ASTM A269 TP304LN Stainless Steel Tube
What is ASTM A269 TP304LN Stainless Steel Tube
ASTM A269 / A269M specifies nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP304LN is the nitrogen-bearing low-carbon 18-8 listing under UNS S30453: carbon ≤0.035%, nitrogen controlled at 0.10–0.16%, chromium 18.0–20.0%, and nickel 8.0–11.0%. The LN designation is the ASTM grade buyers put on the purchase order when they want L-grade as-welded behaviour plus nitrogen for austenite stability and strength — not a heat-treatment suffix stamped on ordinary TP304L. Shop language still says “304LN tube,” but the MTC must carry ASTM A269 Grade TP304LN so nominal-wall tolerances, hardness, and flaring or flange tests apply rather than an A213 or A312 product text.
SHH STEEL can produce and supply ASTM A269 TP304LN stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates covering Table 1 chemistry and Table 2 hardness. Typical enquiry sizes run about 6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare the family on the A269/A269M hub alongside A269 TP304L, A269 TP304, and A269 TP316LN. Keep the wall basis nominal — A269 is not a minimum-wall boiler-tube standard.
If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP304LN, SA213 TP304LN, A312 TP304LN and SA312 TP304LN and match the product standard to the drawing.
Chemical Composition of A269 TP304LN
Heat analysis under Table 1 is mandatory for every TP304LN heat; product analysis applies when ordered through A1016/A1016M and A480 Table A1.1. SHH STEEL reports measured ladle and, when ordered, product values — never unpublished tighter catalogue windows.
The melting limits below come from public A269 Table 1 excerpts for TP304LN / UNS S30453 (ASTM abstract cross-checked with the tubingchina A269 PDF). Footnote B on carbon for small-OD / light-wall drawing practice applies to TP304LN as it does to TP304L. Confirm the purchased edition.
Melting analysis (heat / ladle analysis) — Table 1
| Element | TP304LN (UNS S30453) melting analysis |
|---|---|
| Carbon (C) | ≤ 0.035 B |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 18.0 – 20.0 |
| Nickel (Ni) | 8.0 – 11.0 |
| Nitrogen (N) | 0.10 – 0.16 |
| Molybdenum (Mo) | … (no requirement) |
Source: ASTM A269/A269M Table 1 for TP304LN / UNS S30453 (public excerpts). Read carbon and nitrogen together: C ≤0.035% protects as-welded intergranular behaviour, while N at 0.10–0.16% restores austenite stability and contributes strength that low carbon would otherwise give away. Nickel stays in the 8–11% band (unlike TP304L’s 8–12%). No molybdenum — chloride-heavy duty still belongs on TP316LN or TP316L under A269.
Mechanical Properties of A269 TP304LN
A269 does not publish a tensile acceptance table for TP304LN. Lot acceptance rests on Table 2 hardness (192 HBW / 200 HV or 90 HRB), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Nitrogen strengthens the annealed austenite in service, but that engineering effect is not written as an A269 tensile floor — do not invent one from A213 or A312.
| Property | TP304LN requirement (A269 Table 2) |
|---|---|
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Tensile / yield / elongation | Not specified as an A269 acceptance table for this grade |
Source: ASTM A269/A269M Table 2 for TP304LN / UNS S30453 (public PDF excerpt). Hardness ceiling matches TP304 / TP304L; confirm thin-wall superficial Rockwell alternatives in the purchased edition’s hardness clause.
Seamless and Welded Tube
TP304LN may be seamless or welded under A269, hot- or cold-finished. Welded A269 tube is autogenous (no filler metal), cold-worked, and solution-treated with the tube — not an A312 WLD/HCW pipe product. Seamless takes flaring; welded takes flange and reverse flattening; both share hardness and hydro/NDE.
LN chemistry is often chosen specifically because fabrication welds will remain as-welded and the designer wants nitrogen on the MTC. The mill anneal still covers only the as-shipped tube. SHH STEEL can produce and supply both seamless and welded A269 TP304LN against the same Table 1 / Table 2 floors.
Dimensions and Tolerances
Order by OD and nominal wall. Table 4 sets OD, wall, and cut-length tolerances; clause 12.2 covers thin-wall ovality.
| OD group (A269 Table 4) | Outside diameter tolerance | Wall thickness tolerance |
|---|---|---|
| Up to ½ in. [13 mm] | ±0.005 in. [0.13 mm] | ±15% |
| ½ to 1½ in. [13–38 mm], excl. | ±0.005 in. [0.13 mm] | ±10% |
| 1½ to 3½ in. [38–89 mm], excl. | ±0.010 in. [0.25 mm] | ±10% |
| 3½ to 5½ in. [89–140 mm], excl. | ±0.015 in. [0.38 mm] | ±10% |
| 5½ to 8 in. [140–203 mm], excl. | ±0.030 in. [0.76 mm] | ±10% |
Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow ±12.5% wall on heavy wall / low ID/OD and ±15% on sub-½ in. ID non-mandrel tube. Flag A213 minimum-wall drawings explicitly on the enquiry.
Equivalent Grades
TP304LN / UNS S30453 is the ASTM tubing grade for nitrogen-bearing low-carbon 18-8. Related forms appear under A213 and A312 where those standards list S30453; plate cousins sit under A240 where listed. EN designations are commercial cousins only after a chemistry check.
| Reference | Designation | Note |
|---|---|---|
| ASTM A269 | TP304LN / UNS S30453 | This product standard |
| UNS | S30453 | Chemistry identity |
| ASTM A269 sister | TP304L / S30403 | Low C without mandatory N range |
| ASTM A213 / A312 | TP304LN (where listed) | Different product form / mechanical tables |
Step to A269 TP316LN when molybdenum plus nitrogen is required, or to A269 TP304L when nitrogen is not on the material list.
Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP304LN, SA213 TP304LN, A312 TP304LN and SA312 TP304LN. Confirm the product form before treating any of those pages as acceptance text for an A269 order.
Heat Treatment and Delivery Condition
All A269 TP304LN ships solution heat-treated. Table 2 requires ≥1900 °F [1040 °C] austenitizing with water quench or rapid cool. Ordered anneals below 1900 °F must be stenciled with the actual temperature after “HT.”
| Item | TP304LN (A269 Table 2) |
|---|---|
| Austenitizing temperature, min | 1900 °F [1040 °C] |
| Cooling | Water quench or rapid cool |
| Hardness after heat treatment, max | 192 HBW / 200 HV or 90 HRB |
| Delivery condition | Solution heat-treated; pickled or bright-annealed by agreement |
Source: ASTM A269/A269M §6 and Table 2 for TP304LN. SHH STEEL’s MTC states the heat-treatment condition applied to the shipped lengths.
Corrosion Resistance
TP304LN combines L-grade carbon control with specified nitrogen. Low carbon protects welded HAZs against sensitization; nitrogen supports austenite stability in the leaner solidification paths that low-C 18-8 can show. The passive film remains an 18-8 chromium-nickel film without molybdenum, so chloride pitting resistance stays below Mo-bearing A269 grades.
A269 publishes no PREN for S30453 — do not invent one. Use LN for as-welded mild aqueous and hygienic lines that call out nitrogen; use A269 TP316LN or TP316L when chlorides demand Mo.
Applications of A269 TP304LN Tube
A269 TP304LN appears on welded instrument and hygienic tubing specs that explicitly require nitrogen on the MTC, on process skids left as-welded, and on projects that standardized on LN chemistry across plate, pipe, and tube. Bright-annealed cold-finished LN is common in panel shops; pickled welded LN covers larger utility runs.
It is not boiler tube (A213) or pipe (A312), and it is not a Mo grade. SHH STEEL can produce and supply A269 TP304LN in the general-service band above and will redirect when the medium needs molybdenum or a higher alloy.
When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP304LN, SA213 TP304LN, A312 TP304LN and SA312 TP304LN instead of stretching an A269 tubing page into the wrong product form.
Weldability
Low carbon plus controlled nitrogen makes TP304LN a deliberate as-welded choice. GTAW/GMAW with 308L-type filler (when filler is used) is routine; mill autogenous seams on A269 welded tube are already solution-treated with the tube. Shop welds on cut lengths remain the fabricator’s procedure scope.
If molybdenum is also on the material list, order A269 TP316LN rather than stretching 304LN into chloride duty. SHH STEEL supplies the mill product and MTC.
Surface Finishes
Pickled and bright-annealed finishes cover most A269 TP304LN orders; named OD polish is supplementary when required. Bright anneal is preferred for instrumentation and hygienic ID/OD.
Write Ra or scrubbed-ID notes into the enquiry. SHH STEEL can produce and supply those finishes when the mill can measure and report them.
Inspection and Testing
Lots are hardness-tested to Table 2, flare-tested when seamless, and flange- plus reverse-flattening-tested when welded. Each length takes hydro or NDE; the mill chooses unless the order locks the method.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry (including nitrogen), heat treatment, hardness, and hydro/NDE. PMI and third-party holds are available when named on the order.
Packaging and Shipping
End caps, bundled sleeves or crates, and waterproof wrap protect TP304LN in transit. Bright-annealed and polished OD get extra sleeve protection. Coiled product follows A269’s continuous-coil rule.
Stencil carries ASTM A269, TP304LN / S30453, size, heat, seamless or welded identity, and NDE when applicable. SHH STEEL matches marking to the purchase-order clause.
Why Choose SHH STEEL
SHH STEEL can produce and supply ASTM A269 TP304LN as solution-treated seamless or welded tubing with Table 1 chemistry — including the mandatory nitrogen range — Table 2 hardness, and EN 10204 3.1 documentation. We will not ship TP304L and call it LN, and we will not omit nitrogen from the certificate when the grade requires it.
If the duty also needs molybdenum, we point to A269 TP316LN or A269 TP316L rather than selling nitrogen as a substitute for Mo.
Supply Capability
SHH STEEL can produce and supply ASTM A269 TP304LN to the edition, route, and finish on your enquiry. Capability and Stock / Available sizes follow.
| Item | SHH STEEL capability for TP304LN |
|---|---|
| Standard | ASTM A269 / A269M |
| Grade | TP304LN / UNS S30453 |
| Product form | Seamless and welded tube (no filler metal for welded), hot- or cold-finished |
| Delivery condition | Solution heat-treated ≥1900 °F [1040 °C]; pickled or bright-annealed |
| Typical size band | ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement) |
| Testing | Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range — not a frozen tonnage list. Confirm against near-term production when you send the OD × wall list.
| OD (mm) | Typical nominal walls (mm) | Notes |
|---|---|---|
| 6 / 8 / 10 / 12 / 14 | 0.5 / 0.8 / 1.0 / 1.2 / 1.5 | Instrument / hygienic; often BA |
| 12.7 / 15.9 / 19.1 / 25.4 / 31.8 | 1.0 / 1.2 / 1.5 / 2.0 / 2.5 | Inch OD skid tubing |
| 38.1 / 48.3 / 60.3 / 76.1 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Welded utility — LN when N is specified |
| 88.9 / 114.3 / 141.3 / 168.3 | 2.0 / 3.0 / 4.0 / 6.0 / 8.0 | Larger process tube; lock seamless vs welded |
Parallel quotes against A269 TP304L and A269 TP316LN keep nitrogen and molybdenum choices visible on one size list.
FAQ
-
What does LN mean in A269 TP304LN?
- LN marks the low-carbon, nitrogen-controlled 18-8 tubing grade under A269. Carbon is ≤0.035% (with Footnote B where it applies) and nitrogen is specified at 0.10–0.16% under UNS S30453. That combination improves as-welded intergranular behaviour versus TP304 while putting nitrogen on the MTC — it is a separate ASTM grade, not a heat-treatment suffix on TP304L.
-
TP304L vs TP304LN under A269 — which should I buy?
- Buy TP304L when low carbon is enough and nitrogen is not on the material list. Buy TP304LN when the specification explicitly requires nitrogen at 0.10–0.16% along with low carbon. Nickel bands also differ slightly (TP304L allows up to 12.0% Ni; TP304LN stays 8.0–11.0%). They must not share one grade stamp on the MTC.
-
Does A269 TP304LN include welded tube?
- Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both seamless and welded A269 TP304LN against the same chemistry and hardness floors named in Tables 1 and 2.
-
What hardness limit applies to A269 TP304LN?
- Table 2 caps TP304LN at 192 HBW / 200 HV or 90 HRB after solution treatment at ≥1900 °F [1040 °C]. Nitrogen strengthens service behaviour, but A269 still does not publish a tensile/yield/elongation acceptance table for this grade. Do not invent tensile floors from A213 or A312 unless the purchase order adds them.
-
Is nitrogen reported on the MTC for TP304LN?
- Yes. Nitrogen is a Table 1 requirement with a 0.10–0.16% range for TP304LN / UNS S30453, so the ladle analysis on an EN 10204 3.1 certificate should report nitrogen. If a certificate for an “LN” order omits nitrogen, treat that as a documentation problem and stop before accepting the heat.
-
Is A269 TP304LN nominal wall or minimum wall?
- Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs OD, wall, and cut-length tolerances. Do not assume A213 minimum-wall boiler-tube practice applies to an A269 TP304LN order.
-
What size range can SHH STEEL produce for TP304LN?
- SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP304LN, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes are quoted by agreement. Send the OD × wall list and process preference for a firm near-term availability answer.
-
When should I choose TP316LN instead of TP304LN?
- Choose TP316LN when the medium needs molybdenum for chloride pitting resistance and the material list also wants controlled nitrogen. TP304LN remains appropriate for milder aqueous and hygienic as-welded duties where Mo is not justified. Nitrogen is not a substitute for molybdenum in chloride service.
-
Which tests are mandatory on A269 TP304LN?
- Hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Product analysis and PMI are supplementary when ordered.
-
What certificate does SHH STEEL provide for A269 TP304LN?
- EN 10204 3.1 MTCs report ladle chemistry including nitrogen, solution-treatment condition, hardness, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, TP304LN / S30453, size, heat, and seamless or welded identity.
-
How should I enquire for A269 TP304LN with SHH STEEL?
- List ASTM A269, grade TP304LN / UNS S30453, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Note that nitrogen must appear on the MTC. SHH STEEL can produce and supply to that enquiry or recommend TP304L / TP316LN when the material list points that way.
Conclusion
ASTM A269 TP304LN / UNS S30453 is the nitrogen-bearing low-carbon 18-8 tubing grade for general-service lines that need as-welded corrosion behaviour and a reported nitrogen range on the certificate. SHH STEEL can produce and supply seamless and welded A269 TP304LN, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.