GB 712 Grade A Shipbuilding Steel Plate

GB 712 Grade A shipbuilding steel plate

GB 712 Grade A normal-strength hull plate to the Chinese national standard GB 712 (IACS UR W11 basis): yield 235 N/mm², no Charpy test up to 50 mm. From Chinese plate mills via SHH STEEL — stock or mill-rolled, class certificate on request.
Keywords
GB 712 Grade A steel plate, GB712 A shipbuilding steel, GB 712 A hull plate, Chinese standard Grade A ship plate, normal strength hull structural steel
Equivalent Grades:
CCS Grade A; ABS A; DNV VL A; LR Grade A; BV Grade A; KR Grade A (RA); NK Grade A (KA); RINA Grade A; ASTM A131 Grade A; IACS UR W11 A
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

GB 712 Grade A shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

GB 712 Grade A is the basic mild hull steel of the Chinese national standard GB 712 and the plate Chinese yards use in the largest tonnage: 235 N/mm² minimum yield, 400–520 N/mm² tensile strength and, up to 50 mm, no Charpy test at all. The letter A is the same as in IACS UR W11, so a designer anywhere reads the grade at once; what the national standard adds is a Chinese product framework — testing, sampling, marking and certificate rules written for domestic mills.

Equivalent grades: ASTM A131 Grade A · ABS A · DNV NV A · LR Grade A · BV Grade A · CCS Grade A · NK KA · KR RA · RINA Grade A.

Current edition: GB/T 712-2022 (Structural steel for ships and ocean engineering) (replaced GB 712-2011; implementation date 2023-05-01). English page titles keep the form “GB 712 Grade …”. Chemistry and tensile figures on this page are verified against the GB 712-2011 OCR tables and Caishuku consensus; full 2022 tables were not obtained free — do not assume 2022-only UHSS grades beyond this pack.

Because Grade A is the cheapest hull plate, it is also the one most often used in the wrong place. Check the approved drawing: if it says B, D or E for a strake, Grade A cannot be fitted there, however good its tensile results look.

GB 712 is a national standard (the GB prefix without “/T”), and it sits next to — not inside — the general structural steel standard GB/T 1591. That separation matters: a Q235 or Q355 plate is not hull steel, even when the numbers look close, because it has no hull-steel deoxidation, toughness grading or marking rules.

SHH STEEL supplies GB 712 Grade A from Chinese plate mills, as plain GB 712 plate for domestic-style projects or with a classification certificate added on the same heat for export. Common sizes are in stock; the rest is rolled to order. The full range is under GB 712 Grade A.

How GB 712 names it. For normal-strength steel GB 712 uses the bare letter — A, B, D or E — and the plate is stencilled “GB 712 A” with the mill mark. There is no prefix or number to decode, so mistakes come from mixing the hull grade up with a Q-grade, not from the name itself.

GB 712 Grade A: key data at a glance

ItemGB 712 Grade A
StandardGB 712 (Chinese national standard for hull and offshore structural steel), normal-strength Grade A; values on the IACS UR W11 basis (GB 712 table/clause numbers not quoted — UNCERTAIN)
DesignationGrade A: same letter as IACS UR W11
Strength classnormal strength, ReH ≥ 235 N/mm²
Deoxidationany except rimmed ≤50 mm; killed >50 mm
Grain refinementnot required at every thickness
Condition of supplyAR / CR / N / TM as permitted for the ordered thickness
Charpy Vgenerally not required ≤50 mm; >50 mm at +20 °C unless fine-grain N (TM at Society discretion)
Thickness rangeplates typically up to 100 mm; sections are also covered by GB 712
DimensionsGB/T 709 for hot-rolled plate dimensions (minus tolerance per hull-steel practice — confirm)
CertificateGB 712 mill quality certificate (EN 10204 3.1 type); class certificate or 3.2 on request

Size window. Chinese mills roll GB 712 Grade A from about 5 mm to 100 mm thick, 1500–4000 mm wide on wide-plate mills, and up to about 18 m long. Plate below 6 mm may come from a hot strip mill as cut-to-length coil; confirm that the mill’s certification covers that route.

Reading the table. For Grade A the deoxidation and grain-refinement lines matter more than the strength lines, which are the same for all four mild letters. They decide whether a plate from a given heat can be certified as Grade A at the ordered thickness.

GB 712 Grade A chemistry — every element on the certificate

ElementHeat (ladle) analysis, %Product (check) analysis, %Comment
C0.21 max.0.23 max. (0.21 + 0.02)
Si0.50 max.0.55 max. (0.50 + 0.05)
Mn2.5 × C min.2.5 × C min. (ratio requirement – no tolerance row applies)
P0.035 max.0.040 max. (0.035 + 0.005)
S0.035 max.0.040 max. (0.035 + 0.005)
Al (acid-soluble)not specified (report if added)no heat limit specified – report actual value
Nbreport if intentionally addedno numeric heat limit – report actual value
Vreport if intentionally addedno numeric heat limit – report actual value
Tireport if intentionally addedno numeric heat limit – report actual value
Cu0.35 max. (residual)0.35 max. (residual element – GB/T 222 §5.1.1: no product tolerance)residual
Cr0.30 max. (residual)0.30 max. (residual element – GB/T 222 §5.1.1: no product tolerance)residual
Ni0.40 max. (residual)0.40 max. (residual element – GB/T 222 §5.1.1: no product tolerance)residual
Mo0.08 max. (residual)0.08 max. (residual element – GB/T 222 §5.1.1: no product tolerance)residual
Nnot specifiedno heat limit specified – report actual valuereport on request
Nb+V+Tinot specified for normal strength (calculated if added)not applicable (calculated from heat analysis)
C + Mn/6 (Ceq)0.40 max. (calculated)not applicable (calculated from heat analysis)carbon equivalent cap

Product (check) analysis column = heat (ladle) limit adjusted by GB/T 222-2006 Table 1 (non-alloy and low-alloy steel), as invoked by GB 712 clause 6.1.3 (upper limit + upper deviation, lower limit − lower deviation; row chosen by the specified upper limit; values for cross-sections up to 6 500 mm², larger sections by agreement); arithmetic shown in brackets.

Limits shown are the IACS UR W11 values that GB 712 follows for normal-strength steel; the published GB 712 text governs where it differs (not checked against a local copy — UNCERTAIN). For Grade A the manganese minimum is tied to carbon (Mn ≥ 2.5 × C) and silicon may reach 0.50 %. It is the only letter that may be semi-killed up to 50 mm, which is why Grade A can be made on the simplest route.

Chinese mill certificates normally print a fixed element list for the grade — C, Si, Mn, P, S, Als and the residuals — even where GB 712 sets no limit. Read the residual Cu, Cr, Ni and Mo values: electric-arc steel made from scrap runs higher in residuals than converter steel, and that matters for welding.

Chinese converter (BOF) steel made largely from hot metal tends to show low residuals; electric-furnace heats show more Cu and Ni. Both are acceptable if inside the limits, but the welding engineer should see the real values.

GB 712 Grade A tensile requirements

PropertyRequirement
Upper yield strength ReH235 N/mm² min.
Tensile strength Rm400–520 N/mm²
Elongation A (5.65√S0)22 % min.
Charpy test temperature+20 °C only above 50 mm (no test up to 50 mm)

All four GB 712 mild grades share these tensile values. Chinese certificates report yield as ReH and tensile as Rm in MPa (1 MPa = 1 N/mm²), with elongation as A on a proportional specimen; check that the specimen type is stated, because thin plate is often tested on flat non-proportional pieces with lower elongation minimums.

Tensile tests are taken transversely for plate, one test per batch, with the batch defined by heat, thickness range and condition (GB 712 batch rules not quoted — UNCERTAIN).

Tensile specimens are taken transverse to the rolling direction for plate, following UR W11/W16 practice; the certificate should show the specimen orientation and type. Where no clear yield point appears, Rp0.2 is reported instead of ReH.

GB 712 Grade A: Charpy V-notch and delivery condition

Grade A needs no Charpy test up to 50 mm. Above 50 mm a test at +20 °C applies unless the plate is normalized or TM-rolled under the conditions allowed for that thickness.

ThicknessAvg. longitudinal (J)Avg. transverse (J)
≤ 50 mm2720
50–70 mm3424
70–100 mm4127

Each value is the average of three full-size specimens; one may be lower but not below 70 % of the required average. Longitudinal specimens are standard unless transverse ones are ordered (UR W11 basis; GB clause not quoted).

On Chinese certificates the condition of supply may appear in Chinese — for example as-rolled, normalized or TMCP (thermo-mechanical controlled processing). Ask the mill to print the English code too, so the receiving inspector abroad can match it to the order.

Where the yard specification adds requirements beyond the standard — for example Charpy on Grade A below 50 mm — that is an order extra and must be written on the purchase order.

Thickness tolerance, flatness and surface

Dimensions and plus tolerances of GB 712 plate are usually supplied to GB/T 709, the Chinese standard for hot-rolled plate dimensions, while hull-steel practice limits the minus tolerance (commonly quoted as −0.3 mm following IACS UR W13 — confirm on the order). For export, buyers often ask for EN 10029 Class B or ASTM A6 tolerances instead; that is fine provided it is agreed before rolling.

Surface defects may be ground out as long as the remaining thickness stays inside the minus tolerance. Weld repair of plate surfaces needs the purchaser’s agreement and, for classed work, the surveyor’s.

If the plate is ordered with a classification certificate, the class minus tolerance applies whatever dimension standard is named, so state both on the order. For thin plate under 10 mm, also state the flatness requirement; GB/T 709 flatness classes differ from EN 10029.

GB 712 Grade A stock and lead time

Thickness (mm)Width (mm)Length (mm)ConditionApprox. qty
51500 / 18006000–12000AR / CR / N / TM80+ t
61800 / 20006000–12000AR / CR / N / TM100+ t
820006000–12000AR / CR / N / TM150+ t
102000 / 22006000–12000AR / CR / N / TM200+ t
122000 / 25006000–12000AR / CR / N / TM250+ t
162200 / 25006000–12000AR / CR / N / TM200+ t
2025006000–12000AR / CR / N / TM150+ t
2525006000–12000AR / CR / N / TM120+ t
302200 / 25006000–12000AR / CR / N / TM100+ t
4022006000–12000AR / CR / N / TM60+ t
5022006000–12000AR / CR / N / TM40+ t

Quantities change weekly — confirm before booking. Stock plate is sold as GB 712 Grade A with the original mill certificate. Other sizes go into the next mill campaign: about 3–5 weeks.

Packing and shipping: bundled by size with steel strapping, stencilled with standard, grade and heat number, and shipped from Shanghai, Tianjin, Qingdao or other Chinese ports in containers (≤ 11.8 m) or break bulk.

Processing before shipping. We cut Grade A to drawing by plasma or oxy-fuel, bevel edges, shot-blast and prime, and transfer grade, heat and plate number to every piece so that GB 712 traceability survives cutting. Cut parts ship with a cutting list cross-referencing each piece to its mother plate and certificate.

GB 712 Grade A against class societies and ASTM A131

Standard / societyDesignationRemark
GB 712 (this page)GB 712 Grade AChinese national product standard; no class stamp by itself
CCSCCS Grade Asame letters as GB 712; the usual class mark on domestic Chinese hulls
ABSABS A
DNVDNV VL AVL prefix
LRLR Grade A
BVBV Grade A
KRKR Grade A (RA)R-prefix
NKNK Grade A (KA)K-prefix
RINARINA Grade A
ASTM A131ASTM A131/A131M Grade AUS product standard

GB 712 and the CCS Rules. GB 712 was drafted to mirror the IACS unified requirements, which the China Classification Society (CCS) also applies in its Rules for Materials and Welding. In practice a Chinese mill rolls one heat to the shared chemistry and test plan; the plate becomes GB 712 Grade A through the national standard and CCS A through CCS survey. The two are parallel documents, not one replacing the other (CCS chapter numbering not quoted — UNCERTAIN).

Class certification on a GB 712 base. Export buyers often order “GB 712 A with CCS, ABS or DNV certificate” (or another IACS society). The class surveyor must witness or audit the tests at the mill before shipment; a plain GB 712 certificate cannot be converted into a class certificate afterwards. Several marks on one plate are possible when every society is booked in advance and the mill holds the relevant approvals.

Choosing A, B, D or E within GB 712

Grade A is untested up to 50 mm; B adds 0 °C, D −20 °C and E −40 °C. The letter is fixed by the structural category and thickness on the approved drawing; GB 712 supplies the material, it does not choose it.

GB 712 or GB/T 1591? Shore structures, steel buildings and machinery frames use GB/T 1591 grades such as Q355; hull structure uses GB 712. A Q235B plate is not interchangeable with GB 712 Grade A, even though the yield level is the same, because the hull grade adds deoxidation, toughness and identification rules.

Typical uses of GB 712 Grade A: inland and coastal vessels, barges, river cargo ships, internal decks, tank tops, floors and bulkheads, and general structure of ships built at Chinese yards for domestic owners.

Using a higher mild letter than needed adds cost without improving the design; using a lower one is a non-conformity. Follow the drawing exactly and let the purchase order repeat it.

Cutting, forming and welding GB 712 Grade A

GB 712 Grade A cuts by oxy-fuel, plasma or laser without preheat and forms easily, including cold flanging. Weld with consumables suited to normal-strength hull steel of matching toughness — for example GB/T 5117 or GB/T 10045 classifications chosen in the yard’s WPS — or class-approved consumables when the hull is classed.

Because the carbon equivalent is capped at 0.40, preheat is normally not needed, but thick restrained joints and cold, damp shop conditions in northern Chinese winters can still call for a modest preheat set by the procedure.

For offshore steelwork see offshore platform steel plates.

Where Grade A fits. On bulk carriers and river vessels Grade A is used for internal structure where stiffness and minimum thickness govern. Grade A is the cheapest and most widely stocked GB 712 plate, so it is also the easiest to substitute wrongly. Keep mild and high-tensile plates of similar thickness clearly apart in the yard: they look identical and differ only in the stencil.

GB 712 tests, certificate and receiving checks

Each GB 712 delivery carries the mill quality certificate giving the standard and grade, heat number, plate numbers, sizes, heat analysis, tensile results, Charpy results where required, condition of supply and the mill’s quality stamp. Plates are marked with the mill’s logo, standard, grade, heat and plate number by stencil or hard stamp.

On receipt: check that the stencil reads GB 712 and Grade A, that heat and plate numbers match the certificate, that Charpy results (if required) are at +20 °C only above 50 mm (no test up to 50 mm), and measure thickness at several points. An independent inspection company or your own inspector can witness tests at the mill if booked before rolling.

Mill quality system. Chinese plate mills supplying GB 712 normally run ISO 9001-certified quality systems and hold their own national product certification; when a class certificate is wanted, the mill must also hold that society’s works approval for the grade and thickness (details per mill — UNCERTAIN). Ask for that approval scope before ordering; it is the single most useful check a buyer can make.

Mistakes we see on GB 712 Grade A orders

  • Ordering “Q235B” when the drawing calls for hull steel Grade A
  • Using Grade A where the drawing says B, D or E
  • Accepting a plain GB 712 certificate where the hull needs a class certificate
  • Not checking C + Mn/6 ≤ 0.40
  • Confusing Grade A with AH32/AH36 in a quick enquiry

Write the full standard and grade, the condition of supply, the certificate type and any class requirement on the purchase order and the pro-forma invoice. Most problems start where one document differs from the other.

With mild plate the expensive mistakes are rarely about strength; they are about the toughness letter, the certificate type and the condition of supply. A rejected certificate at the yard can stop a block for weeks.

Buying GB 712 Grade A from China: concerns and answers

ConcernAnswer
Is the certificate genuine?Original mill certificate for GB 712 Grade A, traceable by heat and plate number; mill verification and third-party witness on request
Will a foreign yard or inspector read it?Bilingual Chinese/English certificate; supply-condition codes translated
Export paperworkcommercial invoice, packing list, bill of lading, certificate of origin (Form E or general CO on request)
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed ordersseveral sizes and grades in one container
Ready-to-fit partscutting, bevelling, shot-blasting and priming in our own workshop

If you have not bought GB 712 plate from China before, we can send sample certificates in advance, arrange a trial lot, and let your inspector visit the mill during rolling and testing. For buyers outside China we also check that the bilingual certificate wording matches the purchase order line by line before shipment.

Ordering GB 712 Grade A

Send SHH STEEL: standard and grade (GB 712 Grade A), sizes and quantity per size, condition of supply, tolerance standard, any class certificate, UT or third-party inspection, surface finish and destination port.

Sample line: “Hull structural steel plate to GB 712, Grade A, 12 × 2500 × 12000 mm, 50 pcs, mill certificate in Chinese and English, EN 10204 3.1, FOB Shanghai.”

Order checklist:

  • Standard: GB 712 (state edition if your contract requires one)
  • Grade: Grade A
  • Condition of supply (AR / N / TMCP as allowed)
  • Sizes and quantity per size; tolerance standard and flatness class
  • Certificate: bilingual GB 712 mill certificate, EN 10204 3.1 or 3.2; class certificate if required
  • Extras: UT, Z-direction, shot-blast/prime, cutting
  • Delivery terms, destination port and documents (CO, Form E)

FAQ

What is GB 712 Grade A?
It is the normal-strength hull steel Grade A of GB 712, the Chinese national standard for ship and offshore structural steel. The letter matches IACS UR W11, so designers worldwide recognise it, while testing, marking and certification follow the Chinese standard. GB 712 is the standard Chinese mills, yards and stockists use for hull steel, so it is the reference point for domestic projects and the base for most export plate. In short, Grade A under GB 712 is defined by its letter; the Chinese standard, the IACS unified requirement and the classification rules all describe the same steel from different angles, so a clear order line covering standard, grade and certificate type removes most confusion. Grade A plate is often bought by stockists in bulk for river and coastal yards.
What Charpy toughness does Grade A need?
Generally not required ≤50 mm; >50 mm at +20 °c unless fine-grain n (tm at society discretion). Average energies are 27/20 J up to 50 mm, 34/24 J at 50–70 mm and 41/27 J at 70–100 mm (longitudinal/transverse), with one value allowed down to 70 % of the average. For thick plate ask for the specimen position and orientation on the certificate so the results can be compared with the right column of the table. Grade A is the cheapest and most widely stocked GB 712 plate, so it is also the easiest to substitute wrongly. When comparing certificates from different Chinese mills, compare the average and the lowest single Charpy value at no test up to 50 mm, not only whether the plate passed; a comfortable margin is the better sign of a stable process.
Is GB 712 Grade A the same as Q235B?
No. Q235B to GB/T 700 is a general structural steel. The yield level is similar, but the hull grade adds hull-steel deoxidation rules, toughness grading by letter and its own marking; a classification surveyor will not accept Q235B for hull structure. Hull steel is also not interchangeable with Q235 in the other direction: a GB 712 plate can be used for general structures, but buyers then pay for testing they do not need. For design offices outside China, GB 712 is a convenient reference because it uses the same letters and levels as the IACS tables; the drawing can say Grade A and the class requirement in one line, and the mill will understand both.
Where is Grade A used?
Typically inland and coastal vessels, barges, river cargo ships, internal decks, tank tops, floors and bulkheads, and general structure of ships built at Chinese yards for domestic owners. The approved drawing decides the letter from structural category and thickness. On bulk carriers and river vessels Grade A is used for internal structure where stiffness and minimum thickness govern. Mild steel is still a large share of a merchant hull’s tonnage, because internal structure is designed for stiffness and minimum thickness rather than strength. Typical Grade A enquiries from export buyers come with a cutting list and a delivery schedule by block; sending both early lets the mill group sizes and saves rolling slots.
Can Grade A be swapped with another letter?
Grade A cannot replace any other letter. B, D or E may be supplied against an A order if they meet the A limits, which Chinese mills sometimes do with surplus plate. Any substitute plate must carry its own certificate and stencil with the grade actually supplied; a substitution never shares paperwork with the original order. Any change of grade after the mill has rolled the plate means new plate; there is no way to re-grade Grade A on paper once the tests are done.
Does Grade A need preheat?
Usually not in normal thicknesses, because C + Mn/6 is capped at 0.40. The yard’s qualified welding procedure still sets the rule for thick or restrained joints and cold, damp conditions. Cold-shop welding in northern Chinese, Korean or Baltic winters can call for a modest preheat even on mild steel to drive off moisture; follow the WPS. If a class certificate is needed, booking the surveyor before rolling is the step that decides whether Grade A can be delivered on time; we arrange it with the mill when the order is placed.
Which sizes of Grade A are in stock?
Mostly 5–50 mm thick, 1500–2500 mm wide and 6–12 m long. Other sizes are rolled in about 3–5 weeks. Plate under 6 mm may be supplied cut from coil; confirm the processing line is covered by the mill’s certification. For Grade A, ask the mill to state plate weight on the certificate as theoretical or actual weight, because Chinese invoices may use either and the difference matters on large orders.
What are delivery times and payment terms?
About 7–15 days from stock and 3–5 weeks for mill rolling, plus sea freight (estimates confirmed per quote). T/T deposit and balance after inspection, or L/C at sight. Export paperwork normally includes commercial invoice, packing list, bill of lading, mill certificate and certificate of origin; Form E applies for ASEAN-China FTA destinations. Quotations for Grade A are normally valid for a short period because Chinese plate prices move with iron ore and coking coal; fix price and rolling slot together.

Conclusion

GB 712 Grade A is the normal-strength hull structural steel of the Chinese national standard GB 712, on the IACS UR W11 basis: yield 235 N/mm², tensile 400–520 N/mm², no Charpy test up to 50 mm. Order it by standard and grade, and add a classification certificate on the same heat when the hull is classed.

SHH STEEL supplies GB 712 Grade A from Chinese mills with bilingual certificates, cutting, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X