EN 10025-2 S235J0 Steel Plate | S235J0 Structural Steel - SHH STEEL

EN 10025-2 S235J0 Steel Plate | S235J0 Structural Steel

EN 10025-2 S235J0 is a non-alloy structural steel plate with a minimum yield strength of 235 MPa and impact tested at 0°C. It offers good weldability, formability and improved low-temperature toughness compared with S235JR. SHH STEEL is a China Mill-Direct Exporter supplying S235J0 steel plate worldwide.
Equivalent Grades:
ASTM A283 Gr C / JIS SS400 (0℃ imp) / GB Q235B (0℃) / ISO E235C
Specification:
EN 10025-2 — Delivery: As-rolled or normalized rolling (N)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-2 S235J0 Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 S235J0 Steel Plate (Material Number: 1.0114).

S235J0 is a non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 235 MPa (for thickness ≤ 16 mm) and is impact tested at 0°C with a minimum energy of 27 J. Compared with S235JR, the lower impact test temperature of S235J0 makes it more suitable for applications requiring better toughness in colder environments. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S235J0 steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-2 S235J0 steel plate is produced in accordance with EN 10025-2.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-2 Full compliance
Steel Grade S235J0 (1.0114) Confirmed
Delivery Condition +AR (As-rolled) or +N (Normalized) Available
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-2, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Thickness ≤ 40 mm Thickness > 40 mm Max. Limit
Carbon (C) ≤ 0.17% ≤ 0.20% —
Manganese (Mn) ≤ 1.40% ≤ 1.40% —
Phosphorus (P) ≤ 0.030% ≤ 0.030% —
Sulfur (S) ≤ 0.030% ≤ 0.030% —
Nitrogen (N) ≤ 0.012% ≤ 0.012% —
Copper (Cu) ≤ 0.55% ≤ 0.55% —

Product Analysis

Element Thickness ≤ 40 mm Thickness > 40 mm Max. Limit
Carbon (C) ≤ 0.19% ≤ 0.23% —
Manganese (Mn) ≤ 1.50% ≤ 1.50% —
Phosphorus (P) ≤ 0.040% ≤ 0.040% —
Sulfur (S) ≤ 0.040% ≤ 0.040% —
Nitrogen (N) ≤ 0.014% ≤ 0.014% —
Copper (Cu) ≤ 0.60% ≤ 0.60% —

Note:

  • The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.
  • Carbon Equivalent (CEV) is controlled to ensure good weldability.

Mechanical Properties

Mechanical properties of EN 10025-2 S235J0 (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 235 MPa 360 – 510 MPa 26% 27 J at 0°C
> 16 ≤ 40 225 MPa 360 – 510 MPa 26% 27 J at 0°C
> 40 ≤ 63 215 MPa 360 – 510 MPa 25% 27 J at 0°C
> 63 ≤ 100 215 MPa 360 – 510 MPa 24% 27 J at 0°C
> 100 ≤ 150 195 MPa 350 – 500 MPa 22% 27 J at 0°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 S235J0 steel plate mainly in the following conditions:

  • +AR (As-rolled) – most common
  • +N (Normalized) – available on request

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S235J0 steel plate follow EN 10029 (for plates) or EN 10051 (for strips).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S235J0 has excellent weldability due to its low carbon content and controlled carbon equivalent. It can be welded by all conventional methods (SMAW, SAW, GMAW, FCAW, etc.) without preheating in most cases for thinner plates. Low-hydrogen consumables are recommended for thicker sections or critical applications.

Equivalent Material Grades

Grade Standard Notes
S235J0 EN 10025-2 —
1.0114 EN Material number
Q235C GB/T 700 Closest Chinese equivalent
A36 (approximate) ASTM Similar strength level
St37-3U DIN (old) Former designation

Applications

EN 10025-2 S235J0 is widely used in structural applications requiring better low-temperature toughness than S235JR. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Beams, columns, frames – S235J0 Structural Steel
Bridges Bridge components – S235J0 Bridge
Machinery Base plates, frames – S235J0 Machinery
Construction General construction in colder regions – S235J0 Construction
Storage Tanks Non-pressure tanks and silos – S235J0 Storage
General Fabrication Welded structures – S235J0 Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 S235J0 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “J0” in S235J0 mean?
“J0” indicates that the steel meets the impact energy requirement of minimum 27 J at 0°C
What is the difference between S235JR, S235J0 and S235J2?
he difference is the impact test temperature: JR: +20°C J0: 0°C J2: –20°C
What is the material number of S235J0?
1.0114
What is the density of S235J0?
7.85 g/cm³.
Can SHH STEEL supply normalized S235J0 (+N)?
Yes. Both as-rolled (+AR) and normalized (+N) conditions are available.

Conclusion

EN 10025-2 S235J0 (1.0114) Steel Plate from SHH STEEL offers reliable structural performance with improved toughness at 0°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S235J0 structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X