CCS EH460 Shipbuilding Steel Plate

CCS EH460 Shipbuilding Steel Plate

CCS CCS EH460 (EH460) extra-high-strength hull structural steel plate, yield 460 N/mm², tensile 570–720 N/mm², Charpy at −40 °C, stamped CCS EH460 / CCS EH460 with China Classification Society–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
CCS EH460 steel plate, CCS EH460 shipbuilding steel plate, CCS EH460 marine plate, EH460 extra high strength hull steel, China Classification Society EH460 plate, CCS AH420 FH690, GB 712 Grade EH460
Equivalent Grades:
ASTM A131 (no direct); ABS EH46 / EQ47; DNV NV E460; LR EH46 / LR/EH46; BV E460; NK KE460; KR RE47; RINA per rules; GB 712 Grade EH460
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

CCS EH460 / CCS EH460 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

Cold-route extra-high scantlings under CCS call for CCS EH460 (CCS EH460) with −40 °C Charpy — CCS’s W16-style EHS naming keeps H (EH420…EH690). IACS Unified Requirement W16 covers this strength band (yield 460 N/mm²); CCS implements corresponding requirements in CCS Rules for Materials. Minimum yield is 460 N/mm², tensile 570–720 N/mm², elongation 17 % min., with Charpy at −40 °C. It sits above the A/AH–F/FH 40 higher-strength family (max yield 390 N/mm² under UR W11). GB 712 lists Grade EH460 in the same EHS band as a Chinese product standard; CCS class work still needs the CCS EH460 stamp. Commercial enquiries use CCS EH460 or CCS EH460 shipbuilding steel plate.

Equivalent grades: CCS EH460 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS EH46 / EQ47 ≈ DNV NV E460 ≈ LR EH46 ≈ BV E460 ≈ NK KE460 ≈ KR RE47 ≈ RINA E460 ≈ GB 712 Grade EH460 (all class-approved, stamped by the issuing society).

Naming note: China Classification Society titles this strength band as EH460 / CCS EH460 (with H — write AH420, not A420 or AH42). Bureau Veritas titles the same yield as E460 (no H). DNV often titles EH460 / DNV NV E460. LR titles EH46. ABS often titles EH46 (official ABS EQ47). ASTM A131 has no grade at this strength. Write CCS EH460 on the CCS purchase order.

CCS EH460 is almost always produced TM or QT by a CCS-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with China Classification Society approval for the grade, under Surveyor attendance, with optional multi-class (ABS/DNV/LR/BV) and EN 10204 3.2.

CCS CCS EH460 plate: specification summary

ItemCCS CCS EH460 / EH460 data
Rule basisCCS Rules for Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for CCS Materials paragraph cross-refs without local CCS PDF)
Commercial / stampCCS EH460 (CCS EH460) — W16 form with H
Related product standardGB 712 Grade EH460 — listed in GB 712 EHS band; not class approval alone
Yield / tensile / elongation460 / 570–720 N/mm² / 17 % min.
Impact−40 °C; ≈ 46 J L or 31 J T average (IACS UR W16 / aligned tables — confirm on mill certificate)
Deoxidationfully killed, fine grain; N-binding elements per manufacturing specification
Delivery conditionTM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits
MarkingCCS EH460 / CCS EH460 (plus delivery-condition / Z / U where ordered)
UTcommonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO
Thickness toleranceIACS UR W13 as adopted by CCS (confirm class on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the CCS Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request

Maximum plate thickness depends on delivery condition and the mill’s CCS approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local CCS Materials PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and CCS survey confirm otherwise.

CCS CCS EH460 chemical composition (heat analysis — full alloy set)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.21 max. (often 0.14–0.20 by route/condition; TM/QT may tighten)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificateTM/QT and letter routes may tighten C — UNCERTAIN exact CCS Materials table without local PDF
Mn1.70 max. (typically 1.00–1.70; QT route may differ)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificateas per mill approval / UR W16 envelope
Si0.55 max. (QT may allow up to ~0.80 — confirm on mill approval)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate
P0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificateEQ-style routes may be tighter
S0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificateEQ-style routes may be tighter
Al (acid soluble / total)0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control unless other N-binders)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificategrain refining / N control
Nb0.05 max. (when used; combined microalloy caps apply)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificatewhen intentionally added
V0.10 max. (when used; combined caps apply)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificatewhen intentionally added
Ti0.05 max. (when used; combined caps apply)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificatewhen intentionally added
Cu0.50 max. (route-dependent; often ≤0.35 in practice)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate
Cr0.20–0.25 max. (route-dependent)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate
Ni2.00 max. or per mill approval (often lower on AH/DH routes)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate
Mo0.08–0.50 (route-dependent; QT may allow higher)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificate
B0.005 max. (when intentionally added)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificatereport when intentionally added
N0.015 max. (tighter control when Al is the sole N-binder)numeric tolerance not tabulated in CCS Rules for Materials and Welding – agree on order / mill certificateAl/N practice unless other N-binders
Nb+V+Ti (combined)Nb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approvalnot applicable (calculated from heat analysis)combined microalloy cap
Ceq / CET / PcmCeq / CET / Pcm maxima by category and condition on mill approval — report on certificatenot applicable (calculated from heat analysis)report on certificate; choice agreed mill/purchaser

Product (check) analysis column: CCS Rules for Materials and Welding specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W16 chemistry envelope (ABS 2-1-8 Table 4A aligned) as implemented by China Classification Society for CCS EH460 via CCS Rules for Materials — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. GB 712 Grade EH460 lists a related product-standard chemistry band; class work follows the CCS / UR W16 envelope on the mill approval. Values above are the rule envelope with every alloy / microalloy row listed; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local CCS Materials PDF was not available to quote paragraph numbers.

CCS CCS EH460 tensile and impact properties

PropertyRequirement (IACS UR W16 aligned)
Yield strength ReH (or Rp0.2)460 N/mm² min.
Tensile strength Rm570–720 N/mm²
Elongation (transverse, 5.65√A)17 % min.
Impact test temperature−40 °C
Impact energy (indicative)46 J L or 31 J T average

Final acceptance values are as per standard and mill certificate under CCS survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.

Delivery condition and toughness for CCS EH460

Charpy temperature is fixed by the grade letter: EH → −40 °C. Indicative average energy 46 / 31 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the CCS-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.

Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for EH460.

Thickness tolerance and surface condition

China Classification Society applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable CCS / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.

CCS CCS EH460 plate — mill-roll supply in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
102000 / 22008000 / 12000TM / QT200+ tChina
122000 / 2200 / 250012000TM / QT200+ tChina
142000 / 220012000TM / QT100+ tChina
162000 / 250012000TM / QT200+ tChina
202000 / 250012000TM / QT100+ tChina
252200 / 250012000TM / QT100+ tChina
30220010000 / 12000TM / QT100+ tChina
40220010000TM / QT50+ tChina
5022008000 / 10000TM / QT50+ tChina

Extra-high grades such as CCS EH460 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as CCS class carry CCS EH460 marking and a China Classification Society–endorsed mill certificate. Typical mill lead time including CCS survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and CCS stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

CCS CCS EH460 equivalents in other rules and standards

Standard / societyDesignationComment
CCS (China Classification Society)CCS EH460 (CCS EH460)this page; CCS uses AH420…FH690 (with H)
GB 712GB 712 Grade EH460listed in GB 712 EHS band; not class approval alone
ASTM A131/A131MASTM A131/A131M — no direct Grade EH460A131 stops at FH40
ABSABS EH46 / EQ47commercial EH46 / official EQ47
DNVDNV NV E460DNV titles EH460 for this yield band
LRLR EH46 / LR/EH46LR titles EH46 (AH69 not AH70 / AH690)
BVBV E460BV titles E460 (no H — A420 not AH420)
NK (ClassNK)NK KE460NK KE460
KRKR RE47KR RE47 (KR uses ABS-style category numbers)
RINARINA (per rules)EHS name not verified from local RINA PDF

These are comparisons, not substitutions. Always write the CCS stamp CCS EH460 on the PO, plus any additional society stamps you need. Other CCS EHS siblings are linked via CCS until each product page is live.

CCS CCS EH460 vs higher-strength and other EHS grades

Use EH460 when scantlings need yield 460 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 460 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Neighbouring strengths are 420 / 500 — swapping strength needs class approval of the drawing change.

When CCS CCS EH460 is the right choice: typical uses are extra-high-strength special/primary category members and cold-route structure needing −40 °C toughness at elevated yield at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 460 N/mm² is specified. See offshore platform steel plates for related offshore grades.

Applications and welding notes for CCS CCS EH460

Typical uses: extra-high-strength special/primary category members and cold-route structure needing −40 °C toughness at elevated yield at ReH 460 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.

Welding: CCS EH460 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by CCS. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.

Processing notes: CCS EH460 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and CCS. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.

Certificates, CCS survey and third-party inspection

CCS survey at the mill; certificate includes ladle chemistry (full alloy set + Ceq/CET/Pcm as applicable), tensile (ReH ≥ 460, Rm 570–720, A ≥ 17 %), Charpy at −40 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class with ABS/DNV/LR/BV.

On receipt: verify CCS EH460 stamp, −40 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement (not GB 712 alone), UT report if required.

Charpy acceptance for CCS EH460 (IACS UR W16 aligned; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
as per UR W16 / mill approval (typically t/4 position)−40 °C4631

For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes when ordering CCS EH460 / CCS EH460

  • Ordering “CCS 460” without the letter (EH) — toughness missing
  • Writing A460 / BV E460 style (no H) on a CCS PO — CCS official W16 form is EH460 (with H)
  • Writing ABS EH46 or DNV EH460 or LR EH46 or BV E460 on a CCS-class PO without arranging that society’s survey (wrong stamp)
  • Leaving delivery condition blank (TM vs QT changes price, mill and properties)
  • Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
  • Skipping UT on thick EHS plate when the yard specification requires it
  • Missing CCS endorsement / assuming GB 712 Grade EH460 alone is class approval
  • Omitting alloy / microalloy rows (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N) from the certificate check

Write grade (EH460, with H), TM/QT, impact temperature, UT level and certificate type into the PO.

Sourcing CCS CCS EH460: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateCCS-approved mills only; traceable CCS EH460 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mill minimum / long lead timecombine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit
Welding / heat-input risksend ladle Ceq/CET/Pcm before shipment; support WPS review with mill data
Prep before shipcutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT)

How to order CCS CCS EH460 plate

Specify CCS EH460 (CCS EH460), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to China Classification Society Rules for Materials, Grade EH460 (CCS EH460), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked CCS EH460 / CCS EH460, certificate endorsed by CCS Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for CCS EH460 / CCS EH460 plate?
CCS EH460 is ordered as China Classification Society extra-high-strength grade EH460 (IACS UR W16 strength band; CCS W16 naming with H). The plate is fully killed, and the maximum thickness depends on the delivery condition (TM or QT) and the mill’s CCS approval. In practice CCS EH460 is nearly always produced by an approved mill to order rather than taken from stock, so a mill minimum per heat or rolling usually applies. Send thickness × width × length × quantity per size and we will say whether the order fits a scheduled rolling or needs its own heat. Small balance quantities can sometimes ride on another EH460 order.
How is CCS CCS EH460 certified, and can you arrange EN 10204 3.2 or dual-class with ABS/DNV/LR/BV?
Every plate is made by a CCS-approved mill under China Classification Society survey. It is die-stamped or stencilled CCS EH460 / CCS EH460 with the heat or plate number, and the mill test certificate is endorsed by the CCS Surveyor. The certificate gives ladle chemistry (full alloy set including Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N where applicable), Ceq/CET/Pcm as applicable, tensile (ReH ≥ 460 N/mm², Rm 570–720 N/mm², A ≥ 17 %), Charpy at −40 °C, delivery condition, UT if ordered, and plate identity. A GB 712 Grade EH460 certificate alone is not CCS class approval. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (e.g. CCS + ABS, DNV, LR or BV) must be booked before testing. 3.2 cannot be added afterwards.
What is the impact test temperature and energy for CCS EH460 / CCS EH460, and do thickness limits apply?
CCS EH460 is tested at −40 °C with an indicative average of at least 46 J longitudinal or 31 J transverse (IACS UR W16 aligned tables). Impact specimens typically come from the quarter-thickness position (t/4). For thicker plates, CCS / UR W16 may require additional positions. Rule maximum thickness depends on whether the plate is TM or QT and on mill approval, so give the delivery condition as well as the thickness, and we will check the approved mill’s range before quoting. Final values are as per standard and mill certificate (see UNCERTAIN).
What welding and preheat guidance applies to CCS CCS EH460?
CCS EH460 is an extra-high-strength steel (yield ≥ 460 N/mm²) supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by CCS. Ceq is calculated from the ladle analysis and limited by the approval chemistry; the mill may also report CET or Pcm for low-carbon TM/QT steel. Hydrogen control, preheat, interpass temperature and heat-input windows come from the approved WPS and the mill’s recommendations. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits.
What is the delivery time for CCS CCS EH460 plate?
CCS EH460 is normally rolled to order. Typical commercial lead time is about 6–10 weeks from confirmed PO and deposit, depending on the mill rolling schedule, QT capacity, UT and any 3.2 witness. Ocean transit comes on top of that. This is a commercial estimate, not a rule value, and we confirm it with each quotation. Every week, your coordinator sends the rolling, heat-treatment, testing and stamping status with photos. Delays are reported as soon as the mill tells us, not at the shipping date.
Which payment terms do you accept for CCS EH460, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the CCS EH460 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (CCS EH460 / CCS EH460), TM/QT, sizes and certificate type.
Why does CCS write EH460 (with H) while BV uses E460 (no H), and what are the equivalents?
China Classification Society lists CCS EH460 for commercial EH460 (W16 form with H — AH420 not A420). ASTM A131/A131M stops at FH40, so it has no direct equivalent. ABS EH46 / EQ47 is the usual ABS counterpart. DNV NV E460 is the DNV counterpart (DNV titles EH460). LR EH46 / LR/EH46 is the LR counterpart (LR titles EH46). BV E460 is the BV counterpart (BV titles E460 without H). NK KE460 and KR RE47 are the NK/KR counterparts. RINA EHS names are written “per rules” until verified. GB 712 Grade EH460 is listed in the GB 712 EHS band but is not class approval by itself. Always write CCS EH460 on the PO, plus any additional society stamps you need.
Can you cut, bevel or machine CCS CCS EH460 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut EH460 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the CCS EH460 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For QT extra-high-strength plate, thermal cutting parameters follow the mill’s recommendations so the cut edge is not damaged. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. See SHH STEEL for our processing capabilities.

Conclusion

CCS EH460 / CCS EH460 is extra-high-strength hull steel (IACS UR W16 band; CCS W16 naming with H): yield 460 N/mm², tensile 570–720 N/mm², Charpy at −40 °C, marking CCS EH460. GB 712 Grade EH460 lists the same EHS band as a product standard — CCS Surveyor endorsement is still required. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.

SHH STEEL supplies CCS EH460 plate rolled by Chinese mills that hold China Classification Society works approval for the grade, so every plate carries the CCS EH460 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with CCS survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, BV, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or CCS EH460 with neighbouring EHS sizes or higher-strength A/AH–F/FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (CCS EH460 / CCS EH460), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X