EN 10028-4 13MnNi6-3 Steel Plate | 13MnNi6-3 0.75Ni Low Temp Vessel Plate
What is EN 10028-4 13MnNi6-3 Steel?
13MnNi6-3 is the next nickel step above 11MnNi5-3 in EN 10028-4. Buyers search EN 10028-4 13MnNi6-3, 13MnNi6-3 steel plate, 1.6217, 13MnNi6-3 0.75Ni low temp vessel plate and 13MnNi6-3 supplier. Nickel is about 0.50–1.00%. That is why the title says 0.75Ni. This is not 11MnNi5-3. That grade is 0.5Ni. This is not 12Ni14. 12Ni14 is 3.5Ni. This is not X8Ni9. X8Ni9 is 9Ni. This is not P355NL2. P355NL2 is EN 10028-3 carbon-manganese plate.
Yield is in the 355 MPa class at the usual thin-plate column. Tensile is 490–640 MPa. Steel number is 1.6217. Delivery is usually normalized (+N). Charpy is specified at −80 °C when the order follows this grade. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-4, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
Do not ship 11MnNi5-3 against a 13MnNi6-3 drawing and call 0.5Ni close to 0.75Ni. Do not ship 13MnNiDR steel plate and call the names identical unless both books are met. Do not ship SA203 Grade A. That grade is 2.25Ni. Dual marking is possible only when chemistry, tensile, impact temperature and delivery all fit.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | EN 10028-4 13MnNi6-3 | Confirmed |
| Steel number | 1.6217 | Confirmed |
| Product specification | EN 10028-4 + EN 10028-1 | Applied |
| Steel type | Ni-Mn low-temperature vessel plate | Confirmed |
| Usual delivery | +N normalized | Confirmed |
| Yield idea | 355 MPa class | Confirmed |
| Tensile | 490–640 MPa | Confirmed |
| Impact idea | −80 °C | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. Chinese Mn-Ni comparisons belong on GB/T 713.3. 3.5Ni / 9Ni comparisons belong on GB/T 713.4 and ASME SA-203.
Chemical Composition
Cast analysis follows EN 10028-4. Product analysis follows EN 10028-1 when ordered. People who search 13MnNi6-3 chemical composition and 1.6217 chemistry want nickel on the certificate, not an 11MnNi5-3 table copied across.
Cast Analysis and Product Analysis — EN 10028-4 13MnNi6-3 (1.6217)
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.16 | 0.18 |
| Silicon (Si), max | 0.35 | 0.40 |
| Manganese (Mn) | 0.80 – 1.50 | 0.75 – 1.60 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.013 |
| Aluminum total (Al), min | 0.020 | 0.015 |
| Nitrogen (N), max | 0.020 | 0.024 |
| Nickel (Ni) | 0.50 – 1.00 | 0.45 – 1.05 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Copper (Cu), max | 0.30 | 0.35 |
| Molybdenum (Mo), max | 0.08 | 0.10 |
| Vanadium (V), max | 0.05 | 0.06 |
Nickel at 0.50–1.00% is the grade marker. That is 0.75Ni class, not 0.5Ni and not 3.5Ni. Carbon stays limited because toughness at −80 °C is the job. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search 13MnNi6-3 mechanical properties, 13MnNi6-3 yield strength and 13MnNi6-3 impact. Yield falls as thickness rises.
Tensile and Yield — EN 10028-4 13MnNi6-3
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| ≤ 16 | 355 | 490 – 640 |
| 16 – 40 | 345 | 490 – 640 |
| 40 – 60 | 335 | 490 – 640 |
| 60 – 100 | 315 | 470 – 640 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is typically 22% min on thinner plate. Charpy for this grade is −80 °C. Energy is commonly 27 J average when the order follows the book. Location and orientation must be written. Do not assume −60 °C from 11MnNi5-3 is enough. Do not assume −100 °C. That is 3.5Ni.
Do not quote 355 MPa yield on an 80 mm plate. Do not treat −80 °C as permission to stamp 13MnNiDR steel plate or SA203 Grade A without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| EN 10028-4 11MnNi5-3 | EN 10028-4 | 11MnNi5-3 steel plate | No |
| EN 10028-4 13MnNi6-3 | EN 10028-4 | 13MnNi6-3 steel plate | This page |
| EN 10028-4 12Ni14 | EN 10028-4 | 12Ni14 3.5Ni | No |
| EN 10028-3 P355NL2 | EN 10028-3 | P355NL2 | No |
| 13MnNiDR steel plate | GB/T 713.3 | 13MnNiDR | No auto swap |
| 09MnNiDR steel plate | GB/T 713.3 | 09MnNiDR | No |
| 15MnNiNbDR steel plate | GB/T 713.3 | 15MnNiNbDR | No |
| SA203 Grade A | SA-203 | SA203 Gr.A | No |
| SA203 Grade D | SA-203 | SA203 Gr.D | No |
Equivalent Material Grades
| Designation | Standard / region | Notes |
|---|---|---|
| EN 10028-4 13MnNi6-3 / 1.6217 | EN 10028-4 | Name on this page |
| 11MnNi5-3 / 1.6212 | EN 10028-4 | 0.5Ni sister |
| 13MnNiDR steel plate | GB/T 713.3 | Chinese Mn-Ni |
| 09MnNiDR steel plate | GB/T 713.3 | Chinese 0.5Ni −70 °C |
| 15MnNiNbDR steel plate | GB/T 713.3 | −50 °C Nb grade |
| 11MnNiMoDR steel plate | GB/T 713.3 | Mn-Ni-Mo |
| SA203 Grade A | SA-203 | 2.25Ni |
| 08Ni3DR steel plate | GB/T 713.4 | 3.5Ni |
| 06Ni9DR steel plate | GB/T 713.4 | 9Ni |
0.75Ni Low-Temperature Pressure-Vessel Service
Buyers pick 13MnNi6-3 when a PED file wants more nickel than 11MnNi5-3 for −80 °C toughness and does not want to jump to 3.5Ni. Search phrases such as 13MnNi6-3 boiler plate, 1.6217 steel plate and 13MnNi6-3 0.75Ni vessel plate all point here.
It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni around −100 °C. It is not a substitute for 06Ni9DR steel plate. That grade is 9Ni −196 °C. It is not LNG inner-tank plate.
An ASME file that wants nickel vessel plate should name SA-203 on ASME SA203 and then write the grade. Dual marking is possible only when both books are met. SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
13MnNi6-3 is 0.75Ni-Mn vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must keep toughness at −80 °C. A carbon procedure written for SA516 Grade 70 is not automatically valid. A 0.5Ni procedure written for 11MnNi5-3 is the previous family. A 3.5Ni procedure written for SA203 Grade D is the next family. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized EN 10028-4 13MnNi6-3 (+N).
If the vessel will see PWHT, say so. Impact after simulated PWHT is worth naming on a −80 °C file. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists EN 10028-4 13MnNi6-3; 1.6217; heat number; cast analysis including nickel; product analysis when ordered; tensile to the correct thickness column; +N; Charpy at −80 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for 13MnNi6-3 0.75Ni low temp vessel plate:
- Thickness: commonly 6 mm – 120 mm, thicker by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
0.5Ni plate belongs on the 11MnNi5-3 page. 3.5Ni plate belongs on 08Ni3DR steel plate. 9Ni plate belongs on 06Ni9DR steel plate.
Tolerances
Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED −80 °C nickel plate without writing them.
Supplementary Requirements
Charpy details. Write −80 °C, joules, location and orientation.
Impact after simulated PWHT. When the vessel will be stress-relieved.
Product analysis. Especially nickel, P, S and Al.
NDE. EN 10160 or ASTM A435 / A578 as named.
Third-party. EN 10204 3.2 when written.
Applications
| Industry | Typical components |
|---|---|
| PED low-temp vessels | EN 10028-4 13MnNi6-3 shells at −80 °C |
| 0.75Ni storage / process drums | 13MnNi6-3 courses |
| Dual-certified export | 13MnNi6-3 / 13MnNiDR steel plate when both books fit |
| Comparison vs 3.5Ni | 13MnNi6-3 next to SA203 Grade D |
13MnNi6-3 is the plate for a PED file that wants more nickel than 11MnNi5-3 at −80 °C and does not want to pay 3.5Ni or 9Ni. It is the wrong plate for LNG inner tanks. That work belongs on 06Ni9DR steel plate.
Supply Capability
SHH STEEL sources EN 10028-4 13MnNi6-3 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement.
Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days; standard +N about 45 days; simulated PWHT / 3.2 about 2 months.
Company scope: worldwide delivery SHH STEEL.
Why Choose SHH STEEL
Experience on this grade is simple: 0.75Ni and −80 °C must both be on the certificate. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices 13MnNi6-3 from first-line mills, reports 1.6217 chemistry including nickel, records +N, prints Charpy at −80 °C when ordered, and issues 3.1 as standard or 3.2 when specified.
We keep the grade on the order. 13MnNi6-3 is not 11MnNi5-3. 13MnNi6-3 is not 12Ni14. 13MnNi6-3 is not X8Ni9. 13MnNi6-3 is not Q345R steel plate. If the drawing says 3.5Ni, we will not ship 0.75Ni and call nickel close.
Company scope: global exporter SHH STEEL.
FAQ
- What is 13MnNi6-3 steel plate?
- 13MnNi6-3 is an EN 10028-4 0.75Ni low-temperature pressure-vessel plate, steel number 1.6217. Yield is in the 355 MPa class at the thin-plate column and tensile is 490–640 MPa. Impact is typically −80 °C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
- What is the equivalent of 13MnNi6-3?
- Related comparisons are 13MnNiDR and 09MnNiDR. SA-203 Grade A is 2.25Ni, not the same nickel band. Dual marking is possible only when both books are fully met.
- How is 13MnNi6-3 different from 11MnNi5-3?
- 11MnNi5-3 is 0.5Ni at about −60 °C. 13MnNi6-3 is 0.75Ni at about −80 °C.
- How is 13MnNi6-3 different from 12Ni14?
- 12Ni14 is 3.5Ni at about −100 °C. 13MnNi6-3 is 0.75Ni.
- How is 13MnNi6-3 different from X8Ni9?
- X8Ni9 is 9Ni plate for −196 °C LNG service. 13MnNi6-3 is not LNG inner-tank plate.
Conclusion
EN 10028-4 13MnNi6-3 Steel Plate is European 0.75Ni low-temperature pressure-vessel plate, steel number 1.6217, at the 355 MPa yield class and 490–640 MPa tensile, usually +N, with Charpy at −80 °C when ordered. Whether the inquiry says EN 10028-4 13MnNi6-3, 1.6217 or 13MnNi6-3 0.75Ni Low Temp Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 13MnNi6-3 chemistry, recorded +N, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies EN 10028-4 13MnNi6-3 0.75Ni Low Temp Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
EN 10028-4 13MnNi6-3 Steel Plate, 13MnNi6-3 0.75Ni low temp vessel plate, 1.6217, 13MnNi6-3 supplier, global exporter SHH STEEL