ASTM A269 TP201LN Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 TP201LN Stainless Steel Tube

ASTM A269 TP201LN / UNS S20153 nominal-wall seamless and welded austenitic tubing with C ≤0.03%, N 0.10–0.25%, Mn 6.4–7.5%, Ni 4.0–5.0% and Cr 16.0–17.5%, solution annealed at ≥1900 °F [1040 °C] with hardness max 250 HBW / 263 HV or 100 HRB. SHH STEEL can produce and supply A269 TP201LN tube with EN 10204 3.1 MTCs.
Grade
TP201LN / UNS S20153
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 114 mm OD × 0.5–6.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 TP201LN Stainless Steel Tube

ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP201LN is the low-carbon, nitrogen-strengthened sister of TP201 inside that Table 1 list, recorded as UNS S20153. Carbon is held to ≤0.03%, nitrogen is controlled at 0.10–0.25%, manganese sits in a tighter high band of 6.4–7.5%, nickel is 4.0–5.0%, and chromium is 16.0–17.5%, with copper allowed up to 1.00%. The “LN” tag is not a marketing nickname — it is the ASTM grade that buyers should put on the purchase order when they want 200-series economy with better as-welded intergranular behaviour than standard TP201.

SHH STEEL can produce and supply ASTM A269 TP201LN stainless steel tube as seamless and welded product in the instrument, hydraulic, and process OD × nominal-wall band, solution annealed, and shipped with EN 10204 3.1 mill test certificates covering Table 1 ladle chemistry and Table 2 hardness. Typical sizes we quote run roughly 6–114 mm outside diameter with 0.5–6.0 mm nominal wall; other sizes follow by agreement. Start from the A269/A269M hub when comparing LN against standard 201 or the 300-series A269 grades.

Shop language still says “201LN tube” or “S20153 instrumentation tube,” but the MTC and stencil must carry ASTM A269 Grade TP201LN. Sister pages under this series include A269 TP201, A269 TP304L, and A269 TP316L. A269 remains a nominal-wall tubing standard — contrast that briefly with A213’s common minimum-wall boiler-tube practice, then keep the enquiry in OD × nominal wall so the mill builds the correct product.

Chemical Composition of A269 TP201LN

Heat analysis under A269 Table 1 is mandatory for every TP201LN heat; product analysis applies only when the order or supplementary wording pulls it in through ASTM A1016/A1016M and the A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle results — and product results when ordered — without publishing tighter “mill catalogue” windows that ASTM does not set.

The melting limits below come from public A269 Table 1 excerpts for TP201LN / UNS S20153 (ASTM abstract table text cross-checked with the tubingchina A269 PDF reproduction). Values are maxima unless a range is shown. Confirm the purchased A269/A269M edition, because public block-1 columns are reproduced from older excerpt copies.

Melting analysis (heat / ladle analysis) — Table 1

Element TP201LN (UNS S20153) melting analysis
Carbon (C) ≤ 0.03
Manganese (Mn) 6.4 – 7.5
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 0.75
Chromium (Cr) 16.0 – 17.5
Nickel (Ni) 4.0 – 5.0
Nitrogen (N) 0.10 – 0.25
Copper (Cu) ≤ 1.00
Molybdenum (Mo) … (no requirement)

Source: ASTM A269/A269M Table 1 for TP201LN / UNS S20153 (public excerpts cross-checked). Read carbon and nitrogen together: C ≤0.03% is the L-grade move against sensitization, while N at 0.10–0.25% restores austenite stability and strength that low carbon would otherwise give away. Sulfur is tighter (≤0.015%) and silicon lower (≤0.75%) than standard TP201, which matters for clean weldability and surface finish on instrumentation tube. Copper up to 1.00% is an allowed addition, not a mandatory range.

Mechanical Properties of A269 TP201LN

A269 does not give TP201LN a tensile / yield / elongation acceptance table. Lot acceptance rests on Table 2 hardness, the flaring test for seamless tube, flange and reverse-flattening tests for welded tube, and hydro or nondestructive electric testing of each length. Borrowing a tensile floor from A213 or A312 for the same UNS number and calling it an A269 requirement would mis-state the product standard.

Table 2 sets a higher hardness ceiling for TP201LN than for standard TP201 — 250 HBW / 263 HV or 100 HRB — reflecting the nitrogen-strengthened lean austenite after the mandatory solution treatment. Hardness is still a maximum; properly annealed tube should clear it. Thin-wall superficial Rockwell alternatives and small-ID exemptions follow the hardness clause of the ordered edition.

Property TP201LN requirement (A269 Table 2)
Hardness, max 250 HBW / 263 HV or 100 HRB
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for TP201LN / UNS S20153 (public PDF excerpt). The hardness clause also notes superficial-scale limits specific to S20153 / TPXM-29 thin-wall tube; confirm those figures in the purchased edition before writing them into a quality plan.

Seamless and Welded Tube

TP201LN under A269 may be seamless or welded, hot-finished or cold-finished, at the manufacturer’s option unless the purchase order locks the route. Welded A269 tubing is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube body. That is not the same stencil language as A312 WLD/HCW pipe; A269 simply records seamless or welded on the product.

Seamless TP201LN takes the flaring test; welded TP201LN takes the flange test and reverse flattening so the seam is qualified in both modes. Both share Table 2 hardness and the mandatory hydro or NDE test per length. The LN chemistry is often chosen specifically because fabrication welds will remain as-welded — still, the mill’s solution treatment covers the tube as shipped, not later shop welds on cut lengths. SHH STEEL can produce and supply both seamless and welded A269 TP201LN against the same Table 1 / Table 2 floors.

Dimensions and Tolerances

Order A269 TP201LN by outside diameter and nominal wall thickness. Table 4 of A269 (via A1016/A1016M general requirements) sets OD, wall, and cut-length tolerances by OD group; thin-wall ovality rules in clause 12.2 apply when wall falls below the thin-wall thresholds for that group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow ±12.5% wall on heavy wall or low ID/OD ratios, and ±15% wall on sub-½ in. ID tube that cannot be mandrel-drawn. If a drawing is written to A213 minimum-wall language, say so on the enquiry — SHH STEEL will not silently convert LN tubing to a min-wall boilertube build.

Equivalent Grades

TP201LN / UNS S20153 is the ASTM tubing grade for low-carbon, nitrogen-bearing 201-type austenitic. Related product forms with the same UNS idea include A213 and A312 listings where those standards carry S20153, but wall basis and mechanical acceptance differ. Plate/sheet chemistry cousins appear under A240 Type 201LN language where that standard lists the UNS.

Reference Designation Note
ASTM A269 TP201LN / UNS S20153 This product standard
UNS S20153 Chemistry identity
ASTM A269 sister TP201 / S20100 Higher C, no mandatory N range
ASTM A240 201LN / S20153 (where listed) Plate / sheet cousin

Inside A269, step from LN to A269 TP304L or A269 TP316L when nickel-richer or molybdenum-bearing resistance is required. Do not treat EN X-grade labels as automatic substitutes without a chemistry and product-form check against the purchased A269 edition.

Heat Treatment and Delivery Condition

A269 requires all TP201LN tube to ship solution heat-treated. Table 2 sets the minimum austenitizing temperature at 1900 °F [1040 °C] with water quench or other rapid cool. Seamless tube may be quenched directly after hot forming while still at or above that temperature. Ordered final anneals below 1900 °F must be stenciled with the actual temperature after “HT” — that is purchaser-directed, not default practice.

Item TP201LN (A269 Table 2)
Austenitizing temperature, min 1900 °F [1040 °C]
Cooling Water quench or rapid cool
Hardness after heat treatment, max 250 HBW / 263 HV or 100 HRB
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for TP201LN. Bright anneal or pickle is a surface choice on top of the mandatory solution treatment. SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.

Corrosion Resistance

TP201LN keeps the lean Cr-Mn-Ni passive-film story of the 200 series, with the decisive upgrade that carbon ≤0.03% sharply reduces chromium-carbide precipitation risk in heat-affected zones. That is why LN is the A269 201-family grade buyers reach for when tubing will be welded into manifolds or skids and left as-welded in mildly corrosive service. Nitrogen in the specified range supports austenite stability that low carbon would otherwise weaken.

It is still not a molybdenum grade. Chloride pitting and crevice performance remain below TP316L / 6Mo A269 grades, and A269 publishes no PREN table for S20153 — do not invent one. Match the medium: clean utilities and low-chloride process lines suit LN; seawater, strong chlorides, or reducing acids need a step up the A269 alloy ladder.

Applications of A269 TP201LN Tube

A269 TP201LN shows up on instrumentation manifolds, hydraulic lines, food and beverage utility tubing, and light process skids where a welded lean austenitic must keep as-welded corrosion behaviour under control without stepping all the way to 304L/316L cost. Coiled LN tubing is also quoted for long instrument runs when the order is written for coil rather than cut length.

Skip LN for Code boiler tube (use A213), for pipe headers (use A312), and for chloride-heavy offshore or chemical duties that need Mo-bearing A269 grades. SHH STEEL can produce and supply A269 TP201LN in the general-service band above and will redirect the enquiry when the stated medium outgrows S20153.

Weldability

Low carbon is the welding reason to choose TP201LN over TP201. GTAW/GMAW fabrication with appropriate austenitic filler (when filler is used) is routine; the mill’s autogenous A269 weld has already been solution-treated with the tube. Shop or field welds on cut lengths are outside that mill anneal, so procedure qualification, purge, and filler choice remain the fabricator’s scope.

If even LN’s corrosion margin is short for the medium, move to A269 TP304L or A269 TP316L rather than compensating with procedure tricks alone. SHH STEEL supplies the mill product and MTC; we do not pretend a welding procedure specification is included unless the order buys that service separately.

Surface Finishes

Pickled and bright-annealed finishes are the two workhorse deliveries for A269 TP201LN. Bright anneal is preferred on instrumentation and hygienic utility tube where ID/OD must stay scale-free; pickle is the default for general process tube. OD polish (named grit) is a supplementary finish when the purchase order requires it.

Write any max-Ra or scrubbed-ID note into the enquiry. SHH STEEL can produce and supply those finishes on TP201LN when the mill can measure and report them; we will not claim an unverified polish grade.

Inspection and Testing

TP201LN lots are hardness-tested to Table 2, flare-tested when seamless, and flange- plus reverse-flattening-tested when welded. Every length takes hydrostatic or nondestructive electric testing; the mill chooses unless the order locks the method, and NDE-marked tube is certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry, heat treatment, hardness, and the hydro/NDE route. PMI, product analysis, and third-party hold points are available when named on the purchase order.

Packaging and Shipping

Export and domestic packs use end caps, bundled sleeves or crates by size, and waterproof wrap for sea freight. Polished or bright-annealed OD gets extra sleeve protection. Coiled TP201LN follows A269’s continuous-coil rule — no circumferential butt welds inside a coil.

Stencil and tags carry ASTM A269, TP201LN / S20153, size, heat, seamless or welded identity, and NDE when applicable. SHH STEEL matches marking to the purchase-order clause before shipment.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 TP201LN as solution-treated seamless or welded tubing with Table 1 chemistry, Table 2 hardness, and EN 10204 3.1 documentation — not as a relabelled “201” heat. We keep LN distinct from standard TP201 on the MTC, we state nominal wall and process route clearly, and we will recommend a 300-series A269 grade when the medium needs more than lean Cr-Mn-Ni can give.

That honesty matters on welded skids: selling standard TP201 into an as-welded corrosive duty to save a few percent on nickel is how projects inherit HAZ problems. We would rather quote TP201LN — or step you to A269 TP304L — than win an order that fails the medium.

Supply Capability

SHH STEEL can produce and supply ASTM A269 TP201LN stainless steel tube to the edition, seamless/welded route, and finish on your enquiry. Capability and the Stock / Available sizes enquiry map follow.

Item SHH STEEL capability for TP201LN
Standard ASTM A269 / A269M
Grade TP201LN / UNS S20153
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated ≥1900 °F [1040 °C]; pickled or bright-annealed
Typical size band ~6–114 mm OD × 0.5–6.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range for A269 TP201LN — not a frozen tonnage list. Confirm against near-term production or partner stock when you send the OD × wall list.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 0.5 / 0.8 / 1.0 / 1.2 Instrument / hydraulic; often bright-annealed
12.7 / 15.9 / 19.1 / 25.4 1.0 / 1.2 / 1.5 / 2.0 Inch OD skid and utility tube
32 / 38 / 42 / 48.3 1.5 / 2.0 / 2.5 / 3.0 Welded manifolds — LN preferred over TP201
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 6.0 Larger process tube; lock seamless vs welded on PO

Compare parallel enquiries against A269 TP201 and A269 TP304L when cost versus as-welded corrosion margin is still open.

FAQ

What does the LN mean in A269 TP201LN?
LN marks the low-carbon, nitrogen-controlled variant of 201-type tubing under A269. Carbon is ≤0.03% and nitrogen is specified at 0.10–0.25% (UNS S20153), which improves as-welded intergranular corrosion behaviour versus standard TP201 while keeping the lean Cr-Mn-Ni alloy balance. It is a separate ASTM grade, not a heat treatment suffix on TP201.
TP201 vs TP201LN — which A269 grade should I order?
Order TP201 when standard carbon is acceptable and service is mild or the tube will be re-annealed after fabrication. Order TP201LN when welded joints will stay as-welded in corrosive or hygiene-sensitive service and you still want 200-series economics. They are not interchangeable stamps; chemistry, hardness ceiling, and MTC grade lines differ.
Does A269 TP201LN come as welded tube?
Yes. A269 covers seamless and welded TP201LN. Welded tube is made without filler metal, cold-worked, and solution-treated with the tube, then flange- and reverse-flattening-tested. Say seamless or welded on the purchase order; SHH STEEL can produce and supply both routes.
What hardness limit applies to A269 TP201LN?
Table 2 caps TP201LN at 250 HBW / 263 HV or 100 HRB after solution treatment at ≥1900 °F [1040 °C]. That ceiling is higher than standard TP201’s 220 HBW / 96 HRB limit because of nitrogen strengthening. A269 still does not publish a tensile acceptance table for this grade.
Is A269 TP201LN suitable for chloride process duty?
Only in low-chloride, general-service conditions. LN improves as-welded intergranular behaviour; it does not add molybdenum for pitting resistance. For chloride-bearing process lines, step to A269 TP316L or a 6Mo grade rather than stretching S20153 past its envelope.
Nominal wall or minimum wall for A269 TP201LN?
A269 is a nominal-wall tubing specification. Write OD × nominal wall on the enquiry unless you and the mill agree a different wall basis. Do not assume A213 minimum-wall boiler-tube tolerances apply to an A269 LN order.
What size range can SHH STEEL produce for TP201LN?
SHH STEEL can produce and supply roughly 6–114 mm OD × 0.5–6.0 mm nominal wall in seamless or welded A269 TP201LN, with pickled or bright-annealed finish and EN 10204 3.1 MTCs. Other sizes are quoted by agreement against mill capability — send the size list for a firm answer.
Which tests are mandatory on A269 TP201LN tube?
Hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Product analysis and PMI are supplementary when ordered.
Can TP201LN replace TP304L on a welded skid?
Sometimes on cost, rarely on corrosion margin. TP304L brings higher nickel and a more familiar 18-8 passive film; TP201LN stays lean Cr-Mn-Ni with low carbon. A materials engineer should compare the medium before swapping. SHH STEEL will quote both A269 grades on the same OD × wall list when you ask.
What certificate does SHH STEEL provide for A269 TP201LN?
EN 10204 3.1 MTCs reporting ladle chemistry, solution-treatment condition, hardness, and hydro or NDE. Third-party inspection can be added on the order. Stencil shows ASTM A269, TP201LN / S20153, size, heat, and seamless or welded identity.
How should I write an enquiry for A269 TP201LN?
List ASTM A269, grade TP201LN / UNS S20153, seamless or welded, OD × nominal wall and length (or coil), finish, and any hydro/NDE lock. Add the service medium if corrosion selection is still open — SHH STEEL can produce and supply to that enquiry or recommend a sister A269 grade when LN is not enough.

Conclusion

ASTM A269 TP201LN / UNS S20153 is the low-carbon, nitrogen-controlled 200-series tubing grade for general-service lines that will be welded and expected to keep intergranular corrosion under control without jumping straight to 304L cost. SHH STEEL can produce and supply seamless and welded A269 TP201LN, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Compare options on the A269/A269M hub, then send the OD × nominal-wall list and medium notes. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X