EN 10217-7 1.4401 Welded Stainless Steel Tube
What is EN 10217-7 1.4401 Welded Stainless Steel Tube
EN 10217-7 covers welded stainless pressure tube only — seamless twins live under EN 10216-5. For welded product, steel number 1.4401 (X5CrNiMo17-12-2) sits in the austenitic grade tables and is the designation that belongs on the MTC when the commercial conversation still says 316. Specifying EN 10217-7, 1.4401, test category, and delivery-condition / options on the purchase order is what makes cast chemistry, weld-seam manufacture, heat treatment, mechanical floors, leak-tightness, and marking line up. Engineering role: standard-carbon Mo-bearing austenitic welded pressure tube when the order names 1.4401 / X5CrNiMo17-12-2 rather than the L grade.
SHH STEEL can produce and supply EN 10217-7 1.4401 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover same Mo austenitic welded size conversation as 1.4404. Browse the series hub at EN 10217-7.
1.4401 is not “almost 1.4404” on a PED weldment — carbon ceiling and IGC footnotes differ, and the MTC must show the ordered steel number. Typical welded pressure duties include general chemical and utility PED lines where as-welded IGC is controlled by procedure or post-weld treatment, and Mo is still required. Design caution: carbon up to 0.07% raises as-welded sensitisation risk versus 1.4404 — do not substitute 1.4401 for an L-grade drawing without design review Commercially the grade is often called 316; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4401 / X5CrNiMo17-12-2 on the MTC. Sister numbers on this hub include EN 10217-7 1.4404, EN 10217-7 1.4571, EN 10217-7 1.4436, EN 10217-7 1.4301.4404, 1.4571, 1.4436, 1.4301.
Do not mix product forms: EN 10217-7 1.4401 is welded tube; seamless pressure tube is EN 10216-5. EN ISO 1127 guides preferred sizes. Longitudinal arc/laser routes in Table 1 are the manufacture story — spiral is not treated as a standard Part 7 route on this page. Live seamless sister: EN 10216-5 1.4401. Related live ASTM/ASME anchors: A269 TP316, A213 TP316.
Chemical Composition of EN 10217-7 1.4401
For X5CrNiMo17-12-2 ordered as EN 10217-7 1.4401, cast (ladle) analysis is mandatory against the grade table. Option 6 covers product analysis deviations. SHH STEEL reports the cast that was melted and will not present unpublished tighter ranges as if they were Part 7 limits.
Composition limits shown for 1.4401 follow BSSA’s EN 10217-7 chemical article with public standard cross-check. Ranges beat single maxima where printed. Use the purchased 2021 edition as the contractual text.
| Element | 1.4401 cast analysis (mass %) |
|---|---|
| Carbon (C) | ≤0.07 |
| Silicon (Si) | ≤1.00 |
| Manganese (Mn) | ≤2.00 |
| Phosphorus (P) | ≤0.045 |
| Sulfur (S) | ≤0.015 |
| Nitrogen (N) | ≤0.10 |
| Chromium (Cr) | 16.5–18.5 |
| Nickel (Ni) | 10.0–13.0 |
| Molybdenum (Mo) | 2.0–2.5 |
Cast limits tabulated for 1.4401 follow BSSA’s EN 10217-7 chemical publication with a public Part 7 cross-check. For this austenitic X5CrNiMo17-12-2 entry, intentional addition of unlisted elements needs purchaser agreement; finishing additions remain under scrap controls that protect corrosion and toughness.
Mechanical Properties of EN 10217-7 1.4401
The austenitic ambient mechanical table under EN 10217-7 governs 1.4401 / X5CrNiMo17-12-2 after solution annealing (+AT), typically through walls near 60 mm unless agreed otherwise. Proof stresses are listed as Rp0.2 and Rp1.0. Impact energies at −196 °C are published as characterisation — order Options when the certificate must show them.
BSSA’s EN 10217-7 ambient mechanical article is the public crib behind the 1.4401 table. Annealing bands for X5CrNiMo17-12-2 are cross-checked from public EN stainless documents and marked UNCERTAIN vs paid Part 7:2021 footnotes. SHH STEEL refuses to blend ASTM or seamless-only tensile floors into this welded certificate.
| Property | 1.4401 ambient (solution annealed +AT) |
|---|---|
| Rp0.2 min (MPa) | 205 |
| Rp1.0 min (MPa) | 240 |
| Rm (MPa) | 510–710 |
| A min % long / trans | 40 / 30 |
| IGC resistance (delivery) | Yes* (method A; normally not in sensitised condition) |
| Solution annealing (public EN band) | 1020–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges |
| Cooling | water or air |
| Charpy sub-zero (transverse min J) | 60 at -196 °C (Option to verify) |
Citation for 1.4401 / X5CrNiMo17-12-2: BSSA mechanical properties to BS EN 10217-7 (ambient) plus public EN annealing bands flagged UNCERTAIN vs paid Part 7 footnotes. Impact lines are characterisation until Options convert them to tested results.
Welded Tube Manufacture for EN 10217-7 1.4401
The weld seam on EN 10217-7 1.4401 is longitudinal, not spiral. Arc or laser welding joins the formed edges of X5CrNiMo17-12-2 strip or plate under one of the Table 1 manufacturing routes, with subsequent outside grind or bead work when that path is selected. Continuous strip forming dominates everyday OD; plate routes cover larger diameters and thicker walls. Welds that only joined coil ends before forming must not remain in the finished tube. Specify EN 10216-5 when the line needs seamless pressure stainless instead of this welded Part 7 product.
Molybdenum-bearing austenitic 1.4401 (X5CrNiMo17-12-2) uses the same longitudinal arc/laser Table 1 routes, typically without filler or with matching Mo-bearing filler by wall and procedure. Options 3 and 4 cover inside remelt or bead working for smoothed ID. Delivery symbols W0–W2R, WCA/WCR, WG/WP follow Table 2; Option 5 locks the choice. SHH STEEL can produce and supply 1.4401 as W1A/W2A descaled or WCA/WCR cold-finished in the common pressure-tube band, and as WG/WP when roughness scope is agreed. 316/316L fillers depending on procedure; prefer L fillers when as-welded corrosion is in scope
Mandatory order data for 1.4401 includes the test category. TC2 means a heavier seam NDT story than TC1; leak testing remains 100% with Option 15 available to lock hydrostatic or eddy current. SHH STEEL writes the executed Table 1 route and Table 2 symbol onto the X5CrNiMo17-12-2 inspection package.
Dimensions and Tolerances for EN 10217-7 1.4401
For X5CrNiMo17-12-2 welded pressure tube as 1.4401, the purchase order states outside diameter and wall. Preferred dimensions track EN ISO 1127; mass calculations use stainless densities. Tolerance language is EN 10217-7 / EN ISO 1127, with Option 20 for D4. Keep ovality and eccentricity inside their parent tolerances; watch radial offset at the seam.
When lengths must be exact, call Option 19; when ends need bevels on wall ≥ 3.2 mm, call Option 18. Instrumentation and hygienic OD on 1.4401 often prefer cold-finished WCA/WCR. Size, tolerance, and delivery-condition symbol are aligned by SHH STEEL before the forming/weld slot is booked.
| Route / condition | Typical use | Notes |
|---|---|---|
| W1 / W1A / W1R | Hot-rolled starting flat product | Descaled or bright-annealed per symbol |
| W2 / W2A / W2R | Cold-rolled starting flat product | Smoother OD than W1 family except at weld |
| WCA / WCR | Cold finished ≥20% after weld | Recrystallized weld metal; OD often ≤168.3 mm |
| WG / WP | Ground / polished | Agree ID/OD scope and grit at enquiry |
Measured OD × wall for 1.4401 appear on the EN 10204 document against the class you ordered. Straightness and ends for X5CrNiMo17-12-2 track Part 7; if Option 20 D4 is named, the finishing route must be capable of holding it. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4401 / X5CrNiMo17-12-2 on the inspection document rather than assuming mid-tolerance catalogue values.
Equivalent Grades for EN 10217-7 1.4401
Under Part 7 the correct welded designation is 1.4401 (X5CrNiMo17-12-2). The alias 316 helps humans talk, not mills accept. ASTM/ASME equivalents are live cross-links for comparison; seamless EN 10216-5 is the product-form sister when a weld seam is forbidden.
When dual marking is requested, each standard’s mechanical and test regime still has to be satisfied on its own terms — an ASTM alias of 316 does not waive EN 10217-7 tensile, leak-tightness, or TC1/TC2 rules for 1.4401 / X5CrNiMo17-12-2. Keep the welded versus seamless product-form split explicit on the purchase order and on the MTC.
| Reference | Designation | Note |
|---|---|---|
| EN 10217-7 | 1.4401 / X5CrNiMo17-12-2 | This product standard (welded pressure tube) |
| EN steel name | X5CrNiMo17-12-2 | EN 10027-1 designation used in body and marking |
| Commercial alias (body only) | 316 | Not a substitute for the steel number on the MTC |
| EN 10216-5 (seamless sister) | 1.4401 | Related live page — different product form (seamless) |
| A269 TP316 | A269 TP316 | Related live page — different product standard |
| A213 TP316 | A213 TP316 | Related live page — different product standard |
Inside this welded series, compare EN 10217-7 1.4404, EN 10217-7 1.4571, EN 10217-7 1.4436, EN 10217-7 1.4301. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4401. Live cross-standard anchors: A269 TP316, A213 TP316.
Heat Treatment and Delivery Condition for EN 10217-7 1.4401
Heat treatment on 1.4401 is not a separate afterthought — it is built into many Table 2 delivery symbols (W1A, W2A, WCA, WCR, W1R/W2R among them). The mechanical tables for X5CrNiMo17-12-2 assume solution-annealed (+AT) material after uniform heating and rapid cool. For X5CrNiMo17-12-2 under steel number 1.4401, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
Annealing temperature listed for 1.4401 / X5CrNiMo17-12-2 is 1020–1120 °C; cooling water or air. These figures are public EN cross-checks and stay UNCERTAIN until a paid Part 7 footnote is confirmed. Option 5 freezes whether the tube is descaled, bright-annealed, ground, or polished after that heat treatment.
| Item | 1.4401 |
|---|---|
| Solution annealing band (public) | 1020–1120 °C (UNCERTAIN vs paid Part 7 footnote) |
| Cooling | water or air |
| Delivery condition symbols | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify) |
| Inspection document | EN 10204 3.1 default; 3.2 under Option 21 |
For 1.4401, SHH STEEL treats delivery condition as a certified fact. The EN 10204 document states which Table 2 symbol was applied to X5CrNiMo17-12-2, what heat treatment that implied, and how the weld seam was left after finishing — especially important when WCA/WCR recrystallized-weld routes were ordered.
Corrosion Resistance of EN 10217-7 1.4401
Choose 1.4401 (X5CrNiMo17-12-2) when welded PED tubing must carry this corrosion story: Mo-bearing passive film similar to 316; IGC in the delivery condition is marked with the usual “normally not sensitised” caveat for the higher-carbon Mo grades. Delivery-condition IGC resistance is characterised to EN ISO 3651-2 methods in the Part 7 tables, but a tested IGC result still requires Option 13 on the order.
Sensitisation guidance temperatures published with EN 10217-7 are not substitutes for allowable stress tables on 1.4401. When as-welded corrosive service looks marginal for X5CrNiMo17-12-2, change steel number among EN 10217-7 1.4404, EN 10217-7 1.4571, EN 10217-7 1.4436, EN 10217-7 1.4301 instead of inventing PREN floors as Part 7 acceptance.
Applications of EN 10217-7 1.4401 Tube
Applications for steel number 1.4401 / X5CrNiMo17-12-2 cluster around welded PED service that tolerates a mill seam: general chemical and utility PED lines where as-welded IGC is controlled by procedure or post-weld treatment, and Mo is still required. Delivery condition and test category on the order decide how that tube is finished and inspected before it reaches the spool.
Skip 1.4401 when the specification locks seamless product (EN 10216-5 — see EN 10216-5 1.4401), when ASTM A269/A312 text is the only acceptance language, or when corrosion/strength clearly points at another family. SHH STEEL can produce and supply X5CrNiMo17-12-2 welded tube in the enquiry band and will redirect to a sister or live ASTM/ASME page when that is wiser. Related live pages: A269 TP316, A213 TP316.
Weldability of EN 10217-7 1.4401
Mill welding of EN 10217-7 1.4401 is the longitudinal arc/laser seam on the ordered Table 1 route; field or shop welding is a separate PED joint design. Filler and procedure choices track the austenitic chemistry of X5CrNiMo17-12-2. Practical note: 316/316L fillers depending on procedure; prefer L fillers when as-welded corrosion is in scope
Shop and field welding decisions on 1.4401 (filler, heat input, PWHT, ferrite targets on duplex) belong to the fabricator’s WPS and the PED file. SHH STEEL’s mill scope for X5CrNiMo17-12-2 stops at ordered chemistry, longitudinal route, delivery-condition heat treatment, mechanical acceptance, and leak-tightness / NDT as specified.
Surface Finishes for EN 10217-7 1.4401
Delivery-condition symbols double as surface codes on 1.4401. Descaled W1A/W2A, bright-annealed W1R/W2R/WCR, and WG/WP ground or polished map the common finishes for X5CrNiMo17-12-2. Anything marketed as “hygienic” without a symbol and a measurable note is incomplete order text. Keep carbon-steel strap and rusty fixtures away from the OD — free-iron staining is a stainless-specific failure mode on 316 tube.
Call out interior roughness, electropolish, or protective films explicitly when they matter to the PED spool. SHH STEEL can produce and supply reported descaled, bright-annealed, and polished finishes on 1.4401 / X5CrNiMo17-12-2 and will not substitute marketing adjectives for measured surface data on 316 welded pressure tube.
Surface and delivery condition are one conversation on Part 7. Changing from W2A to WCR on 1.4401 is a process change for X5CrNiMo17-12-2, not a sticker change. SHH STEEL plans bright-anneal or polish capacity with the weld slot and documents the symbol that was really applied to this 316 shipment.
Inspection and Testing for EN 10217-7 1.4401
Every 1.4401 length sees leak-tightness testing; chemistry is cast-based; tensile follows TC1 or TC2 sampling; technological tests track diameter and wall. Option 15 can lock hydro versus eddy current. Visual, dimensional, and identification checks apply to X5CrNiMo17-12-2 as ordered. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4401 purchase order so X5CrNiMo17-12-2 inspection planning matches the PED file before weld slots are locked.
Choose TC2 when the PED file wants denser seam NDT on 1.4401. Add Option 13 for IGC and the impact Options when verified toughness is required. Certificates from SHH STEEL list cast chemistry, delivery-condition status, ambient tensile, and leak/NDT statements; lead time is not improved by omitting mandatory work.
PMI at goods-in is common on 1.4401 projects; it does not replace cast analysis or tensile sampling under Part 7. SHH STEEL can arrange PMI when ordered and still keeps the EN 10204 3.1 chemistry and mechanical package intact for X5CrNiMo17-12-2.
Packaging and Shipping for EN 10217-7 1.4401
Packaging for welded 1.4401 tube is built around surface protection and traceability. Ends are capped, lengths are grouped by OD × wall, and export units take waterproof wrap. Bright-annealed and polished OD (W1R/W2R, WCR, WP) take sleeve or paper wrap against transit galling; descaled W1A/W2A utility tube still needs clean supports under the longitudinal seam. No carbon-steel strap bears on the X5CrNiMo17-12-2 OD; stainless or padded contact is mandatory so 316 finishes do not arrive with free-iron rust tracks that fail goods-in visual checks.
Expect manufacturer ID, size, EN 10217-7, 1.4401/X5CrNiMo17-12-2, cast, TC1 or TC2, and inspection correlation on the tube marking set. Option 5 symbols are shown when locked. SHH STEEL checks marking against the order text for every 316 shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4401 / X5CrNiMo17-12-2 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Crates and bundles for 1.4401 carry IDs that map to MTC heats. Special lengths and bevels are isolated in the pack. SHH STEEL treats the packaging paragraph of the order as production input, not afterthought, for X5CrNiMo17-12-2. SHH STEEL treats packing and marking for EN 10217-7 1.4401 / X5CrNiMo17-12-2 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Why Choose SHH STEEL
SHH STEEL can supply and produce EN 10217-7 1.4401 as ordered welded tube: correct Table 2 condition, ordered test category, and EN 10204 3.1 documents for X5CrNiMo17-12-2. Generic “316” rack stock is not re-stamped as Part 7, and ASTM or seamless tensile tables are not borrowed onto this certificate.
Sister guidance on this hub includes EN 10217-7 LINKPLACE1.4404, EN 10217-7 LINKPLACE1.4571, EN 10217-7 LINKPLACE1.4436, EN 10217-7 LINKPLACE1.4301. For 1.4401 specifically: carbon up to 0.07% raises as-welded sensitisation risk versus LINKPLACE1.4404 — do not substitute 1.4401 for an L-grade drawing without design review Closing a sale on the wrong chemistry is treated as a failure mode, not a success metric. Live ASTM/ASME anchors: A269 TP316, A213 TP316.
Supply Capability
For X5CrNiMo17-12-2 as EN 10217-7 1.4401, SHH STEEL can produce and supply to the ordered edition and inspection package. Read the capability grid and Stock / Available sizes map as an enquiry aid, not a frozen inventory promise. Same mo austenitic welded size conversation as 1.4404.
| Item | SHH STEEL capability for 1.4401 |
|---|---|
| Standard | EN 10217-7 |
| Grade | 1.4401 / X5CrNiMo17-12-2 |
| Product form | Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition |
| Delivery condition | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock) |
| Typical size band | ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement |
| Testing | TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options |
| Documents | EN 10204 3.1 (3.2 Option 21); third-party inspection on request |
Stock / Available sizes
No published tonnage claim is made for EN 10217-7 1.4401. The matrix shows enquiry-typical OD × wall bands for X5CrNiMo17-12-2; live answer needs your size list, test category, and delivery-condition symbol.
| OD (mm) | Typical walls (mm) | Notes |
|---|---|---|
| 12 / 14 / 16 / 19 / 21.3 / 25 | 1.0 / 1.5 / 2.0 / 2.5 | Instrument / hygienic; often WCA/WCR or W2R |
| 26.9 / 33.7 / 38 / 42.4 / 48.3 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Process and utility welded pressure tube |
| 60.3 / 76.1 / 88.9 / 114.3 | 2.0 / 3.0 / 4.0 / 5.0 / 6.0 | Utility and process; lock W1A/W2A vs WCA |
| 141.3 / 168.3 / 219.1 | 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 | Larger welded pressure tube; watch family wall ceiling |
Routine extras include Option 19 lengths, Option 18 bevels, Option 13 IGC, and parallel asks on 1.4404, 1.4571, 1.4436, 1.4301. OD × wall examples are not a substitute for the standard. SHH STEEL can produce and supply 1.4401 inside this enquiry framework when materials and weld slots are open.
FAQ
-
What is EN 10217-7 1.4401 welded stainless steel tube used for?
- EN 10217-7 1.4401 (X5CrNiMo17-12-2) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is general chemical and utility PED lines where as-welded IGC is controlled by procedure or post-weld treatment, and Mo is still required. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
-
Is EN 10217-7 1.4401 the same as 316 under ASTM A269 or A312?
- No. Commercial alias 316 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP316, A213 TP316.
-
Does EN 10217-7 1.4401 include seamless tube?
- No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4401. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
-
What mechanical properties does EN 10217-7 require for 1.4401?
- In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm 510–710 MPa, and elongation 40% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
-
1.4401 vs sister grades — which EN 10217-7 number should I buy?
- Buy 1.4401 when the enquiry names this steel number or the duty matches standard-carbon Mo-bearing austenitic welded pressure tube when the order names 1.4401 / X5CrNiMo17-12-2 rather than the L grade. Compare EN 10217-7 1.4404, EN 10217-7 1.4571, EN 10217-7 1.4436, EN 10217-7 1.4301 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: carbon up to 0.07% raises as-welded sensitisation risk versus 1.4404 — do not substitute 1.4401 for an L-grade drawing without design review
-
What delivery conditions are available for EN 10217-7 1.4401?
- Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
-
What size range can SHH STEEL supply for EN 10217-7 1.4401?
- SHH STEEL can produce and supply EN 10217-7 1.4401 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Same mo austenitic welded size conversation as 1.4404.
-
TC1 or TC2 for EN 10217-7 1.4401?
- Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
-
Is the intergranular corrosion test mandatory for 1.4401?
- No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4401.
-
What documents come with SHH STEEL EN 10217-7 1.4401?
- EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4401, size, cast, and test category.
-
How do I enquire for EN 10217-7 1.4401 with SHH STEEL?
- Send EN 10217-7, steel number 1.4401 / X5CrNiMo17-12-2, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.
Conclusion
EN 10217-7 1.4401 (X5CrNiMo17-12-2) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4401 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.