VT1-0, with conversion factors for the alloys. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of VT6S titanium sheet
Typical uses of VT6S sheet include:
- Welded high-strength structures
- Pressure vessels and tanks
- Formed sheet parts
- Cryogenic and marine components
Alpha-beta alloys resist seawater and many oxidizing media well, but they are less resistant than CP titanium in hot reducing acids. They are not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. Maximum service temperature and fatigue design values come from the applicable design code, not from the plate specification.
When selecting VT6S, compare it with VT5-1, VT6, VT14. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare VT6S with other GOST 22178 grades
The grades below are the closest neighbours of VT6S in GOST 22178. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| VT5-1 | 735 MPa min (>1.8–6.0 mm) | — | 10% | Ti-5Al-2.5Sn alpha alloy |
| VT6 | 885 MPa min (1.0–10.5 mm) | — | 8% | Ti-6Al-4V alpha-beta |
| VT6S | 835 MPa min (1.0–6.0 mm) | — | 12% | Ti-6Al-4V lower-interstitial variant |
| VT14 | 885 MPa min (0.8–5.0 mm) | — | 8% | Ti-4.5Al-3Mo-1V heat-treatable |
| VT20 | 930 MPa min (>1.8–4.0 mm) | — | 10% | Ti-6Al-2Zr-1Mo-1V near-alpha |
A higher strength level is not automatically better. Interstitial limits, toughness, bend radius and fatigue behaviour differ between grades, so changes need engineer approval.
GOST 22178 VT6S equivalent grades
The designations below are commonly compared with GOST 22178 VT6S. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to GOST 22178 VT6S |
|---|---|---|
| ASTM B265 | Grade 23 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 23 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| JIS H4600 | Class 60E (TAP6400E) | Close equivalent; JIS strength range and tests differ |
| GB/T 3621 | TC4ELI | Close equivalent; confirm grade name and limits in the ordered edition |
| UNS | R56407 | Same unified number as ASTM Grade 23 |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for VT6S titanium sheet
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to GOST 22178 VT6S sheet with the surface finish group and flatness you need
- Certificates are checked against GOST 19807 chemistry, tensile strength, elongation and bend angle
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for GOST 22178 VT6S sheet
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | GOST 22178 VT6S, revision |
| Product form | Sheet 0.3–10.5 mm; surface finish group and flatness class |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Bend test, any quenched-and-aged tests where applicable |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Why is GOST 22178 VT6S called sheet rather than plate?
- GOST 22178 covers sheets from 0.3 to 10.5 mm thick. Thicker plate in Russian grades is ordered to other GOST or OST documents, so this page uses the term sheet.
-
What is the tensile strength of GOST 22178 VT6S titanium sheet?
- The requirement is 835 MPa minimum. Minimum elongation is 12%. Values apply to the condition and thickness range stated in the standard.
-
What is VT6S mainly used for?
- Typical uses include welded high-strength structures, pressure vessels and tanks and formed sheet parts. The design engineer should confirm the grade for the actual service.
-
What thickness range applies to GOST 22178 VT6S?
- For this grade the standard lists 1.0–10.5 mm thick. Width and length depend on thickness, so confirm the full sheet size against the standard's size table when ordering.
-
What should I send for a quotation?
- Send GOST 22178 VT6S, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for GOST 22178 VT6S titanium sheet
GOST 22178 VT6S is Ti-6Al-4V variant (BT6S) titanium alloy specified for 835 MPa minimum tensile strength and 12% minimum elongation in the annealed condition. Typical uses include welded high-strength structures and pressure vessels and tanks.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GOST 22178 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com