ABS FQ43 shipbuilding steel plate at SHH STEEL

ABS FQ43 Shipbuilding Steel Plate Supplier

ABS FH42 Extra High Strength hull plate (ABS rule grade FQ43), yield 420 N/mm², Charpy at −60 °C, stamped AB/FQ43. SHH STEEL supplies mill-approved plate in China with UT, multi-class and 3.2 inspection.
Keywords
ABS FH42 steel plate, ABS FQ43, Extra High Strength hull steel, AB/FQ43, 420 MPa ship plate
Equivalent Grades:
ABS FQ43; society extra-high ~420 MPa class; GB 712 / A131 — verify listing
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ABS FH42 (ABS FQ43) shipbuilding steel plate?

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

Equivalent grades: ABS FH42 / FQ43 ≈ ASTM A131 (no direct grade at this strength) ≈ DNV NV F420 ≈ LR FH42 ≈ BV F420 ≈ CCS FH420 ≈ NK KF420 ≈ KR RF43 ≈ RINA F420 ≈ GB 712 Grade FH420 (all class-approved, stamped by the issuing society).

Naming note: commercial and many yard enquiries use ABS FH42 for the ~420 N/mm² yield band. In ABS Rules Part 2, Section 2-1-8 Extra High Strength Steel, the official designation is FQ43 (category 43 = 420 N/mm² yield; letter FQ sets Charpy temperature). This page uses the title grade FH42 and states the ABS rule grade FQ43 wherever requirements are cited.

FQ43 provides minimum yield 420 N/mm², tensile 530–680 N/mm², elongation 18 % min., and Charpy at −60 °C with average energy 41 J longitudinal or 27 J transverse (2-1-8/5.11 Table 5A). It sits above the AH–FH 40 higher-strength family (2-1-3, max yield 390 N/mm²).

SHH STEEL sources Extra High Strength plate from mills with ABS approval for the grade, under Surveyor attendance. Related: ABS AH40 / ABS FH40 (higher-strength 40 band); live ABS Grade A; BV FH36 / BV FH40.

Category 43 (420 N/mm²) is the first Extra High Strength step above FH40’s 390 N/mm². It is often specified where a modest yield increase avoids a thickness jump on deck or longitudinals.

ABS FH42 / FQ43: specification summary

ItemData
RuleABS Rules Part 2, 2-1-8 Extra High Strength Steel (2018/2022 updates in 2023 edition); plus applicable 2-1-1/2/3
ABS official gradeFQ43
Commercial / title gradeFH42
Yield / tensile / elongation420 / 530–680 N/mm² / 18 % min.
Impact−60 °C; 41 J L or 27 J T average
Deoxidationfully killed, fine grain (≥6 capability); N-binding elements per manufacturing specification
Delivery conditionN, NR/CR, TM (+AcC/+DQ), or QT — within Table 3 thickness limits and mill approval
Vacuum degassingmandatory for category 70 (and 91/98) and for all EHS grades t > 50 mm
MarkingAB/FQ43 (plus delivery-condition marking; “R” suffix for MOU leg/rack/chord)
UT≥15 mm: EN10160 or ASTM A578 or agreed standard (2-1-8/11.1)
Thickness tolerance2-1-1/15 (0.3 mm minus for hull plates unless otherwise agreed)
CertificateABS Surveyor-endorsed; includes Ceq/CET/Pcm as applicable

Maximum plate thickness depends on delivery condition (Table 3): e.g. N/QT up to 250 mm, TM/NR/CR up to 150 mm — actual approval limit is as per standard and mill certificate.

ABS FQ43 chemical composition (heat analysis envelope)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C (depends on route)0.14–0.20 max. by grade/condition (Table 4A)0.17–0.24 max. (each heat max.: 0.14 + 0.03; 0.20 + 0.04)EQ/FQ and TM routes tighter than N/NR/CR AQ/DQ
Mn1.0–1.70 (QT: 1.70 max.)0.89–1.84 (1.0 − 0.11; 1.70 + 0.14)
Si0.60 max. (QT 0.80 max.)0.66 max. (0.60 + 0.06)
P / S0.010–0.030 max. by route0.020–0.040 max. (each heat max. + 0.010, same row for P and S)EQ/FQ and QT tighter; sections may be +0.005
Al total min.0.02 (N/TM) / 0.018 (QT)0.02 (N/TM) / 0.018 (QT) (Al not listed in ASTM A6/A6M Table A – heat limit applies)Al/N ≥ 2:1 unless other N-binders used
Nb / V / Tilimits per Table 4ATable 4A heat max. + 0.01 for each of Nb, V, Ti (ASTM A6/A6M Table A: Nb to 0.10, V to 0.10, Ti to 0.15 incl.)Nb+V+Ti < 0.26 % for N/TM (not QT)
Ni / Cu / Cr / Moper Table 4ATable 4A heat max. + Ni 0.03 (to 1.00), Cu 0.03 (to 1.00), Cr 0.04 (to 0.90), Mo 0.01 (to 0.20) / 0.03 (0.20–0.40) / 0.04 (0.40–1.15) per ASTM A6/A6M Table ANi agreement at qualification for some routes
Ceq / CET / Pcmmaxima in Table 4B by category and conditionnot applicable (calculated from heat analysis)report on certificate; choice agreed mill/purchaser

Product (check) analysis column = heat (ladle) limit adjusted by ASTM A6/A6M-19 Table A “Permitted Variations in Product Analysis”, as required by ABS Rules Part 2, 2-1-2/5.3 (maximum + “over”, minimum − “under”; row chosen by the specified upper limit); arithmetic shown in brackets.

Source: ABS 2-1-8/4 Tables 4A and 4B. Exact ladle limits depend on delivery condition (N/NR/CR vs TM vs QT) and on AQ/DQ vs EQ/FQ. Values above are the rule envelope — the purchase order and mill approval sheet govern. Product analysis tolerances: as per standard and mill certificate (ABS references general sampling; numeric product limits are not tabulated like ASTM A6 offsets in 2-1-2). All intentionally added elements and Ceq (or CET/Pcm) are to be reported.

ABS FQ43 tensile and impact properties

PropertyRequirement (Table 5A)
Yield strength ReH (or Rp0.2)420 N/mm² min.
Tensile strength Rm530–680 N/mm²
Elongation (transverse, 5.65√A)18 % min.
Impact test temperature−60 °C
Impact energy41 J L or 27 J T average

Alternative B specimen elongations: 2-1-8 Table 5B (thickness-dependent). For t > 100 mm, tensile reductions may be considered except MOU leg/rack/chord “R” material (Note 3). Test frequency: each heat-treatment batch of same cast/condition/thickness for plates (2-1-8/5.7).

Delivery condition and toughness for FQ43

Charpy temperature is fixed by the grade letter: FQ → −60 °C. Energy does not increase with thickness in Table 5A the way 2-1-3 Table 4 does — the listed 41 / 27 J applies, with mid-thickness rules for t > 100 mm (at least 2/3 energy or +10 °C test option).

Allowed delivery conditions and max thicknesses are in Table 3 (N, NR/CR, TM, QT). Vacuum degassing is mandatory when t > 50 mm and for category 70. State N / TM / QT on the PO; do not assume AR for Extra High Strength.

Thickness tolerance, UT and surface

Tolerances per 2-1-1/15 unless agreed otherwise (hull plates: 0.3 mm minus). Internal soundness: ultrasonic examination required for thickness ≥ 15 mm (EN10160 / ASTM A578 or agreed). Surface per EN 10163 or equivalent agreed with ABS. Edge discontinuities > 25 mm need investigation (2-1-8/9.1).

ABS FH42 / FQ43 plate availability in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000N / TM / QT100+ tChina
81800 / 20008000 / 12000N / TM / QT200+ tChina
102000 / 22008000 / 12000N / TM / QT200+ tChina
122000 / 2200 / 250012000N / TM / QT200+ tChina
142000 / 220012000N / TM / QT100+ tChina
162000 / 250012000N / TM / QT200+ tChina
202000 / 250012000N / TM / QT100+ tChina
252200 / 250012000N / TM / QT100+ tChina
30220010000 / 12000N / TM / QT100+ tChina
40220010000N / TM / QT50+ tChina
5022008000 / 10000N / TM / QT50+ tChina

Quantities are approximate and change daily; all stock plates carry AB/FQ43 marking and ABS-endorsed mill certificates. Sizes outside the table are produced in the next mill rolling cycle, typically 3–6 weeks including ABS survey (as per standard and mill certificate for exact lead time). Send your size list and we will reply with stock vs roll.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and ABS stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

Extra High Strength FQ43 is less commonly stocked than AH36; many sizes are mill-roll only. Confirm available approved thicknesses with us before fixing the cutting plan.

ABS FH42 / FQ43 equivalents

Standard / societyDesignationComment
ABS Rules 2-1-8FQ43official ABS Extra High Strength grade for this page’s FH42 title
ASTM A131/A131MASTM A131/A131Mno direct FH42/FQ43 listing; A131 stops at FH40 for higher-strength hull grades
IACS / other societiesextra-high / 420 MPa class (society designation as per their rules)confirm exact society grade mark at enquiry
GB 712GB 712verify whether the specific extra-high grade is listed; otherwise as per standard and mill certificate
ABS higher-strength 40ABS AH40 / ABS EH40 / ABS FH40390 N/mm² band below EHS
Same letter other EHSABS FH46 / ABS FH50 / ABS FH55 / ABS FH62 / ABS FH70FH commercial family

Comparisons, not substitutions. Dual classification for Extra High Strength needs mills approved by each society for that strength level.

When to order FH42 / FQ43

Use Extra High Strength when design yield exceeds the 390 N/mm² of AH–FH 40. Category steps: 43→420, 47→460, 51→500, 56→550, 63→620, 70→690 N/mm². Letter AQ/DQ/EQ/FQ (commercial AH/DH/EH/FH) sets 0/−20/−40/−60 °C.

Do not substitute ABS FH40 for FH42 without design approval — yield and rule section differ (2-1-3 vs 2-1-8).

When ABS FH42 is the right choice: typical uses are low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified. The Charpy temperature (−60 °C) is fixed by the letter, and the strength by the number (ReH 420 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing. Swapping to a different letter or strength needs class approval of the drawing change, not just a new purchase order.

Applications and fabrication notes for FQ43

Typical uses: weight-critical hull and offshore members, MOU legs/racks/chords (order “R” designation when required), high-stress deck and bulkhead plating specified at 420 N/mm². See offshore platform steel plates.

Fabrication: welding and PWHT windows are narrower than for AH36; use WPS qualified for the strength level and follow mill Ceq/CET/Pcm and hydrogen-control guidance. Incorrect post-weld or flame-straightening heat can damage toughness (2-1-8/13). Parameters from weldability tests may be requested from the mill (2-1-8/15).

Project pattern for category 43: Typical projects: large crude / product tanker longitudinals, weight-sensitive pontoons, and MOU braces where 420 MPa is drawn but 460 MPa is not required. Compared with ABS AH36 / ABS FH40, this grade changes both rule section (2-1-8 vs 2-1-3) and yield.

Order checklist unique to FH42: write ABS FQ43 on the PO; Charpy −60 °C; yield 420 N/mm²; UT level for t≥15 mm; vacuum degassing if t>50 mm; delivery condition N/TM/QT; optional R suffix for MOU leg/rack/chord.

Processing notes for ABS FH42: FQ43 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and ABS. Cold forming and bending radii should follow the mill’s data sheet.

Survey, UT and documentation

Surveyor witnesses mechanical tests and verifies process/NDE. Certificates include cast/batch/plate ID, grade, chemistry + Ceq/CET/Pcm, delivery condition with heat-treatment temperatures, mechanical results, surface and UT reports (2-1-8/23). Optional EN 10204 3.2 and multi-class.

Charpy acceptance for ABS FH42 by thickness (from 2-1-8; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
as per 2-1-8 Table 5A−60 °C4127

On receipt, check that the test temperature on the certificate is −60 °C and that the energy matches the band for the delivered thickness, not the thinnest band. Also check that the plate number on the stamp matches the certificate line, and that the ABS Surveyor endorsement is present. For thickness ≥ 15 mm, 2-1-8 requires ultrasonic examination; check the UT report and the agreed acceptance level. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes ordering ABS FH42

  • Using title FH42 on the PO without ABS grade FQ43 / 2-1-8 reference — mill may mis-route to 2-1-3
  • Assuming A131 / GB 712 automatically cover Extra High Strength
  • Omitting delivery condition (N/TM/QT) and UT class
  • Skipping vacuum-degassing / t>50 mm requirements
  • No “R” suffix when ordering MOU leg/rack/chord plate
  • Substituting FH40 for EHS without design change
  • How does ABS FH42 differ from ABS FH40?: FH40 is higher-strength 2-1-3 steel at 390 N/mm² yield and −60 °C. FH42 is Extra High Strength 2-1-8 (official FQ43) at 420 N/mm² and −60 °C. Chemistry, UT rules and vacuum-degassing requirements differ — do not substitute without design approval.

Sourcing ABS FH42: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Mill not approved for EHS gradewe only quote mills with ABS approval for the specific FQ43 / condition
Payment / quality riskT/T or L/C; inspection before balance; 3.2 witness available
Long lead timephoto updates; combine with AH36/FH40 tonnage when possible
Fabrication damage riskmill WPS data forwarded on request; cutting plan reviewed before ship
Prepcutting, bevelling, drilling, machining in-house

How to order ABS FH42 / FQ43

State both ABS FQ43 (rule) and commercial FH42 if used in the yard BOM; delivery condition; thickness × width × length × qty; UT level; Z/R if needed; multi-class; certificate type; port. Email SHH STEEL.

Sample PO line: “Steel plate to ABS Rules Part 2 2-1-8, Grade FQ43 (commercial FH42), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked AB/FQ43, certificate endorsed by ABS Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].” Each bracketed item changes price, lead time and which mills can supply, so fix them at enquiry stage.

FAQ

What sizes and minimum order quantity can you supply for ABS FH42 plate?
ABS FH42 is ordered as ABS Extra High Strength grade FQ43 under 2-1-8. The plate is fully killed, and the maximum thickness depends on the delivery condition (TM or QT) under 2-1-8/3.3 Table 3. In practice FQ43 is nearly always produced by an approved mill to order rather than taken from stock, so a mill minimum per heat or rolling usually applies. Send thickness × width × length × quantity per size and we will say whether the order fits a scheduled rolling or needs its own heat. Small balance quantities can sometimes ride on another FQ43 order.
How is ABS FH42 certified, and can you arrange EN 10204 3.2 witness inspection?
Every plate is made by an ABS-approved mill under ABS survey. It is die-stamped or stencilled AB/FQ43 with the heat or plate number, and the mill test certificate is endorsed by the ABS Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 420 N/mm², Rm 530–680 N/mm², A ≥ 18 %), the Charpy results at −60 °C, the delivery condition and the plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. The witness can be the ABS Surveyor, a second class society (dual or multi-class stamping, e.g. ABS + DNV or LR), or a third-party inspector such as SGS or BV who witnesses the tests and checks the markings. 3.2 cannot be added after the plates have been tested, so please state it on the enquiry.
What is the impact test temperature and energy for ABS FH42 (FQ43), and do thickness limits apply?
FQ43 is tested at −60 °C with an average of at least 41 J longitudinal or 27 J transverse (2-1-8 Table 5A). Impact specimens come from the quarter-thickness position (t/4). For plates thicker than 100 mm, ABS requires additional positions. Rule maximum thickness depends on whether the plate is TM or QT (2-1-8/3.3 Table 3), so give the delivery condition as well as the thickness, and we will check the approved mill’s range before quoting. Final values are as per standard and mill certificate.
What welding and preheat guidance applies to ABS FH42?
FQ43 is an extra high strength steel (yield ≥ 420 N/mm²) supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by ABS. Under 2-1-8/4, Ceq is calculated from the ladle analysis and limited by Table 4B. For grades 47 and above, the mill may report CET, and for low-carbon TM/QT steel (C ≤ 0.12 %) it may report Pcm. Hydrogen control, preheat, interpass temperature and heat-input windows come from the approved WPS and the mill’s recommendations. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits.
What is the delivery time for ABS FH42 plate?
FQ43 is normally rolled to order. Typical commercial lead time is about 6–10 weeks from confirmed PO and deposit, depending on the mill rolling schedule, QT capacity, UT and any 3.2 witness. Ocean transit comes on top of that. This is a commercial estimate, not a rule value, and we confirm it with each quotation. Every week, your coordinator sends the rolling, heat-treatment, testing and stamping status with photos. Delays are reported as soon as the mill tells us, not at the shipping date.
Which payment terms do you accept for ABS FH42, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the AB/FQ43 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance, so the plate is verified before most of the money moves. With L/C, payment is tied to the presented documents (commercial invoice, packing list, B/L, mill certificate, and the 3.2 or class certificate if you require one). For first orders we can start with a smaller trial lot. The proforma invoice shows the grade, sizes and certificate type, so the contract and the delivered plate match.
What are the equivalent grades of ABS FH42 among class societies and GB 712?
ABS lists ABS FH42 as FQ43 in 2-1-8; "FH42" is the commercial name. ASTM A131/A131M stops at FH40, so it has no direct equivalent. Other societies (DNV / LR / BV / CCS / NK / KR / RINA) have their own extra-high-strength grades at 420 N/mm² and −60 °C, and their marks must be confirmed against each society’s rules. Whether GB 712 lists this exact grade has to be checked per edition; otherwise the requirements are as per standard and mill certificate. Always write FQ43 on the PO, plus any additional society stamps you need.
Can you cut, bevel or machine ABS FH42 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut FH42 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the AB/FQ43 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For QT extra high strength plate, thermal cutting parameters follow the mill’s recommendations so the cut edge is not damaged. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. Loading photos and a packing list come with each shipment. See SHH STEEL for our processing capabilities.

Conclusion

ABS FH42 maps to rule grade FQ43: yield 420 N/mm², tensile 530–680 N/mm², Charpy −60 °C (41 J L / 27 J T). Fix on the order: official grade, delivery condition, UT, vacuum-degassing/t>50 needs, R-suffix if MOU, multi-class and 3.2.

SHH STEEL quotes only ABS-approved EHS mills, arranges Surveyor attendance, and can add third-party 3.2 and multi-class stamps.

T/T or L/C with inspection before balance; dedicated photo follow-up; workshop cutting/bevelling/drilling/machining.

Request a quotation: send SHH STEEL ABS FQ43 (title FH42), sizes, qty, delivery condition, port and inspection needs.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X