GB/T 3621 TC18 Titanium Plate | Ti-5Al-Mo-V-Cr-Fe
What is GB/T 3621 TC18 titanium plate?
GB/T 3621 TC18 titanium plate is made to GB/T 3621, the Chinese national standard for titanium and titanium alloy plate and sheet. TC18 is Ti-5Al-4.75Mo-4.75V-1Cr-1Fe, a high-strength near-beta alloy (counterpart of the Russian VT22) with deep hardenability for large airframe sections.
This is an alpha-beta titanium alloy. Aluminium strengthens the alpha phase and vanadium or molybdenum stabilises the beta phase, so the structure and properties depend on hot working and heat treatment. Plate is normally supplied mill annealed, giving high strength, good fatigue performance and a strength-to-weight ratio well above that of steels.
Its typical density of about 4.65 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Chinese titanium designations use TA for alpha and near-alpha grades, including unalloyed titanium, TB for beta alloys and TC for alpha-beta alloys. The 2022 edition renamed the unalloyed industrial grades with a G suffix, such as TA1G and TA2G, and added or removed several alloy grades.
SHH STEEL handles TC18 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered GB/T 3621 edition, product form and certificate type before confirming supply. Related designations covered on this site include GB/T 3621 TC4.
Material specification for GB/T 3621 TC18
GB/T 3621 is the Chinese national standard for titanium and titanium alloy plate and sheet produced by rolling. The current edition, GB/T 3621-2022, replaced the 2007 edition from 1 May 2023. Chemical composition is taken from GB/T 3620.1, and product analysis tolerances from GB/T 3620.2.
| Ordering item | GB/T 3621 basis |
|---|---|
| Standard | GB/T 3621-2022 (state the edition if an older one is required) |
| Grade | TC18 (Ti-5Al-Mo-V-Cr-Fe) |
| Condition | Annealed (M) |
| Size range (2022) | 0.3–5.0 mm thick, 400–1800 mm wide, 1000–4000 mm long; over 5.0–100.0 mm thick, 400–3000 mm wide, 1000–6000 mm long |
| Marking example | Plate TC18 M 1.0×1000×2000 GB/T 3621 |
| Certificate | Quality certificate with chemistry, tensile results and other agreed tests |
Recommended nominal thicknesses are multiples of 0.1 mm up to 5.0 mm and multiples of 0.5 mm above that. Unless the order asks for longitudinal tests, tensile properties are tested in the transverse direction. Supply route, testing and inspection are confirmed on the contract.
The 2022 edition changed more than grade names. It revised the size ranges, tightened several dimensional tolerances, updated the surface quality clauses and reorganised the property tables. Purchase orders that still cite GB/T 3621-2007 remain valid if both parties agree, but the edition, grade name and property table that govern acceptance should be written on the contract so that inspection and certification follow one document.
Chemical composition of GB/T 3621 TC18
Composition follows GB/T 3620.1, the Chinese standard for titanium and titanium alloy grades and compositions. Single values are maximums; titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.05 max |
| Carbon (C) | 0.08 max |
| Hydrogen (H) | 0.015 max |
| Iron (Fe) | 0.5–1.5 |
| Oxygen (O) | 0.18 max |
| Aluminium (Al) | 4.4–5.7 |
| Vanadium (V) | 4–5.5 |
| Zirconium (Zr) | 0.3 max |
| Molybdenum (Mo) | 4–5.5 |
| Chromium (Cr) | 0.5–1.5 |
| Silicon (Si) | 0.15 max |
| Other elements, each | 0.1 max |
| Other elements, total | 0.3 max |
| Titanium (Ti) | Balance |
Product analysis tolerances follow GB/T 3620.2. Other elements are not normally reported unless the contract asks for them. Grades renamed in the newer editions, such as TA1 to TA1G, keep closely related limits, but the edition named on the order governs.
Mechanical properties of GB/T 3621 TC18
The values below are the requirements for TC18 plate in the annealed (M) condition.
| Thickness, mm | Tensile strength Rm, MPa | Proof strength Rp0.2, MPa | Elongation A, min, % |
|---|---|---|---|
| As agreed | 1080 min | 1000 min | 10 |
TC18 is not listed in the property table of the published GB/T 3621-2022 edition. The values above are typical agreed values for annealed plate and must be fixed in the contract or technical agreement before production.
Tensile properties are tested in the transverse direction unless the order asks for longitudinal tests. Elevated-temperature properties and bend tests are supplied only when agreed.
Delivery condition, finish and marking
GB/T 3621 plate is supplied in the condition listed for the grade. The 2022 edition revised the surface quality requirements; plate is normally pickled, ground or machined, and must be free of cracks, laps and inclusions that affect use.
- Condition: Annealed (M)
- Surface: pickled, ground or machined, as agreed
- Marking: grade, condition, size, heat number and standard number
- Packing: to GB/T 8180, or as stated on the contract
Plate is supplied annealed. Solution treating and ageing, where wanted, is normally done on the part and its properties are agreed separately. State whether the plate will be cold formed, welded or clad so the surface condition and flatness can be agreed.
Welding and fabrication of TC18 titanium plate
TC18 can be welded by gas tungsten arc, plasma arc, electron beam and laser processes, but it needs more control than CP titanium.
- Shield the weld, heat-affected zone and root with inert gas until below about 400 °C
- Use qualified procedures and matching or engineer-approved filler metal
- Expect lower weld-zone ductility than in the base plate; stress relief after welding is common
- Clean joints thoroughly and avoid iron contamination
Cold formability is limited. Most forming of alpha-beta plate is done hot or by creep forming, and machining needs sharp tools, rigid set-ups and generous coolant.
Plan machining around the low thermal conductivity of the alloy: heat stays at the tool edge, so cutting speeds are low and coolant flow is high. Avoid interrupted light cuts that work-harden the surface, and keep fine chips away from ignition sources.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
GB/T 3621-2022 tightened the dimensional tolerances of the 2007 edition. Thickness tolerances depend on thickness and width, for example ±0.05 mm for 0.3–0.5 mm sheet up to 1000 mm wide and ±2.00 mm for 70–100 mm plate. Width and length tolerances are plus-only, and flatness per 1000 mm ranges from 20 mm for thin wide sheet to 8 mm or less for thick plate.
If a one-sided thickness tolerance is required, the value is twice the tabulated figure. State thickness, width, length, quantity and any cutting drawing on the order. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of TC18 titanium plate
Typical uses of TC18 plate include:
- Large airframe structural parts
- Landing gear and high-load fittings
- Thick-section machined parts
- High-strength structures
Plate in TC18 is less common than bar and forgings; supply terms need agreement. Alpha-beta alloys resist seawater and many oxidizing media well, but they are less resistant than CP titanium in hot reducing acids. They are not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. Maximum service temperature and fatigue design values come from the applicable design code, not from the plate specification.
When selecting TC18, compare it with TC1, TC2, TC3. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare TC18 with other GB/T 3621 grades
The grades below are the closest neighbours of TC18 in GB/T 3621. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| TC1 | 590–735 MPa | — | 25% | Ti-2Al-1.5Mn near-alpha |
| TC2 | 685 MPa min | — | 25% | Ti-4Al-1.5Mn near-alpha |
| TC3 | 880 MPa min | — | 12% | Ti-5Al-4V alpha-beta |
| TC4 | 895 MPa min | 830 MPa min | 12% | Ti-6Al-4V alpha-beta |
| TC4ELI | 860 MPa min | 795 MPa min | 10% | Ti-6Al-4V ELI |
| TC11 | 1030 MPa min | 900 MPa min | 10% | Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alpha-beta |
| TC18 | 1080 MPa min | 1000 MPa min | 10% | Ti-5Al-5Mo-5V-1Cr-1Fe near-beta |
A higher strength level is not automatically better. Interstitial limits, toughness, bend radius and fatigue behaviour differ between grades, so changes need engineer approval.
GB/T 3621 TC18 equivalent grades
The designations below are commonly compared with GB/T 3621 TC18. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to GB/T 3621 TC18 |
|---|---|---|
| GB/T 3621 | TC4 | Nearest by role only; composition and properties differ |
| GOST 19807 designation | VT22 (Ti-5Al-5Mo-5V-1Cr-1Fe) | Similar nominal composition |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for TC18 titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to the GB/T 3621 edition you name and keep old and new grade names (such as TA2 and TA2G) distinct
- Certificates are checked against GB/T 3620.1 chemistry and the agreed tensile values
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for GB/T 3621 TC18 plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | GB/T 3621 TC18, edition |
| Product form | Plate or sheet; condition as listed for the grade |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Which edition of GB/T 3621 applies to TC18?
- GB/T 3621-2022 has applied since 1 May 2023 and replaces the 2007 edition. If a drawing still cites 2007, agree on the order which edition, grade name and property table govern acceptance.
-
What is the tensile strength of GB/T 3621 TC18 titanium plate?
- The requirement is 1080 MPa minimum. The 0.2% proof or yield strength is 1000 MPa minimum. Minimum elongation is 10%. Values apply to the condition and thickness range stated in the standard.
-
What is TC18 mainly used for?
- Typical uses include large airframe structural parts, landing gear and high-load fittings and thick-section machined parts. Plate in TC18 is less common than bar and forgings; supply terms need agreement.
-
What sizes does GB/T 3621-2022 cover?
- Annealed plate and sheet from 0.3 to 100.0 mm thick: 400–1800 mm wide up to 5.0 mm thick, and 400–3000 mm wide above 5.0 mm. Lengths run from 1000 to 6000 mm.
-
What should I send for a quotation?
- Send GB/T 3621 TC18, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for GB/T 3621 TC18 titanium plate
GB/T 3621 TC18 is Ti-5Al-Mo-V-Cr-Fe titanium alloy specified for 1080 MPa minimum tensile strength, 1000 MPa minimum yield or proof strength and 10% minimum elongation in the annealed (M) condition. Typical uses include large airframe structural parts and landing gear and high-load fittings.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GB/T 3621 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com