GB/T 3280 022Cr17Ni12Mo2 S31603 Cold Rolled Stainless Steel Plate at SHH STEEL warehouse

GB/T 3280 022Cr17Ni12Mo2 S31603 Cold Rolled Stainless Steel Plate

GB/T 3280 022Cr17Ni12Mo2 S31603 Cold Rolled Stainless Steel Plate: austenitic grade to GB/T 3280-2015, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
GB/T 3280 022Cr17Ni12Mo2 sheet, 022Cr17Ni12Mo2 sheet, 022Cr17Ni12Mo2 stainless sheet supplier, GB/T 3280-2015 022Cr17Ni12Mo2, 022Cr17Ni12Mo2 sheet stock China
Equivalent Grades:
UNS S31603; EN 1.4404 X2CrNiMo17-12-2; JIS SUS316L
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is GB/T 3280 022Cr17Ni12Mo2 S31603 Cold Rolled Stainless Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: 022Cr17Ni12Mo2 (S31603) ≈ UNS S31603 ≈ EN 1.4404 X2CrNiMo17-12-2 ≈ JIS SUS316L.

022Cr17Ni12Mo2 (S31603) is a austenitic grade. 022Cr17Ni12Mo2 is the low-carbon 316L version, the standard grade for welded equipment in chloride service.

GB/T 3280-2015 is the Chinese national standard for cold-rolled stainless steel plate, sheet and strip. It is the cold-rolled counterpart of GB/T 4237 (hot rolled) and uses the same grade names and unified numeric codes (ISC) from GB/T 20878. Cold-rolled sheet is the normal product for thin gauges with 2B, BA or polished finishes.

This page sets out the GB/T 3280-2015 requirements for 022Cr17Ni12Mo2 (S31603) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

022Cr17Ni12Mo2 (S31603) sheet: specification summary

Item 022Cr17Ni12Mo2 (S31603) data
Standard GB/T 3280-2015, cold-rolled stainless steel plate, sheet and strip
Product form cold-rolled plate, sheet and strip
Typical thickness 0.3–6.0 mm
Widths 1000, 1219, 1250, 1500 mm; slit coil to order
Lengths 2000, 2438, 2500, 3000 mm or cut to size
Finishes 2D, 2B, BA, No.3, No.4, HL
Heat treatment solution treated (austenitic, duplex) or annealed (ferritic)
Tests chemical analysis, tensile, hardness; bend and intergranular corrosion (GB/T 4334) where specified
Certificates mill certificate to GB/T 18253 (EN 10204 3.1 type); 3.2 on request
Grade family austenitic

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. 022Cr17Ni12Mo2 (S31603) is one of the high-volume grades produced by most Chinese stainless mills, so common sizes are held in stock and non-stock sizes are usually rolled within a normal mill cycle.

Chemical composition of 022Cr17Ni12Mo2 (S31603) (GB/T 3280-2015)

Element wt %
C 0.03 max
Si 0.75 max
Mn 2 max
P 0.045 max
S 0.03 max
Cr 16–18
Ni 10–14
Mo 2–3
N 0.1 max

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 22.6 at the specification minimums and about 26.1 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of 022Cr17Ni12Mo2 (S31603) sheet

Rp0.2 min, MPa Rm min, MPa A min, % HBW max HRB max HV max
180 485 40 217 95 220

The minimum yield strength of 180 MPa is about 1.1 times the 170 MPa minimum of ASTM 316L. Annealed austenitic and 200-series material work-hardens quickly, so cold-formed parts are stronger than these minimums. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

Corrosion resistance of 022Cr17Ni12Mo2 (S31603): PREN and limits

Austenitic stainless steels are non-hardenable by heat treatment, tough down to cryogenic temperatures and easy to form and weld. Corrosion resistance rises with chromium, molybdenum and nitrogen; the PREN of this grade at the specification minimum is about 22.6. Low-carbon (L) and stabilised versions protect welds against intergranular corrosion.

Austenitic grades are prone to chloride stress-corrosion cracking above about 60 °C in chloride environments. Where that risk exists, duplex or super-austenitic grades are the usual upgrade. Cold work raises strength but also makes some grades slightly magnetic.

How 022Cr17Ni12Mo2 (S31603) compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
022Cr17Ni12Mo2 (S31603) 16–18 10–14 2–3 0.1 max 22.6 180
06Cr19Ni10 (S30408) 17.5–19.5 8–10.5 — 0.1 max 17.5 205
022Cr19Ni10 (S30403) 17.5–19.5 8–12 — 0.1 max 17.5 180
06Cr17Ni12Mo2 (S31608) 16–18 10–14 2–3 0.1 max 22.6 205
06Cr18Ni11Ti (S32168) 17–19 9–12 — 0.1 max 17.0 205

Choose 022Cr17Ni12Mo2 (S31603) for general corrosion resistance with easy forming and welding. In warm chloride environments consider a molybdenum-bearing or duplex grade instead.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of 022Cr17Ni12Mo2 (S31603)

Heat treatment: ≥ 1 040 °C, water quench or other rapid cooling.

Austenitic grades are solution annealed and cooled rapidly to keep carbides in solution. They cannot be hardened by heat treatment, only by cold work.

Surface finishes for 022Cr17Ni12Mo2 (S31603) sheet

GB/T 3280 sheet is supplied in cold-rolled finishes: 2D (dull, for deep drawing), 2B (skin passed, the general-purpose finish), BA (bright annealed), and polished No.3, No.4 or HL (hairline). Decorative finishes and PVC or laser film are available. State the finish and film side on the order.

Dimensions, tolerances and flatness

Thickness, width, length and flatness tolerances are tabulated in GB/T 3280, with normal and higher precision classes. For laser-cut blanks, specify flatness and, if needed, tension-levelled sheet. Coil slit to width keeps edge camber low.

Chinese grade names and codes. GB/T 3280 uses the GB/T 20878 grade names, which spell out the composition (carbon in hundredths of a percent followed by alloying elements), and the unified numeric code (ISC) such as S31603. GB/T 20878-2024 renamed a few grades, so a certificate may show either the 2007 or the 2024 form; the ISC code is the safest identifier. Order with both the grade name and the code, the finish, the thickness tolerance class and the certificate type. Export orders often also ask for the ASTM or JIS designation on the certificate as a reference only.

022Cr17Ni12Mo2 (S31603) sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 300+ t China
0.8 1219 2438 2B 300+ t China
1.0 1219 / 1250 2438 / 2500 2B 300+ t China
1.5 1219 / 1500 2438 / 3000 2B 200+ t China
2.0 1219 / 1500 2438 / 3000 2B 200+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

022Cr17Ni12Mo2 (S31603) equivalents in other standards

Standard Designation Comment
ASTM / UNS UNS S31603 same alloy family and limits closely matched; compare each limit on the certificate
EN 1.4404 X2CrNiMo17-12-2 same alloy family and limits closely matched; compare each limit on the certificate
JIS SUS316L same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Austenitic

General-purpose austenitic grades for comparison: A240 S30400, A240 S30403, A240 S31600, A240 S30500, A240 S32100, A240 S30100, 1.4301 plate, 1.4307 plate.

Same standard

Other grades in this standard: GB/T 3280 S35350, GB/T 3280 S35450, GB/T 3280 S30408.

Same grade, other specification

GB/T 4237 S31603.

Applications, forming and welding of 022Cr17Ni12Mo2 (S31603)

Typical uses: pharmaceutical and semiconductor equipment, chemical tanks, marine equipment, and heat exchangers.

Austenitic sheet and plate form and weld easily. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L, ER316L or ER347 filler matching the grade (AWS A5.9). Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Austenitic sheet is welded with GTAW, GMAW, SMAW or laser without preheat. Keep the interpass temperature below about 150 °C, use back-purging on corrosion-critical joints and pickle afterwards. Low-carbon or stabilised grades avoid sensitisation; standard-carbon grades used at temperature may need a solution anneal after heavy welding.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to GB/T 3280-2015 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A262 Practice E or EN ISO 3651-2 / GB/T 4334), PMI and surface inspection. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying 022Cr17Ni12Mo2 (S31603)

  • Mixing L and standard-carbon grades in welded equipment.
  • Leaving out the finish and film side for visible parts.
  • Using the grade in warm chlorides where stress-corrosion cracking is likely.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing 022Cr17Ni12Mo2 (S31603): buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Mixed-up 304/316 or L/non-L grades PMI and heat-number tracking for every sheet
Surface scratches on finished sheet PVC film, interleaving paper and wooden-case packing
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order 022Cr17Ni12Mo2 (S31603) sheet

State the standard and edition (GB/T 3280-2015), the grade (022Cr17Ni12Mo2 (S31603)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

What is the difference between GB/T 3280 and GB/T 4237 022Cr17Ni12Mo2?
GB/T 3280 covers cold-rolled plate, sheet and strip; GB/T 4237 covers hot-rolled material. The grade names and chemistry are the same, but thickness ranges, finishes and tolerances differ.
Is 022Cr17Ni12Mo2 (S31603) equivalent to UNS S31603?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Is 022Cr17Ni12Mo2 (S31603) magnetic?
It is essentially non-magnetic when annealed; cold work can make it slightly magnetic.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

022Cr17Ni12Mo2 (S31603) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X