Product Showcase
GB/T 3621 Titanium Alloys
SHH STEEL offers GB/T 3621-compliant TA1/TA2 titanium and titanium alloy sheets and strips. GB/T 3621 specifies hot-rolled and cold-rolled products for chemical equipment and marine engineering. Strong, lightweight, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 3621 TC2 Titanium Plate | Ti-4Al-1.5Mn
GB/T 3621 TC2 titanium plate is Ti-4Al-1.5Mn titanium alloy supplied annealed (M). It is specified for 685 MPa minimum tensile strength and 25% minimum elongation. Typical uses include formed and welded aerospace sheet parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA9-1 Titanium Plate | Ti-0.2Pd
GB/T 3621 TA9-1 titanium plate is Ti-0.2Pd titanium supplied annealed (M). It is specified for 240 MPa minimum tensile strength, 140–310 MPa yield and 24% minimum elongation. Typical uses include linings and cladding in reducing-acid service. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA10 Titanium Plate | Ti-0.3Mo-0.8Ni
GB/T 3621 TA10 titanium plate is Ti-0.3Mo-0.8Ni titanium supplied annealed (M). It is specified for 485 MPa minimum tensile strength, 345 MPa yield and 18% minimum elongation. Typical uses include salt-production evaporators and brine heaters. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA11 Titanium Plate | Ti-8Al-1Mo-1V
GB/T 3621 TA11 titanium plate is Ti-8Al-1Mo-1V titanium alloy supplied annealed (M). It is specified for 895 MPa minimum tensile strength, 825 MPa yield and 10% minimum elongation. Typical uses include compressor and engine parts at elevated temperature. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA15 Titanium Plate | Ti-6.5Al-Mo-V-Zr
GB/T 3621 TA15 titanium plate is Ti-6.5Al-Mo-V-Zr titanium alloy supplied annealed (M). It is specified for 930–1130 MPa tensile strength, 855 MPa yield and 12% minimum elongation. Typical uses include welded airframe structures. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA17 Titanium Plate | Ti-2Al-2V
GB/T 3621 TA17 titanium plate is Ti-2Al-2V titanium alloy supplied annealed (M). It is specified for 685–835 MPa tensile strength and 25% minimum elongation. Typical uses include welded pressure vessels. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA18 Titanium Plate | Ti-3Al-2.5V
GB/T 3621 TA18 titanium plate is Ti-3Al-2.5V titanium alloy supplied annealed (M). It is specified for 590–735 MPa tensile strength and 25% minimum elongation. Typical uses include lightweight sheet structures and ducting. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA6 Titanium Plate | Ti-5Al Titanium
GB/T 3621 TA6 titanium plate is Ti-5Al titanium supplied annealed (M). It is specified for 685 MPa minimum tensile strength and 20% minimum elongation. Typical uses include elevated-temperature sheet structures. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA7 Titanium Plate | Ti-5Al-2.5Sn
GB/T 3621 TA7 titanium plate is Ti-5Al-2.5Sn titanium alloy supplied annealed (M). It is specified for 735–930 MPa tensile strength, 685 MPa yield and 20% minimum elongation. Typical uses include aero-engine casings and hot-section sheet. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA8 Titanium Plate | Lean Pd Titanium
GB/T 3621 TA8 titanium plate is lean-Pd titanium supplied annealed (M). It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA8-1 Titanium Plate | Lean Pd Titanium
GB/T 3621 TA8-1 titanium plate is lean-Pd titanium supplied annealed (M). It is specified for 240 MPa minimum tensile strength, 140–310 MPa yield and 24% minimum elongation. Typical uses include clad layers and linings in crevice-prone service. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
GB/T 3621 TA9 Titanium Plate | Ti-0.2Pd
GB/T 3621 TA9 titanium plate is Ti-0.2Pd titanium supplied annealed (M). It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.View More
GB/T 3621 Titanium Alloys
Titanium Alloy Plates and Sheets
SHH STEEL, a premier Titanium Alloy Plates and Sheets exporter, produces and exports titanium alloy plates and sheets for aerospace, marine, and chemical industries. Our products, like Grade 2 and Grade 5 (ASTM B265), offer high strength and corrosion resistance. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Grade 5 titanium plates and custom solutions for high-performance projects.
Titanium Alloy Plates and Sheets
X