GB/T 1591 Q420MB thermomechanically rolled high-strength low-alloy structural steel plate, 420 MPa yield, +20 °C impact, SHH STEEL

Q420MB TMCP Steel Plate GB/T 1591 Supplier

GB/T 1591 Q420MB is thermomechanical controlled process plate with 420 MPa minimum yield and +20°C impact. SHH STEEL supplies Q420MB plate mill-direct for buildings, bridges and fabrication that names the M condition. This is not normalized Q420NB.
Keywords
Q420MB, Q420MB steel plate, GB/T 1591 Q420MB, Q420MB TMCP, Q420MB supplier, EN 10025-4 S420M, ASTM A572 Gr.60, Q420NB, Q390MB
Equivalent Grades:
GB/T 1591 Q420MB / ASTM A572 Gr 60 / JIS G3106 SM570 (near) / EN 10025-4 S420M (near) — Material Specification: GB/T 1591 — Delivery: TMCP; improved toughness
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q420MB TMCP Steel Plate GB/T 1591?

Q420MB, also searched as GB/T 1591 Q420MB, Q420MB steel plate, Q420MB TMCP plate and Q420 MB, is the 420 MPa quality-grade-B grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 420 is the thin-plate minimum yield in MPa, M is the delivery letter, and B is the quality letter for Charpy impact at +20°C.

The M is the point of this page. Normalized GB/T 1591 Q420NB has an N. A normalized certificate cannot be stamped MB. Hot-rolled GB/T 1591 Q420B has neither M nor N. Normalized C is GB/T 1591 Q420NC. D is GB/T 1591 Q420ND. E is GB/T 1591 Q420NE. The 390 MPa TMCP sister at the same temperature is GB/T 1591 Q390MB. The full family sits on GB/T 1591. Do not drop a 420 MPa drawing onto a 390 MPa plate, and do not upgrade it to GB/T 1591 Q460C without a price check.

The closest European TMCP comparison is EN 10025-4 S420M, tested at −20°C, not +20°C. EN 10025-3 S420N is normalized and closer to Q420NB in process. On the US side, ASTM A572 Grade 60 is 60 ksi / 415 MPa, one step lower, and it is not an MB twin. ASTM A572 Gr.55 is 55 ksi. JIS G3106 SM570 is the usual Japanese comparison. Dual mark only when both books are fully met. See EN 10025-4 and high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q420MB from first-line structural mills that can actually run the TMCP schedule, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q420MB Confirmed
Other search names Q420MB steel plate, Q420 MB, Q420MB TMCP Covered
Delivery condition Thermomechanical controlled process Confirmed
Yield, ≤ 16 mm 420 MPa min Confirmed
Quality grade B, impact at +20°C Confirmed
Not this page Normalized GB/T 1591 Q420NB Different condition
Lower yield TMCP GB/T 1591 Q390MB 390 MPa
EN comparison EN 10025-4 S420M is −20°C Not a swap
US comparison ASTM A572 Gr.60 is 415 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q420D, GB/T 1591 Q390MC and ASTM A572 Gr.55.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q420. Product analysis, when ordered, follows GB/T 222. Q420MB is a microalloyed HSLA plate. Grade B allows a wider phosphorus and sulfur window than grade D or E. That is acceptable at +20°C. It is not a reason to use Q420MB on a −20°C drawing. Mills may add Nb, V or Ti. The certificate shows the elements actually used. TMCP chemistry is often leaner than a normalized heat of the same yield, because the rolling schedule does part of the grain refinement.

Heat Analysis and Product Analysis — GB/T 1591 Q420MB, TMCP

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.50 0.55
Manganese (Mn), max 1.70 1.80
Phosphorus (P), max 0.035 0.040
Sulfur (S), max 0.035 0.040
Niobium (Nb), max 0.07 0.08
Vanadium (V), max 0.20 0.22
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.30 0.35
Nickel (Ni), max 0.80 0.85
Copper (Cu), max 0.40 0.45
Molybdenum (Mo), max 0.20 0.21
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than normalized GB/T 1591 Q420NB. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as quenched-and-tempered GB/T 16270 Q460C. A 390 MPa file is GB/T 1591 Q390MB, not this grade.

Mechanical Properties

Buyers search Q420MB mechanical properties, Q420MB yield strength, GB/T 1591 Q420MB tensile and Q420MB impact 20°C.

Tensile and impact — GB/T 1591 Q420MB, TMCP

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 420 MPa 520–680 MPa 19% +20°C, grade B
> 16–40 mm 400 MPa 520–680 MPa 19% +20°C, grade B
> 40–63 mm 390 MPa 520–680 MPa 18% +20°C, grade B
> 63–80 mm 380 MPa 520–680 MPa 18% +20°C, grade B
> 80–100 mm 370 MPa 520–680 MPa 18% +20°C, grade B
> 100–150 mm 360 MPa 500–660 MPa 17% +20°C, grade B

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at +20°C. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 420 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 420 MPa is about 61 ksi. ASTM A572 Grade 60 is 60 ksi and is not this book. SHH STEEL quotes the thickness band and the M condition on the offer.

Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the B letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 1591 Q420NB GB/T 1591-2018 Normalized 420 MPa +20°C Different process
GB/T 1591 Q420B GB/T 1591-2018 Hot rolled 420 MPa +20°C Different process
Q420MB GB/T 1591-2018 TMCP 420 MPa +20°C This page
Q420MC GB/T 1591-2018 TMCP 420 MPa 0°C Colder M sister
GB/T 1591 Q390MB GB/T 1591-2018 TMCP 390 MPa +20°C Lower yield
GB/T 1591 Q460C GB/T 1591-2018 Hot rolled 460 MPa 0°C Higher yield
EN 10025-4 S420M EN 10025-4 TMCP 420 MPa −20°C Colder comparison
ASTM A572 Gr.55 ASTM A572 As rolled 380 MPa Different Lower yield

A colder normalized file is GB/T 1591 Q420ND. A 355 MPa file is GB/T 1591 Q355MB.

Equivalent Material Grades

There is no official one-to-one substitute for Q420MB. What buyers compare is a 420 MPa TMCP plate tested at +20°C.

EN 10025-4 S420M is the process comparison, but it is tested at −20°C. EN 10025-3 S420N is normalized. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A572 Grade 60 is 60 ksi / 415 MPa. ASTM A572 Gr.55 is 55 ksi. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM570 is the usual comparison. SHH STEEL will not stamp EN 10025-4 S420M or ASTM A572 Gr.60 on a Q420MB certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q420MB China GB/T 1591-2018 Name on this page
GB/T 1591 Q420NB China GB/T 1591-2018 Normalized, not this page
GB/T 1591 Q420B China GB/T 1591-2018 Hot rolled, not this page
GB/T 1591 Q390MB China GB/T 1591-2018 390 MPa, TMCP
EN 10025-4 S420M Europe EN 10025-4 TMCP, −20°C
EN 10025-3 S420N Europe EN 10025-3 Normalized comparison
ASTM A572 Gr.60 USA ASTM A572 60 ksi, lower yield
JIS G3106 SM570 Japan JIS G3106 Usual Japanese comparison

Structural Service

Buyers pick Q420MB when a building, bridge member or welded fabrication wants about 420 MPa yield, a TMCP condition, and impact at +20°C. Search phrases such as Q420MB steel plate and GB/T 1591 Q420MB all point here. The family index is GB/T 1591.

It is the wrong plate when the drawing says normalized. That work is GB/T 1591 Q420NB. It is the wrong plate when the drawing says hot rolled. That work is GB/T 1591 Q420B. It is the wrong plate for a 0°C file. That work is Q420MC, and the normalized sister is GB/T 1591 Q420NC. It is the wrong plate for a −20°C file. That work is Q420MD, and the normalized sister is GB/T 1591 Q420ND. It is the wrong plate for a −40°C file. That work is Q420ME, and the normalized sister is GB/T 1591 Q420NE. It is the wrong plate for a 390 MPa file. That work is GB/T 1591 Q390MB or GB/T 1591 Q390NE. It is the wrong plate for a 460 MPa file. That work is GB/T 1591 Q460NC. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade B, and the M condition at 420 MPa.

Weldability

Q420MB is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q420MB. Carbon equivalent on the M route is often lower than normalized GB/T 1591 Q420NB, which helps the root pass, but the TMCP microstructure still needs a qualified procedure.

Typical consumables are matching 60 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 is a useful strength reference after chemistry is checked, but it does not cover 420 MPa. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q420MB procedure on GB/T 1591 Q355ME without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q460NE either.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q420MB is thermomechanical controlled process. The plate is not normalized as GB/T 1591 Q420NB and not hot rolled as GB/T 1591 Q420B.

TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q420MB as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.

The certificate lists GB/T 1591 Q420MB, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and +20°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-4 S420M is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q420MB steel plate:

  • Thickness: commonly 8 mm – 80 mm, heavier plate to 100 mm by enquiry
  • Width: 1500 mm – 3200 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q420MB follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q420MB plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 60 −0.6 +1.3
60 – 80 −0.7 +1.5
80 – 100 −0.8 +1.6

Width on 1500–3200 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q420MB unless the order says so.

Supplementary Requirements

Q420MB already defines 420 MPa yield, TMCP delivery and +20°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q420MB. Do not write only Q420, and do not write Q420NB if the mill must stamp M. The family page is GB/T 1591.

Impact. Grade B is +20°C. Write a higher energy if the owner requires it. Do not expect a −20°C result unless the grade is changed.

Delivery condition. Write thermomechanical controlled process. Write GB/T 1591 Q420NB if normalized is required.

EN or US comparison. Write EN 10025-4 S420M or ASTM A572 Gr.60 only if dual mark is required and both tables are met. S420M is −20°C, not +20°C.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q420MB, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Buildings and workshops Q420MB columns, beams and base plates
Bridges and towers Q420MB webs and flanges from SHH STEEL
Construction machinery Q420MB frames where the drawing names M
General fabrication Q420MB gussets and connection plates
Comparison vs EN 10025-4 Q420MB next to EN 10025-4 S420M
Comparison vs ASTM A572 Q420MB next to ASTM A572 Gr.55
Lower yield option GB/T 1591 Q390MD when 390 MPa is enough

Q420MB is the plate for a 420 MPa TMCP file tested at +20°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A colder 460 MPa normalized file is GB/T 1591 Q460ND.

Supply Capability

SHH STEEL sources Q420MB from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm, 60 mm, 80 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an M heat is in yard; standard TMCP about 25–40 days; 3.2 inspection about 35–45 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q420MB that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule, so the M is on the certificate and not only in the enquiry.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard M heat about 25–40 days, 3.2 inspection about 35–45 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q420MB, keep the TMCP route, and do not ship GB/T 1591 Q420NB or GB/T 1591 Q420B as MB. We will not drop the M to save a cooling cycle, and we will not change B to a colder letter without a new test. If the drawing needs normalized plate, we will move the inquiry to Q420NB. If the drawing needs 460 MPa, we will move it to GB/T 1591 Q460D or GB/T 1591 Q460NE.

FAQ

What is Q420MB steel plate?
Q420MB in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 420 MPa minimum yield on thin plate and Charpy impact at +20°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q420MB the same as Q420NB?
No. Both yield at 420 MPa and both are tested at +20°C. Q420NB is normalized. Q420MB is TMCP.
Is Q420MB the same as Q420B?
No. Q420B is hot rolled. Q420MB is TMCP. The impact letter is the same. The process is not.
Is Q420MB the same as Q390MB?
No. Both are TMCP and both are tested at +20°C. Q390MB is 390 MPa. Q420MB is 420 MPa.
What is the European equivalent of Q420MB?
The nearest process comparison is EN 10025-4 S420M, which is TMCP but tested at −20°C. EN 10025-3 S420N is the normalized comparison. Dual mark only when both books are fully met.
What is the US equivalent of Q420MB?
There is no official ASTM twin. ASTM A572 Grade 60 is 60 ksi / 415 MPa, slightly lower, and it does not carry an MB letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
What thickness can SHH STEEL supply?
Common supply is 8 mm to 80 mm. Plate to 100 mm is quoted by enquiry. Yield on plate over 16 mm is lower than the 420 MPa thin-plate number.

Conclusion

Q420MB steel plate to GB/T 1591 is 420 MPa TMCP structural plate with impact at +20°C. It is not normalized GB/T 1591 Q420NB and not hot-rolled GB/T 1591 Q420B. EN 10025-4 S420M is the TMCP comparison, tested at −20°C. ASTM A572 Grade 60 is 415 MPa and is not a substitute. Whether the inquiry says Q420MB, GB/T 1591 Q420MB or Q420MB TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q420MB chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q420MB Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition. The grade family is listed on GB/T 1591.

Contact SHH STEEL for mill rolling, TMCP Q420MB, cutting, UT, 3.2 inspection or a worldwide quotation.

Q420MB, Q420MB steel plate, GB/T 1591 Q420MB, Q420MB TMCP, Q420MB supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X