EN 10216-5 1.4912 Seamless Stainless Steel Tube

EN 10216-5 1.4912 / X7CrNiNb18-10 seamless stainless pressure tube (347H-type creep), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm 510–710, solution annealed at 1070–1125 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4912 / X7CrNiNb18-10 (347H-type creep — body alias)
Standard
EN 10216-5
Product form
Seamless tube for pressure purposes (hot-finished or cold-finished), solution annealed
Size
Typical seamless OD × wall from ~6 mm to 219 mm OD × 0.5–12.7 mm wall within the 50 mm wall characterisation band; other OD × wall by agreement (Options 7/8 above band)
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10216-5 1.4912 Seamless Stainless Steel Tube

EN 10216-5:2021 (BS EN 10216-5:2021) is the European product standard for seamless stainless steel tubes for pressure purposes — Part 5 of the EN 10216 series, and the only part that covers austenitic and austenitic-ferritic stainless grades for pressure plus corrosion-resisting service at room, low, or elevated temperature. Steel number 1.4912 (X7CrNiNb18-10) sits in the austenitic creep-resisting family under EN 10216-5 Table 3 / Table 7. Writing a commercial alias alone on a bill of materials is not enough: the purchase order must name EN 10216-5, the steel number, the test category (TC1 or TC2), and the delivery-condition / options list so the mill applies the correct cast analysis, solution anneal, mechanical floors, leak-tightness, and marking.

SHH STEEL can produce and supply EN 10216-5 1.4912 seamless stainless steel tube — hot-finished or cold-finished, solution annealed over the full length, with EN 10204 3.1 inspection documents (3.2 under Option 21) that report cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes run from about 6 mm to 219 mm outside diameter with walls from roughly 0.5 mm into the double-digit millimetre band within the standard’s 50 mm characterisation ceiling for this family; walls above that band need Options 7 or 8 and agreed properties. Browse the series hub at EN 10216-5.

The grade is the Nb-stabilised creep-resisting austenitic for elevated-temperature pressure duty. Typical pressure duties include boiler and process tubing in the creep range needing Nb carbides. Design caution: do not treat as a drop-in for corrosion-grade 1.4550 without checking IGC and creep tables. Commercially the grade is often called 347H-type creep; that shop name belongs in the body and on the enquiry note, never as a substitute for the steel number on the MTC. Sister numbers on this hub include EN 10216-5 1.4550, EN 10216-5 1.4948, EN 10216-5 1.4940. When the same chemistry idea is needed under ASTM/ASME product standards, open A213 TP347H and A269 TP347 and match the product form — those pages are not drop-in acceptance text for an EN 10216-5 order.

These grades are characterised for elevated-temperature and creep-range pressure service; Annex A creep rupture data applies only to Table 3 numbers, and intergranular corrosion resistance is marked No in the delivery condition. EN 10216-5 covers seamless product only — welded pressure stainless tube belongs under EN 10217, not on this page. Preferred dimensions follow EN ISO 1127 rather than the carbon-steel EN 10220 lists used in Parts 1–4.

Chemical Composition of EN 10216-5 1.4912

Every 1.4912 heat under EN 10216-5 must meet the cast (ladle) analysis for its table — Table 2 for corrosion-resisting austenitics, Table 3 for creep-resisting austenitics, or Table 4 for duplex. Product analysis is Option 4, with permissible deviations in Table 5 of the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unpublished “tighter than table” catalogue windows as if they were EN limits.

The table below reproduces public BSSA EN 10216-5 chemical limits for 1.4912 / X7CrNiNb18-10, cross-checked against xtd BS EN 10216-5:2021 grade tables. Values are maximum unless a range is shown. Confirm the purchased EN 10216-5:2021 edition before treating any secondary catalogue as the acceptance text.

Element 1.4912 cast analysis (mass %)
Carbon (C) 0.04–0.10
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.040
Sulfur (S) ≤0.015
Nitrogen (N) ≤0.10
Chromium (Cr) 17.00–19.00
Nickel (Ni) 9.00–12.00
Niobium (Nb) 10×C–1.20

Source: BSSA “Chemical compositions of stainless steels to EN 10216-5” (Tables 2/3/4) with xtd 2021 cross-check. Elements not listed shall not be intentionally added without purchaser agreement, except finishing additions, with scrap controls to protect mechanical and corrosion behaviour.

Mechanical Properties of EN 10216-5 1.4912

Ambient mechanical properties for 1.4912 are taken from EN 10216-5 Table 7 for austenitic creep-resisting steels in the solution-annealed (+AT) condition, for wall thicknesses up to 50 mm. Austenitic grades list both Rp0.2 and Rp1.0 because they lack a sharp yield point. Creep rupture characterisation lives in informative Annex A — do not invent rupture digits from marketing sheets.

The figures below follow xtd’s BS EN 10216-5:2021 ambient tables as the primary public 2021 framing, cross-checked against the BSSA ambient mechanical-properties article (historically based on the 2005 edition). SHH STEEL will not paste sister-standard tensile floors onto an EN 10216-5 certificate to make the document look busier.

Property 1.4912 ambient (solution annealed)
Rp0.2 min (MPa) 205
Rp1.0 min (MPa) 240
Rm (MPa) 510–710
A min % long / trans 40 / 30
IGC resistance (delivery) No
Solution annealing 1070–1125 °C
Cooling water or air as tabulated

Source: xtd BS EN 10216-5:2021 Tables 6/7/8 (ambient) with BSSA ambient article cross-check; solution-annealing bands from the same public tables. Impact energies apply irrespective of whether Options 6/11 verify them — order the option when the certificate must show tested joules.

Seamless Tube Manufacture

EN 10216-5 is a seamless-only product standard. 1.4912 tube is manufactured by a seamless process and may be hot finished or cold finished, but it is always supplied solution annealed over its full length. Welded pressure stainless tube is outside this page — specify EN 10217 when a weld seam is required.

Delivery condition symbols distinguish surface finish on top of that heat-treated seamless route: HFD (hot finished, heat treated, descaled), CFD (cold finished, heat treated, descaled), CFA (cold finished, bright annealed), CFG (ground), and CFP (polished). Unless Option 2 locks the condition, the manufacturer chooses. SHH STEEL can produce and supply 1.4912 as HFD or CFD in the common pressure-tube band, and as CFA/CFG/CFP when the enquiry names the finish and roughness scope.

Cold-finished tube with Option 20 (D4/T4) is the usual instrumentation and precision HX conversation; hot-finished HFD dominates heavier walls. State TC1 or TC2 on every order — test category is mandatory marking information for every grade in Part 5.

Dimensions and Tolerances

For steel number 1.4912 (X7CrNiNb18-10), order EN 10216-5 1.4912 by outside diameter D and wall thickness T. Preferred sizes follow EN ISO 1127. Mass per unit length uses stainless densities from EN 10088-1 / EN 10028-7 — not the carbon-steel 7.85 kg/dm³ default. Tolerance classes are D1–D4 on diameter and T1–T4 on wall (EN ISO 1127), with out-of-roundness inside the diameter tolerance and eccentricity inside the wall tolerance.

Hot-finished tube typically uses D2 with T1 or T2 up to 219.1 mm OD, and D1 above that diameter. Cold-finished tube defaults to D3/T3; Option 20 selects the tighter D4/T4 band (±0.5% or ±0.1 mm on D; ±7.5% or ±0.15 mm on T, whichever is greater). Exact lengths are Option 18; bevelled ends for T ≥ 3.2 mm are Option 17.

Route Typical diameter class Typical wall class Notes
Hot finished (HFD) D2 (≤219.1 mm) / D1 (>219.1 mm) T1 or T2 Descaled metallically clean
Cold finished default D3 T3 CFD / CFA common
Cold finished Option 20 D4 T4 Instrumentation / precision HX

Straightness shall not exceed 0.0015×L over the tube length, and not more than 3 mm over any one-metre length. SHH STEEL aligns OD × wall and tolerance class to the purchase order before rolling slots are locked.

Equivalent Grades

1.4912 / X7CrNiNb18-10 is the EN 10216-5 designation for this chemistry and product form. ASTM/ASME tubing or pipe pages that share a commercial alias are related product standards with different wall bases, mechanical tables, and test regimes — confirm before treating them as interchangeable with an EN pressure-tube order.

Reference Designation Note
EN 10216-5 1.4912 / X7CrNiNb18-10 This product standard (seamless pressure tube)
EN steel name X7CrNiNb18-10 EN 10027-1 designation used in body and marking
Commercial alias (body only) 347H-type creep Not a substitute for the steel number on the MTC
A213 TP347H A213 TP347H Related live page — different product standard
A269 TP347 A269 TP347 Related live page — different product standard

Inside this series, compare EN 10216-5 1.4550, EN 10216-5 1.4948, EN 10216-5 1.4940. Hub: EN 10216-5. Live cross-standard anchors: A213 TP347H and A269 TP347.

Heat Treatment and Delivery Condition

Tubes in 1.4912 are supplied solution annealed over the full length. Reference heat treatment heats the tube uniformly into the tabulated solution-temperature band and cools rapidly; alternatively, solution-annealed properties may be obtained directly by extrusion and subsequent cooling when all specified mechanical and corrosion properties still conform — including after a subsequent reference heat treatment if required.

For 1.4912, public EN 10216-5 tables place solution annealing at 1070–1125 °C, with cooling by water or air as tabulated. Pickled versus bright-annealed versus ground/polished is a surface choice on top of that mandatory solution treatment (Option 2 to lock it).

Item 1.4912
Solution annealing band 1070–1125 °C
Cooling water or air as tabulated
Delivery condition symbols HFD / CFD / CFA / CFG / CFP (Option 2 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

SHH STEEL ships EN 10216-5 1.4912 only in a heat-treated condition that meets the ordered table, and the inspection document states what was done.

Corrosion Resistance

Table 7 creep-resisting grades including 1.4912 are marked No for resistance to intergranular corrosion in the delivery condition — the footnote notes that IGC resistance is normally not fulfilled in the sensitised condition. Specifying 1.4912 for aqueous corrosive duty is usually a category error; Table 2 corrosion-resisting numbers are where Clause 8.4 IGC design lives.

Annex A creep rupture data (informative) is the elevated-temperature selection story for Table 3 grades. Public summaries give temperature bands and mean rupture strengths with large batch scatter; SHH STEEL will not invent 10 000 h or 100 000 h digits on a datasheet without the purchased Annex A text in hand. Oxidation and total stressing still govern continuous duty — Annex A temperatures are not automatic continuous-service ceilings.

Applications of EN 10216-5 1.4912 Tube

EN 10216-5 1.4912 seamless tube is used where PED-oriented pressure tubing must also resist corrosion (or, for Table 3, carry creep characterisation). For this number the practical band is boiler and process tubing in the creep range needing Nb carbides, supplied as solution-annealed seamless tube with TC1 or TC2 testing.

It is the wrong first choice when a welded seam is mandatory (use EN 10217), when the drawing is ASTM A269 instrumentation tubing or A213 boiler tube without an EN dual mark, or when the medium clearly needs a different family — for example duplex when chloride SCC governs and an austenitic is on the page by habit. SHH STEEL can produce and supply 1.4912 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit. Related live pages: A213 TP347H and A269 TP347.

Weldability

1.4912 is welded in fabrication with processes and fillers chosen for the EN chemistry family — typically matching or overlying austenitic fillers for Table 2/3 grades, and duplex-rated fillers with heat-input control for Table 4 grades. Autogenous mill seams do not exist on EN 10216-5 product because the standard is seamless-only; shop welds are a fabrication step outside the mill solution anneal.

As-welded corrosive service, ferrite balance on duplex, and post-weld heat treatment decisions stay with the fabricator and the PED joint calculations. SHH STEEL’s scope on this page is the mill tube — chemistry, solution anneal, mechanical floors, leak-tightness, and options named on the purchase order.

Surface Finishes

Surface finish on EN 10216-5 1.4912 is carried by the delivery-condition symbol: descaled HFD/CFD for general pressure tube, bright-annealed CFA for cleaner OD/ID appearance, and ground CFG or polished CFP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the tubes (Clause 13) — free iron staining is a stainless-specific packing rule.

Interior Ra limits, electropolish, or special protection fall under Option 25 or explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4912 when the mill can measure and report the finish; we do not claim an unverified grit or Ra grade.

Inspection and Testing

Specific inspection applies to every EN 10216-5 1.4912 tube. Cast analysis is one per cast. Room-temperature tensile testing is one per test unit in TC1 and two per test unit from different tubes in TC2 (2021 frequency). Technological tests (flattening, ring expanding, drift expanding, or ring tensile per the D/T matrix) follow Table 16. Every tube takes a leak-tightness test — hydrostatic, eddy current, or ultrasonic by agreement — plus dimensional and visual checks and material identification.

TC2 adds mandatory ultrasonic testing for longitudinal imperfections when D > 101.6 mm or T > 5.6 mm; below both thresholds, longitudinal NDT is Option 14. Transverse NDT is Option 15; laminar end NDT for thick wall is Option 16. IGC is Option 12; impact verification is Options 6/11. SHH STEEL EN 10204 3.1 documents report cast chemistry, heat-treatment condition, ambient tensile results, and the leak-tightness / NDT statement ordered. We do not drop mandatory tests to shorten lead time.

Packaging and Shipping

1.4912 tube ships with end protection, size-sorted bundles or crates, and waterproof wrap for ocean freight. Bright-annealed and polished OD get sleeve protection against transit galling. Packaging must keep carbon-steel strapping off the stainless surface.

Marking typically includes manufacturer identity, dimensions, EN 10216-5, steel name or number 1.4912, cast/code, test category, inspection mark, and correlation number; delivery-condition symbols may appear at the manufacturer’s discretion. SHH STEEL aligns stencil and tags with the purchase-order marking clause and Option 24 extras before dispatch.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10216-5 1.4912 as seamless pressure tube — solution annealed, tested to the ordered TC1/TC2 regime, and documented on EN 10204 3.1 certificates — not as a generic “347H-type creep tube” label on whatever is in the rack. We keep Part 5 distinct from EN 10217 welded product and from ASTM A269/A213/A312 on the inspection document, and we will not paste creep or tensile figures from the wrong table onto a 1.4912 shipment.

Grade advice stays practical. If the duty needs a sister chemistry, we point to EN 10216-5 1.4550, EN 10216-5 1.4948, EN 10216-5 1.4940 or to live A213 TP347H and A269 TP347. Winning the order with the wrong steel number is not a win for the PED file or for us.

Supply Capability

SHH STEEL can produce and make EN 10216-5 1.4912 seamless stainless steel tube against the edition, test category, delivery condition, and options named on your enquiry. The capability table and Stock / Available sizes enquiry map below are what buyers use to frame a first-pass size list for pressure duty.

Item SHH STEEL capability for 1.4912
Standard EN 10216-5
Grade 1.4912 / X7CrNiNb18-10
Product form Seamless tube (hot-finished or cold-finished), solution annealed
Delivery condition HFD / CFD / CFA / CFG / CFP (Option 2 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within 50 mm family ceiling; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; NDT per options / thresholds
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range for EN 10216-5 1.4912 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats and finishing slots; send the OD × wall list, TC1/TC2 preference, and delivery-condition symbol for confirmation.

OD (mm) Typical walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument / hydraulic; often CFA + Option 20
16 / 19 / 21.3 / 25 / 26.9 / 33.7 1.0 / 1.5 / 2.0 / 2.5 / 3.0 Process and utility pressure tube
38 / 42.4 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 2.5 / 3.0 / 4.0 / 5.0 Utility and process; lock HFD vs CFD
88.9 / 114.3 / 141.3 / 168.3 / 219.1 2.0 / 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger pressure tube; watch 50 mm family ceiling

Cut lengths (Option 18), bevelled ends (Option 17), IGC (Option 12), and dual enquiries against sister numbers on the same size list are routine. Peer mill catalogues were used only to sanity-check typical OD × wall bands — acceptance remains EN 10216-5 + EN ISO 1127 classes.

FAQ

What is EN 10216-5 1.4912 seamless stainless steel tube used for?
EN 10216-5 1.4912 (X7CrNiNb18-10) is seamless pressure tube for PED-oriented duties that need the austenitic creep-resisting family chemistry story. Typical service is boiler and process tubing in the creep range needing Nb carbides. Put EN 10216-5, the steel number, and TC1/TC2 on the purchase order so chemistry, solution anneal, and tests match Part 5 — not a welded EN 10217 or ASTM tubing habit.
Is EN 10216-5 1.4912 the same as 347H-type creep under ASTM A269 or A213?
No. Commercial alias 347H-type creep may point at a similar chemistry idea, but EN 10216-5 is a European seamless pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing (seamless or welded); A213 is seamless boiler/HX tube. Order the standard that matches the drawing; see also A213 TP347H and A269 TP347.
Does EN 10216-5 1.4912 include welded tube?
No. EN 10216-5 covers seamless tubes only. If the line specification requires a weld seam, the correct European series is EN 10217 for welded pressure tubes. Site titles for this series always say Seamless Tube; the body does not pretend Part 5 can supply welded product.
What mechanical properties does EN 10216-5 require for 1.4912?
In the solution-annealed condition, public 2021 ambient tables list Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm 510–710 MPa, and elongation 40% longitudinal / 30% transverse for walls within the 50 mm band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4912 vs sister grades — which EN 10216-5 number should I buy?
Buy 1.4912 when the enquiry names this steel number or the duty matches Nb-stabilised creep-resisting austenitic for elevated-temperature pressure duty. Compare EN 10216-5 1.4550, EN 10216-5 1.4948, EN 10216-5 1.4940 when carbon, Mo, stabilisation, duplex strength, or creep characterisation points elsewhere. Design caution for this grade: do not treat as a drop-in for corrosion-grade 1.4550 without checking IGC and creep tables.
What delivery conditions are available for EN 10216-5 1.4912?
Tubes are always solution annealed. Surface/delivery symbols are HFD, CFD, CFA, CFG, and CFP. Unless Option 2 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common HFD/CFD routes and bright or polished finishes when the order locks Option 2 and any roughness scope.
What size range can SHH STEEL supply for EN 10216-5 1.4912?
SHH STEEL can produce and supply EN 10216-5 1.4912 in a typical band of about 6–219 mm OD × 0.5–12.7 mm wall within the family’s 50 mm characterisation ceiling, with EN 10204 3.1 documents. Larger or heavier sizes need agreement (Options 7/8 above band) — send the OD × wall list for a firm availability answer.
TC1 or TC2 for EN 10216-5 1.4912?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling, raises technological-test frequency, and adds mandatory ultrasonic longitudinal NDT above D 101.6 mm or T 5.6 mm. Small-bore TC2 still needs Option 14 if you want that NDT below both thresholds. Choose TC2 when the PED file or purchaser specification demands the heavier regime.
Is the intergranular corrosion test mandatory for 1.4912?
No. IGC testing to EN ISO 3651-2 is Option 12. Tables assign method A/B/C and mark resistance in the delivery condition for corrosion-resisting and duplex grades, but the test appears on the certificate only when ordered. Creep-table grades are marked No for IGC in delivery condition — do not expect Option 12 to turn them into Table 2 corrosion grades.
What documents come with SHH STEEL EN 10216-5 1.4912?
EN 10204 3.1 inspection documents report cast chemistry, solution-treatment condition, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10216-5, 1.4912, size, cast, and test category.
How do I enquire for EN 10216-5 1.4912 with SHH STEEL?
Send EN 10216-5, steel number 1.4912 / X7CrNiNb18-10, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 2), and any Options (12 IGC, 14/15 NDT, 18 exact length, 20 D4/T4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10216-5 1.4912 / X7CrNiNb18-10 is the seamless pressure-tube designation for this austenitic creep-resisting family chemistry under the European Part 5 standard. SHH STEEL can produce and supply solution-annealed seamless 1.4912 tube, tested to the ordered test category, and documented on EN 10204 3.1 certificates. For sister grades and size discussions, start from the EN 10216-5 hub, then send your OD × wall list, TC1/TC2 preference, and medium notes. Contact admin@steelspecs.com with the size list and options for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X