GB/T 3621 TA23 Titanium Plate | Ti-2.5Al-2Zr-1Fe
What is GB/T 3621 TA23 titanium plate?
GB/T 3621 TA23 titanium plate is made to GB/T 3621, the Chinese national standard for titanium and titanium alloy plate and sheet. TA23 is Ti-2.5Al-2Zr-1Fe, a Chinese near-alpha alloy using iron as a low-cost addition. It combines medium strength with good weldability and corrosion resistance for marine structures.
This is an alpha or near-alpha titanium alloy. Aluminium (and in some grades tin or zirconium) strengthens the alpha phase, while only small amounts of beta stabilisers such as manganese, molybdenum or vanadium are present. Such alloys keep good weldability and creep strength at elevated temperature, are normally used annealed, and respond little to strengthening heat treatment.
Chinese titanium designations use TA for alpha and near-alpha grades, including unalloyed titanium, TB for beta alloys and TC for alpha-beta alloys. The 2022 edition renamed the unalloyed industrial grades with a G suffix, such as TA1G and TA2G, and added or removed several alloy grades.
SHH STEEL handles TA23 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered GB/T 3621 edition, product form and certificate type before confirming supply. Related designations covered on this site include GB/T 3621 TA22, GB/T 3621 TA24.
Material specification for GB/T 3621 TA23
GB/T 3621 is the Chinese national standard for titanium and titanium alloy plate and sheet produced by rolling. The current edition, GB/T 3621-2022, replaced the 2007 edition from 1 May 2023. Chemical composition is taken from GB/T 3620.1, and product analysis tolerances from GB/T 3620.2.
| Ordering item | GB/T 3621 basis |
|---|---|
| Standard | GB/T 3621-2022 (state the edition if an older one is required) |
| Grade | TA23 (Ti-2.5Al-2Zr-1Fe) |
| Condition | Annealed (M) |
| Size range (2022) | 0.3–5.0 mm thick, 400–1800 mm wide, 1000–4000 mm long; over 5.0–100.0 mm thick, 400–3000 mm wide, 1000–6000 mm long |
| Marking example | Plate TA23 M 1.0×1000×2000 GB/T 3621 |
| Certificate | Quality certificate with chemistry, tensile results and other agreed tests |
Recommended nominal thicknesses are multiples of 0.1 mm up to 5.0 mm and multiples of 0.5 mm above that. Unless the order asks for longitudinal tests, tensile properties are tested in the transverse direction. Supply route, testing and inspection are confirmed on the contract.
The 2022 edition changed more than grade names. It revised the size ranges, tightened several dimensional tolerances, updated the surface quality clauses and reorganised the property tables. Purchase orders that still cite GB/T 3621-2007 remain valid if both parties agree, but the edition, grade name and property table that govern acceptance should be written on the contract so that inspection and certification follow one document.
Chemical composition of GB/T 3621 TA23
Composition follows GB/T 3620.1, the Chinese standard for titanium and titanium alloy grades and compositions. Single values are maximums; titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.04 max |
| Carbon (C) | 0.1 max |
| Hydrogen (H) | 0.01 max |
| Iron (Fe) | 0.8–1.2 |
| Oxygen (O) | 0.15 max |
| Aluminium (Al) | 2.2–3 |
| Zirconium (Zr) | 1.7–2.3 |
| Silicon (Si) | 0.15 max |
| Other elements, each | 0.1 max |
| Other elements, total | 0.3 max |
| Titanium (Ti) | Balance |
Product analysis tolerances follow GB/T 3620.2. Other elements are not normally reported unless the contract asks for them. Grades renamed in the newer editions, such as TA1 to TA1G, keep closely related limits, but the edition named on the order governs.
Mechanical properties of GB/T 3621 TA23
The values below are the requirements for TA23 plate in the annealed (M) condition.
| Thickness, mm | Tensile strength Rm, MPa | Proof strength Rp0.2, MPa | Elongation A, min, % |
|---|---|---|---|
| As ordered | 590 min | Report measured value | 18 |
GB/T 3621-2022 sets minimum tensile strength and elongation for this grade, and the proof strength is reported as measured unless the contract sets a value. Confirm the property values against the edition named on the order.
Tensile properties are tested in the transverse direction unless the order asks for longitudinal tests. Elevated-temperature properties and bend tests are supplied only when agreed.
Delivery condition, finish and marking
GB/T 3621 plate is supplied in the condition listed for the grade. The 2022 edition revised the surface quality requirements; plate is normally pickled, ground or machined, and must be free of cracks, laps and inclusions that affect use.
- Condition: Annealed (M)
- Surface: pickled, ground or machined, as agreed
- Marking: grade, condition, size, heat number and standard number
- Packing: to GB/T 8180, or as stated on the contract
The alloy is supplied annealed; stress relieving after forming or welding is agreed with the purchaser. State whether the plate will be cold formed, welded or clad so the surface condition and flatness can be agreed.
Welding and fabrication of TA23 titanium plate
TA23 is weldable by gas tungsten arc, plasma arc, electron beam and laser processes, provided the weld zone is fully shielded from air.
- Use trailing shields and back purging until the weld cools below about 400 °C
- Use matching or engineer-approved filler metal and qualified procedures
- Clean joints and filler wire; remove oil, moisture and iron contamination
- Consider post-weld stress relief for highly restrained or precision parts, as agreed in the procedure
Room-temperature formability is lower than for CP titanium. Moderate bends can be cold formed with generous radii, but severe shapes are normally hot formed or creep formed.
Machining needs sharp carbide tools, rigid set-ups, low cutting speeds and generous coolant, because titanium alloys conduct heat poorly and the heat stays at the cutting edge. Avoid dwelling, which work-hardens the surface, and keep fine chips away from ignition sources.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
GB/T 3621-2022 tightened the dimensional tolerances of the 2007 edition. Thickness tolerances depend on thickness and width, for example ±0.05 mm for 0.3–0.5 mm sheet up to 1000 mm wide and ±2.00 mm for 70–100 mm plate. Width and length tolerances are plus-only, and flatness per 1000 mm ranges from 20 mm for thin wide sheet to 8 mm or less for thick plate.
If a one-sided thickness tolerance is required, the value is twice the tabulated figure. State thickness, width, length, quantity and any cutting drawing on the order. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of TA23 titanium plate
Typical uses of TA23 plate include:
- Ship and marine structures
- Welded pressure parts
- Seawater equipment
- Offshore components
As with all titanium, the alloy is not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. High-aluminium alloys can be sensitive to hot-salt stress corrosion, and maximum service temperatures depend on the alloy and design code. The design engineer must confirm suitability for the actual service.
When selecting TA23, compare it with TA17, TA18, TA22. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare TA23 with other GB/T 3621 grades
The grades below are the closest neighbours of TA23 in GB/T 3621. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| TA17 | 685–835 MPa | — | 25% | Ti-4Al-2V near-alpha |
| TA18 | 590–735 MPa | — | 25% | Ti-3Al-2.5V, Grade 9-type |
| TA22 | 490 MPa min | — | 18% | Ti-3Al-1Mo-1Ni-1Zr |
| TA23 | 590 MPa min | — | 18% | Ti-2.5Al-2Zr-1Fe |
| TA24 | 550 MPa min | — | 13% | Ti-3Al-2Mo-2Zr |
| TA31 | 800 MPa min | 700 MPa min | 10% | Ti-6Al-3Nb-2Zr-1Mo (Ti-80) |
| TA36 | 520 MPa min | 400 MPa min | 20% | Ti-1Al-1Fe |
Alpha and near-alpha alloys trade formability for strength and elevated-temperature performance. Compare the full requirements, not only tensile strength, before changing grade.
GB/T 3621 TA23 equivalent grades
The designations below are commonly compared with GB/T 3621 TA23. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to GB/T 3621 TA23 |
|---|---|---|
| GB/T 3621 | TA22 | Nearest by role only; composition and properties differ |
| GB/T 3621 | TA24 | Nearest by role only; composition and properties differ |
| ASTM | No direct grade | Chinese marine alloy; nearest by role only |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for TA23 titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to the GB/T 3621 edition you name and keep old and new grade names (such as TA2 and TA2G) distinct
- Certificates are checked against GB/T 3620.1 chemistry and the agreed tensile values
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for GB/T 3621 TA23 plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | GB/T 3621 TA23, edition |
| Product form | Plate or sheet; condition as listed for the grade |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Which edition of GB/T 3621 applies to TA23?
- GB/T 3621-2022 has applied since 1 May 2023 and replaces the 2007 edition. If a drawing still cites 2007, agree on the order which edition, grade name and property table govern acceptance.
-
What is the tensile strength of GB/T 3621 TA23 titanium plate?
- The requirement is 590 MPa minimum. The 0.2% proof or yield strength is reported as measured. Minimum elongation is 18%. Values apply to the condition and thickness range stated in the standard.
-
What is TA23 mainly used for?
- Typical uses include ship and marine structures, welded pressure parts and seawater equipment. The design engineer should confirm the grade for the actual service.
-
What sizes does GB/T 3621-2022 cover?
- Annealed plate and sheet from 0.3 to 100.0 mm thick: 400–1800 mm wide up to 5.0 mm thick, and 400–3000 mm wide above 5.0 mm. Lengths run from 1000 to 6000 mm.
-
What should I send for a quotation?
- Send GB/T 3621 TA23, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for GB/T 3621 TA23 titanium plate
GB/T 3621 TA23 is Ti-2.5Al-2Zr-1Fe titanium alloy specified for 590 MPa minimum tensile strength and 18% minimum elongation in the annealed (M) condition. Typical uses include ship and marine structures and welded pressure parts.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GB/T 3621 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com