Product Showcase
CCS Steel Plates Carbon Steel Plates
SHH STEEL offers CCS Rules-compliant CCS AH32/DH32/EH36 steel plates. China Classification Society Rules for Sea-going Steel Ships detail materials and welding for international voyages and hull integrity. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
CCS Grade E Shipbuilding Steel Plate
CCS Grade E (CCS E) normal-strength hull structural steel plate, yield 235 N/mm² min., Charpy at −40 °C where required, stamped CCS Grade E / CCS E with China Classification Society–endorsed certificates. SHH STEEL supplies CCS Grade E / CCS E shipbuilding plate from stock in China, with cutting, multi-class certification and third-party inspection.View More -
CCS Grade D Shipbuilding Steel Plate
CCS Grade D (CCS D) normal-strength hull structural steel plate, yield 235 N/mm² min., Charpy at −20 °C where required, stamped CCS Grade D / CCS D with China Classification Society–endorsed certificates. SHH STEEL supplies CCS Grade D / CCS D shipbuilding plate from stock in China, with cutting, multi-class certification and third-party inspection.View More -
CCS Grade B Shipbuilding Steel Plate
CCS Grade B (CCS B) normal-strength hull structural steel plate, yield 235 N/mm² min., Charpy at 0 °C where required, stamped CCS Grade B / CCS B with China Classification Society–endorsed certificates. SHH STEEL supplies CCS Grade B / CCS B shipbuilding plate from stock in China, with cutting, multi-class certification and third-party inspection.View More -
CCS Grade A Shipbuilding Steel Plate
CCS Grade A (CCS A) normal-strength hull structural steel plate, yield 235 N/mm² min., Charpy at +20 °C where required, stamped CCS Grade A / CCS A with China Classification Society–endorsed certificates. SHH STEEL supplies CCS Grade A / CCS A shipbuilding plate from stock in China, with cutting, multi-class certification and third-party inspection.View More
CCS Steel Plates Carbon Steel Plates
Shipbuilding Steel Plates
SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.
Shipbuilding Steel Plates