EN 10025-5 S355J0W Steel Plate | S355J0W Weathering Steel - SHH STEEL

EN 10025-5 S355J0W Steel Plate | S355J0W Weathering Steel

SHH STEEL, a China Mill-Direct Exporter, supplies EN 10025-5 S355J0W weathering steel plate. 355 MPa yield strength with improved atmospheric corrosion resistance. Competitive price, fast delivery, full MTCs. Contact us now.
Equivalent Grades:
ASTM A588 Gr A / JIS SMA490AW / GB Q355NH / ISO E355W
Material Specification:
EN 10025-5 — Delivery: As-rolled (AR) or TMCP, 0℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

General Description

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-5 S355J0W Steel Plate (Material Number: 1.8959).

S355J0W is a structural steel with improved atmospheric corrosion resistance under the European standard EN 10025-5. The “W” designation indicates enhanced resistance to atmospheric corrosion through the formation of a stable protective oxide layer (patina). It provides a minimum yield strength of 355 MPa (for thickness ≤ 16 mm) and is impact tested at 0°C with a minimum energy of 27 J. This grade is frequently used as an alternative to conventional structural steels in outdoor applications where painting costs need to be reduced or eliminated.

SHH STEEL sources S355J0W plates directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery. We supply thicknesses from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-5 Full compliance
Steel Grade S355J0W (1.8959) Confirmed
Delivery Condition As-rolled, Normalized or TMCP Available
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-5, the chemical composition is specified for ladle analysis. The presence of chromium, copper and nickel enables the formation of a protective rust layer.

Ladle Analysis (Cast Analysis)

Element Max. / Range (%)
Carbon (C) ≤ 0.16
Silicon (Si) ≤ 0.50
Manganese (Mn) 0.50 – 1.50
Phosphorus (P) ≤ 0.035
Sulfur (S) ≤ 0.035
Chromium (Cr) 0.40 – 0.80
Nickel (Ni) ≤ 0.65
Copper (Cu) 0.25 – 0.55
Molybdenum (Mo) ≤ 0.30
Nitrogen (N) ≤ 0.009
Zirconium (Zr) ≤ 0.15

Note: The combination of Cr, Cu and Ni provides the improved atmospheric corrosion resistance that distinguishes weathering steels from conventional structural steels.

Mechanical Properties

Mechanical properties of EN 10025-5 S355J0W (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 355 MPa 470 – 630 MPa 22% 27 J at 0°C
> 16 ≤ 40 345 MPa 470 – 630 MPa 22% 27 J at 0°C
> 40 ≤ 63 335 MPa 470 – 630 MPa 21% 27 J at 0°C
> 63 ≤ 80 325 MPa 470 – 630 MPa 20% 27 J at 0°C
> 80 ≤ 100 315 MPa 470 – 630 MPa 20% 27 J at 0°C
> 100 ≤ 150 295 MPa 450 – 600 MPa 18% 27 J at 0°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-5 S355J0W steel plate in as-rolled, normalized or thermomechanically rolled condition according to customer requirements.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S355J0W steel plate follow EN 10029.

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S355J0W has good weldability similar to conventional S355 structural steels. The presence of alloying elements for corrosion resistance does not significantly impair welding performance when proper procedures are followed.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E7016
GMAW (MIG/MAG) ER70S-6
FCAW E71T-1
SAW EM12K + suitable flux

Preheating is generally not required for thin and medium thicknesses. Matching weathering steel consumables can be used when the weld itself must also form a protective patina.

Equivalent Material Grades

Grade Standard Notes
S355J0W EN 10025-5 —
1.8959 EN Material number
Q355NHD / Q355GNH GB/T 4171 Closest Chinese weathering steels
Corten B (approx.) ASTM A588 / A242 Similar weathering concept
WTSt 52-3 DIN (old) Former designation

Applications

EN 10025-5 S355J0W is widely used in outdoor structures where atmospheric corrosion resistance is required and painting costs need to be minimized. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Bridges Bridge girders, components – S355J0W Bridge
Building Structures Facades, external frames – S355J0W Structural Steel
Containers & Shipping Containers, cargo handling – S355J0W Container
Railway Vehicles Wagon structures – S355J0W Railway
Sculptures & Architecture Outdoor sculptures, architectural elements – S355J0W Architecture
General Outdoor Fabrication Weathering steel structures – S355J0W Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-5 S355J0W Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for weathering steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “W” in S355J0W mean?
“W” indicates improved atmospheric corrosion resistance (weathering steel). The steel forms a stable protective oxide layer (patina) when exposed to the atmosphere.
What is the difference between S355J0W and S355J2W?
Both are weathering steels with the same strength level. S355J0W is impact tested at 0°C (27 J), while S355J2W is tested at –20°C (27 J).
What is the material number of S355J0W?
1.8959

Conclusion

EN 10025-5 S355J0W (1.8959) Steel Plate from SHH STEEL is a weathering structural steel offering 355 MPa yield strength and improved atmospheric corrosion resistance. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S355J0W weathering steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-5 S355J0W Steel Plate, S355J0W steel plate, S355J0W weathering steel, EN 10025 S355J0W, S355J0W equivalent, S355J0W supplier, 1.8959

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X