EN 10028-4 15NiMn6 is European Ni-Mn low-temperature vessel plate, steel number 1.6228. Yield is 390 MPa class. Impact is −80 °C. SHH STEEL supplies 15NiMn6 worldwide as a global steel mill sourcing partner.
Keywords
EN 10028-4 15NiMn6, 15NiMn6, 15NiMn6 steel plate, 1.6228, 15NiMn6 Ni-Mn vessel plate, 15NiMn6 equivalent, 15NiMn6 supplier
Equivalent Grades:
EN 15NiMn6 / ASTM A203 Gr D (near) / ASME SA203 Gr D / GB 09MnNiDR (near) — Material Specification: EN 10028-4 — Delivery: Normalized (N) or N+T; low-temp Mn-Ni
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Ni-Mn Low-Temperature Pressure-Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-4 15NiMn6 Steel?

15NiMn6 is the higher Ni-Mn step in the low-nickel end of EN 10028-4. Buyers search EN 10028-4 15NiMn6, 15NiMn6 steel plate, 1.6228, 15NiMn6 Ni-Mn low temp vessel plate and 15NiMn6 supplier. Nickel is about 1.20–1.70%. Manganese is about 0.80–1.50%. This is not 11MnNi5-3. That grade is 0.5Ni. This is not 13MnNi6-3. That grade is 0.75Ni. This is not 12Ni14. 12Ni14 is 3.5Ni. This is not X8Ni9. X8Ni9 is 9Ni.

Yield is in the 390 MPa class at the usual thin-plate column. Tensile is 530–710 MPa. Steel number is 1.6228. Delivery is usually normalized (+N). Charpy is specified at −80 °C when the order follows this grade. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-4, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

Do not ship 13MnNi6-3 against a 15NiMn6 drawing and call 0.75Ni close to 1.5Ni. Do not ship 15MnNiNbDR steel plate and call the names identical unless both books are met. Do not ship SA203 Grade A. That grade is 2.25Ni. Dual marking is possible only when chemistry, tensile, impact temperature and delivery all fit.

Company scope: global exporter SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-4 15NiMn6 Confirmed
Steel number 1.6228 Confirmed
Product specification EN 10028-4 + EN 10028-1 Applied
Steel type Ni-Mn low-temperature vessel plate Confirmed
Usual delivery +N normalized Confirmed
Yield idea 390 MPa class Confirmed
Tensile 530–710 MPa Confirmed
Impact idea −80 °C Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates. Chinese Mn-Ni comparisons belong on GB/T 713.3. 3.5Ni / 9Ni comparisons belong on GB/T 713.4 and ASME SA-203.

Chemical Composition

EN 10028-4 15NiMn6 Steel Plate | 15NiMn6 Ni-Mn Low Temp Vessel Plate

Brief Description
EN 10028-4 15NiMn6 is European Ni-Mn low-temperature vessel plate, steel number 1.6228. Yield is 390 MPa class. Impact is −80 °C. SHH STEEL supplies 15NiMn6 worldwide as a global steel mill sourcing partner.

SEO Title
EN 10028-4 15NiMn6 Steel Plate | 15NiMn6 Ni-Mn Low Temp Vessel Plate – SHH STEEL

SEO Keywords
EN 10028-4 15NiMn6, 15NiMn6, 15NiMn6 steel plate, 1.6228, 15NiMn6 Ni-Mn vessel plate, 15NiMn6 equivalent, 15NiMn6 supplier

SEO Description
SHH STEEL supplies EN 10028-4 15NiMn6 Ni-Mn low-temp vessel plate worldwide, 390 MPa yield class, −80 °C impact, steel number 1.6228. EN 10204 3.1/3.2 mill-direct supply. Contact now.


General Description

15NiMn6 is the higher Ni-Mn step in the low-nickel end of EN 10028-4. Buyers search EN 10028-4 15NiMn6, 15NiMn6 steel plate, 1.6228, 15NiMn6 Ni-Mn low temp vessel plate and 15NiMn6 supplier. Nickel is about 1.20–1.70%. Manganese is about 0.80–1.50%. This is not 11MnNi5-3. That grade is 0.5Ni. This is not 13MnNi6-3. That grade is 0.75Ni. This is not 12Ni14. 12Ni14 is 3.5Ni. This is not X8Ni9. X8Ni9 is 9Ni.

Yield is in the 390 MPa class at the usual thin-plate column. Tensile is 530–710 MPa. Steel number is 1.6228. Delivery is usually normalized (+N). Charpy is specified at −80 °C when the order follows this grade. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-4, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

Do not ship 13MnNi6-3 against a 15NiMn6 drawing and call 0.75Ni close to 1.5Ni. Do not ship 15MnNiNbDR steel plate and call the names identical unless both books are met. Do not ship SA203 Grade A. That grade is 2.25Ni. Dual marking is possible only when chemistry, tensile, impact temperature and delivery all fit.

Company scope: global exporter SHH STEEL.


Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-4 15NiMn6 Confirmed
Steel number 1.6228 Confirmed
Product specification EN 10028-4 + EN 10028-1 Applied
Steel type Ni-Mn low-temperature vessel plate Confirmed
Usual delivery +N normalized Confirmed
Yield idea 390 MPa class Confirmed
Tensile 530–710 MPa Confirmed
Impact idea −80 °C Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates. Chinese Mn-Ni comparisons belong on GB/T 713.3. 3.5Ni / 9Ni comparisons belong on GB/T 713.4 and ASME SA-203.


Chemical Composition

Cast analysis follows EN 10028-4. Product analysis follows EN 10028-1 when ordered. People who search 15NiMn6 chemical composition and 1.6228 chemistry want nickel and manganese on the certificate, not a 13MnNi6-3 table copied across.

Cast Analysis and Product Analysis — EN 10028-4 15NiMn6 (1.6228)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.50 0.55
Manganese (Mn) 0.80 – 1.50 0.75 – 1.60
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.010 0.013
Aluminum total (Al), min 0.020 0.015
Nitrogen (N), max 0.020 0.024
Nickel (Ni) 1.20 – 1.70 1.15 – 1.75
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.30 0.35
Molybdenum (Mo), max 0.08 0.10
Vanadium (V), max 0.05 0.06

Nickel at 1.20–1.70% is the grade marker. That is still a Ni-Mn plate, not 3.5Ni and not 9Ni. Carbon stays limited because toughness at −80 °C is the job. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search 15NiMn6 mechanical properties, 15NiMn6 yield strength and 15NiMn6 impact. Yield falls as thickness rises.

Tensile and Yield — EN 10028-4 15NiMn6

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 16 390 530 – 710
16 – 40 380 530 – 710
40 – 60 370 520 – 700
60 – 100 350 510 – 690
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 20% min on thinner plate. Charpy for this grade is −80 °C. Energy is commonly 27 J average when the order follows the book. Location and orientation must be written. Do not assume −60 °C from 11MnNi5-3 is enough. Do not assume −100 °C. That is 3.5Ni.

Do not quote 390 MPa yield on an 80 mm plate. Do not treat −80 °C as permission to stamp 15MnNiNbDR steel plate or SA203 Grade A without checking both books.

Material Comparison

Grade Book What buyers search Swap?
EN 10028-4 11MnNi5-3 EN 10028-4 11MnNi5-3 steel plate No
EN 10028-4 13MnNi6-3 EN 10028-4 13MnNi6-3 steel plate No
EN 10028-4 15NiMn6 EN 10028-4 15NiMn6 steel plate This page
EN 10028-4 12Ni14 EN 10028-4 12Ni14 3.5Ni No
15MnNiNbDR steel plate GB/T 713.3 15MnNiNbDR No auto swap
13MnNiDR steel plate GB/T 713.3 13MnNiDR No
11MnNiMoDR steel plate GB/T 713.3 11MnNiMoDR No
SA203 Grade A SA-203 SA203 Gr.A No
SA203 Grade D SA-203 SA203 Gr.D No

Equivalent Material Grades

Designation Standard / region Notes
EN 10028-4 15NiMn6 / 1.6228 EN 10028-4 Name on this page
13MnNi6-3 / 1.6217 EN 10028-4 0.75Ni sister
11MnNi5-3 / 1.6212 EN 10028-4 0.5Ni sister
15MnNiNbDR steel plate GB/T 713.3 Chinese −50 °C Nb
13MnNiDR steel plate GB/T 713.3 Chinese Mn-Ni
11MnNiMoDR steel plate GB/T 713.3 Mn-Ni-Mo
SA203 Grade A SA-203 2.25Ni
08Ni3DR steel plate GB/T 713.4 3.5Ni
06Ni9DR steel plate GB/T 713.4 9Ni

Ni-Mn Low-Temperature Pressure-Vessel Service

Buyers pick 15NiMn6 when a PED file wants more nickel than 13MnNi6-3 and a 390 MPa step, without jumping to 3.5Ni. Search phrases such as 15NiMn6 boiler plate, 1.6228 steel plate and 15NiMn6 Ni-Mn vessel plate all point here.

It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni around −100 °C. It is not a substitute for 06Ni9DR steel plate. That grade is 9Ni −196 °C. It is not LNG inner-tank plate.

An ASME file that wants nickel vessel plate should name SA-203 on ASME SA203 and then write the grade. Dual marking is possible only when both books are met. SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

15NiMn6 is Ni-Mn vessel plate at about 1.5% nickel. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. Consumables must keep toughness at −80 °C. A carbon procedure written for SA516 Grade 70 is not automatically valid. A 0.75Ni procedure written for 13MnNi6-3 is the previous family. A 3.5Ni procedure written for SA203 Grade D is the next family. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized EN 10028-4 15NiMn6 (+N).

If the vessel will see PWHT, say so. Impact after simulated PWHT is worth naming on a −80 °C file. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-4 15NiMn6; 1.6228; heat number; cast analysis including nickel and manganese; product analysis when ordered; tensile to the correct thickness column; +N; Charpy at −80 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for 15NiMn6 Ni-Mn low temp vessel plate:

  • Thickness: commonly 6 mm – 120 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

0.5Ni plate is 11MnNi5-3. 0.75Ni plate is 13MnNi6-3. 3.5Ni plate belongs on 08Ni3DR steel plate. 9Ni plate belongs on 06Ni9DR steel plate.

Tolerances

Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED −80 °C Ni-Mn plate without writing them.

Supplementary Requirements

Charpy details. Write −80 °C, joules, location and orientation.

Impact after simulated PWHT. When the vessel will be stress-relieved.

Product analysis. Especially nickel, manganese, P, S and Al.

NDE. EN 10160 or ASTM A435 / A578 as named.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
PED low-temp vessels EN 10028-4 15NiMn6 shells at −80 °C
Ni-Mn storage / process drums 15NiMn6 courses
Dual-certified export 15NiMn6 / 15MnNiNbDR steel plate when both books fit
Comparison vs 3.5Ni 15NiMn6 next to SA203 Grade D

15NiMn6 is the plate for a PED file that wants more nickel than 13MnNi6-3 and a 390 MPa step, without paying 3.5Ni or 9Ni. It is the wrong plate for LNG inner tanks. That work belongs on 06Ni9DR steel plate.

Supply Capability

SHH STEEL sources EN 10028-4 15NiMn6 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement.

Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard +N about 45 days; simulated PWHT / 3.2 about 2 months.

Company scope: worldwide delivery SHH STEEL.

Why Choose SHH STEEL

Experience on this grade is simple: Ni-Mn chemistry and −80 °C must both be on the certificate. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices 15NiMn6 from first-line mills, reports 1.6228 chemistry including nickel, records +N, prints Charpy at −80 °C when ordered, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. 15NiMn6 is not 13MnNi6-3. 15NiMn6 is not 12Ni14. 15NiMn6 is not X8Ni9. 15NiMn6 is not Q345R steel plate. If the drawing says 3.5Ni, we will not ship 1.5Ni and call nickel close.

Company scope: global exporter SHH STEEL.

FAQ

What is 15NiMn6 steel plate?
15NiMn6 is an EN 10028-4 Ni-Mn low-temperature pressure-vessel plate, steel number 1.6228. Yield is in the 390 MPa class at the thin-plate column and tensile is 530–710 MPa. Impact is typically −80 °C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of 15NiMn6?
Related comparisons are 15MnNiNbDR, 13MnNiDR and 11MnNiMoDR. SA-203 Grade A is 2.25Ni, not the same nickel band. Dual marking is possible only when both books are fully met.
How is 15NiMn6 different from 13MnNi6-3?
13MnNi6-3 is 0.75Ni at about 355 MPa. 15NiMn6 is about 1.5Ni at about 390 MPa. Both sit near −80 °C.
How is 15NiMn6 different from 12Ni14?
12Ni14 is 3.5Ni at about −100 °C. 15NiMn6 is Ni-Mn at about 1.5% nickel.
How is 15NiMn6 different from X8Ni9?
X8Ni9 is 9Ni plate for −196 °C LNG service. 15NiMn6 is not LNG inner-tank plate.

Conclusion

EN 10028-4 15NiMn6 Steel Plate is European Ni-Mn low-temperature pressure-vessel plate, steel number 1.6228, at the 390 MPa yield class and 530–710 MPa tensile, usually +N, with Charpy at −80 °C when ordered. Whether the inquiry says EN 10028-4 15NiMn6, 1.6228 or 15NiMn6 Ni-Mn Low Temp Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 15NiMn6 chemistry, recorded +N, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-4 15NiMn6 Ni-Mn Low Temp Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

EN 10028-4 15NiMn6 Steel Plate, 15NiMn6 Ni-Mn low temp vessel plate, 1.6228, 15NiMn6 supplier, global exporter SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X