EN 10217-7 1.4362 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4362 Welded Stainless Steel Tube

EN 10217-7 1.4362 / X2CrNiN23-4 welded stainless pressure tube (2304 / S32304), austenitic-ferritic (duplex), cast analysis per EN table, ambient Rp0.2 min 400 MPa, Rm 600–820, solution annealed 950–1050 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4362 / X2CrNiN23-4 (2304 / S32304 — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~12–219 mm OD × 1.0–12.7 mm wall within duplex characterisation (~30 mm wall band unless agreed); other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4362 Welded Stainless Steel Tube

When an enquiry still reads “2304 / S32304 welded pressure tube” without a European product standard, the PED paperwork is incomplete. EN 10217-7:2021 closes that gap for circular welded austenitic and duplex stainless tubes; within that list, 1.4362 / X2CrNiN23-4 is the austenitic-ferritic (duplex) entry that matches this chemistry. SHH STEEL treats the steel number, not the shop alias, as the acceptance key on cast analysis, longitudinal arc or laser seam route, solution annealing where the delivery symbol requires it, and the TC1/TC2 inspection regime. Duty focus: lean duplex welded pressure tube for chloride-bearing PED service needing higher strength than 304/316 at lower Ni cost than 2205.

SHH STEEL can produce and supply EN 10217-7 1.4362 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover welded OD common in water and utility projects; wall characterisation typically to 30 mm family band. Browse the series hub at EN 10217-7.

2304 / S32304 welded pressure under EN rules is 1.4362 on EN 10217-7 — strength and SCC behaviour are duplex, not “cheap 316.” Typical welded pressure duties include water treatment, district energy, light chloride process lines, and structural-adjacent pressure piping where lean duplex is approved. Design caution: lean duplex still needs duplex WPS discipline — ferrite balance, heat input, and 475 °C embrittlement awareness. Not a drop-in for every 1.4404 line without design check Commercially the grade is often called 2304 / S32304; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4362 / X2CrNiN23-4 on the MTC. Sister numbers on this hub include EN 10217-7 1.4462, EN 10217-7 1.4307, EN 10217-7 1.4404.4462, 1.4307, 1.4404.

Welded-only scope matters on every 1.4362 order. Seamless sisters are a different standard (EN 10216-5). Sizes prefer EN ISO 1127. Table 1 manufacture is longitudinal automatic arc or laser from strip/plate; do not specify spiral and expect automatic Part 7 acceptance without a written agreement outside the listed routes. Live seamless sister: EN 10216-5 1.4362. Related live ASTM/ASME anchors: A789 S32304.

Chemical Composition of EN 10217-7 1.4362

Ladle analysis controls 1.4362. The austenitic-ferritic (duplex) table entry for X2CrNiN23-4 is what the cast must satisfy; product analysis remains Option 6. SHH STEEL’s EN 10204 paperwork shows real cast results — catalogue “typical” chemistries are not substituted for EN acceptance on 2304 / S32304-class welded pressure tube.

Below is the BSSA-published EN 10217-7 cast window for X2CrNiN23-4 (steel number 1.4362), aligned to the 2021 list. Maxima apply unless a min–max range appears. Edition confirmation beats brochure reprint.

Element 1.4362 cast analysis (mass %)
Carbon (C) ≤0.030
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.035
Sulfur (S) ≤0.015
Nitrogen (N) 0.05–0.20
Chromium (Cr) 22.0–24.0
Nickel (Ni) 3.5–5.5
Molybdenum (Mo) 0.10–0.60
Copper (Cu) 0.10–0.60

Chemistry source for steel number 1.4362: BSSA EN 10217-7 chemical article plus public standard cross-check. Do not treat unlisted elements as free additions on X2CrNiN23-4 without purchaser agreement (finishing additions excepted under controlled scrap practice).

Mechanical Properties of EN 10217-7 1.4362

For welded duplex X2CrNiN23-4 under steel number 1.4362, EN 10217-7 ambient mechanical acceptance is written for solution-annealed tube in the duplex table — Rp0.2, Rm, elongation — inside roughly a 30 mm wall band unless agreed wider. Charpy checks at ambient or sub-zero are Option territory, not automatic certificate lines.

Primary ambient source for 1.4362: BSSA mechanical properties for stainless steels to BS EN 10217-7. Heat-treatment bands for X2CrNiN23-4 are public EN stainless figures with an UNCERTAIN flag against paid EN 10217-7:2021 footnotes. Sister-standard tensile values are not silently copied onto this Part 7 document.

Property 1.4362 ambient (solution annealed +AT)
Rp0.2 min (MPa) 400
Rp1.0 min (MPa) — (duplex tables use Rp0.2)
Rm (MPa) 600–820
A min % long / trans 25 / 25
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 950–1050 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 40 at -40 °C (Option to verify)

Ambient mechanical citation for steel number 1.4362: BSSA EN 10217-7 article; annealing bands public EN cross-check (UNCERTAIN vs paid 2021 footnotes). Order impact Options when tested toughness for X2CrNiN23-4 must be certified.

Welded Tube Manufacture for EN 10217-7 1.4362

For austenitic-ferritic (duplex) grade 1.4362, Part 7 manufacture starts with strip or plate of X2CrNiN23-4 chemistry, forms a circular section, and closes it with a longitudinal automatic arc or laser weld per Table 1. Filler may or may not be used depending on route and wall. Outside grinding or bead working before heat treatment appear where the ordered path requires them. Commodity sizes usually run on continuous strip lines; heavier walls move to plate forming. Spiral weld is not invented here as a standard Part 7 route. Seamless product is a different standard — EN 10216-5.

On duplex 1.4362, mill weld procedure and any cold work on WCA/WCR routes (commonly OD ≤ 168.3 mm) must protect the austenite–ferrite balance that underwrites chloride SCC resistance for X2CrNiN23-4. Table 2 symbols separate starting flat-product path and surface: W1/W1A/W1R from hot-rolled, W2/W2A/W2R from cold-rolled, WCA/WCR for cold-finished recrystallized-weld routes, WG/WP when ground or polished scope is agreed. Option 5 locks the symbol; otherwise the manufacturer chooses. SHH STEEL can produce and supply 1.4362 on the common heat-treated descaled and cold-finished routes when the enquiry names the symbol and any bead-work suffix. Shop note from this grade: lean-duplex rated fillers; heat-input windows; no austenitic “whatever is on the cart” substitution

Buyers of 1.4362 must pick TC1 or TC2 before manufacture release. That pick flows into marking and into weld-seam NDT scope; leak-tightness covers every tube, with Option 15 available. SHH STEEL writes the true Table 1 path and Table 2 symbol for X2CrNiN23-4 onto the inspection documents.

Dimensions and Tolerances for EN 10217-7 1.4362

Specify D and T when buying EN 10217-7 1.4362 (X2CrNiN23-4). EN ISO 1127 preferred sizes are the usual starting list; mass uses stainless density tables. Diameter/wall classes follow Part 7 with EN ISO 1127, including Option 20 D4. Out-of-roundness and eccentricity are absorbed inside those tolerances; weld-edge radial mismatch is separately limited.

Cut-to-length (Option 19) and bevelled ends (Option 18, wall ≥ 3.2 mm) are everyday extras on X2CrNiN23-4 welded tube. Tighter OD conversations usually move toward WCA/WCR. SHH STEEL matches the ordered D × T, tolerance class, and delivery symbol before committing 1.4362 weld capacity.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

For X2CrNiN23-4 welded tube, SHH STEEL verifies OD, wall, and the selected tolerance class on EN 10217-7 1.4362 before marking. Straightness and end-finish rules in the dimensional clauses still apply — they are not waived by a tight delivery promise. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4362 / X2CrNiN23-4 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4362

Designation discipline: EN 10217-7 writes 1.4362 / X2CrNiN23-4; shops say 2304 / S32304. Related ASTM/ASME product pages are cross-references only — wall basis, tensile tables, and inspection differ. EN 10216-5 seamless pages are chemistry cousins with a different manufacture and acceptance route.

Bill-of-materials writers sometimes list 2304 / S32304 next to EN and ASTM numbers interchangeably. For this product, steel number 1.4362 with name X2CrNiN23-4 under EN 10217-7 is the welded acceptance path; confirm any dual mark against both mechanical tables before release to fabrication.

Reference Designation Note
EN 10217-7 1.4362 / X2CrNiN23-4 This product standard (welded pressure tube)
EN steel name X2CrNiN23-4 EN 10027-1 designation used in body and marking
Commercial alias (body only) 2304 / S32304 Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4362 Related live page — different product form (seamless)
A789 S32304 A789 S32304 Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4462, EN 10217-7 1.4307, EN 10217-7 1.4404. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4362. Live cross-standard anchors: A789 S32304.

Heat Treatment and Delivery Condition for EN 10217-7 1.4362

For X2CrNiN23-4 ordered as 1.4362, pick a Table 2 symbol that encodes the required heat treatment and surface. Solution annealing (+AT) underpins the ambient mechanical table: bring the tube into the solution-temperature window and cool quickly enough to satisfy strength and corrosion notes. For X2CrNiN23-4 under steel number 1.4362, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Solution band used on this page for 1.4362: 950–1050 °C, cool by water or air (public EN stainless cross-check; UNCERTAIN vs paid EN 10217-7:2021 footnotes). Lock the delivery-condition symbol with Option 5 when pickle versus bright anneal versus WG/WP must be contractual for X2CrNiN23-4.

Item 1.4362
Solution annealing band (public) 950–1050 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

Heat-treatment honesty is part of the X2CrNiN23-4 supply package: SHH STEEL documents the delivery-condition symbol actually run on EN 10217-7 1.4362, including whether the longitudinal weld was recrystallized on cold-finished routes, rather than implying a generic “annealed” stamp without Table 2 language. For X2CrNiN23-4 under steel number 1.4362, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Corrosion Resistance of EN 10217-7 1.4362

Choose 1.4362 (X2CrNiN23-4) when welded PED tubing must carry this corrosion story: duplex microstructure for chloride SCC resistance superior to Mo-free austenitics in many aqueous chloride duties; Mo is low versus 2205. Delivery-condition IGC resistance is characterised to EN ISO 3651-2 methods in the Part 7 tables, but a tested IGC result still requires Option 13 on the order.

For PED files that mention both IGC and elevated temperature on 1.4362, separate the conversations: sensitisation guidance versus strength. X2CrNiN23-4 acceptance remains the Part 7 tables. Step to EN 10217-7 1.4462, EN 10217-7 1.4307, EN 10217-7 1.4404 when corrosion resistance is the real gap.

Applications of EN 10217-7 1.4362 Tube

Applications for steel number 1.4362 / X2CrNiN23-4 cluster around welded PED service that tolerates a mill seam: water treatment, district energy, light chloride process lines, and structural-adjacent pressure piping where lean duplex is approved. Delivery condition and test category on the order decide how that tube is finished and inspected before it reaches the spool.

Skip 1.4362 when the specification locks seamless product (EN 10216-5 — see EN 10216-5 1.4362), when ASTM A269/A312 text is the only acceptance language, or when corrosion/strength clearly points at another family. SHH STEEL can produce and supply X2CrNiN23-4 welded tube in the enquiry band and will redirect to a sister or live ASTM/ASME page when that is wiser. Related live pages: A789 S32304.

Weldability of EN 10217-7 1.4362

Mill welding of EN 10217-7 1.4362 is the longitudinal arc/laser seam on the ordered Table 1 route; field or shop welding is a separate PED joint design. Filler and procedure choices track the austenitic-ferritic (duplex) chemistry of X2CrNiN23-4. Practical note: lean-duplex rated fillers; heat-input windows; no austenitic “whatever is on the cart” substitution

PED joint design — including whether X2CrNiN23-4 can remain as-welded in corrosive service — is outside mill scope. SHH STEEL’s deliverable for 1.4362 is compliant welded tube with documented chemistry, route, delivery condition, mechanical results, and leak/NDT statements.

Surface Finishes for EN 10217-7 1.4362

For X2CrNiN23-4 welded under EN 10217-7 1.4362, finish language equals Table 2 language: descaled for utility, bright-annealed for cleaner OD, ground or polished when roughness is contractual. Agree WP/WG at enquiry with inspectable criteria. Transit contact with carbon steel is forbidden because free-iron rust blooms on 2304 / S32304 OD fail goods-in visual checks and contaminate stainless systems downstream of the weld seam.

Special ID finishes are order lines. When measurement is possible, SHH STEEL can produce and supply pickled, bright-annealed, and polished 1.4362; we will not invent an Ra number for 2304 / S32304 or imply electropolish that was never run on X2CrNiN23-4. Exterior polish without an agreed grit is equally unacceptable as certificate language.

When 2304 / S32304 welded tube must look like instrumentation stock, bright anneal or polish belongs on the order with 1.4362. Descaled W1A/W2A remains correct for many lagged utility runs. SHH STEEL can produce and supply only the finish path X2CrNiN23-4 can actually certify under EN 10217-7 on the promised date.

Inspection and Testing for EN 10217-7 1.4362

For EN 10217-7 1.4362 / X2CrNiN23-4, expect cast chemistry per heat, ambient tensile at TC1/TC2 frequency, technological tests from the standard’s table, and 100% leak-tightness (hydrostatic or eddy current). Dimensional, visual, and material-identification checks close the baseline regime. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4362 purchase order so X2CrNiN23-4 inspection planning matches the PED file before weld slots are locked.

Heavier weld-seam NDT is the TC2 differentiator on 1.4362. Laminar/edge NDT Options, IGC Option 13, and Charpy Options are purchaser choices. SHH STEEL’s EN 10204 3.1 file records what was melted, how X2CrNiN23-4 was heat-treated, what tensile was achieved, and which leak/NDT path ran — without skipping required tests for speed.

Retests on 1.4362 follow the standard’s rules — they are not an informal “try again until it passes” loop. SHH STEEL documents retest logic for X2CrNiN23-4 when a unit fails and a conforming replacement heat or tube is offered.

Packaging and Shipping for EN 10217-7 1.4362

SHH STEEL ships EN 10217-7 1.4362 in end-protected, size-sorted bundles or wooden crates with waterproof wrapping for sea freight. Duplex 1.4362 OD that was ordered bright-annealed or polished gets sleeve protection so the W1R/W2R/WCR/WP surface survives handling; descaled W1A/W2A utility tube still needs clean dunnage under the weld seam region. Because X2CrNiN23-4 is stainless, packing deliberately keeps carbon-steel strapping and rusty fixtures off the tube surface — free-iron transfer is a common transit complaint on 2304 / S32304 and is prevented at the dock, not debated later.

Traceability marking on X2CrNiN23-4 welded tube carries EN 10217-7, steel number 1.4362, size, cast, test category, and inspection/correlation marks. Delivery symbols are added when ordered or when clarity helps receiving. SHH STEEL aligns stencil language with the PO before dispatch. SHH STEEL treats packing and marking for EN 10217-7 1.4362 / X2CrNiN23-4 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Heat-to-bundle correlation on export documents saves receiving time for 2304 / S32304 welded tube. Cut-to-length and bevelled lots are packed apart with caps fitted. SHH STEEL applies the agreed packing note on every 1.4362 shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4362 / X2CrNiN23-4 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and make EN 10217-7 1.4362 welded pressure tube for buyers who need documented X2CrNiN23-4 chemistry, delivery-condition heat treatment, and leak-tightness — not a shop-floor 2304 / S32304 stamp. We refuse to blur this page into EN 10216-5 seamless acceptance or to decorate MTCs with foreign tensile floors.

When 2304 / S32304 is the wrong tool, SHH STEEL steers toward EN 10217-7 LINKPLACE1.4462, EN 10217-7 LINKPLACE1.4307, EN 10217-7 LINKPLACE1.4404. Keep this caution in view: lean duplex still needs duplex WPS discipline — ferrite balance, heat input, and 475 °C embrittlement awareness. Not a drop-in for every LINKPLACE1.4404 line without design check A mis-selected steel number helps no PED dossier. Live ASTM/ASME anchors: A789 S32304.

Supply Capability

SHH STEEL can produce and supply welded EN 10217-7 1.4362 when your enquiry states standard edition, test category, delivery condition, and options. Capability and Stock / Available sizes tables below support first sizing for this 2304 / S32304 pressure grade. Welded od common in water and utility projects; wall characterisation typically to 30 mm family band.

Item SHH STEEL capability for 1.4362
Standard EN 10217-7
Grade 1.4362 / X2CrNiN23-4
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~12–219 mm OD × 1.0–12.7 mm wall within duplex characterisation (~30 mm wall band unless agreed); other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Treat the size map as availability language for 2304 / S32304 welded pressure tube, not a tonnage inventory. 1.4362 depends on X2CrNiN23-4 flat-product supply and weld finishing. Confirm against your OD × wall and TC1/TC2 list.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Exact length, bevel, IGC, and sister-grade duals (1.4462, 1.4307, 1.4404) can share one enquiry. Catalogue size patterns are indicative; EN 10217-7 governs. SHH STEEL can produce and supply X2CrNiN23-4 welded tube in this map when the mill path fits.

FAQ

What is EN 10217-7 1.4362 welded stainless steel tube used for?
EN 10217-7 1.4362 (X2CrNiN23-4) is welded pressure tube for PED-oriented duties that need the austenitic-ferritic (duplex) chemistry story with a longitudinal mill seam. Typical service is water treatment, district energy, light chloride process lines, and structural-adjacent pressure piping where lean duplex is approved. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4362 the same as 2304 / S32304 under ASTM A269 or A312?
No. Commercial alias 2304 / S32304 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A789 S32304.
Does EN 10217-7 1.4362 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4362. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4362?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 400 MPa, Rm 600–820 MPa, and elongation 25% longitudinal / 25% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4362 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4362 when the enquiry names this steel number or the duty matches lean duplex welded pressure tube for chloride-bearing PED service needing higher strength than 304/316 at lower Ni cost than 2205. Compare EN 10217-7 1.4462, EN 10217-7 1.4307, EN 10217-7 1.4404 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: lean duplex still needs duplex WPS discipline — ferrite balance, heat input, and 475 °C embrittlement awareness. Not a drop-in for every 1.4404 line without design check
What delivery conditions are available for EN 10217-7 1.4362?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4362?
SHH STEEL can produce and supply EN 10217-7 1.4362 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~12–219 mm OD × 1.0–12.7 mm wall within duplex characterisation (~30 mm wall band unless agreed); other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Welded od common in water and utility projects; wall characterisation typically to 30 mm family band.
TC1 or TC2 for EN 10217-7 1.4362?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4362?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4362.
What documents come with SHH STEEL EN 10217-7 1.4362?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4362, size, cast, and test category.
How do I enquire for EN 10217-7 1.4362 with SHH STEEL?
Send EN 10217-7, steel number 1.4362 / X2CrNiN23-4, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4362 (X2CrNiN23-4) is welded stainless pressure tube for PED-oriented service in the austenitic-ferritic (duplex) family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4362 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X