EN 10217-7 1.4436 Welded Stainless Steel Tube
What is EN 10217-7 1.4436 Welded Stainless Steel Tube
European pressure equipment that needs circular welded stainless tube looks to EN 10217-7:2021 (BS EN 10217-7:2021), Part 7 of the EN 10217 series — not to a seamless Part 5 page and not to an ASTM tubing habit. Steel number 1.4436 is listed as X3CrNiMo17-13-3 in the austenitic tables. Buyers still say “316 (higher Mo)” on the shop floor, yet that commercial alias does not select cast chemistry, longitudinal weld route, delivery-condition heat treatment, or TC1/TC2. The purchase order has to name EN 10217-7, 1.4436, the test category, and the delivery-condition / options list so the mill applies the correct analysis, seam procedure, solution treatment where required, mechanical floors, leak-tightness, and marking. This number’s job on welded pressure duty is: mid-carbon higher-Mo austenitic welded pressure tube parallel to commercial 316 with Mo pushed toward 2.5–3%.
SHH STEEL can produce and supply EN 10217-7 1.4436 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover process welded OD×wall with descaled delivery conditions common. Browse the series hub at EN 10217-7.
1.4436 is easy to confuse with 1.4401 on a rushed RFQ — Mo range and carbon ceiling differ, and EN 10217-7 wants the steel number written out. Typical welded pressure duties include chemical plant piping that names 1.4436 specifically, and duties needing more Mo than 1.4401 without switching to an L analysis. Design caution: carbon up to 0.05% is below 1.4401’s ceiling but still above L grades — treat as-welded IGC deliberately Commercially the grade is often called 316 (higher Mo); keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4436 / X3CrNiMo17-13-3 on the MTC. Sister numbers on this hub include EN 10217-7 1.4401, EN 10217-7 1.4432, EN 10217-7 1.4404, EN 10217-7 1.4435.4401, 1.4432, 1.4404, 1.4435.
EN 10217-7 is welded product only. Match product form when a seamless X3CrNiMo17-13-3 twin is required under EN 10216-5 — Part 5 acceptance text does not clear a welded Part 7 order. Preferred dimensions follow EN ISO 1127. Public Table 1 routes are longitudinal automatic arc or laser welding from strip or plate; spiral seam is not listed and is not invented here. Live seamless sister: EN 10216-5 1.4436. Related live ASTM/ASME anchors: A269 TP316.
Chemical Composition of EN 10217-7 1.4436
Every 1.4436 heat under EN 10217-7 must meet the cast (ladle) analysis for X3CrNiMo17-13-3 in the austenitic table. Product analysis is Option 6, with permissible deviations tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unpublished “tighter than table” catalogue windows as if they were EN limits for 316 (higher Mo).
The table below reproduces public BSSA EN 10217-7 chemical limits for 1.4436 / X3CrNiMo17-13-3, cross-checked against the 2021 grade-list framing. Values are maximum unless a range is shown. Confirm the purchased EN 10217-7:2021 edition before treating any secondary catalogue as the acceptance text.
| Element | 1.4436 cast analysis (mass %) |
|---|---|
| Carbon (C) | ≤0.05 |
| Silicon (Si) | ≤1.00 |
| Manganese (Mn) | ≤2.00 |
| Phosphorus (P) | ≤0.045 |
| Sulfur (S) | ≤0.015 |
| Nitrogen (N) | ≤0.10 |
| Chromium (Cr) | 16.5–18.5 |
| Nickel (Ni) | 10.5–13.0 |
| Molybdenum (Mo) | 2.50–3.00 |
Source note for 1.4436 / X3CrNiMo17-13-3: BSSA “Chemical compositions of stainless steels to BS EN 10217-7” with public EN 10217-7 cross-check. Elements not listed for this austenitic grade shall not be intentionally added without purchaser agreement, except finishing additions, with scrap controls protecting mechanical and corrosion behaviour.
Mechanical Properties of EN 10217-7 1.4436
Ambient mechanical properties for 1.4436 / X3CrNiMo17-13-3 come from the EN 10217-7 austenitic ambient table for solution-annealed (+AT) tubes, for walls up to about 60 mm unless Options agree properties above that band. Austenitic grades list both Rp0.2 and Rp1.0. Public tables also carry cryogenic impact characterisation at −196 °C; verification is by Option unless the project specification mandates tested joules.
Figures below follow the BSSA mechanical-properties article for BS EN 10217-7 (2021 framing) as the primary public ambient source for 1.4436. Solution-annealing bands are taken from public EN stainless tables for the same steel number (cross EN 10216-5 / EN 10028-7 framing) and labelled UNCERTAIN where a paid EN 10217-7:2021 footnote has not been opened. SHH STEEL will not paste sister-standard tensile floors onto an EN 10217-7 certificate for X3CrNiMo17-13-3.
| Property | 1.4436 ambient (solution annealed +AT) |
|---|---|
| Rp0.2 min (MPa) | 205 |
| Rp1.0 min (MPa) | 240 |
| Rm (MPa) | 510–710 |
| A min % long / trans | 40 / 30 |
| IGC resistance (delivery) | Yes (method A) |
| Solution annealing (public EN band) | 1020–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges |
| Cooling | water or air |
| Charpy sub-zero (transverse min J) | 60 at -196 °C (Option to verify) |
Source: BSSA “Mechanical properties for stainless steels to BS EN 10217-7” (ambient); solution-annealing bands from public EN stainless tables with UNCERTAIN flag vs paid Part 7:2021 footnotes. Impact energies in the table apply as characterisation whether or not Options verify them — order the option when the certificate must show tested joules for 1.4436.
Welded Tube Manufacture for EN 10217-7 1.4436
EN 10217-7 does not offer a seamless route for 1.4436. Tube in X3CrNiMo17-13-3 is made by longitudinal automatic arc welding or laser welding across abutting strip or plate edges, with or without filler, on one of the public Table 1 paths (as-welded, outside ground, or bead worked before heat treatment as applicable). Continuous strip forming covers commodity OD; plate forming covers larger or heavier walls. Strip-join welds from before forming are not permitted in the finished tube. Spiral/helical seam is not a listed Table 1 route — do not assume Part 7 acceptance for spiral without a written agreement outside the standard. Seamless pressure stainless stays on EN 10216-5.
Molybdenum-bearing austenitic 1.4436 (X3CrNiMo17-13-3) uses the same longitudinal arc/laser Table 1 routes, typically without filler or with matching Mo-bearing filler by wall and procedure. Options 3 and 4 cover inside remelt or bead working for smoothed ID. Delivery symbols W0–W2R, WCA/WCR, WG/WP follow Table 2; Option 5 locks the choice. SHH STEEL can produce and supply 1.4436 as W1A/W2A descaled or WCA/WCR cold-finished in the common pressure-tube band, and as WG/WP when roughness scope is agreed. Mo austenitic fillers; prefer low-carbon fillers when as-welded corrosion is in the PED joint scope
Part 7 marking for 1.4436 includes test category, so the purchase order must too. Seam NDT weight tracks TC1/TC2; leak-tightness is universal with Option 15 as an optional method lock. SHH STEEL attaches the real manufacturing route and delivery symbol to each X3CrNiMo17-13-3 certificate set.
Dimensions and Tolerances for EN 10217-7 1.4436
Order EN 10217-7 1.4436 by outside diameter D and wall thickness T for steel name X3CrNiMo17-13-3. Preferred sizes follow EN ISO 1127. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Tolerance classes on diameter and wall follow the EN 10217-7 / EN ISO 1127 framework (tighter D4 under Option 20 when specified). Out-of-roundness sits inside the diameter tolerance; eccentricity inside the wall tolerance; radial weld-edge offset is limited (public text: within about 10% of specified wall).
Exact lengths are Option 19; bevelled ends for wall ≥ 3.2 mm are Option 18. Cold-finished WCA/WCR routes are the usual conversation for tighter instrumentation and hygienic OD on this austenitic grade. SHH STEEL aligns OD × wall, tolerance class, and delivery-condition symbol to the purchase order before welding slots are locked for 1.4436.
| Route / condition | Typical use | Notes |
|---|---|---|
| W1 / W1A / W1R | Hot-rolled starting flat product | Descaled or bright-annealed per symbol |
| W2 / W2A / W2R | Cold-rolled starting flat product | Smoother OD than W1 family except at weld |
| WCA / WCR | Cold finished ≥20% after weld | Recrystallized weld metal; OD often ≤168.3 mm |
| WG / WP | Ground / polished | Agree ID/OD scope and grit at enquiry |
Straightness and end-finish requirements follow EN 10217-7 dimensional clauses for X3CrNiMo17-13-3. SHH STEEL measures and reports the ordered OD × wall against the selected tolerance class on the inspection document for 1.4436, and will flag orders that mix D4 aspirations with hot-finished utility walls that cannot hold that class without a cold-finished route.
Equivalent Grades for EN 10217-7 1.4436
1.4436 / X3CrNiMo17-13-3 is the EN 10217-7 designation for this chemistry as welded pressure tube. ASTM/ASME pages that share the commercial alias 316 (higher Mo) are related product standards with different wall bases, mechanical tables, and tests — confirm before treating them as interchangeable with a Part 7 order. Seamless EN 10216-5 shares chemistry ideas, not the weld-seam acceptance path.
When dual marking is requested, each standard’s mechanical and test regime still has to be satisfied on its own terms — an ASTM alias of 316 (higher Mo) does not waive EN 10217-7 tensile, leak-tightness, or TC1/TC2 rules for 1.4436 / X3CrNiMo17-13-3. Keep the welded versus seamless product-form split explicit on the purchase order and on the MTC.
| Reference | Designation | Note |
|---|---|---|
| EN 10217-7 | 1.4436 / X3CrNiMo17-13-3 | This product standard (welded pressure tube) |
| EN steel name | X3CrNiMo17-13-3 | EN 10027-1 designation used in body and marking |
| Commercial alias (body only) | 316 (higher Mo) | Not a substitute for the steel number on the MTC |
| EN 10216-5 (seamless sister) | 1.4436 | Related live page — different product form (seamless) |
| A269 TP316 | A269 TP316 | Related live page — different product standard |
Inside this welded series, compare EN 10217-7 1.4401, EN 10217-7 1.4432, EN 10217-7 1.4404, EN 10217-7 1.4435. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4436. Live cross-standard anchors: A269 TP316.
Heat Treatment and Delivery Condition for EN 10217-7 1.4436
Tubes in 1.4436 ship in a Table 2 delivery condition that includes heat treatment when the symbol requires it (for example W1A, W2A, WCA, WCR, and bright-annealed W1R/W2R). Reference heat treatment for the mechanical tables is solution annealing (+AT): heat uniformly into the tabulated band for X3CrNiMo17-13-3 and cool rapidly so ordered ambient properties and corrosion footnotes are met.
For 1.4436, public EN stainless tables place solution annealing at 1020–1120 °C, with cooling by water or air. That band is cross-checked from public EN 10216-5 / EN 10028-7 framing for the same steel number and is UNCERTAIN against a paid EN 10217-7:2021 footnote until confirmed. Pickled versus bright-annealed versus ground/polished is a surface choice on top of the required heat treatment (Option 5 to lock the delivery-condition symbol).
| Item | 1.4436 |
|---|---|
| Solution annealing band (public) | 1020–1120 °C (UNCERTAIN vs paid Part 7 footnote) |
| Cooling | water or air |
| Delivery condition symbols | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify) |
| Inspection document | EN 10204 3.1 default; 3.2 under Option 21 |
SHH STEEL ships EN 10217-7 1.4436 only after the ordered Table 2 heat-treatment / delivery path is complete. The inspection document names the symbol used for X3CrNiMo17-13-3, records solution-annealing practice where required, and states weld-seam heat-treatment status on cold-finished recrystallized routes so the PED file can reconcile mechanical results with the actual finishing route.
Corrosion Resistance of EN 10217-7 1.4436
Corrosion-resisting austenitic 1.4436 / X3CrNiMo17-13-3 is selected for welded pressure duty where the medium and temperature need higher Mo than standard 316/1.4401 for localised corrosion; IGC behaviour depends on carbon and thermal history. EN 10217-7 marks intergranular-corrosion behaviour in the delivery condition against EN ISO 3651-2 methods in the mechanical tables; verification of IGC remains Option 13 even when the table says the grade resists IGC as delivered.
A single 1.4436 stamp will not cover every chloride map. X3CrNiMo17-13-3 is one chemistry; EN 10217-7 1.4401, EN 10217-7 1.4432, EN 10217-7 1.4404, EN 10217-7 1.4435 are the adjacent tools. Sensitisation guidance in Part 7 remains a long-service warning, and PREN/CPT are not EN acceptance digits on this page.
Applications of EN 10217-7 1.4436 Tube
EN 10217-7 1.4436 welded tube is used where PED-oriented pressure tubing must also resist corrosion and a longitudinal weld seam is accepted on the drawing. For X3CrNiMo17-13-3 the practical band is chemical plant piping that names 1.4436 specifically, and duties needing more Mo than 1.4401 without switching to an L analysis, supplied as welded tube in the ordered delivery condition with TC1 or TC2 testing.
It is the wrong first choice when a seamless product is mandatory (use EN 10216-5 — see EN 10216-5 1.4436), when the drawing is ASTM A269 instrumentation tubing or A312 pipe without an EN dual mark, or when the medium clearly needs a different family. SHH STEEL can produce and supply 1.4436 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit. Related live pages: A269 TP316.
Weldability of EN 10217-7 1.4436
1.4436 / X3CrNiMo17-13-3 is welded both as a mill seam under EN 10217-7 manufacturing routes and later as a fabricator joint on the PED spool. Mill seams follow the qualified longitudinal arc or laser procedures for the ordered route; shop welds use processes and fillers chosen for the EN chemistry family. For this grade: Mo austenitic fillers; prefer low-carbon fillers when as-welded corrosion is in the PED joint scope
As-welded corrosive service, ferrite balance on duplex where applicable, and post-weld heat treatment decisions for 1.4436 stay with the fabricator and the PED joint calculations. SHH STEEL’s scope on this page is the mill tube — chemistry, weld route, delivery-condition heat treatment, mechanical floors, leak-tightness, and options named on the purchase order for X3CrNiMo17-13-3.
Surface Finishes for EN 10217-7 1.4436
Surface finish on EN 10217-7 1.4436 is not a free-text afterthought — it is carried by the Table 2 delivery-condition symbol that also encodes heat treatment. Descaled W1A/W2A covers general PED utility tube in X3CrNiMo17-13-3; bright-annealed W1R/W2R or WCR is the usual step-up when cleaner OD is wanted for sanitary, pharmaceutical, or visible runs; ground WG or polished WP applies only when grit or Ra is agreed at enquiry and can be measured. Carbon-steel strapping must never contact the stainless OD — free-iron staining on 316 (higher Mo)-class tube is treated as a packing defect, not a cosmetic footnote.
Interior Ra limits, electropolish, special transit films, or capped-end cleanliness notes belong in explicit order text, not in a vague “food grade finish” phrase. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4436 when the mill can measure and report the finish on X3CrNiMo17-13-3; we will not claim an unverified grit or Ra grade on the certificate just to win a quotation comparison.
Practical selection tip for 1.4436: pair bright-annealed or polished OD with sleeve protection in packing so the finish that justified the symbol survives handling; leave descaled utility tube on clean non-contaminating supports. SHH STEEL aligns finish symbol, measurement capability, and packing protection for X3CrNiMo17-13-3 before the pack line closes, because a damaged bright OD is still a nonconformance even when chemistry and tensile are perfect.
Inspection and Testing for EN 10217-7 1.4436
Specific inspection applies to every EN 10217-7 1.4436 tube. Cast analysis is one per cast. Room-temperature tensile testing is one per test unit in TC1 and two per test unit from different tubes in TC2. Technological tests follow the standard’s matrix for the ordered diameter and wall. Every tube takes a leak-tightness test — hydrostatic or eddy current (Option 15 to lock the method) — plus dimensional and visual checks and material identification for X3CrNiMo17-13-3.
TC2 adds a heavier NDT regime on the weld seam and opens Options for laminar testing and edge NDT of starting strip/plate. IGC is Option 13; impact verification is by the Options that select room-temperature or low-temperature Charpy testing. SHH STEEL EN 10204 3.1 documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and the leak-tightness / NDT statement ordered. We do not drop mandatory tests to shorten lead time for 1.4436.
Combined orders of several steel numbers including 1.4436 still need per-grade inspection planning. SHH STEEL will not blend X3CrNiMo17-13-3 tensile units with a sister heat to pad a test report.
Packaging and Shipping for EN 10217-7 1.4436
Finished EN 10217-7 1.4436 (X3CrNiMo17-13-3) welded tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (W1R/W2R, WCR, WP) take sleeve or paper wrap against transit galling; descaled W1A/W2A utility tube still needs clean supports under the longitudinal seam. Strapping and contact materials stay stainless-compatible — carbon-steel banding on the OD is rejected because free-iron staining on 316 (higher Mo)-class surfaces creates site cleanup and NCR noise that a PED spool does not need.
Marking typically includes manufacturer identity, dimensions, EN 10217-7, steel name or number 1.4436, cast/code, test category, inspection mark, and correlation number; delivery-condition symbols may appear at the manufacturer’s discretion. When Option 5 locked a symbol, SHH STEEL keeps that symbol visible so goods-in matches the X3CrNiMo17-13-3 order.
Export packing lists cross-reference heat numbers to bundle IDs so the EN 10204 3.1 document matches without opening every crate. Option 19 cut lengths and Option 18 bevelled ends are segregated and capped before wrap. SHH STEEL aligns packaging with the order text before dispatch of 1.4436 welded pressure tube.
Why Choose SHH STEEL
SHH STEEL can produce and supply EN 10217-7 1.4436 as welded pressure tube — heat-treated to the ordered delivery condition, tested to the ordered TC1/TC2 regime, and documented on EN 10204 3.1 certificates — not as a generic “316 (higher Mo) tube” label on whatever is in the rack. We keep Part 7 distinct from EN 10216-5 seamless product and from ASTM A269/A213/A312 on the inspection document, and we will not paste tensile figures from the wrong table onto a X3CrNiMo17-13-3 shipment.
Grade advice stays practical. If the duty needs a sister chemistry, we point to EN 10217-7 LINKPLACE1.4401, EN 10217-7 LINKPLACE1.4432, EN 10217-7 LINKPLACE1.4404, EN 10217-7 LINKPLACE1.4435. Design caution for this number: carbon up to 0.05% is below LINKPLACE1.4401’s ceiling but still above L grades — treat as-welded IGC deliberately Winning the order with the wrong steel number is not a win for the PED file or for us. Live ASTM/ASME anchors: A269 TP316.
Supply Capability
SHH STEEL can produce and supply EN 10217-7 1.4436 welded stainless steel tube against the edition, test category, delivery condition, and options named on your enquiry. The capability table and Stock / Available sizes enquiry map below frame a first-pass size list for X3CrNiMo17-13-3 welded pressure duty. Process welded od×wall with descaled delivery conditions common.
| Item | SHH STEEL capability for 1.4436 |
|---|---|
| Standard | EN 10217-7 |
| Grade | 1.4436 / X3CrNiMo17-13-3 |
| Product form | Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition |
| Delivery condition | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock) |
| Typical size band | ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement |
| Testing | TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options |
| Documents | EN 10204 3.1 (3.2 Option 21); third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range for EN 10217-7 1.4436 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats of X3CrNiMo17-13-3, strip/plate starting stock, and finishing slots for the ordered delivery-condition symbol; send the OD × wall list, TC1/TC2 preference, and symbol for confirmation.
| OD (mm) | Typical walls (mm) | Notes |
|---|---|---|
| 12 / 14 / 16 / 19 / 21.3 / 25 | 1.0 / 1.5 / 2.0 / 2.5 | Instrument / hygienic; often WCA/WCR or W2R |
| 26.9 / 33.7 / 38 / 42.4 / 48.3 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Process and utility welded pressure tube |
| 60.3 / 76.1 / 88.9 / 114.3 | 2.0 / 3.0 / 4.0 / 5.0 / 6.0 | Utility and process; lock W1A/W2A vs WCA |
| 141.3 / 168.3 / 219.1 | 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 | Larger welded pressure tube; watch family wall ceiling |
Cut lengths (Option 19), bevelled ends (Option 18), IGC (Option 13), and dual enquiries against 1.4401, 1.4432, 1.4404, 1.4435 on the same size list are routine. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10217-7 + EN ISO 1127 classes. SHH STEEL can produce and supply 1.4436 in this enquiry map when strip/plate and weld capacity align.
FAQ
-
What is EN 10217-7 1.4436 welded stainless steel tube used for?
- EN 10217-7 1.4436 (X3CrNiMo17-13-3) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is chemical plant piping that names 1.4436 specifically, and duties needing more Mo than 1.4401 without switching to an L analysis. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
-
Is EN 10217-7 1.4436 the same as 316 (higher Mo) under ASTM A269 or A312?
- No. Commercial alias 316 (higher Mo) may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP316.
-
Does EN 10217-7 1.4436 include seamless tube?
- No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4436. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
-
What mechanical properties does EN 10217-7 require for 1.4436?
- In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm 510–710 MPa, and elongation 40% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
-
1.4436 vs sister grades — which EN 10217-7 number should I buy?
- Buy 1.4436 when the enquiry names this steel number or the duty matches mid-carbon higher-Mo austenitic welded pressure tube parallel to commercial 316 with Mo pushed toward 2.5–3%. Compare EN 10217-7 1.4401, EN 10217-7 1.4432, EN 10217-7 1.4404, EN 10217-7 1.4435 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: carbon up to 0.05% is below 1.4401’s ceiling but still above L grades — treat as-welded IGC deliberately
-
What delivery conditions are available for EN 10217-7 1.4436?
- Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
-
What size range can SHH STEEL supply for EN 10217-7 1.4436?
- SHH STEEL can produce and supply EN 10217-7 1.4436 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Process welded od×wall with descaled delivery conditions common.
-
TC1 or TC2 for EN 10217-7 1.4436?
- Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
-
Is the intergranular corrosion test mandatory for 1.4436?
- No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4436.
-
What documents come with SHH STEEL EN 10217-7 1.4436?
- EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4436, size, cast, and test category.
-
How do I enquire for EN 10217-7 1.4436 with SHH STEEL?
- Send EN 10217-7, steel number 1.4436 / X3CrNiMo17-13-3, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.
Conclusion
EN 10217-7 1.4436 (X3CrNiMo17-13-3) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4436 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.