What is ABS Grade A shipbuilding steel plate?
Equivalent grades: ABS A ≈ ASTM A131 Grade A ≈ DNV NV A ≈ LR Grade A ≈ BV Grade A ≈ CCS Grade A ≈ NK KA ≈ KR RA ≈ RINA Grade A ≈ GB 712 Grade A (all class-approved, stamped by the issuing society).
ABS Grade A is the base grade of ordinary-strength hull structural steel in the ABS Rules for Materials and Welding, Part 2, Chapter 1, Section 2 (2-1-2). It has a minimum yield point of 235 N/mm², a tensile strength of 400–520 N/mm² and 22 % minimum elongation, and it is the only one of the four ordinary-strength grades (A, B, D, E) for which the Rules ask for no Charpy test on plates up to 50 mm thick. Plates that pass the mill tests under ABS survey are die-stamped or stencilled AB/A and are supplied with a certificate the ABS Surveyor endorses.
Because it carries no low-temperature toughness requirement at ordinary thicknesses, Grade A is used where the hull structure is lightly stressed or remains above freezing in service: inner bottom and internal structure of small and medium vessels, superstructures, deckhouses, non-critical bulkheads, inland barges, pontoons and many shipyard fittings. Where the classification drawing calls for Grade B, D or E in a strake, Grade A cannot be substituted; the reverse substitution (B, D or E supplied for A) is normally accepted because the higher grades meet every Grade A requirement.
SHH STEEL supplies ABS Grade A plate from Chinese mills that hold ABS works approval for the grade, from stock in common sizes or from a mill rolling cycle, with ABS survey arranged at the mill.
ABS A plate: specification summary
| Item | ABS Grade A data |
|---|---|
| Rule | ABS Rules for Materials and Welding, Part 2, 2-1-2 Ordinary-strength Hull Structural Steel (2023 edition checked) |
| Strength level | ordinary strength, yield point 235 N/mm² min. |
| Plate thickness covered | up to and including 150 mm |
| Steelmaking | basic oxygen, electric furnace or other approved process; continuous-cast slab reduced at least 3:1 to plate unless specially approved |
| Deoxidation | killed or semi-killed up to 50 mm; killed over 50 mm (rimmed steel only for sections up to 12.5 mm) |
| Condition of supply | any condition up to 50 mm; over 50 mm see the impact-test section below |
| Impact test | none for t ≤ 50 mm; required at +20 °C for t > 50 mm unless normalized or TM |
| Marking | AB/A (plus Z or U where through-thickness or ultrasonic requirements are met) |
| Thickness tolerance | minus 0.3 mm regardless of thickness (2-1-1/15.3); plus tolerance per ASTM A6 or as agreed |
| Certificate | mill certificate endorsed by the ABS Surveyor; EN 10204 3.1 / 3.2 on request |
Size range. Grade A is rolled on wide plate mills in China from about 5 mm to 100 mm and more, widths 1500–3500 mm and lengths up to about 18 m depending on mill; 6–25 mm plate in 1800–2500 mm width is the bulk of the market. Plates under 6 mm are usually cut from ABS-approved hot-rolled coil, which needs separate approval of the coil process (2-1-2/3.1). Ask for confirmation for plates over 100 mm or wider than 3200 mm.
ABS Grade A chemical composition (heat and product analysis)
| Element | Heat (ladle) analysis, % | Product (check) analysis, % | Note |
|---|---|---|---|
| C | 0.21 max. | 0.25 max. (0.21 + 0.04) | 0.23 max. is allowed for Grade A sections, not plates |
| Mn | 2.5 × C min. | 2.5 × C min. (ratio requirement – no tolerance row applies) | e.g. a heat with C 0.16 % needs Mn ≥ 0.40 % |
| Si | 0.50 max. | 0.56 max. (0.50 + 0.06) | |
| P | 0.035 max. | 0.045 max. (0.035 + 0.010) | |
| S | 0.035 max. | 0.045 max. (0.035 + 0.010) | 0.020 max. (heat) for cold-flanging quality |
| Cu | to be determined and reported | no numeric heat limit – report actual value | residual / intentionally added — report when present (may be reported as ≤ 0.02 % when below 0.02 %) |
| Cr | to be determined and reported | no numeric heat limit – report actual value | residual / intentionally added — report when present (may be reported as ≤ 0.02 % when below 0.02 %) |
| Ni | to be determined and reported | no numeric heat limit – report actual value | residual / intentionally added — report when present (may be reported as ≤ 0.02 % when below 0.02 %) |
| Mo | to be determined and reported | no numeric heat limit – report actual value | residual / intentionally added — report when present (may be reported as ≤ 0.02 % when below 0.02 %) |
| C + Mn/6 | 0.40 max. | not applicable (calculated from heat analysis) | carbon-equivalent cap |
Product (check) analysis column = heat (ladle) limit adjusted by ASTM A6/A6M-19 Table A “Permitted Variations in Product Analysis”, as required by ABS Rules Part 2, 2-1-2/5.3 (maximum + “over”, minimum − “under”; row chosen by the specified upper limit); arithmetic shown in brackets.
Source: ABS Rules 2-1-2/5.1 and 15.9 Table 1. The heat (ladle) analysis is determined by the mill on each heat and must meet Table 1. Product (check) analysis on the finished plate is not routine; when it is required by the purchaser or Surveyor, ABS 2-1-2/5.3 applies the chemical tolerances of ASTM A6 (or another nationally recognized standard) to the Table 1 limits. Ask for product analysis at enquiry if you need it on the certificate.
Intentionally added elements must also be reported. Grade A is the only ordinary-strength grade with a manganese minimum written as a ratio of carbon (2.5 × C) instead of a fixed value: Grade B needs 0.80 % Mn, D 0.60 % and E 0.70 %. Grade A also has the widest silicon allowance (0.50 %), which is why semi-killed Grade A is still legitimate under the Rules up to 50 mm. In practice, Chinese mills supply aluminium-killed Grade A with typical C around 0.14–0.18 % and Mn 0.5–1.0 %; check the actual figures on the mill certificate, not a typical sheet.
ABS Grade A tensile properties
| Property | Requirement |
|---|---|
| Tensile strength | 400–520 N/mm² (41–53 kgf/mm², 58–75 ksi) |
| Yield point | 235 N/mm² min. (24 kgf/mm², 34 ksi) |
| Elongation | 22 % min. (alternative A flat or C round specimen; also 22 % on 50 mm gauge for ASTM A370 specimens) |
| Cold-flanging quality (if ordered) | 380–450 N/mm², yield 205 N/mm² min., marked F |
Source: 2-1-2/15.9 Table 2. On the 200 mm gauge alternative B flat specimen, minimum elongation depends on thickness (Table 3):
| Thickness (mm) | ≤5 | 5–10 | 10–15 | 15–20 | 20–25 | 25–30 | 30–40 | 40–50 |
|---|---|---|---|---|---|---|---|---|
| Elongation min. % | 14 | 16 | 17 | 18 | 19 | 20 | 21 | 22 |
Tensile tests are taken on two different plates from each heat (one test if the heat is under 50 t), and from both the thickest and thinnest plate when thicknesses in the heat differ by 9.5 mm or more. One frequent certificate error is quoting a 550 N/mm² upper limit: that relaxed limit applies only to Grade A sections, not to plate.
When does ABS Grade A plate need a Charpy test?
| Plate thickness | Deoxidation | Condition of supply | Charpy V at +20 °C |
|---|---|---|---|
| ≤ 12.5 mm | killed or semi-killed | any | not required |
| 12.5–50 mm | killed or semi-killed | any | not required |
| 50–150 mm | killed | normalized (N) or TM | not required |
| 50–150 mm | killed | control rolled (CR) or as rolled (AR) | one set per 50 t lot |
Required average energy at +20 °C where a test applies (2-1-2/15.9 Table 4, full-size specimens, either direction acceptable):
| Thickness | Longitudinal | Transverse |
|---|---|---|
| 50–70 mm | 34 J | 24 J |
| 70–100 mm | 41 J | 27 J |
| 100–150 mm | 48 J | 32 J |
One individual value may fall below the average if it is at least 70 % of it. Sub-size specimens use 5E/6, 2E/3 or E/2. Note 3 of Table 4 removes the test altogether when heavy Grade A is fine-grain treated and normalized. For buyers this means: if you order 60 mm or 80 mm ABS A for foundations or heavy brackets, ask whether the mill will deliver N/TM (no impact) or AR/CR (impact tested); both are legitimate but the certificate must match the route. If your design or a flag-state rule calls for a 0 °C or −20 °C test on Grade A, order Grade B or D instead of adding a special test.
Thickness tolerance and surface condition
ABS applies a fixed minus tolerance of 0.3 mm on nominal thickness for hull plates regardless of thickness (2-1-1/15.3.2), much tighter than the general ASTM A6 under-tolerance. The mill demonstrates compliance by measuring each plate at defined points; Class C of ISO 7452 may be used instead with ABS agreement. Plus tolerance, flatness, width and length follow ASTM A6 or another recognised standard unless the purchaser specifies otherwise. For plates under 5 mm (cut from coil), tolerances follow a national standard but the minus tolerance still may not exceed 0.3 mm.
Surface defects may be ground out within the limits of 2-1-1/3; grinding areas are excluded from the thickness tolerance. If you plan to shot-blast and prime at the yard, state any surface class (for example ISO 8501-1 rust grade A or B on receipt) in the order.
ABS Grade A plate stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. quantity | Location |
|---|---|---|---|---|---|
| 6 | 1800 / 2000 | 6000 / 8000 | AR / CR | 100+ t | China |
| 8 | 1800 / 2000 | 8000 / 12000 | AR / CR | 200+ t | China |
| 10 | 2000 / 2200 | 8000 / 12000 | AR / CR | 200+ t | China |
| 12 | 2000 / 2200 / 2500 | 12000 | AR / CR | 200+ t | China |
| 14 | 2000 / 2200 | 12000 | AR / CR | 100+ t | China |
| 16 | 2000 / 2500 | 12000 | AR / CR | 200+ t | China |
| 20 | 2000 / 2500 | 12000 | AR / CR | 100+ t | China |
| 25 | 2200 / 2500 | 12000 | AR / CR | 100+ t | China |
| 30 | 2200 | 10000 / 12000 | AR / CR | 100+ t | China |
| 40 | 2200 | 10000 | AR / CR | 50+ t | China |
| 50 | 2200 | 8000 / 10000 | AR / CR | 50+ t | China |
Quantities are approximate and change daily; all stock plates carry AB/A marking and ABS-endorsed mill certificates. Sizes outside the table (for example 3000 mm width, 60–100 mm thickness, or fixed lengths for a cutting plan) are produced in the next mill rolling cycle, typically 3–6 weeks including ABS survey. Send your size list and we will reply with what is in stock and what must be rolled.
Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and ABS stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.
ABS A equivalents in other rules and standards
| Standard / society | Designation | Comment |
|---|---|---|
| ASTM A131/A131M | ASTM A131/A131M Grade A | same base chemistry and tensile values; A131 is a product standard, not class approval |
| DNV, LR, BV, CCS, NK, KR, RINA | Grade A | IACS UR W11 unified requirements; each society stamps its own mark. See BV Grade FH36 / BV Grade FH40 for higher-strength BV plate |
| GB 712 | Grade A | Chinese ship steel standard; GB 712 alone is not class approval |
| ASTM A36 | ASTM A36 | similar strength (250 MPa yield) but not a hull steel; no class marking |
| EN 10025-2 | EN 10025-2 S235JR / S235J0 / S235J2 | structural; S235J0 has a 0 °C test, J2 −20 °C |
| JIS G3106 | JIS G3106 SM400A / SM400B | welded-structure steel; SM400B adds a 0 °C test |
These are comparisons, not substitutions. A classed hull needs plate made by a mill approved by the society that classes the vessel and certified to that society. Dual or multi-class certification (for example ABS + DNV, or ABS + CCS) can be arranged at the mill when the heat is surveyed by both societies.
ABS A vs B, D and E, and vs structural steels
All four ordinary-strength grades share the same 235 N/mm² yield and 400–520 N/mm² tensile range; they differ in deoxidation and toughness. Grade B needs Charpy at 0 °C (27 J longitudinal) above 25 mm in most conditions; Grade D is tested at −20 °C and must be fine grain above 25 mm; Grade E is killed fine-grain steel tested at −40 °C, with each plate tested when supplied normalized or TM. The hull steel grade for each strake is set by the classification rules according to structural member category and thickness, so check the approved drawing first. In general, Grade A is used for internal and lightly stressed members, while sheer strakes, bilge strakes, deck stringers and ice-belt plating usually call for B, D, E or higher-strength ABS steel plates.
Compared with land structural steels, Grade A is close in strength to ASTM A36, ASTM A283 Grade C and S275JR class steels but differs in three practical ways: the tighter 0.3 mm minus tolerance, the C + Mn/6 ≤ 0.40 cap, and above all the class survey and stamp. For a barge or pontoon that will be classed, only class-certified plate is accepted; for an unclassed workboat or a dock structure, buyers sometimes choose A36 or S235 for price, and Grade A can also be dual-certified to A131 and ABS for such use.
When ABS A is the right choice: typical uses are non-critical hull plating, internal structure, decks and bulkheads of vessels working in temperate water, barges and pontoons. The Charpy temperature (+20 °C) is fixed by the letter, and the strength by the ordinary-strength level (ReH 235 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing. Swapping to a different letter or strength needs class approval of the drawing change, not just a new purchase order.
Applications, cutting and welding of ABS Grade A
Typical uses: internal hull structure, double-bottom floors and girders, non-watertight and watertight bulkheads in lightly stressed areas, superstructure and deckhouse plating, hatch covers, inland and coastal barges, pontoons, floating docks, fishing vessels and tugs, rudder and skeg internal plates, and ship repair replacement steel. Offshore and port structures also use Grade A for secondary steel; see offshore platform steel plates for primary structure grades.
Cutting: oxy-fuel, plasma and laser cutting all work without preheat in normal thicknesses. Welding: with C + Mn/6 at or below 0.40 %, Grade A is welded with ordinary-strength consumables approved for the grade (for example ABS Grade 1, 2 or 3 consumables depending on required weld-metal toughness); preheat is generally unnecessary below about 25–30 mm except in cold or humid conditions — follow your approved welding procedure. Forming: plates intended for cold flanging should be ordered as flanging quality (marked F) with S 0.020 % max.
Processing notes for ABS A: cold forming and flanging of ordinary-strength plate are routine. The minimum Mn is set so that this grade can be cold-flanged where noted in 2-1-2. Keep the cut edges of plate thicker than 50 mm free of notches, because thick plate of this grade is controlled more tightly for deoxidation (killed or semi-killed ≤50 mm; killed >50 mm).
Certificates, ABS survey and third-party inspection
Every plate is tested and marked at the mill under ABS survey; the mill certificate lists heat number, ladle chemistry including Ni, Cr, Mo and Cu, tensile results, impact results where required, condition of supply and plate numbers, and is endorsed by the attending Surveyor. On request we add EN 10204 3.2 certificates with third-party witness by TÜV, SGS, BV or another agency, ultrasonic testing (U mark) or through-thickness testing (Z mark), and multi-class certification with any of the nine major class societies (ABS, DNV, LR, BV, CCS, NK, KR, RINA and the former GL, now part of DNV).
On receipt, check: AB/A stamp and heat number on each plate match the certificate; the certificate shows ABS endorsement, not just a mill stamp; thickness at several points is not below nominal minus 0.3 mm; for plates over 50 mm, the condition of supply and impact results agree with the table above.
Charpy acceptance for ABS A by thickness (from 2-1-2; actual results as per standard and mill certificate):
| Thickness t (mm) | Test temperature | Average energy, longitudinal (J min.) | Average energy, transverse (J min.) |
|---|---|---|---|
| t ≤ 50 | +20 °C | 27 | 20 |
| 50 < t ≤ 70 | +20 °C | 34 | 24 |
| 70 < t ≤ 100 | +20 °C | 41 | 27 |
| 100 < t ≤ 150 | +20 °C | 48 | 32 |
On receipt, check that the test temperature on the certificate is +20 °C and that the energy matches the band for the delivered thickness, not the thinnest band. Also check that the plate number on the stamp matches the certificate line, and that the ABS Surveyor endorsement is present. If UT was ordered (e.g. EN 10160 or ASTM A578 level), check the UT report as well. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.
Common mistakes when ordering ABS Grade A
- Ordering “ABS A” without specifying that ABS certification is required, then receiving GB 712 or A131 plate without class endorsement.
- Accepting a 550 N/mm² upper tensile limit on plate; that limit is for sections only.
- Ordering heavy plate (> 50 mm) without agreeing N/TM or impact testing, then finding no Charpy results on the certificate.
- Substituting Grade A where the drawing requires B or D in a high-stress or low-temperature strake.
- Plates cut from coil without the mill holding approval for coiled plate.
- Ignoring the 0.3 mm minus tolerance when accepting re-rolled or trader stock.
Each of these is avoided by writing the requirement into the purchase order and checking it on the certificate before the plates are cut.
Sourcing ABS A plate: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Fake or re-stamped class plate | plates from ABS-approved mills only; certificate and stamp traceable to the heat; third-party witness and EN 10204 3.2 on request |
| Unsafe deposit or payment risk | T/T or L/C payment; inspection before balance payment |
| Small quantities across many sizes | mixed thicknesses and grades (A, B, AH36, etc.) combined in one container or shipment |
| Slow delivery | dedicated staff follow each order with weekly production and shipping updates and photos |
| Cutting and preparation | own workshop for cutting to size, bevelling, drilling and machining before shipment |
How to order ABS Grade A plate
State the grade and rule (ABS Grade A, ABS Rules Part 2), whether multi-class certification is needed, thickness, width, length and quantity per size, condition of supply for plates over 50 mm, any Z or U requirement, surface or primer requirements, certificate type (mill certificate with ABS endorsement, EN 10204 3.2 with third-party witness), packing and destination port. Send the list to SHH STEEL for price, available stock and lead time.
Sample PO line: “Steel plate to ABS Rules Part 2 2-1-2, Grade A, delivery condition [AR/CR/N/TM], 20 × 2500 × 12000 mm, 30 pcs, marked AB/A, certificate endorsed by ABS Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].” Each bracketed item changes price, lead time and which mills can supply, so fix them at enquiry stage.
FAQ
-
What sizes and minimum order quantity can you supply for ABS A plate?
- Plates under 2-1-2 cover thicknesses up to and including 150 mm. Common A hull plate runs 6–50 mm thick, 1500–3000 mm wide and 6000–12000 mm long; thinner and wider sizes are mill-roll items. Stock plate has no fixed minimum — one plate can be supplied, cut to size if you like. A mill rolling for a special width or length usually needs a minimum quantity per size, which depends on the mill and the slot, so we confirm it with each quote.
-
How is ABS A certified, and can you arrange EN 10204 3.2 witness inspection?
- Every plate is made by an ABS-approved mill under ABS survey. It is die-stamped or stencilled AB/A with the heat or plate number, and the mill test certificate is endorsed by the ABS Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 235 N/mm², Rm 400–520 N/mm², A ≥ 22 %), the Charpy results at +20 °C, the delivery condition and the plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. The witness can be the ABS Surveyor, a second class society (dual or multi-class stamping, e.g. ABS + DNV or LR), or a third-party inspector such as SGS or BV who witnesses the tests and checks the markings. 3.2 cannot be added after the plates have been tested, so please state it on the enquiry.
-
What is the impact test temperature and energy for ABS A, and do thickness limits apply?
- Up to 50 mm thick, ABS Grade A needs no Charpy test. Above 50 mm, Charpy V-notch tests are run at +20 °C on as-rolled or controlled-rolled plate, with the average energies set by thickness band in 2-1-2. Bands, as longitudinal/transverse J min.: 50–70 mm 34/24; 70–100 mm 41/27; 100–150 mm 48/32. Grade A over 50 mm must also be killed. If your design needs guaranteed toughness on thinner plate, choose Grade B or D. Do not order "Grade A with impact test", which the rule does not define.
-
What welding and preheat guidance applies to ABS A?
- ABS A is a C–Mn hull steel with C 0.21 max. and is generally easy to weld. ABS does not set a preheat value for the plate grade. Preheat, interpass temperature, heat input and consumables come from the shipyard’s ABS-approved welding procedure (WPS/PQR), using consumables approved for the +20 °C toughness level needed. Thick or highly restrained joints may need preheat under the approved procedure. Ask us for the actual ladle analysis on the mill certificate early so your welding engineer can check the carbon equivalent. We do not give fixed preheat numbers for the grade, because the approved procedure always governs.
-
What is the delivery time for ABS A plate?
- Stock sizes of ABS A can usually be cut, inspected and loaded in about 7–15 days. Mill-rolled orders typically take about 3–6 weeks plus inspection, depending on thickness, delivery condition and the mill schedule. These are commercial estimates, confirmed with each quote. If 3.2 witness or multi-class survey is required, we book the inspector when we place the mill order so testing is not delayed. A dedicated coordinator sends weekly progress photos (rolling, marking, testing, packing, loading) until the bill of lading is issued.
-
Which payment terms do you accept for ABS A, and how is my deposit protected?
- We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the AB/A stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance, so the plate is verified before most of the money moves. With L/C, payment is tied to the presented documents (commercial invoice, packing list, B/L, mill certificate, and the 3.2 or class certificate if you require one). For first orders we can start with a smaller trial lot. The proforma invoice shows the grade, sizes and certificate type, so the contract and the delivered plate match.
-
What are the equivalent grades of ABS A among class societies and GB 712?
- ABS A is treated as equivalent to ASTM A131/A131M Grade A, Grade A of DNV / LR / BV / CCS / NK / KR / RINA, and GB 712 Grade A. All follow the IACS unified requirements for ordinary-strength hull steel (ReH ≥ 235 N/mm², Rm 400–520 N/mm²). "Equivalent" does not mean interchangeable on paper, though. Each society accepts only its own stamp and certificate, so ABS-classed construction needs AB/A, not a GB 712 certificate. Where a vessel is dual-classed, we can arrange joint survey so one plate carries both stamps.
-
Can you cut, bevel or machine ABS A plates, and how are they packed for export?
- Yes. In our workshop we can flame, plasma or laser cut A to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the AB/A marking and heat number before cutting, and the cutting list is tied to the mill certificate. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. Loading photos and a packing list come with each shipment. See SHH STEEL for our processing capabilities.
Conclusion
ABS Grade A is the economical base hull steel: 235 N/mm² minimum yield, 400–520 N/mm² tensile, no impact test up to 50 mm and a 0.3 mm minus thickness tolerance. What the Rules leave open has to be fixed in the order: ABS (or multi-class) certification, the supply condition and impact testing for plates over 50 mm, whether product analysis is required, and the certificate type.
SHH STEEL supplies AB/A plate rolled by Chinese mills that hold ABS works approval for the grade, so every plate carries the AB/A stamp and a Surveyor-endorsed certificate traceable to its heat. Common thicknesses are available from stock; other sizes are scheduled into the mill rolling cycle with ABS survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, BV or another agency) and joint certification with DNV, LR, BV, CCS, NK, KR or RINA.
We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or Grade A mixed with B, D or higher-strength grades, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.
Request a quotation: send SHH STEEL the grade (ABS A), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.