EN 10217-7 1.4432 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4432 Welded Stainless Steel Tube

EN 10217-7 1.4432 / X2CrNiMo17-12-3 welded stainless pressure tube (316L (higher Mo)), austenitic, cast analysis per EN table, ambient Rp0.2 min 190 MPa, Rm 490–690, solution annealed 1020–1120 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4432 / X2CrNiMo17-12-3 (316L (higher Mo) — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4432 Welded Stainless Steel Tube

When an enquiry still reads “316L (higher Mo) welded pressure tube” without a European product standard, the PED paperwork is incomplete. EN 10217-7:2021 closes that gap for circular welded austenitic and duplex stainless tubes; within that list, 1.4432 / X2CrNiMo17-12-3 is the austenitic entry that matches this chemistry. SHH STEEL treats the steel number, not the shop alias, as the acceptance key on cast analysis, longitudinal arc or laser seam route, solution annealing where the delivery symbol requires it, and the TC1/TC2 inspection regime. Duty focus: low-carbon austenitic with Mo raised into the 2.5–3.0% band for welded pressure tube needing more pitting resistance than standard 1.4404.

SHH STEEL can produce and supply EN 10217-7 1.4432 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover mid to large welded OD where strip/plate forming routes dominate. Browse the series hub at EN 10217-7.

1.4432 exists on EN 10217-7 even when a seamless EN 10216-5 sister page is thin on the site — welded pressure buyers who need the higher-Mo L analysis should order this number explicitly. Typical welded pressure duties include chloride-rich process water, warm seawater-adjacent utilities, and chemical lines where 1.4404 PREN-type thinking is marginal. Design caution: higher Mo helps pitting; SCC under chloride + stress + temperature may still push the design to duplex — do not stretch 1.4432 into 2205 territory on price alone Commercially the grade is often called 316L (higher Mo); keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4432 / X2CrNiMo17-12-3 on the MTC. Sister numbers on this hub include EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4436, EN 10217-7 1.4462.4404, 1.4435, 1.4436, 1.4462.

Welded-only scope matters on every 1.4432 order. Seamless sisters are a different standard (EN 10216-5). Sizes prefer EN ISO 1127. Table 1 manufacture is longitudinal automatic arc or laser from strip/plate; do not specify spiral and expect automatic Part 7 acceptance without a written agreement outside the listed routes. A seamless EN 10216-5 page for 1.4432 was not confirmed live on steelspecs.com when this pack was audited (HTTP check 2026-10-30 Asia/Shanghai). Related live ASTM/ASME anchors: A269 TP316L, A312 TP316L.

Chemical Composition of EN 10217-7 1.4432

Ladle analysis controls 1.4432. The austenitic table entry for X2CrNiMo17-12-3 is what the cast must satisfy; product analysis remains Option 6. SHH STEEL’s EN 10204 paperwork shows real cast results — catalogue “typical” chemistries are not substituted for EN acceptance on 316L (higher Mo)-class welded pressure tube.

Below is the BSSA-published EN 10217-7 cast window for X2CrNiMo17-12-3 (steel number 1.4432), aligned to the 2021 list. Maxima apply unless a min–max range appears. Edition confirmation beats brochure reprint.

Element 1.4432 cast analysis (mass %)
Carbon (C) ≤0.030
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.045
Sulfur (S) ≤0.015
Nitrogen (N) ≤0.10
Chromium (Cr) 16.5–18.5
Nickel (Ni) 10.5–13.0
Molybdenum (Mo) 2.50–3.00

Chemistry source for steel number 1.4432: BSSA EN 10217-7 chemical article plus public standard cross-check. Do not treat unlisted elements as free additions on X2CrNiMo17-12-3 without purchaser agreement (finishing additions excepted under controlled scrap practice).

Mechanical Properties of EN 10217-7 1.4432

For X2CrNiMo17-12-3 ordered as EN 10217-7 1.4432, room-temperature mechanical acceptance follows the austenitic ambient table in the solution-annealed (+AT) condition within about 60 mm wall unless Options extend the band. Expect Rp0.2 and Rp1.0 minima plus Rm and elongation. Cryogenic Charpy characterisation exists; tested joules require the relevant Options.

Primary ambient source for 1.4432: BSSA mechanical properties for stainless steels to BS EN 10217-7. Heat-treatment bands for X2CrNiMo17-12-3 are public EN stainless figures with an UNCERTAIN flag against paid EN 10217-7:2021 footnotes. Sister-standard tensile values are not silently copied onto this Part 7 document.

Property 1.4432 ambient (solution annealed +AT)
Rp0.2 min (MPa) 190
Rp1.0 min (MPa) 225
Rm (MPa) 490–690
A min % long / trans 40 / 30
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1020–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 60 at -196 °C (Option to verify)

Ambient mechanical citation for steel number 1.4432: BSSA EN 10217-7 article; annealing bands public EN cross-check (UNCERTAIN vs paid 2021 footnotes). Order impact Options when tested toughness for X2CrNiMo17-12-3 must be certified.

Welded Tube Manufacture for EN 10217-7 1.4432

For austenitic grade 1.4432, Part 7 manufacture starts with strip or plate of X2CrNiMo17-12-3 chemistry, forms a circular section, and closes it with a longitudinal automatic arc or laser weld per Table 1. Filler may or may not be used depending on route and wall. Outside grinding or bead working before heat treatment appear where the ordered path requires them. Commodity sizes usually run on continuous strip lines; heavier walls move to plate forming. Spiral weld is not invented here as a standard Part 7 route. Seamless product is a different standard — EN 10216-5.

Molybdenum-bearing austenitic 1.4432 (X2CrNiMo17-12-3) uses the same longitudinal arc/laser Table 1 routes, typically without filler or with matching Mo-bearing filler by wall and procedure. Options 3 and 4 cover inside remelt or bead working for smoothed ID. Delivery symbols W0–W2R, WCA/WCR, WG/WP follow Table 2; Option 5 locks the choice. SHH STEEL can produce and supply 1.4432 as W1A/W2A descaled or WCA/WCR cold-finished in the common pressure-tube band, and as WG/WP when roughness scope is agreed. overmatching Mo austenitic fillers are often selected; confirm ferrite and corrosion testing when Option 13 is on the order

The 1.4432 order is unfinished until TC1 or TC2 is chosen. That choice shapes NDT and tensile frequency on the longitudinal seam while leak-tightness remains per tube (Option 15 to prescribe method). SHH STEEL states the Table 1 route and Table 2 symbol actually run on X2CrNiMo17-12-3.

Dimensions and Tolerances for EN 10217-7 1.4432

Specify D and T when buying EN 10217-7 1.4432 (X2CrNiMo17-12-3). EN ISO 1127 preferred sizes are the usual starting list; mass uses stainless density tables. Diameter/wall classes follow Part 7 with EN ISO 1127, including Option 20 D4. Out-of-roundness and eccentricity are absorbed inside those tolerances; weld-edge radial mismatch is separately limited.

Cut-to-length (Option 19) and bevelled ends (Option 18, wall ≥ 3.2 mm) are everyday extras on X2CrNiMo17-12-3 welded tube. Tighter OD conversations usually move toward WCA/WCR. SHH STEEL matches the ordered D × T, tolerance class, and delivery symbol before committing 1.4432 weld capacity.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

For X2CrNiMo17-12-3 welded tube, SHH STEEL verifies OD, wall, and the selected tolerance class on EN 10217-7 1.4432 before marking. Straightness and end-finish rules in the dimensional clauses still apply — they are not waived by a tight delivery promise. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4432 / X2CrNiMo17-12-3 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4432

Designation discipline: EN 10217-7 writes 1.4432 / X2CrNiMo17-12-3; shops say 316L (higher Mo). Related ASTM/ASME product pages are cross-references only — wall basis, tensile tables, and inspection differ. EN 10216-5 seamless pages are chemistry cousins with a different manufacture and acceptance route.

Bill-of-materials writers sometimes list 316L (higher Mo) next to EN and ASTM numbers interchangeably. For this product, steel number 1.4432 with name X2CrNiMo17-12-3 under EN 10217-7 is the welded acceptance path; confirm any dual mark against both mechanical tables before release to fabrication.

Reference Designation Note
EN 10217-7 1.4432 / X2CrNiMo17-12-3 This product standard (welded pressure tube)
EN steel name X2CrNiMo17-12-3 EN 10027-1 designation used in body and marking
Commercial alias (body only) 316L (higher Mo) Not a substitute for the steel number on the MTC
A269 TP316L A269 TP316L Related live page — different product standard
A312 TP316L A312 TP316L Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4436, EN 10217-7 1.4462. Hub: EN 10217-7. Live cross-standard anchors: A269 TP316L, A312 TP316L.

Heat Treatment and Delivery Condition for EN 10217-7 1.4432

For X2CrNiMo17-12-3 ordered as 1.4432, pick a Table 2 symbol that encodes the required heat treatment and surface. Solution annealing (+AT) underpins the ambient mechanical table: bring the tube into the solution-temperature window and cool quickly enough to satisfy strength and corrosion notes. For X2CrNiMo17-12-3 under steel number 1.4432, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Solution band used on this page for 1.4432: 1020–1120 °C, cool by water or air (public EN stainless cross-check; UNCERTAIN vs paid EN 10217-7:2021 footnotes). Lock the delivery-condition symbol with Option 5 when pickle versus bright anneal versus WG/WP must be contractual for X2CrNiMo17-12-3.

Item 1.4432
Solution annealing band (public) 1020–1120 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

Heat-treatment honesty is part of the X2CrNiMo17-12-3 supply package: SHH STEEL documents the delivery-condition symbol actually run on EN 10217-7 1.4432, including whether the longitudinal weld was recrystallized on cold-finished routes, rather than implying a generic “annealed” stamp without Table 2 language. For X2CrNiMo17-12-3 under steel number 1.4432, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Corrosion Resistance of EN 10217-7 1.4432

For 316L (higher Mo)-class welded pressure tube under steel number 1.4432, corrosion performance rests on elevated Mo versus 1.4404 improves localised corrosion resistance in many chloride media while keeping low carbon for as-welded IGC. Tables may indicate IGC resistance as delivered for X2CrNiMo17-12-3; ordering Option 13 is what puts a tested EN ISO 3651-2 result onto the certificate.

Corrosion footnotes and IGC options on 1.4432 exist so purchasers can prove delivery-condition resistance when required. They do not authorise PREN claims for X2CrNiMo17-12-3. Move among EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4436, EN 10217-7 1.4462 for alloy upgrades instead of stretching certificate language.

Applications of EN 10217-7 1.4432 Tube

Specify EN 10217-7 1.4432 when the line list wants 316L (higher Mo)-class welded pressure tube for duties such as chloride-rich process water, warm seawater-adjacent utilities, and chemical lines where 1.4404 PREN-type thinking is marginal. The steel name X2CrNiMo17-12-3 belongs on the MTC with TC1 or TC2 and the chosen Table 2 symbol.

Do not force 1.4432 into seamless-only drawings (switch to EN 10216-5), pure ASTM tubing/pipe scopes without EN dual marking, or media that outclass this chemistry. SHH STEEL can produce and supply EN 10217-7 1.4432 and will recommend EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4436, EN 10217-7 1.4462 or a live cross-standard page when selection is still open. Related live pages: A269 TP316L, A312 TP316L.

Weldability of EN 10217-7 1.4432

Weldability talk for 316L (higher Mo) under steel number 1.4432 splits mill seam versus fabricator joint. The mill follows Part 7 longitudinal routes for X2CrNiMo17-12-3; the fabricator picks process and filler for the spool. Shop guidance on this page: overmatching Mo austenitic fillers are often selected; confirm ferrite and corrosion testing when Option 13 is on the order

PED joint design — including whether X2CrNiMo17-12-3 can remain as-welded in corrosive service — is outside mill scope. SHH STEEL’s deliverable for 1.4432 is compliant welded tube with documented chemistry, route, delivery condition, mechanical results, and leak/NDT statements.

Surface Finishes for EN 10217-7 1.4432

For X2CrNiMo17-12-3 welded under EN 10217-7 1.4432, finish language equals Table 2 language: descaled for utility, bright-annealed for cleaner OD, ground or polished when roughness is contractual. Agree WP/WG at enquiry with inspectable criteria. Transit contact with carbon steel is forbidden because free-iron rust blooms on 316L (higher Mo) OD fail goods-in visual checks and contaminate stainless systems downstream of the weld seam.

Special ID finishes are order lines. When measurement is possible, SHH STEEL can produce and supply pickled, bright-annealed, and polished 1.4432; we will not invent an Ra number for 316L (higher Mo) or imply electropolish that was never run on X2CrNiMo17-12-3. Exterior polish without an agreed grit is equally unacceptable as certificate language.

When 316L (higher Mo) welded tube must look like instrumentation stock, bright anneal or polish belongs on the order with 1.4432. Descaled W1A/W2A remains correct for many lagged utility runs. SHH STEEL can produce and supply only the finish path X2CrNiMo17-12-3 can actually certify under EN 10217-7 on the promised date.

Inspection and Testing for EN 10217-7 1.4432

For EN 10217-7 1.4432 / X2CrNiMo17-12-3, expect cast chemistry per heat, ambient tensile at TC1/TC2 frequency, technological tests from the standard’s table, and 100% leak-tightness (hydrostatic or eddy current). Dimensional, visual, and material-identification checks close the baseline regime. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4432 purchase order so X2CrNiMo17-12-3 inspection planning matches the PED file before weld slots are locked.

Heavier weld-seam NDT is the TC2 differentiator on 1.4432. Laminar/edge NDT Options, IGC Option 13, and Charpy Options are purchaser choices. SHH STEEL’s EN 10204 3.1 file records what was melted, how X2CrNiMo17-12-3 was heat-treated, what tensile was achieved, and which leak/NDT path ran — without skipping required tests for speed.

Hardness is not a substitute for tensile acceptance on EN 10217-7 1.4432. SHH STEEL reports the ambient tensile package required for X2CrNiMo17-12-3 and treats hardness, when requested, as supplementary data only.

Packaging and Shipping for EN 10217-7 1.4432

SHH STEEL ships EN 10217-7 1.4432 in end-protected, size-sorted bundles or wooden crates with waterproof wrapping for sea freight. Bright-annealed and polished OD (W1R/W2R, WCR, WP) take sleeve or paper wrap against transit galling; descaled W1A/W2A utility tube still needs clean supports under the longitudinal seam. Because X2CrNiMo17-12-3 is stainless, packing deliberately keeps carbon-steel strapping and rusty fixtures off the tube surface — free-iron transfer is a common transit complaint on 316L (higher Mo) and is prevented at the dock, not debated later.

Traceability marking on X2CrNiMo17-12-3 welded tube carries EN 10217-7, steel number 1.4432, size, cast, test category, and inspection/correlation marks. Delivery symbols are added when ordered or when clarity helps receiving. SHH STEEL aligns stencil language with the PO before dispatch. SHH STEEL treats packing and marking for EN 10217-7 1.4432 / X2CrNiMo17-12-3 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Heat-to-bundle correlation on export documents saves receiving time for 316L (higher Mo) welded tube. Cut-to-length and bevelled lots are packed apart with caps fitted. SHH STEEL applies the agreed packing note on every 1.4432 shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4432 / X2CrNiMo17-12-3 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and make EN 10217-7 1.4432 welded pressure tube for buyers who need documented X2CrNiMo17-12-3 chemistry, delivery-condition heat treatment, and leak-tightness — not a shop-floor 316L (higher Mo) stamp. We refuse to blur this page into EN 10216-5 seamless acceptance or to decorate MTCs with foreign tensile floors.

When 316L (higher Mo) is the wrong tool, SHH STEEL steers toward EN 10217-7 LINKPLACE1.4404, EN 10217-7 LINKPLACE1.4435, EN 10217-7 LINKPLACE1.4436, EN 10217-7 LINKPLACE1.4462. Keep this caution in view: higher Mo helps pitting; SCC under chloride + stress + temperature may still push the design to duplex — do not stretch 1.4432 into 2205 territory on price alone A mis-selected steel number helps no PED dossier. Live ASTM/ASME anchors: A269 TP316L, A312 TP316L.

Supply Capability

SHH STEEL can produce and supply welded EN 10217-7 1.4432 when your enquiry states standard edition, test category, delivery condition, and options. Capability and Stock / Available sizes tables below support first sizing for this 316L (higher Mo) pressure grade. Mid to large welded od where strip/plate forming routes dominate.

Item SHH STEEL capability for 1.4432
Standard EN 10217-7
Grade 1.4432 / X2CrNiMo17-12-3
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Treat the size map as availability language for 316L (higher Mo) welded pressure tube, not a tonnage inventory. 1.4432 depends on X2CrNiMo17-12-3 flat-product supply and weld finishing. Confirm against your OD × wall and TC1/TC2 list.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Exact length, bevel, IGC, and sister-grade duals (1.4404, 1.4435, 1.4436, 1.4462) can share one enquiry. Catalogue size patterns are indicative; EN 10217-7 governs. SHH STEEL can produce and supply X2CrNiMo17-12-3 welded tube in this map when the mill path fits.

FAQ

What is EN 10217-7 1.4432 welded stainless steel tube used for?
EN 10217-7 1.4432 (X2CrNiMo17-12-3) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is chloride-rich process water, warm seawater-adjacent utilities, and chemical lines where 1.4404 PREN-type thinking is marginal. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4432 the same as 316L (higher Mo) under ASTM A269 or A312?
No. Commercial alias 316L (higher Mo) may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP316L, A312 TP316L.
Does EN 10217-7 1.4432 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. A seamless EN 10216-5 page for 1.4432 was not confirmed live when this pack was written. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4432?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 190 MPa, Rp1.0 min 225 MPa, Rm 490–690 MPa, and elongation 40% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4432 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4432 when the enquiry names this steel number or the duty matches low-carbon austenitic with Mo raised into the 2.5–3.0% band for welded pressure tube needing more pitting resistance than standard 1.4404. Compare EN 10217-7 1.4404, EN 10217-7 1.4435, EN 10217-7 1.4436, EN 10217-7 1.4462 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: higher Mo helps pitting; SCC under chloride + stress + temperature may still push the design to duplex — do not stretch 1.4432 into 2205 territory on price alone
What delivery conditions are available for EN 10217-7 1.4432?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4432?
SHH STEEL can produce and supply EN 10217-7 1.4432 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Mid to large welded od where strip/plate forming routes dominate.
TC1 or TC2 for EN 10217-7 1.4432?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4432?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4432.
What documents come with SHH STEEL EN 10217-7 1.4432?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4432, size, cast, and test category.
How do I enquire for EN 10217-7 1.4432 with SHH STEEL?
Send EN 10217-7, steel number 1.4432 / X2CrNiMo17-12-3, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4432 (X2CrNiMo17-12-3) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4432 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X