EN 10025-2 S275JR Steel Plate | S275JR Structural Steel - SHH STEEL

EN 10025-2 S275JR Steel Plate | S275JR Structural Steel

EN 10025-2 S275JR is a non-alloy structural steel plate with a minimum yield strength of 275 MPa. It offers good weldability, formability and economy for general structural applications. SHH STEEL is a China Mill-Direct Exporter supplying S275JR steel plate worldwide.
Equivalent Grades:
ASTM A283 Gr D / JIS SS490 / GB Q275B / ISO E275B
Specification:
EN 10025-2 — Delivery: As-rolled or normalized rolling (N)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-2 S275JR Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 S275JR Steel Plate (Material Number: 1.0044).

S275JR is a widely used non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 275 MPa (for thickness ≤ 16 mm) combined with good weldability, formability and toughness. The “JR” designation indicates that the material meets impact requirements of 27 J at +20°C. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S275JR steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-2 S275JR steel plate is produced in accordance with EN 10025-2.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-2 Full compliance
Steel Grade S275JR (1.0044) Confirmed
Delivery Condition +AR (As-rolled) or +N (Normalized) Available
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-2, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Thickness ≤ 40 mm Thickness > 40 mm Max. Limit
Carbon (C) ≤ 0.21% ≤ 0.22% —
Manganese (Mn) ≤ 1.50% ≤ 1.50% —
Phosphorus (P) ≤ 0.035% ≤ 0.035% —
Sulfur (S) ≤ 0.035% ≤ 0.035% —
Nitrogen (N) ≤ 0.012% ≤ 0.012% —
Copper (Cu) ≤ 0.55% ≤ 0.55% —

Product Analysis

Element Thickness ≤ 40 mm Thickness > 40 mm Max. Limit
Carbon (C) ≤ 0.24% ≤ 0.25% —
Manganese (Mn) ≤ 1.60% ≤ 1.60% —
Phosphorus (P) ≤ 0.045% ≤ 0.045% —
Sulfur (S) ≤ 0.045% ≤ 0.045% —
Nitrogen (N) ≤ 0.014% ≤ 0.014% —
Copper (Cu) ≤ 0.60% ≤ 0.60% —

Note:

  • The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.
  • Carbon Equivalent (CEV) is controlled to ensure good weldability.

Mechanical Properties

Mechanical properties of EN 10025-2 S275JR (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 275 MPa 410 – 560 MPa 23% 27 J at +20°C
> 16 ≤ 40 265 MPa 410 – 560 MPa 23% 27 J at +20°C
> 40 ≤ 63 255 MPa 410 – 560 MPa 22% 27 J at +20°C
> 63 ≤ 100 245 – 235 MPa 410 – 560 MPa 21% 27 J at +20°C
> 100 ≤ 150 225 MPa 400 – 540 MPa 19% 27 J at +20°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 S275JR steel plate mainly in the following conditions:

  • +AR (As-rolled) – most common
  • +N (Normalized) – available on request

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

EN 10025-2 S275JR Tolerances

Dimensional tolerances for S275JR steel plate follow EN 10029 (for plates) or EN 10051 (for strips).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

EN 10025-2 S275JR Weldability

S275JR has good weldability due to its controlled carbon content and carbon equivalent. It can be welded by all conventional methods (SMAW, SAW, GMAW, FCAW, etc.). Preheating may be required for thicker plates. Low-hydrogen consumables are recommended for critical applications.

Equivalent Material Grades

Grade Standard Notes
S275JR EN 10025-2 —
1.0044 EN Material number
Q275B GB/T 700 Closest Chinese equivalent
A572 Grade 42 / A36 ASTM (approximate) Similar strength level
St44-2 DIN (old) Former designation

Applications

EN 10025-2 S275JR is widely used in general structural applications requiring higher strength than S235. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Beams, columns, frames – S275JR Structural Steel
Bridges Bridge components – S275JR Bridge
Machinery Base plates, frames, heavy equipment – S275JR Machinery
Construction General construction steel – S275JR Construction
Storage Tanks Non-pressure tanks and silos – S275JR Storage
General Fabrication Welded structures – S275JR Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 S275JR Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “JR” in S275JR mean?
“JR” indicates that the steel meets the impact energy requirement of minimum 27 J at +20°C.
What is the difference between S235JR and S275JR?
S275JR has a higher minimum yield strength (275 MPa vs 235 MPa) and higher tensile strength, making it suitable for more demanding structural applications.
What is the material number of S275JR?
1.0044
Can SHH STEEL supply normalized S275JR (+N)?
Yes. Both as-rolled (+AR) and normalized (+N) conditions are available.

Conclusion

EN 10025-2 S275JR (1.0044) Steel Plate from SHH STEEL is a reliable non-alloy structural steel with higher strength than S235 grades, widely used in construction and general engineering. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S275JR structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X