EN 10217-7 1.4429 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4429 Welded Stainless Steel Tube

EN 10217-7 1.4429 / X2CrNiMoN17-13-3 welded stainless pressure tube (316LN), austenitic, cast analysis per EN table, ambient Rp0.2 min 295 MPa, Rm 580–800, solution annealed 1020–1120 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4429 / X2CrNiMoN17-13-3 (316LN — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4429 Welded Stainless Steel Tube

Steel name X2CrNiMoN17-13-3 under steel number 1.4429 is the austenitic chemistry EN 10217-7 uses when a welded pressure-tube order must carry that analysis into the PED file. The product standard is EN 10217-7:2021 — welded stainless circular tubes for pressure and corrosion-resisting service at room, low, or elevated temperature. Writing only “316LN welded tube” on a bill of materials leaves cast limits, weld route, delivery condition, and test category unspecified. Order EN 10217-7, 1.4429, TC1 or TC2, and the delivery-condition / options list so mill documentation matches the drawing. Role in practice: nitrogen-strengthened low-carbon Mo austenitic (316LN-type) for welded pressure tube needing higher proof strength in chloride-bearing service.

SHH STEEL can produce and supply EN 10217-7 1.4429 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover same welded size map as other Mo austenitics with attention to higher Rm/Rp on certificates. Browse the series hub at EN 10217-7.

When the calculation needs 316LN welded pressure tube under EN rules, 1.4429 is the EN 10217-7 steel number — not a handwritten “316L + N” note on an A312 PO. Typical welded pressure duties include higher-design-stress chemical PED lines, nitrogen-specified Mo austenitic replacements for over-thick 316L walls, and cryogenic-adjacent Mo service. Design caution: nitrogen raises strength; it is not a substitute for duplex when chloride SCC is the governing damage mode Commercially the grade is often called 316LN; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4429 / X2CrNiMoN17-13-3 on the MTC. Sister numbers on this hub include EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4311, EN 10217-7 1.4439.4404, 1.4435, 1.4311, 1.4439.

Remember the product-form split: this page is welded EN 10217-7 1.4429; seamless pressure stainless in the same chemistry idea belongs under EN 10216-5. Dimension preference is EN ISO 1127. Manufacturing routes stay longitudinal arc or laser per Table 1 — helical seam is outside the listed Part 7 paths used for this series. Live seamless sister: EN 10216-5 1.4429. Related live ASTM/ASME anchors: A269 TP316L.

Chemical Composition of EN 10217-7 1.4429

Cast chemistry for 1.4429 / X2CrNiMoN17-13-3 is the acceptance gate on every EN 10217-7 heat. Option 6 opens product analysis with the standard’s deviation table. SHH STEEL prints the measured cast figures on the inspection document and will not market private melt windows as EN 10217-7 limits for this austenitic grade.

Public BSSA EN 10217-7 chemistry for 1.4429 / X2CrNiMoN17-13-3 is tabulated below after cross-check to the 2021 framing. Figures are maxima unless shown as ranges. Always reconcile secondary datasheets to the purchased Part 7 edition.

Element 1.4429 cast analysis (mass %)
Carbon (C) ≤0.030
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.045
Sulfur (S) ≤0.015
Nitrogen (N) 0.12–0.22
Chromium (Cr) 16.5–18.5
Nickel (Ni) 11.0–14.0
Molybdenum (Mo) 2.50–3.00

Reference for X2CrNiMoN17-13-3: public BSSA EN 10217-7 chemical compositions article, cross-checked to the 2021 grade list framing. Unlisted elements are not intentional additions without agreement, aside from finishing additions under scrap discipline that protects 1.4429 properties.

Mechanical Properties of EN 10217-7 1.4429

Solution-annealed (+AT) ambient data for steel number 1.4429 (X2CrNiMoN17-13-3) are taken from the EN 10217-7 austenitic table that characterises walls up to roughly 60 mm unless the order agrees values beyond that band. Both Rp0.2 and Rp1.0 appear for austenitics. Sub-zero impact figures at −196 °C are characterisation data until Options make them certified.

The ambient numbers for X2CrNiMoN17-13-3 are taken from BSSA’s BS EN 10217-7 mechanical article (2021 framing). Solution annealing temperatures are public EN cross-checks and stay UNCERTAIN versus paid Part 7 footnotes. SHH STEEL keeps 1.4429 tensile acceptance on the EN 10217-7 table — foreign standard floors are not mixed onto the MTC.

Property 1.4429 ambient (solution annealed +AT)
Rp0.2 min (MPa) 295
Rp1.0 min (MPa) 330
Rm (MPa) 580–800
A min % long / trans 35 / 30
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1020–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 60 at -196 °C (Option to verify)

Reference trail for X2CrNiMoN17-13-3: BSSA EN 10217-7 ambient mechanical article; public EN solution bands with UNCERTAIN vs paid Part 7 footnotes. Charpy values are characterisation data — verify by Option when joules must appear on the 1.4429 MTC.

Welded Tube Manufacture for EN 10217-7 1.4429

Manufacture of EN 10217-7 1.4429 (X2CrNiMoN17-13-3) is longitudinal welded only: automatic arc or laser along the abutting edges of formed strip or plate. Public Table 1 sets the allowed weld-preparation and bead-work combinations; continuous forming from strip is the everyday path, while single forming from plate handles the heavier end of the band. The finished product must not include welds used only to join strip lengths prior to forming. Helical seam manufacture is outside the listed routes for this series. If the drawing demands seamless tube, change the standard to EN 10216-5.

Molybdenum-bearing austenitic 1.4429 (X2CrNiMoN17-13-3) uses the same longitudinal arc/laser Table 1 routes, typically without filler or with matching Mo-bearing filler by wall and procedure. Options 3 and 4 cover inside remelt or bead working for smoothed ID. Delivery symbols W0–W2R, WCA/WCR, WG/WP follow Table 2; Option 5 locks the choice. SHH STEEL can produce and supply 1.4429 as W1A/W2A descaled or WCA/WCR cold-finished in the common pressure-tube band, and as WG/WP when roughness scope is agreed. nitrogen-bearing Mo austenitic fillers; protect nitrogen content in the weld metal per WPS

TC1 versus TC2 is mandatory commercial data for EN 10217-7 1.4429. It governs how aggressively the weld seam is examined and how tensile units are taken, while leak-tightness stays comprehensive (Option 15 optional lock). SHH STEEL’s X2CrNiMoN17-13-3 mill pack states route and delivery symbol without guesswork.

Dimensions and Tolerances for EN 10217-7 1.4429

Dimensional ordering for 1.4429 / X2CrNiMoN17-13-3 is OD × wall under EN ISO 1127 preferences. Stainless density, not carbon-steel 7.85, drives mass. EN 10217-7 tolerance classes apply, with Option 20 available for D4. Ovality stays within diameter tolerance; eccentricity within wall tolerance; abutting-edge radial offset at the longitudinal weld is capped by the standard’s dimensional clauses.

Option 19 covers exact lengths; Option 18 covers bevels when wall is at least 3.2 mm. For precision OD on 1.4429, WCA/WCR cold-finished delivery is often the first finish talk after descaled W1A/W2A. SHH STEEL freezes size, tolerance class, and Table 2 symbol against the order before the weld line is scheduled.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

Dimensional conformity on 1.4429 is checked against the ordered EN ISO 1127 / Part 7 class before release. Straightness and end condition for X2CrNiMoN17-13-3 follow the standard’s clauses; SHH STEEL records measured OD × wall on the inspection document rather than assuming catalogue mid-tolerance. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4429 / X2CrNiMoN17-13-3 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4429

The welded pressure-tube nameplate for this chemistry is EN 10217-7 1.4429 with steel name X2CrNiMoN17-13-3. Commercial alias 316LN may appear on ASTM/ASME tubing or pipe pages, but those standards are not automatic substitutes. Seamless EN 10216-5 is a sister product form, not a second way to accept a welded Part 7 seam.

Cross-standard shopping for 316LN chemistry is common; acceptance is not. EN 10217-7 1.4429 remains the welded pressure-tube contract for X2CrNiMoN17-13-3 on this page. Seamless sisters and ASTM/ASME pages are references until the order explicitly dual-certifies under each standard’s clauses.

Reference Designation Note
EN 10217-7 1.4429 / X2CrNiMoN17-13-3 This product standard (welded pressure tube)
EN steel name X2CrNiMoN17-13-3 EN 10027-1 designation used in body and marking
Commercial alias (body only) 316LN Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4429 Related live page — different product form (seamless)
A269 TP316L A269 TP316L Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4311, EN 10217-7 1.4439. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4429. Live cross-standard anchors: A269 TP316L.

Heat Treatment and Delivery Condition for EN 10217-7 1.4429

Delivery condition and heat treatment travel together on EN 10217-7 1.4429. Symbols such as W1A/W2A, WCA/WCR, and W1R/W2R imply the heat-treatment path; mechanical data assume solution-annealed (+AT) X2CrNiMoN17-13-3. Uniform heating into the solution band and rapid cooling are the reference story.

Public solution-annealing guidance for X2CrNiMoN17-13-3 sits at 1020–1120 °C with water or air cooling. Cross-check source is public EN 10216-5 / EN 10028-7 framing — labelled UNCERTAIN versus paid Part 7:2021 footnotes. Surface (pickle, bright anneal, grind, polish) rides on Option 5 / the chosen Table 2 symbol for 1.4429.

Item 1.4429
Solution annealing band (public) 1020–1120 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

No 1.4429 length leaves SHH STEEL outside the ordered delivery-condition story. Certificates for X2CrNiMoN17-13-3 list the Table 2 symbol, confirm heat treatment when the symbol demands it, and call out recrystallized-weld status on WCA/WCR product so goods-in inspectors are not left reading between the lines.

Corrosion Resistance of EN 10217-7 1.4429

For 316LN-class welded pressure tube under steel number 1.4429, corrosion performance rests on Mo plus nitrogen; improved mechanical floors with 316L-family localised corrosion behaviour. Tables may indicate IGC resistance as delivered for X2CrNiMoN17-13-3; ordering Option 13 is what puts a tested EN ISO 3651-2 result onto the certificate.

Corrosion upgrades from 1.4429 are steel-number changes, not certificate footnotes. X2CrNiMoN17-13-3 has a defined window; EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4311, EN 10217-7 1.4439 cover adjacent windows. SHH STEEL declines to invent PREN/CPT floors or to misread sensitisation guidance as a design stress table.

Applications of EN 10217-7 1.4429 Tube

Specify EN 10217-7 1.4429 when the line list wants 316LN-class welded pressure tube for duties such as higher-design-stress chemical PED lines, nitrogen-specified Mo austenitic replacements for over-thick 316L walls, and cryogenic-adjacent Mo service. The steel name X2CrNiMoN17-13-3 belongs on the MTC with TC1 or TC2 and the chosen Table 2 symbol.

Do not force 1.4429 into seamless-only drawings (switch to EN 10216-5 — see EN 10216-5 1.4429), pure ASTM tubing/pipe scopes without EN dual marking, or media that outclass this chemistry. SHH STEEL can produce and supply EN 10217-7 1.4429 and will recommend EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4311, EN 10217-7 1.4439 or a live cross-standard page when selection is still open. Related live pages: A269 TP316L.

Weldability of EN 10217-7 1.4429

Weldability talk for 316LN under steel number 1.4429 splits mill seam versus fabricator joint. The mill follows Part 7 longitudinal routes for X2CrNiMoN17-13-3; the fabricator picks process and filler for the spool. Shop guidance on this page: nitrogen-bearing Mo austenitic fillers; protect nitrogen content in the weld metal per WPS

Fabricator responsibility covers as-welded corrosion risk, duplex phase balance where relevant, and any PWHT the joint calculation demands on 1.4429. SHH STEEL supplies the mill product: ordered chemistry, seam route, heat treatment/delivery symbol, tensile floors, leak-tightness, and listed Options for X2CrNiMoN17-13-3.

Surface Finishes for EN 10217-7 1.4429

Read the finish for steel number 1.4429 from the delivery symbol first. W1A/W2A descaled X2CrNiMoN17-13-3 is the everyday pressure-tube look; W1R/W2R and WCR bright anneal serve buyers who need a cleaner outside diameter; WG/WP are written scopes, not implied catalogue grades. Packing instructions for this austenitic grade keep bare carbon steel off the tube. Free iron from foreign banding creates receiving NCRs that a PED spool does not have time to argue about on 316LN material.

ID cleanliness beyond the Table 2 story — Ra caps, electropolish, solvent wipe — must be written on the 1.4429 purchase order. SHH STEEL can produce and supply descaled, bright-annealed, and polished routes for X2CrNiMoN17-13-3 with measurable results, and refuses phantom surface grades that cannot be shown on the EN 10204 document for this 316LN tube.

Finish upgrades on X2CrNiMoN17-13-3 consume furnace and polishing capacity that descaled 1.4429 does not — schedule them explicitly. SHH STEEL confirms the Table 2 symbol against finishing slots and will say when a requested WP grit cannot be measured on the ordered OD × wall rather than shipping hopeful 316LN tube.

Inspection and Testing for EN 10217-7 1.4429

Inspection on 1.4429 is specific, not statistical sampling theatre. One cast analysis per heat; tensile once per test unit under TC1 and twice from different tubes under TC2; technological tests per the D/T matrix; leak-tightness on every length (hydro or ET, Option 15 to choose); plus dimensions, visuals, and ID of X2CrNiMoN17-13-3.

Under TC2 the longitudinal seam sees a tougher NDT package; laminar and edge Options appear for starting product. Order Option 13 when IGC must be tested; order impact Options when joules must appear on the certificate. SHH STEEL 3.1 documents for 1.4429 state chemistry, heat-treatment/delivery status, tensile, and leak/NDT — mandatory tests stay.

Subcontract NDT on 1.4429, when used, remains under the manufacturer’s Part 7 responsibility. SHH STEEL does not treat a subcontractor stamp as a substitute for the ordered TC1/TC2 regime on X2CrNiMoN17-13-3.

Packaging and Shipping for EN 10217-7 1.4429

Outbound packing for 1.4429 / X2CrNiMoN17-13-3 welded pressure tube starts with protected ends, size segregation, and moisture barrier wrap on export loads. Bright-annealed and polished OD (W1R/W2R, WCR, WP) take sleeve or paper wrap against transit galling; descaled W1A/W2A utility tube still needs clean supports under the longitudinal seam. Bundle contact with carbon steel is forbidden in SHH STEEL packing instructions for this grade: rust blooms from foreign iron are visible defects on 316LN OD and are treated as packing failures, not cosmetic footnotes.

Stencil content for 1.4429 normally shows maker, OD × wall, EN 10217-7, 1.4429 or X2CrNiMoN17-13-3, cast, TC1/TC2, inspection mark, and correlation number. Delivery-condition letters appear when useful or when Option 5 made them contractual. SHH STEEL reconciles tags to the purchase-order marking clause before trucks leave.

Bundle IDs on the packing list point back to heats on the 1.4429 certificate. Exact-length and bevelled pieces are kept separate and end-protected. Packaging clauses in the PO are implemented before X2CrNiMoN17-13-3 leaves the yard. SHH STEEL treats packing and marking for EN 10217-7 1.4429 / X2CrNiMoN17-13-3 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and supply X2CrNiMoN17-13-3 under EN 10217-7 1.4429 with the heat treatment, TC1/TC2 tests, and EN 10204 3.1 paperwork the order names — not a relabelled 316LN remnant. Part 7 stays separate from seamless Part 5 and from ASTM tubing/pipe standards on the certificate; wrong-table tensile paste-ups are refused.

Practical selection beats wishful stamping. Sisters worth comparing: LINKPLACE1.4404, LINKPLACE1.4435, LINKPLACE1.4311, LINKPLACE1.4439. Caution on 1.4429: nitrogen raises strength; it is not a substitute for duplex when chloride SCC is the governing damage mode We would rather redirect the enquiry than ship the wrong EN number Linked sisters on this hub: EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4311, EN 10217-7 1.4439. Live ASTM/ASME anchors: A269 TP316L.

Supply Capability

Enquiry intake for 1.4429 / X2CrNiMoN17-13-3: SHH STEEL can produce and make EN 10217-7 welded tube to the edition, TC1/TC2, delivery symbol, and options you name. Use the capability table and Stock / Available sizes map as a starting size conversation. Same welded size map as other mo austenitics with attention to higher rm/rp on certificates.

Item SHH STEEL capability for 1.4429
Standard EN 10217-7
Grade 1.4429 / X2CrNiMoN17-13-3
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Stock / Available sizes for 1.4429 is an enquiry map. Heats of X2CrNiMoN17-13-3, forming/weld capacity, and finish route decide what can ship when. Provide OD × wall, test category, and delivery symbol rather than assuming shelf SKUs.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Options 19/18/13 and dual quotes with 1.4404, 1.4435, 1.4311, 1.4439 are normal add-ons. Size bands were sense-checked against peer catalogues; contractual acceptance is still EN 10217-7 with EN ISO 1127. SHH STEEL can produce and supply 1.4429 when capacity matches the order.

FAQ

What is EN 10217-7 1.4429 welded stainless steel tube used for?
EN 10217-7 1.4429 (X2CrNiMoN17-13-3) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is higher-design-stress chemical PED lines, nitrogen-specified Mo austenitic replacements for over-thick 316L walls, and cryogenic-adjacent Mo service. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4429 the same as 316LN under ASTM A269 or A312?
No. Commercial alias 316LN may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP316L.
Does EN 10217-7 1.4429 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4429. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4429?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 295 MPa, Rp1.0 min 330 MPa, Rm 580–800 MPa, and elongation 35% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4429 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4429 when the enquiry names this steel number or the duty matches nitrogen-strengthened low-carbon Mo austenitic (316LN-type) for welded pressure tube needing higher proof strength in chloride-bearing service. Compare EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4311, EN 10217-7 1.4439 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: nitrogen raises strength; it is not a substitute for duplex when chloride SCC is the governing damage mode
What delivery conditions are available for EN 10217-7 1.4429?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4429?
SHH STEEL can produce and supply EN 10217-7 1.4429 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Same welded size map as other mo austenitics with attention to higher rm/rp on certificates.
TC1 or TC2 for EN 10217-7 1.4429?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4429?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4429.
What documents come with SHH STEEL EN 10217-7 1.4429?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4429, size, cast, and test category.
How do I enquire for EN 10217-7 1.4429 with SHH STEEL?
Send EN 10217-7, steel number 1.4429 / X2CrNiMoN17-13-3, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4429 (X2CrNiMoN17-13-3) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4429 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X