ASTM A269 TP347 Stainless Steel Tube

ASTM A269 TP347 / UNS S34700 nominal-wall seamless and welded austenitic tubing with Cr 17.0–19.0%, Ni 9.0–12.0%, C ≤0.08% and Nb (Cb) 10×C min to 1.10% max, solution annealed at ≥1900 °F [1040 °C] with hardness max 192 HBW / 200 HV or 90 HRB. SHH STEEL can produce and supply A269 TP347 tube with EN 10204 3.1 MTCs.
Grade
TP347 / UNS S34700
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 TP347 Stainless Steel Tube

ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP347 is the niobium-stabilized (columbium-stabilized) 18-8-family austenitic under UNS S34700, with carbon ≤0.08%, chromium 17.0–19.0%, nickel 9.0–12.0%, and Nb/Cb held at 10 × C minimum up to 1.10% maximum. Buyers specify A269 TP347 when they want Nb stabilization against sensitization for welded or intermittently heated general-service tubing, or when the material list prefers niobium over titanium. The shop name “347 tube” still needs ASTM A269 on the purchase order so nominal-wall rules, hardness, flaring or flange tests, and marking apply to tubing — not to an A213 boiler-tube or A312 pipe text.

SHH STEEL can produce and supply ASTM A269 TP347 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates reporting Table 1 chemistry (including niobium) and Table 2 hardness. Typical sizes run about 6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare sisters on the A269/A269M hub with A269 TP321, A269 TP348, and A269 TP304L. Keep the wall basis nominal. A269 §6.3 warns that solution annealing above 1950 °F [1065 °C] may impair intergranular corrosion resistance after subsequent sensitizing exposure in TP321, TP347, and TP348.

If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP347, SA213 TP347, A312 TP347 and SA312 TP347 and match the product standard to the drawing.

Chemical Composition of A269 TP347

Heat analysis under A269 Table 1 is mandatory for every TP347 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.

Public A269 Table 1 excerpts for TP347 / UNS S34700 are reproduced below (ASTM abstract cross-checked with the tubingchina A269 PDF). Values are maxima unless a range is shown. Confirm the purchased A269/A269M edition before treating any secondary catalogue as the acceptance text.

Melting analysis (heat / ladle analysis) — Table 1

Element TP347 / UNS S34700 melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 12.0
Niobium / Columbium (Nb / Cb) 10 × C min, 1.10 max
Molybdenum (Mo) … (no requirement)
Titanium (Ti) … (no requirement)

Source: ASTM A269/A269M Table 1 for TP347 / UNS S34700 (public excerpts). Niobium (columbium) at 10 × C minimum and 1.10% maximum is the stabilization signature that separates TP347 from TP321’s titanium formula and from unstabilized TP304. No molybdenum — chloride-heavy duty still belongs on Mo-bearing A269 grades. A269 §6.3 also applies to TP347 regarding high solution-anneal temperatures.

Mechanical Properties of A269 TP347

ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for TP347. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.

Property TP347 requirement (A269 Table 2)
Hardness, max 192 HBW / 200 HV or 90 HRB
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for TP347 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.

Seamless and Welded Tube

Under A269, TP347 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.

Seamless TP347 takes a lot-basis flaring test; welded TP347 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 TP347 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.

Dimensions and Tolerances

Order A269 TP347 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for TP347, say so on the enquiry so SHH STEEL does not build the wrong wall basis.

Equivalent Grades

TP347 / UNS S34700 is the ASTM tubing grade for niobium-stabilized 18-8-family austenitic. Cousins include A213 TP347, A312 TP347, A240 Type 347, and EN 1.4550 / X6CrNiNb18-10 — confirm chemistry and product form before substituting across those product standards.

Reference Designation Note
ASTM A269 TP347 / UNS S34700 This product standard
UNS S34700 Chemistry identity
ASTM A213 / A312 TP347 Different product form / mechanical tables
EN (approx.) 1.4550 / X6CrNiNb18-10 Commercial cousin

Inside A269, choose A269 TP321 for Ti stabilization, or A269 TP348 when low tantalum/cobalt limits are also required on the material list.

Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP347, SA213 TP347, A312 TP347 and SA312 TP347. Confirm the product form before treating any of those pages as acceptance text for an A269 order.

Heat Treatment and Delivery Condition

All A269 TP347 tube is furnished solution heat-treated. Table 2 sets austenitizing at ≥1900 °F [1040 °C], followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.” A269 §6.3 high-anneal IGC caution applies to TP347; order Supplementary S3 stabilization language explicitly if required.

Item TP347 (A269 Table 2)
Austenitizing temperature ≥1900 °F [1040 °C]
Cooling Water quench or rapid cool
Hardness after heat treatment, max 192 HBW / 200 HV or 90 HRB
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for TP347 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.

Corrosion Resistance

Niobium stabilization ties up carbon as niobium carbide so chromium stays available for the passive film in heat-affected zones — that is why TP347 is chosen over unstabilized TP304 for welded or intermittently heated general-service tubing. It still lacks molybdenum, so chloride pitting stays below TP316L and 6Mo grades under the same A269 product standard.

A269 publishes no PREN for S34700 — do not invent one from marketing sheets. Use TP347 for Nb-stabilized general service; use A269 TP316L when Mo is required; use A269 TP321 when Ti stabilization is preferred.

Applications of A269 TP347 Tube

A269 TP347 shows up on welded general-service instrument and process lines that see intermittent heating, heat-recovery related tubing specified to A269 rather than A213, and projects that standardized on niobium-stabilized chemistry across product forms. Bright-annealed cold-finished tube is common on skids; pickled welded tube covers larger utility runs.

For Code boiler or superheater tube open A213 TP347; for pipe open A312 TP347. SHH STEEL can produce and supply A269 TP347 in the general-service band above and will redirect when Ti stabilization, low-Ta TP348, or Mo-bearing grades are the better metallurgical fit.

When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP347, SA213 TP347, A312 TP347 and SA312 TP347 instead of stretching an A269 tubing page into the wrong product form.

Weldability

Niobium stabilization is the welding reason to choose TP347 over TP304 for as-welded or intermittently heated fabrications. GTAW and GMAW with 347-type fillers — when filler is used on fabrication joints — are common practice; mill autogenous A269 welds are already cold-worked and solution-treated with the tube body before shipment.

Shop welds on cut lengths sit outside that mill anneal and need proper purge and procedure. Mind the §6.3 high-anneal note when specifying post-fabrication heat treatment. SHH STEEL supplies the mill product and MTC with niobium reported against the 10 × C / 1.10% rule.

Surface Finishes

Pickled and bright-annealed finishes cover most A269 TP347 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.

Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP347 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.

Inspection and Testing

Lot testing for A269 TP347 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including niobium (columbium), solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.

Packaging and Shipping

Export and domestic packs for A269 TP347 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Stencil and tags typically carry ASTM A269, TP347 / S34700, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 TP347 as solution-treated seamless or welded tubing with Table 1 chemistry — including niobium against the stabilization rule — Table 2 hardness, and EN 10204 3.1 documentation. We will not ship TP304 and call it 347, and we will not omit Nb from the certificate when the grade requires it.

If titanium stabilization, low-Ta TP348 limits, or molybdenum is what the duty needs, we point to the matching A269 grade rather than selling the wrong stabilizer or alloy family into the job.

Supply Capability

SHH STEEL can produce and supply ASTM A269 TP347 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.

Item SHH STEEL capability
Standard ASTM A269 / A269M
Grade TP347 / UNS S34700
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated (≥1900 °F [1040 °C]); pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument / hydraulic; often BA
12.7 / 15.9 / 19.1 / 25.4 / 31.8 1.0 / 1.2 / 1.5 / 2.0 / 2.5 Inch OD process and utility
38.1 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Utility and light process
88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Parallel quotes against A269 TP321 and A269 TP348 keep Ti vs Nb vs low-Ta choices visible on one size list.

FAQ

What is ASTM A269 TP347 stainless steel tube used for?
A269 TP347 is niobium-stabilized nominal-wall tubing for welded or intermittently heated general-service lines where sensitization resistance matters and the material list prefers Nb over Ti. It covers seamless and welded tubing under ASTM A269 — not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis and tests match the tubing product standard.
TP347 vs TP321 under A269 — which stabilizer should I buy?
Both are stabilized austenitics under A269. TP347 uses niobium (columbium) at 10 × C min to 1.10% max; TP321 uses titanium against the Footnote D formula. Choice follows the material list, filler practice, and project preference. Compare both on the same OD × wall list with SHH STEEL when the stabilizer decision is still open.
TP347 vs TP348 under A269 — what is the difference?
TP348 is a closely related Nb-stabilized grade with additional tantalum and cobalt limits intended for applications that restrict Ta/Co. TP347 is the standard Nb-stabilized listing without those extra Ta/Co ceilings. Confirm which UNS the drawing names before ordering — they are separate Table 1 grades under A269.
Does ASTM A269 TP347 include welded tube?
Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. Site titles omit the word Welded by house style, but the order and MTC still state seamless or welded. SHH STEEL can produce and supply both routes.
What hardness limit applies to A269 TP347?
Table 2 caps TP347 at 192 HBW / 200 HV or 90 HRB after solution treatment at ≥1900 °F [1040 °C]. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 unless the purchase order adds them as project extras.
Why does A269 warn about annealing TP347 above 1950 °F?
Section 6.3 notes that solution annealing above 1950 °F [1065 °C] may impair intergranular corrosion resistance after subsequent sensitizing exposure in TP321, TP347, and TP348. When needed, a lower-temperature stabilization or re-solution anneal can be ordered — confirm Supplementary Requirement S3 in the purchased edition.
Is A269 TP347 nominal wall or minimum wall?
A269 is written on a nominal-wall-thickness basis. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall boiler-tube practice applies to an A269 TP347 order. Confirm the purchased A269/A269M edition and the seamless or welded route on the purchase order before treating catalogue sheets as acceptance text.
What size range can SHH STEEL produce for TP347?
SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP347, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation against near-term production.
Must niobium appear on the MTC for TP347?
Yes. Niobium (columbium) is the defining Table 1 stabilization requirement, so the ladle analysis should report Nb/Cb against the 10 × C minimum and 1.10% maximum. A 347 nickname certificate without niobium values is incomplete for grade acceptance under A269. Confirm the purchased A269/A269M edition and the seamless or welded route on the purchase order before treating catalogue sheets as acceptance text.
What certificate does SHH STEEL provide for A269 TP347?
EN 10204 3.1 MTCs report ladle chemistry including niobium, solution-treatment condition, hardness, and hydro or NDE. Third-party inspection can be added when named. Stencil shows ASTM A269, TP347 / S34700, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition and the seamless or welded route on the purchase order before treating catalogue sheets as acceptance text.
How should I enquire for A269 TP347 with SHH STEEL?
List ASTM A269, grade TP347 / UNS S34700, seamless or welded, OD × nominal wall, finish, any stabilization/S3 language, and any hydro/NDE lock. SHH STEEL can produce and supply to that enquiry or recommend TP321 / TP348 / TP304L when the material list points that way. Confirm the purchased A269/A269M edition and the seamless or welded route on the purchase order before treating catalogue sheets as acceptance text.

Conclusion

ASTM A269 TP347 / UNS S34700 is the niobium-stabilized austenitic inside the A269 nominal-wall tubing family when welded or intermittently heated general service needs Nb stabilization without molybdenum. SHH STEEL can produce and supply seamless and welded A269 TP347, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X