CCS AH550 Shipbuilding Steel Plate
CCS AH550 / CCS AH550 shipbuilding steel plate — overview
China Classification Society titles extra-high-strength plate at 0 °C as CCS AH550 (CCS AH550) — W16 form with H (AH420, not A420). IACS Unified Requirement W16 covers this strength band (yield 550 N/mm²); CCS implements corresponding requirements in CCS Rules for Materials. Minimum yield is 550 N/mm², tensile 670–835 N/mm², elongation 16 % min., with Charpy at 0 °C. It sits above the A/AH–F/FH 40 higher-strength family (max yield 390 N/mm² under UR W11). GB 712 lists Grade AH550 in the same EHS band as a Chinese product standard; CCS class work still needs the CCS AH550 stamp. Commercial enquiries use CCS AH550 or CCS AH550 shipbuilding steel plate.
Equivalent grades: CCS AH550 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS AH55 / AQ56 ≈ DNV NV A550 ≈ LR AH55 ≈ BV A550 ≈ NK KA550 ≈ KR RA56 ≈ RINA A550 ≈ GB 712 Grade AH550 (all class-approved, stamped by the issuing society).
Naming note: China Classification Society titles this strength band as AH550 / CCS AH550 (with H — write AH420, not A420 or AH42). Bureau Veritas titles the same yield as A550 (no H). DNV often titles AH550 / DNV NV A550. LR titles AH55. ABS often titles AH55 (official ABS AQ56). ASTM A131 has no grade at this strength. Write CCS AH550 on the CCS purchase order.
CCS AH550 is almost always produced TM or QT by a CCS-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with China Classification Society approval for the grade, under Surveyor attendance, with optional multi-class (ABS/DNV/LR/BV) and EN 10204 3.2.
CCS CCS AH550 plate: specification summary
| Item | CCS CCS AH550 / AH550 data |
|---|---|
| Rule basis | CCS Rules for Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for CCS Materials paragraph cross-refs without local CCS PDF) |
| Commercial / stamp | CCS AH550 (CCS AH550) — W16 form with H |
| Related product standard | GB 712 Grade AH550 — listed in GB 712 EHS band; not class approval alone |
| Yield / tensile / elongation | 550 / 670–835 N/mm² / 16 % min. |
| Impact | 0 °C; ≈ 55 J L or 37 J T average (IACS UR W16 / aligned tables — confirm on mill certificate) |
| Deoxidation | fully killed, fine grain; N-binding elements per manufacturing specification |
| Delivery condition | TM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits |
| Marking | CCS AH550 / CCS AH550 (plus delivery-condition / Z / U where ordered) |
| UT | commonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO |
| Thickness tolerance | IACS UR W13 as adopted by CCS (confirm class on PO; see UNCERTAIN) |
| Certificate | mill certificate endorsed by the CCS Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request |
Maximum plate thickness depends on delivery condition and the mill’s CCS approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local CCS Materials PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and CCS survey confirm otherwise.
CCS CCS AH550 chemical composition (heat analysis — full alloy set)
| Element | Heat (ladle) analysis, % | Product (check) analysis, % | Note |
|---|---|---|---|
| C | 0.21 max. (often 0.14–0.20 by route/condition; TM/QT may tighten) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | TM/QT and letter routes may tighten C — UNCERTAIN exact CCS Materials table without local PDF |
| Mn | 1.70 max. (typically 1.00–1.70; QT route may differ) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | as per mill approval / UR W16 envelope |
| Si | 0.55 max. (QT may allow up to ~0.80 — confirm on mill approval) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | |
| P | 0.025 max. (some EQ-style routes tighter — confirm) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | EQ-style routes may be tighter |
| S | 0.025 max. (some EQ-style routes tighter — confirm) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | EQ-style routes may be tighter |
| Al (acid soluble / total) | 0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control unless other N-binders) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | grain refining / N control |
| Nb | 0.05 max. (when used; combined microalloy caps apply) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | when intentionally added |
| V | 0.10 max. (when used; combined caps apply) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | when intentionally added |
| Ti | 0.05 max. (when used; combined caps apply) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | when intentionally added |
| Cu | 0.50 max. (route-dependent; often ≤0.35 in practice) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | |
| Cr | 0.20–0.25 max. (route-dependent) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | |
| Ni | 2.00 max. or per mill approval (often lower on AH/DH routes) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | |
| Mo | 0.08–0.50 (route-dependent; QT may allow higher) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | |
| B | 0.005 max. (when intentionally added) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | report when intentionally added |
| N | 0.015 max. (tighter control when Al is the sole N-binder) | numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate | Al/N practice unless other N-binders |
| Nb+V+Ti (combined) | Nb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approval | not applicable (calculated from heat analysis) | combined microalloy cap |
| Ceq / CET / Pcm | Ceq / CET / Pcm maxima by category and condition on mill approval — report on certificate | not applicable (calculated from heat analysis) | report on certificate; choice agreed mill/purchaser |
Product (check) analysis column: CCS Rules for Materials and Welding specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.
Source: IACS UR W16 chemistry envelope (ABS 2-1-8 Table 4A aligned) as implemented by China Classification Society for CCS AH550 via CCS Rules for Materials — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. GB 712 Grade AH550 lists a related product-standard chemistry band; class work follows the CCS / UR W16 envelope on the mill approval. Values above are the rule envelope with every alloy / microalloy row listed; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local CCS Materials PDF was not available to quote paragraph numbers.
CCS CCS AH550 tensile and impact properties
| Property | Requirement (IACS UR W16 aligned) |
|---|---|
| Yield strength ReH (or Rp0.2) | 550 N/mm² min. |
| Tensile strength Rm | 670–835 N/mm² |
| Elongation (transverse, 5.65√A) | 16 % min. |
| Impact test temperature | 0 °C |
| Impact energy (indicative) | 55 J L or 37 J T average |
Final acceptance values are as per standard and mill certificate under CCS survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.
Delivery condition and toughness for CCS AH550
Charpy temperature is fixed by the grade letter: AH → 0 °C. Indicative average energy 55 / 37 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the CCS-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.
Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for AH550.
Thickness tolerance and surface condition
China Classification Society applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable CCS / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.
CCS CCS AH550 plate — mill-roll supply in China
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. quantity | Location |
|---|---|---|---|---|---|
| 10 | 2000 / 2200 | 8000 / 12000 | TM / QT | 200+ t | China |
| 12 | 2000 / 2200 / 2500 | 12000 | TM / QT | 200+ t | China |
| 14 | 2000 / 2200 | 12000 | TM / QT | 100+ t | China |
| 16 | 2000 / 2500 | 12000 | TM / QT | 200+ t | China |
| 20 | 2000 / 2500 | 12000 | TM / QT | 100+ t | China |
| 25 | 2200 / 2500 | 12000 | TM / QT | 100+ t | China |
| 30 | 2200 | 10000 / 12000 | TM / QT | 100+ t | China |
| 40 | 2200 | 10000 | TM / QT | 50+ t | China |
| 50 | 2200 | 8000 / 10000 | TM / QT | 50+ t | China |
Extra-high grades such as CCS AH550 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as CCS class carry CCS AH550 marking and a China Classification Society–endorsed mill certificate. Typical mill lead time including CCS survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.
Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and CCS stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.
CCS CCS AH550 equivalents in other rules and standards
| Standard / society | Designation | Comment |
|---|---|---|
| CCS (China Classification Society) | CCS AH550 (CCS AH550) | this page; CCS uses AH420…FH690 (with H) |
| GB 712 | GB 712 Grade AH550 | listed in GB 712 EHS band; not class approval alone |
| ASTM A131/A131M | ASTM A131/A131M — no direct Grade AH550 | A131 stops at FH40 |
| ABS | ABS AH55 / AQ56 | commercial AH55 / official AQ56 |
| DNV | DNV NV A550 | DNV titles AH550 for this yield band |
| LR | LR AH55 / LR/AH55 | LR titles AH55 (AH69 not AH70 / AH690) |
| BV | BV A550 | BV titles A550 (no H — A420 not AH420) |
| NK (ClassNK) | NK KA550 | NK KA550 |
| KR | KR RA56 | KR RA56 (KR uses ABS-style category numbers) |
| RINA | RINA (per rules) | EHS name not verified from local RINA PDF |
These are comparisons, not substitutions. Always write the CCS stamp CCS AH550 on the PO, plus any additional society stamps you need. Other CCS EHS siblings are linked via CCS until each product page is live.
CCS CCS AH550 vs higher-strength and other EHS grades
Use AH550 when scantlings need yield 550 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 550 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Neighbouring strengths are 500 / 620 — swapping strength needs class approval of the drawing change.
When CCS CCS AH550 is the right choice: typical uses are extra-high-strength hull girder plating and primary members on CCS-classed ships and offshore units where 0 °C toughness and yield above 390 N/mm² are specified at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 550 N/mm² is specified. See offshore platform steel plates for related offshore grades.
Applications and welding notes for CCS CCS AH550
Typical uses: extra-high-strength hull girder plating and primary members on CCS-classed ships and offshore units where 0 °C toughness and yield above 390 N/mm² are specified at ReH 550 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.
Welding: CCS AH550 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by CCS. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.
Processing notes: CCS AH550 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and CCS. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.
Certificates, CCS survey and third-party inspection
CCS survey at the mill; certificate includes ladle chemistry (full alloy set + Ceq/CET/Pcm as applicable), tensile (ReH ≥ 550, Rm 670–835, A ≥ 16 %), Charpy at 0 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class with ABS/DNV/LR/BV.
On receipt: verify CCS AH550 stamp, 0 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement (not GB 712 alone), UT report if required.
Charpy acceptance for CCS AH550 (IACS UR W16 aligned; actual results as per standard and mill certificate):
| Thickness t (mm) | Test temperature | Average energy, longitudinal (J min.) | Average energy, transverse (J min.) |
|---|---|---|---|
| as per UR W16 / mill approval (typically t/4 position) | 0 °C | 55 | 37 |
For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.
Common mistakes when ordering CCS AH550 / CCS AH550
- Ordering “CCS 550” without the letter (AH) — toughness missing
- Writing A550 / BV A550 style (no H) on a CCS PO — CCS official W16 form is AH550 (with H)
- Writing ABS AH55 or DNV AH550 or LR AH55 or BV A550 on a CCS-class PO without arranging that society’s survey (wrong stamp)
- Leaving delivery condition blank (TM vs QT changes price, mill and properties)
- Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
- Skipping UT on thick EHS plate when the yard specification requires it
- Missing CCS endorsement / assuming GB 712 Grade AH550 alone is class approval
- Omitting alloy / microalloy rows (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N) from the certificate check
Write grade (AH550, with H), TM/QT, impact temperature, UT level and certificate type into the PO.
Sourcing CCS CCS AH550: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Fake class plate | CCS-approved mills only; traceable CCS AH550 stamp + certificate; 3.2 on request |
| Payment risk | T/T or L/C; inspection before balance |
| Mill minimum / long lead time | combine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit |
| Welding / heat-input risk | send ladle Ceq/CET/Pcm before shipment; support WPS review with mill data |
| Prep before ship | cutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT) |
How to order CCS CCS AH550 plate
Specify CCS AH550 (CCS AH550), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.
Sample PO line: “Steel plate to China Classification Society Rules for Materials, Grade AH550 (CCS AH550), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked CCS AH550 / CCS AH550, certificate endorsed by CCS Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”
FAQ
Conclusion
CCS AH550 / CCS AH550 is extra-high-strength hull steel (IACS UR W16 band; CCS W16 naming with H): yield 550 N/mm², tensile 670–835 N/mm², Charpy at 0 °C, marking CCS AH550. GB 712 Grade AH550 lists the same EHS band as a product standard — CCS Surveyor endorsement is still required. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.
SHH STEEL supplies CCS AH550 plate rolled by Chinese mills that hold China Classification Society works approval for the grade, so every plate carries the CCS AH550 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with CCS survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, BV, NK, KR or RINA.
We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or CCS AH550 with neighbouring EHS sizes or higher-strength A/AH–F/FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.