EN 10217-7 1.4547 Welded Stainless Steel Tube
What is EN 10217-7 1.4547 Welded Stainless Steel Tube
Ordering welded pressure stainless under EN 10217-7 means choosing a steel number from the austenitic or duplex tables, a test category, and a delivery-condition path — not pasting a shop alias onto random mill stock. 1.4547 is the EN designation for X1CrNiMoCuN20-18-7 (254 SMO / S31254 in commercial speech) in the austenitic family. Part 7 of EN 10217 defines the welded circular product for pressure plus corrosion-resisting service; the order text must carry EN 10217-7, 1.4547, TC1 or TC2, and options so the mill runs the right strip/plate route and inspection. Use case: 6Mo super-austenitic (254 SMO-type) welded pressure tube for severe chloride and seawater PED service.
SHH STEEL can produce and supply EN 10217-7 1.4547 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover specialty welded sizes; confirm OD×wall early because strip availability drives lead time. Browse the series hub at EN 10217-7.
254 SMO / S31254 welded pressure under EN is 1.4547 on EN 10217-7 — SHH STEEL will not pretend a 1.4404 seam is an equivalent. Typical welded pressure duties include seawater cooling, offshore and coastal chemical PED lines, flue-gas scrubber piping, and high-chloride process systems. Design caution: 6Mo fabrication is not 316L fabrication — fillers, heat input, and cleanliness must match the alloy. Invented PREN floors are not EN limits Commercially the grade is often called 254 SMO / S31254; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4547 / X1CrNiMoCuN20-18-7 on the MTC. Sister numbers on this hub include EN 10217-7 1.4529, EN 10217-7 1.4439, EN 10217-7 1.4410, EN 10217-7 1.4539.4529, 1.4439, 1.4410, 1.4539.
Scope check before release: Part 7 = welded X1CrNiMoCuN20-18-7 tube; Part 5 = seamless. Preferred OD × wall language follows EN ISO 1127. Listed manufacture is longitudinal automatic arc or laser welding — helical seam stays outside the public Table 1 routes referenced here. Live seamless sister: EN 10216-5 1.4547.
Chemical Composition of EN 10217-7 1.4547
EN 10217-7 requires the cast analysis of 1.4547 to meet X1CrNiMoCuN20-18-7 limits in the austenitic listing. Product analysis is the Option 6 path. On the certificate SHH STEEL shows actual cast chemistry for this 254 SMO / S31254 welded pressure grade — not a marketing typical.
Chemical limits for 1.4547 / X1CrNiMoCuN20-18-7 come from the public BSSA EN 10217-7 article, cross-checked to the 2021 grade list. Unless a range is stated, treat values as maxima. Secondary catalogues are not the purchase contract.
| Element | 1.4547 cast analysis (mass %) |
|---|---|
| Carbon (C) | ≤0.020 |
| Silicon (Si) | ≤0.70 |
| Manganese (Mn) | ≤1.00 |
| Phosphorus (P) | ≤0.030 |
| Sulfur (S) | ≤0.010 |
| Nitrogen (N) | 0.18–0.25 |
| Chromium (Cr) | 19.5–20.5 |
| Nickel (Ni) | 17.5–18.5 |
| Molybdenum (Mo) | 6.00–7.00 |
| Copper (Cu) | 0.50–1.00 |
The X1CrNiMoCuN20-18-7 composition window shown for 1.4547 is taken from the BSSA EN 10217-7 chemistry article. Public standard cross-check applies. Unlisted elements stay off the intentional-addition list unless the purchaser agrees, with the usual finishing-addition / scrap exceptions for austenitic melts.
Mechanical Properties of EN 10217-7 1.4547
Mechanical floors for welded 1.4547 tube in X1CrNiMoCuN20-18-7 are the EN 10217-7 austenitic ambient (+AT) figures for walls inside the public characterisation window (about 60 mm unless Options say otherwise). Rp0.2, Rp1.0, Rm, and elongation are the everyday acceptance set; cryogenic impact stays optional until selected.
Ambient mechanical values shown for X1CrNiMoCuN20-18-7 track BSSA BS EN 10217-7 (2021 framing). Public EN solution-annealing ranges are used with an UNCERTAIN tag relative to paid EN 10217-7 footnotes. Acceptance for steel number 1.4547 stays on the Part 7 table SHH STEEL cites — not on a borrowed sister datasheet.
| Property | 1.4547 ambient (solution annealed +AT) |
|---|---|
| Rp0.2 min (MPa) | 300 |
| Rp1.0 min (MPa) | 340 |
| Rm (MPa) | 650–850 |
| A min % long / trans | 35 / 30 |
| IGC resistance (delivery) | Yes (method A) |
| Solution annealing (public EN band) | 1140–1200 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges |
| Cooling | water or air |
| Charpy sub-zero (transverse min J) | 60 at -196 °C (Option to verify) |
Public sources for the X1CrNiMoCuN20-18-7 ambient table: BSSA EN 10217-7 mechanical article; annealing windows from public EN stainless documents (UNCERTAIN vs paid 2021 Part 7). Select impact Options on 1.4547 when certified joules are mandatory.
Welded Tube Manufacture for EN 10217-7 1.4547
Building 1.4547 under EN 10217-7 means committing to a welded circular tube: longitudinal automatic arc or laser weld from X1CrNiMoCuN20-18-7 strip or plate, following Table 1. As-welded, outside-ground, and bead-worked-before-heat-treatment variants are the listed paths; spiral seam is not among them in the public text used for this series. Continuous strip forming and plate forming cover the size map. SHH STEEL will not treat a helical-weld drawing as automatic Part 7 acceptance. Seamless pressure tube belongs on the EN 10216-5 sister conversation.
High-alloy austenitic 1.4547 (X1CrNiMoCuN20-18-7) is welded longitudinally under Table 1 with procedures that respect the Mo-Cu (and nitrogen where present) balance — heat input and cleanliness matter more than on commodity 18-8. Options 3/4 dress the ID weld when required; Table 2 symbols set surface/heat-treatment path with Option 5 to lock. SHH STEEL can produce and supply 1.4547 as heat-treated descaled or cold-finished product when strip chemistry and weld slots align. Filler guidance for this page: overmatching 6Mo / Ni-based fillers per WPS; often full NDT and Option 13 on the mill tube plus fabricator PQRs
On 1.4547, test category is order-critical. TC2 intensifies longitudinal weld NDT relative to TC1; leak-tightness does not disappear either way. Option 15 removes manufacturer choice on hydro versus eddy current. Route and delivery symbol for X1CrNiMoCuN20-18-7 are reported by SHH STEEL as executed facts.
Dimensions and Tolerances for EN 10217-7 1.4547
EN 10217-7 1.4547 is sized by D × T. Start from EN ISO 1127 preferred sizes for X1CrNiMoCuN20-18-7; apply stainless density for mass. Tolerance classes follow the Part 7 framework — Option 20 selects D4 when instrumentation fit-up needs it. Out-of-roundness, eccentricity, and weld-edge radial offset rules in the dimensional clauses still apply.
Options 19 (exact length) and 18 (bevel, wall ≥ 3.2 mm) sit on top of the D × T order for 1.4547. Cold-finished WCA/WCR is the common upgrade path when OD tolerance and weld recrystallization matter. SHH STEEL confirms those choices with the delivery symbol before production release.
| Route / condition | Typical use | Notes |
|---|---|---|
| W1 / W1A / W1R | Hot-rolled starting flat product | Descaled or bright-annealed per symbol |
| W2 / W2A / W2R | Cold-rolled starting flat product | Smoother OD than W1 family except at weld |
| WCA / WCR | Cold finished ≥20% after weld | Recrystallized weld metal; OD often ≤168.3 mm |
| WG / WP | Ground / polished | Agree ID/OD scope and grit at enquiry |
SHH STEEL’s dimensional report on 1.4547 / X1CrNiMoCuN20-18-7 cites the ordered tolerance class, not a generic “per EN” line. Straightness and end-finish checks remain part of release under EN 10217-7 dimensional clauses. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4547 / X1CrNiMoCuN20-18-7 on the inspection document rather than assuming mid-tolerance catalogue values.
Equivalent Grades for EN 10217-7 1.4547
EN 10217-7 identifies this welded product as 1.4547 / X1CrNiMoCuN20-18-7. Keep 254 SMO / S31254 in body text and enquiry notes, not as the sole MTC identity. ASTM/ASME standards that share the alias differ in scope; EN 10216-5 is seamless, not an alternate welded acceptance path.
Cross-standard shopping for 254 SMO / S31254 chemistry is common; acceptance is not. EN 10217-7 1.4547 remains the welded pressure-tube contract for X1CrNiMoCuN20-18-7 on this page. Seamless sisters and ASTM/ASME pages are references until the order explicitly dual-certifies under each standard’s clauses.
| Reference | Designation | Note |
|---|---|---|
| EN 10217-7 | 1.4547 / X1CrNiMoCuN20-18-7 | This product standard (welded pressure tube) |
| EN steel name | X1CrNiMoCuN20-18-7 | EN 10027-1 designation used in body and marking |
| Commercial alias (body only) | 254 SMO / S31254 | Not a substitute for the steel number on the MTC |
| EN 10216-5 (seamless sister) | 1.4547 | Related live page — different product form (seamless) |
Inside this welded series, compare EN 10217-7 1.4529, EN 10217-7 1.4439, EN 10217-7 1.4410, EN 10217-7 1.4539. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4547.
Heat Treatment and Delivery Condition for EN 10217-7 1.4547
EN 10217-7 1.4547 is supplied to a Table 2 delivery condition. Where that symbol requires heat treatment, solution annealing (+AT) is the reference path behind the X1CrNiMoCuN20-18-7 ambient properties: soak in the solution band, cool rapidly, and document what was done. For X1CrNiMoCuN20-18-7 under steel number 1.4547, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
X1CrNiMoCuN20-18-7 solution annealing on public tables: 1140–1200 °C, cooled by water or air. Treat as UNCERTAIN relative to paid EN 10217-7:2021 footnotes. Delivery-condition symbol (Option 5) then selects the surface path for 1.4547. For X1CrNiMoCuN20-18-7 under steel number 1.4547, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
| Item | 1.4547 |
|---|---|
| Solution annealing band (public) | 1140–1200 °C (UNCERTAIN vs paid Part 7 footnote) |
| Cooling | water or air |
| Delivery condition symbols | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify) |
| Inspection document | EN 10204 3.1 default; 3.2 under Option 21 |
Ordered heat treatment on X1CrNiMoCuN20-18-7 is verified before dispatch. SHH STEEL’s paperwork for EN 10217-7 1.4547 ties ambient tensile results to the Table 2 delivery symbol and notes weld-seam treatment on cold-finished product, so the certificate matches the tube that arrives. For X1CrNiMoCuN20-18-7 under steel number 1.4547, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
Corrosion Resistance of EN 10217-7 1.4547
Corrosion-resisting austenitic 1.4547 / X1CrNiMoCuN20-18-7 is selected for welded pressure duty where the medium and temperature need ~6% Mo plus nitrogen for very high pitting/crevice resistance among austenitics; still watch crevice geometry and chlorination practices. EN 10217-7 marks intergranular-corrosion behaviour in the delivery condition against EN ISO 3651-2 methods in the mechanical tables; verification of IGC remains Option 13 even when the table says the grade resists IGC as delivered.
Welded pressure tube in 1.4547 fails projects when corrosion selection is lazy. Read the medium against X1CrNiMoCuN20-18-7, order Option 13 when tested IGC is required, and change to EN 10217-7 1.4529, EN 10217-7 1.4439, EN 10217-7 1.4410, EN 10217-7 1.4539 when Mo/N/stabilisation/duplex is the actual need — not a invented PREN line.
Applications of EN 10217-7 1.4547 Tube
EN 10217-7 1.4547 welded tube is used where PED-oriented pressure tubing must also resist corrosion and a longitudinal weld seam is accepted on the drawing. For X1CrNiMoCuN20-18-7 the practical band is seawater cooling, offshore and coastal chemical PED lines, flue-gas scrubber piping, and high-chloride process systems, supplied as welded tube in the ordered delivery condition with TC1 or TC2 testing.
It is the wrong first choice when a seamless product is mandatory (use EN 10216-5 — see EN 10216-5 1.4547), when the drawing is ASTM A269 instrumentation tubing or A312 pipe without an EN dual mark, or when the medium clearly needs a different family. SHH STEEL can produce and supply 1.4547 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit.
Weldability of EN 10217-7 1.4547
1.4547 / X1CrNiMoCuN20-18-7 is welded both as a mill seam under EN 10217-7 manufacturing routes and later as a fabricator joint on the PED spool. Mill seams follow the qualified longitudinal arc or laser procedures for the ordered route; shop welds use processes and fillers chosen for the EN chemistry family. For this grade: overmatching 6Mo / Ni-based fillers per WPS; often full NDT and Option 13 on the mill tube plus fabricator PQRs
Once X1CrNiMoCuN20-18-7 tube leaves the mill as EN 10217-7 1.4547, spool welding is a separate engineering act. SHH STEEL does not own the fabricator’s as-welded corrosion or PWHT choices; we own the mill certificate package — chemistry, seam route, heat treatment symbol, tensile, and leak/NDT.
Surface Finishes for EN 10217-7 1.4547
Ordered surface on EN 10217-7 1.4547 / X1CrNiMoCuN20-18-7 follows the delivery-condition letter the purchaser locks (Option 5) or the manufacturer selects. Pickle/descaled suits lagged utility; bright anneal suits cleaner OD; grind/polish needs grit or Ra on the PO. Protect 254 SMO / S31254 from carbon-steel contact in every pack design so free-iron transfer never becomes a site cleanup project after ocean freight.
Electropolish and ID Ra belong in the PO alongside steel number 1.4547. SHH STEEL can produce and supply the common descaled and bright-annealed routes for X1CrNiMoCuN20-18-7, plus polished OD when grit is agreed and checked — no catalogue fiction, no unverified “mirror” claims for 254 SMO / S31254.
Buyers sometimes request “same as last 254 SMO / S31254 lot” without a symbol. For 1.4547 / X1CrNiMoCuN20-18-7, SHH STEEL restates the Table 2 finish on the order acknowledgement so there is no silent drift between descaled utility and bright-annealed instrumentation product across releases.
Inspection and Testing for EN 10217-7 1.4547
TC1/TC2 define tensile intensity on 1.4547, but leak-tightness is per tube either way. Cast analysis, technological tests, dimensions, visuals, and material ID complete the baseline for X1CrNiMoCuN20-18-7. Option 15 selects the leak-test method when the purchaser refuses manufacturer choice. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4547 purchase order so X1CrNiMoCuN20-18-7 inspection planning matches the PED file before weld slots are locked.
Weld-seam NDT intensity and optional laminar/edge tests rise with TC2 for X1CrNiMoCuN20-18-7. IGC (Option 13) and Charpy Options remain opt-in. SHH STEEL reports the ordered package on EN 10204 3.1 for 1.4547 and keeps mandatory Part 7 tests on the schedule. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4547 purchase order so X1CrNiMoCuN20-18-7 inspection planning matches the PED file before weld slots are locked.
Laminar and edge NDT Options for starting strip/plate on 1.4547 are purchaser choices that affect plate/strip procurement time. SHH STEEL flags lead-time impact for X1CrNiMoCuN20-18-7 when those Options appear late in the enquiry cycle.
Packaging and Shipping for EN 10217-7 1.4547
When 1.4547 (X1CrNiMoCuN20-18-7) leaves the mill as EN 10217-7 welded tube, packing protects both the weld-seam region and the ordered surface condition. End protection, sorted bundles or crates, and ocean-freight wrap are baseline. High-alloy 254 SMO / S31254 bright-annealed or polished OD is sleeved against transit galling; descaled chemical-service tube still ships on non-contaminating supports with capped ends. Carbon-steel banding against stainless is not used — free-iron staining on 254 SMO / S31254 tube is a packing defect SHH STEEL designs out before dispatch.
Goods-in should read EN 10217-7, 1.4547, dimensions, cast, and test category without decoding gymnastics. Delivery condition may be marked; it is required in spirit when Option 5 applied. SHH STEEL sets stencil and tags for X1CrNiMoCuN20-18-7 before the pack line closes. SHH STEEL treats packing and marking for EN 10217-7 1.4547 / X1CrNiMoCuN20-18-7 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Traceable packing lists link X1CrNiMoCuN20-18-7 heats to physical bundles. Option 19/18 pieces get their own capped packs. Dispatch waits until packing and marking match the 1.4547 purchase order. SHH STEEL treats packing and marking for EN 10217-7 1.4547 / X1CrNiMoCuN20-18-7 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Why Choose SHH STEEL
SHH STEEL can produce and supply welded EN 10217-7 1.4547 / X1CrNiMoCuN20-18-7 against the delivery symbol and inspection package on your enquiry. We will not sell anonymous 254 SMO / S31254 footage as Part 7, and we keep seamless EN 10216-5 and ASTM A269/A213/A312 off this MTC path.
Compare LINKPLACE1.4529, LINKPLACE1.4439, LINKPLACE1.4410, LINKPLACE1.4539 before freezing 1.4547. Caution: 6Mo fabrication is not 316L fabrication — fillers, heat input, and cleanliness must match the alloy. Invented PREN floors are not EN limits SHH STEEL will say no to a mismatched grade rather than force-fit X1CrNiMoCuN20-18-7 into the wrong medium Linked sisters on this hub: EN 10217-7 1.4529, EN 10217-7 1.4439, EN 10217-7 1.4410, EN 10217-7 1.4539.
Supply Capability
SHH STEEL’s supply offer on 1.4547 is welded Part 7 tube made and tested to your stated options. The tables that follow — including Stock / Available sizes — help buyers sketch OD × wall before a firm mill answer. Specialty welded sizes; confirm od×wall early because strip availability drives lead time.
| Item | SHH STEEL capability for 1.4547 |
|---|---|
| Standard | EN 10217-7 |
| Grade | 1.4547 / X1CrNiMoCuN20-18-7 |
| Product form | Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition |
| Delivery condition | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock) |
| Typical size band | ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement |
| Testing | TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options |
| Documents | EN 10204 3.1 (3.2 Option 21); third-party inspection on request |
Stock / Available sizes
Available-size talk for 1.4547 follows mill strip/plate and finishing reality for X1CrNiMoCuN20-18-7. Use the table to draft the enquiry; SHH STEEL confirms against current heats and slots — not against a static warehouse spreadsheet.
| OD (mm) | Typical walls (mm) | Notes |
|---|---|---|
| 12 / 14 / 16 / 19 / 21.3 / 25 | 1.0 / 1.5 / 2.0 / 2.5 | Instrument / hygienic; often WCA/WCR or W2R |
| 26.9 / 33.7 / 38 / 42.4 / 48.3 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Process and utility welded pressure tube |
| 60.3 / 76.1 / 88.9 / 114.3 | 2.0 / 3.0 / 4.0 / 5.0 / 6.0 | Utility and process; lock W1A/W2A vs WCA |
| 141.3 / 168.3 / 219.1 | 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 | Larger welded pressure tube; watch family wall ceiling |
Ask for cut length, bevel, IGC, or sister numbers (1.4529, 1.4439, 1.4410, 1.4539) in the same RFQ. The size table is a starting grid under EN 10217-7 / EN ISO 1127. SHH STEEL can produce and supply 1.4547 when the finishing route is available.
FAQ
-
What is EN 10217-7 1.4547 welded stainless steel tube used for?
- EN 10217-7 1.4547 (X1CrNiMoCuN20-18-7) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is seawater cooling, offshore and coastal chemical PED lines, flue-gas scrubber piping, and high-chloride process systems. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
-
Is EN 10217-7 1.4547 the same as 254 SMO / S31254 under ASTM A269 or A312?
- No. Commercial alias 254 SMO / S31254 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing.
-
Does EN 10217-7 1.4547 include seamless tube?
- No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4547. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
-
What mechanical properties does EN 10217-7 require for 1.4547?
- In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 300 MPa, Rp1.0 min 340 MPa, Rm 650–850 MPa, and elongation 35% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
-
1.4547 vs sister grades — which EN 10217-7 number should I buy?
- Buy 1.4547 when the enquiry names this steel number or the duty matches 6Mo super-austenitic (254 SMO-type) welded pressure tube for severe chloride and seawater PED service. Compare EN 10217-7 1.4529, EN 10217-7 1.4439, EN 10217-7 1.4410, EN 10217-7 1.4539 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: 6Mo fabrication is not 316L fabrication — fillers, heat input, and cleanliness must match the alloy. Invented PREN floors are not EN limits
-
What delivery conditions are available for EN 10217-7 1.4547?
- Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
-
What size range can SHH STEEL supply for EN 10217-7 1.4547?
- SHH STEEL can produce and supply EN 10217-7 1.4547 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Specialty welded sizes; confirm od×wall early because strip availability drives lead time.
-
TC1 or TC2 for EN 10217-7 1.4547?
- Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
-
Is the intergranular corrosion test mandatory for 1.4547?
- No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4547.
-
What documents come with SHH STEEL EN 10217-7 1.4547?
- EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4547, size, cast, and test category.
-
How do I enquire for EN 10217-7 1.4547 with SHH STEEL?
- Send EN 10217-7, steel number 1.4547 / X1CrNiMoCuN20-18-7, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.
Conclusion
EN 10217-7 1.4547 (X1CrNiMoCuN20-18-7) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4547 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.