GOST 22178 VT14 Titanium Sheet | Ti-Al-Mo-V Alloy (BT14)

GOST 22178 VT14 titanium sheet is Ti-Al-Mo-V alloy (BT14) supplied annealed. It is specified for 885 MPa minimum tensile strength and 8% minimum elongation. Typical uses include high-strength formed sheet parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
GOST 22178 VT14 titanium sheet, VT14 titanium sheet, Ti-Al-Mo-V alloy (BT14) sheet, GOST 22178 titanium plate, GOST 22178 VT14 titanium strip
Equivalent Grades:
GOST VT6 (nearest by role)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GOST 22178 VT14 titanium sheet?

GOST 22178 VT14 titanium sheet is made to GOST 22178, the interstate standard for sheets of titanium and titanium alloys. VT14 is a Ti-Al-Mo-V alpha-beta alloy (about 4% aluminium in sheet, 3% molybdenum, 1% vanadium) that can be strengthened by quenching and ageing well above its annealed strength.

This is an alpha-beta titanium alloy. Aluminium strengthens the alpha phase and vanadium or molybdenum stabilises the beta phase, so the structure and properties depend on hot working and heat treatment. Plate is normally supplied mill annealed, giving high strength, good fatigue performance and a strength-to-weight ratio well above that of steels.

Its typical density of about 4.52 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Russian designations follow the original VT (BT in Cyrillic) and OT naming. VT1-00 and VT1-0 are unalloyed titanium, OT4 grades are Ti-Al-Mn alloys, and VT5-1, VT6, VT14 and VT20 are structural alloys used widely in aerospace sheet work.

SHH STEEL handles VT14 sheet enquiries within its range of titanium alloy plates and sheets, checking the ordered GOST 22178 edition, product form and certificate type before confirming supply. Related designations covered on this site include GOST 22178 VT6.

Material specification for GOST 22178 VT14

GOST 22178 is the interstate standard for sheets of titanium and titanium alloys. It covers sheets from 0.3 to 10.5 mm thick, sets sizes, tolerances, surface quality groups and mechanical properties, and refers chemical composition to GOST 19807 or OST 1 90013. Because the standard covers sheet, this page uses the term titanium sheet.

Ordering item GOST 22178 basis
Standard GOST 22178-76 with its amendments; state the revision required
Grade VT14 (Ti-Al-Mo-V Alloy (BT14))
Size range for this grade 0.8–10.5 mm thick
Condition Annealed; quenched-and-aged test samples on request
Surface finish Ordinary or high surface finish; improved flatness on request
Designation example Sheet VT14 5 × 1000 × 1500 GOST 22178-76
Certificate Quality document with chemistry and test results

Width and length tolerances are plus-only: up to +10 mm on width for sheets up to 1500 mm long and up to +20 mm on length for sheets up to 2000 mm long. Order the grade, thickness, width, length, surface finish group and flatness class.

Many Russian aerospace orders cite OST 1 90013 for chemistry or add supplementary technical conditions to GOST 22178. If the drawing names such documents, list them on the order, because they can change impurity limits, test frequency and acceptance criteria. When sheet is bought for use outside the CIS, agree in advance whether a GOST certificate alone is acceptable or a cross-reference to another standard is required.

Chemical composition of GOST 22178 VT14

Composition follows GOST 19807 for the grade. Single values are maximums; titanium is the balance.

Element Limit, %
Nitrogen (N) 0.05 max
Carbon (C) 0.10 max
Hydrogen (H) 0.015 max
Iron (Fe) 0.25 max
Oxygen (O) 0.15 max
Aluminium (Al) 3.5–4.5 (flat products up to 10 mm)
Vanadium (V) 0.9–1.9
Zirconium (Zr) 0.30 max
Molybdenum (Mo) 2.5–3.8
Silicon (Si) 0.15 max
Other impurities, total 0.30 max
Titanium (Ti) Balance

Alloying ranges are wider than in some Western specifications, so a sheet can meet GOST 19807 and still fall outside another standard’s range. Where an order cites both GOST and another standard, both sets of limits must be satisfied.

Mechanical properties of GOST 22178 VT14

The values below are the requirements for VT14 sheet in the annealed condition.

Sheet thickness, mm (condition) Tensile strength, MPa Elongation, min, %
0.8–5.0 (annealed) 885 min 8
>5.0–10.5 (annealed) 835 min 8
0.8–1.5 (quenched and aged) 1080 min 5
>1.5–5.0 (quenched and aged) 1180 min 6
>5.0–7.0 (quenched and aged) 1080 min 4
>7.0–10.5 (quenched and aged) 1100 min 4

GOST 22178 sets minimum tensile strength and elongation; yield strength is not specified and can be agreed separately. Tests are made on transverse specimens. The bend test is made around a mandrel, and the sheet must reach the minimum angle below without cracks.

Sheet thickness, mm Bend angle, min
0.8–1.5 60°
>1.5–3.5 40°
>3.5–10.5 30°

Where sheets are quenched and aged, the properties of heat-treated samples are agreed when ordering.

Delivery condition, finish and marking

GOST 22178 sheets are supplied with an ordinary or high surface finish. Light dressing of surface defects is allowed within the depth limits of the standard, and the angles of the sheet must stay within the flatness requirement for the ordered class.

  • Condition: Annealed; quenched-and-aged test samples on request
  • Surface: ordinary or high surface finish group, as ordered
  • Flatness: normal or improved, as ordered
  • Marking and packing: grade, heat, sheet size and standard number, with protection for transport

Plate is supplied annealed. Solution treating and ageing, where wanted, is normally done on the part and its properties are agreed separately. Mechanical tests are made on 10% of the sheets in a lot, but not fewer than one sheet, and the lot is accepted or retested on the results.

Welding and fabrication of VT14 titanium sheet

VT14 can be welded by gas tungsten arc, plasma arc, electron beam and laser processes, but it needs more control than CP titanium.

  • Shield the weld, heat-affected zone and root with inert gas until below about 400 °C
  • Use qualified procedures and matching or engineer-approved filler metal
  • Expect lower weld-zone ductility than in the base plate; stress relief after welding is common
  • Clean joints thoroughly and avoid iron contamination

Cold formability is limited. Most forming of alpha-beta plate is done hot or by creep forming, and machining needs sharp tools, rigid set-ups and generous coolant.

Plan machining around the low thermal conductivity of the alloy: heat stays at the tool edge, so cutting speeds are low and coolant flow is high. Avoid interrupted light cuts that work-harden the surface, and keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

GOST 22178 sets thickness tolerances in Table 1 by thickness and width, and flatness and corner-gap limits in Table 5 by grade and flatness class. Width tolerance is up to +10 mm for sheets up to 1500 mm long and +15 mm above that; length tolerance is +20 mm up to 2000 mm and +25 mm above.

Order the thickness, width, length, surface finish group and flatness class. Theoretical sheet mass is based on 4.50 g/cm³ for VT1-00 and VT1-0, with conversion factors for the alloys. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of VT14 titanium sheet

Typical uses of VT14 sheet include:

  • High-strength formed sheet parts
  • Heat-treated aerospace structures
  • Pressure vessels
  • Fasteners and fittings

Alpha-beta alloys resist seawater and many oxidizing media well, but they are less resistant than CP titanium in hot reducing acids. They are not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. Maximum service temperature and fatigue design values come from the applicable design code, not from the plate specification.

When selecting VT14, compare it with VT5-1, VT6, VT6S. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare VT14 with other GOST 22178 grades

The grades below are the closest neighbours of VT14 in GOST 22178. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
VT5-1 735 MPa min (>1.8–6.0 mm) — 10% Ti-5Al-2.5Sn alpha alloy
VT6 885 MPa min (1.0–10.5 mm) — 8% Ti-6Al-4V alpha-beta
VT6S 835 MPa min (1.0–6.0 mm) — 12% Ti-6Al-4V lower-interstitial variant
VT14 885 MPa min (0.8–5.0 mm) — 8% Ti-4.5Al-3Mo-1V heat-treatable
VT20 930 MPa min (>1.8–4.0 mm) — 10% Ti-6Al-2Zr-1Mo-1V near-alpha

A higher strength level is not automatically better. Interstitial limits, toughness, bend radius and fatigue behaviour differ between grades, so changes need engineer approval.

GOST 22178 VT14 equivalent grades

The designations below are commonly compared with GOST 22178 VT14. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to GOST 22178 VT14
GOST 22178 VT6 Nearest by role only; composition and properties differ
ASTM / GB No direct grade Heat-treatable Ti-Al-Mo-V alloy; nearest by role only

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for VT14 titanium sheet

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to GOST 22178 VT14 sheet with the surface finish group and flatness you need
  • Certificates are checked against GOST 19807 chemistry, tensile strength, elongation and bend angle
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for GOST 22178 VT14 sheet

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material GOST 22178 VT14, revision
Product form Sheet 0.3–10.5 mm; surface finish group and flatness class
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Bend test, any quenched-and-aged tests where applicable
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Why is GOST 22178 VT14 called sheet rather than plate?
GOST 22178 covers sheets from 0.3 to 10.5 mm thick. Thicker plate in Russian grades is ordered to other GOST or OST documents, so this page uses the term sheet.
What is the tensile strength of GOST 22178 VT14 titanium sheet?
The requirement is 885 MPa minimum. Minimum elongation is 8%. Values apply to the condition and thickness range stated in the standard.
What is VT14 mainly used for?
Typical uses include high-strength formed sheet parts, heat-treated aerospace structures and pressure vessels. The design engineer should confirm the grade for the actual service.
What thickness range applies to GOST 22178 VT14?
For this grade the standard lists 0.8–10.5 mm thick. Width and length depend on thickness, so confirm the full sheet size against the standard's size table when ordering.
What should I send for a quotation?
Send GOST 22178 VT14, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for GOST 22178 VT14 titanium sheet

GOST 22178 VT14 is Ti-Al-Mo-V alloy (BT14) specified for 885 MPa minimum tensile strength and 8% minimum elongation in the annealed condition. Typical uses include high-strength formed sheet parts and heat-treated aerospace structures.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GOST 22178 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X