Q690C QT Carbon Steel Plate GB/T 16270 Supplier
What is Q690C QT Carbon Steel Plate GB/T 16270?
Q690C, also searched as GB/T 16270 Q690C, Q690C QT plate, Q690C carbon steel plate, Q690C steel plate and Q690C quenched and tempered plate, is the 690 MPa quality-grade-C grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 690 is the thin-plate minimum yield in MPa, and C is the quality letter for Charpy impact at 0°C.
Q690C is the grade most buyers mean when they say 100 ksi QT plate from a Chinese mill. It sits above Q620C. Equipment builders use it on crane booms, mine-truck bodies, excavator frames and trailer goosenecks that were too heavy in 550 or 620 MPa plate. It is still a QT carbon plate, not a stainless grade and not a pressure-vessel grade.
Quality grade C means the impact test is at 0°C. D is −20°C. E is −40°C. F is −60°C. Q690C is the right letter for temperate fabrication and mild outdoor service. If the drawing shows winter design at −40°C, the letter is E, not C.
The closest European name is EN 10025-6 S690Q. Both are about 690 MPa QT plate tested at 0°C. S690QL is −40°C and lines up with Q690E. S690QL1 is −60°C and lines up with Q690F. On the US side, A514 Grade Q is also 100 ksi / 690 MPa QT structural plate. The books are not the same. Dual mark only when both tables are fully met. See EN 10025-6 steel plate.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q690C from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 16270 Q690C | Confirmed |
| Other search names | Q690C QT plate, Q690C carbon steel plate | Covered |
| Delivery condition | Quenched and tempered | Confirmed |
| Yield, thin plate | 690 MPa min | Confirmed |
| Quality grade | C, impact at 0°C | Confirmed |
| US comparison | ASTM A514, 100 ksi | Comparison, not a swap |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Not the same strength | Q620C or Q800C | Do not substitute |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include S690Q, S690QL and A514 Gr.Q.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Q690C is a low-alloy QT carbon plate. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 690 MPa heats. The certificate shows the elements actually used.
Heat Analysis and Product Analysis — GB/T 16270 Q690C
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.20 | 0.22 |
| Silicon (Si), max | 0.80 | 0.85 |
| Manganese (Mn), max | 1.80 | 1.88 |
| Phosphorus (P), max | 0.025 | 0.030 |
| Sulfur (S), max | 0.015 | 0.018 |
| Copper (Cu), max | 0.50 | 0.55 |
| Chromium (Cr), max | 1.50 | 1.55 |
| Nickel (Ni), max | 2.00 | 2.05 |
| Molybdenum (Mo), max | 0.70 | 0.75 |
| Boron (B), max | 0.005 | 0.006 |
| Vanadium (V), max | 0.12 | 0.13 |
| Niobium (Nb), max | 0.06 | 0.07 |
| Titanium (Ti), max | 0.05 | 0.06 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
Grade C allows a slightly wider phosphorus and sulfur window than grade E or F. That is acceptable at 0°C. It is not a reason to use Q690C on a −40°C drawing. If the file needs product analysis, SHH STEEL prints both columns and the thickness band used for the mechanical test.
Do not treat this chemistry as weathering plate. Do not treat it as S355JR.
Mechanical Properties
Buyers search Q690C mechanical properties, Q690C yield strength, GB/T 16270 Q690C tensile and Q690C impact 0°C.
Tensile and impact — GB/T 16270 Q690C
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 50 mm | 690 MPa | 770–940 MPa | 14% | 0°C, grade C |
| > 50–100 mm | 670 MPa | 770–940 MPa | 14% | 0°C, grade C |
| > 100–150 mm | 630 MPa | as standard table | 14% | 0°C, grade C |
Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 34 J at 0°C. Write a higher energy on the order if the owner requires it.
Yield steps down with thickness. A 690 MPa name on 20 mm plate is not the minimum on a 120 mm flange. 690 MPa is 100 ksi. ASTM A514 uses the same yield number, but the impact and chemistry tables are not identical. SHH STEEL quotes the thickness band on the offer.
Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| Q620C | GB/T 16270 | QT | 620 MPa | 0°C | Lower sister |
| Q690C | GB/T 16270 | QT | 690 MPa | 0°C | This page |
| Q690D | GB/T 16270 | QT | 690 MPa | −20°C | Colder sister |
| Q690E | GB/T 16270 | QT | 690 MPa | −40°C | Colder sister |
| Q800C | GB/T 16270 | QT | 800 MPa | 0°C | Higher sister |
| S690Q | EN 10025-6 | QT | 690 MPa | 0°C | Closest comparison |
| S690QL | EN 10025-6 | QT | 690 MPa | −40°C | No, unless E |
| A514 Gr.Q | ASTM A514 | QT | 690 MPa | Different | Yield match only |
Equivalent Material Grades
There is no official one-to-one substitute for Q690C. What buyers compare is a 690 MPa QT plate tested at 0°C.
In the United States the nearest name is ASTM A514/A514M, including A514 Grade Q. A514 is 100 ksi / 690 MPa minimum yield up to 65 mm, with a lower yield on thicker plate. That matches the Q690C thin-plate number. The chemistry windows, impact rules and grade letters are not the same. A572 Gr.65 is only 65 ksi. ASTM A656 Grade 80 is 80 ksi. SHH STEEL will not stamp A514 on a Q690C certificate unless the purchase order names both books and both tables are met.
The usual European pair is S690Q. S690QL is colder and closer to Q690E. In Japan, SM570 is a welded structural grade and is well below this yield.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q690C | China | GB/T 16270 | Name on this page |
| Q690D / Q690E / Q690F | China | GB/T 16270 | Colder quality letters |
| Q620C | China | GB/T 16270 | Lower yield sister |
| A514 Gr.Q | USA | ASTM A514 | 100 ksi QT yield comparison |
| ASTM A656 Grade 80 | USA | ASTM A656 | 80 ksi, lower yield |
| A572 Gr.65 | USA | ASTM A572 | 65 ksi, lower yield |
| S690Q | Europe | EN 10025-6 | 0°C QT comparison |
| S690QL | Europe | EN 10025-6 | −40°C, closer to Q690E |
Q690C QT Structural Service
Buyers pick Q690C when a welded frame, boom or chassis wants 690 MPa yield, QT delivery and impact at 0°C. Search phrases such as Q690C steel plate, GB/T 16270 Q690C and Q690C QT plate all point here.
It is the wrong plate for a −40°C mine site. That work is Q690E. It is the wrong plate for a 620 MPa file that was sized on Q620C. Raising the grade without a design check can change weld procedure and deflection. It is the wrong plate for a US file that actually names ASTM A514 and a named grade letter. That work stays on A514 unless the order also accepts GB/T 16270. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates. It is the wrong plate for an unpainted weathering girder.
SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade C at 690 MPa.
Weldability
Q690C is weldable QT carbon plate. Carbon is controlled, but the plate has already been quenched and tempered, and many heats use boron. A procedure written for S355JR is not a Q690C procedure. A procedure qualified only on Q620C may be under-matched.
Typical consumables are matching 690 MPa low-hydrogen electrodes or wires, qualified on a QT 690 MPa family. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S690Q is the usual starting point. An A514 procedure is a useful reference after the 0°C coupon is checked.
Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q690C is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 690 MPa yield and the 0°C impact. Exact temperatures stay on the mill process sheet.
Do not order Q690C as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page unless dual mark is written. Stress relief after fabrication, if used, must stay below the original temper temperature.
The certificate lists GB/T 16270 Q690C, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and 0°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S690Q or A514 is available only when both books are fully met.
Dimensions
Usual supply range from SHH STEEL for Q690C QT carbon steel plate:
- Thickness: commonly 8 mm – 80 mm, heavier plate to 100 mm by enquiry
- Width: 1500 mm – 3500 mm
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.
Tolerances
Dimensional limits for Q690C follow GB/T 709 unless the purchase order names another table.
Typical thickness tolerance idea for Q690C QT plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 10 | −0.3 | +0.8 |
| 10 – 20 | −0.4 | +0.9 |
| 20 – 30 | −0.4 | +1.0 |
| 30 – 40 | −0.5 | +1.1 |
| 40 – 50 | −0.5 | +1.2 |
| 50 – 80 | −0.6 | +1.4 |
| 80 – 100 | −0.8 | +1.6 |
Width on 1500–3500 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q690C unless the order says so.
Supplementary Requirements
Q690C already defines 690 MPa yield, QT delivery and 0°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 16270 Q690C. Do not write only Q690C.
Impact. Grade C is 0°C. Write a higher energy if the owner requires it.
US comparison. Write A514 only if dual mark is required and both tables are met.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Heat-treatment record. QT temperatures when the inspector asks.
Identification. Heat number, Q690C, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Construction machinery | Q690C QT booms, frames and bases |
| Mining equipment | Q690C chassis and body plate from SHH STEEL |
| Cranes and port equipment | Q690C webs and flanges |
| Heavy trailers | Q690C goosenecks and longitudinals |
| Comparison vs S690Q | Q690C next to S690Q |
| Comparison vs S690QL | Q690C next to S690QL |
| Comparison vs A514 | Q690C next to A514 Gr.Q |
Q690C is the plate for a 690 MPa QT file tested at 0°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 800 MPa member.
Supply Capability
SHH STEEL sources Q690C from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm, 60 mm, 80 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 35–45 days; 3.2 inspection about 45–60 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q690C that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 690 MPa quench-and-temper route, so the heat carries the 0°C impact without a second upgrade charge.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 35–45 days, 3.2 inspection about 45–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 16270 Q690C, keep the QT route, and do not ship Q620C or a silent A514 stamp as Q690C. We will not change C to E on the certificate to win an order, and we will not treat Q690C as S355. If the drawing needs −40°C, we will move the inquiry to Q690E and keep the price on the right grade.
FAQ
-
What is Q690C steel plate?
- Q690C in GB/T 16270 is quenched-and-tempered carbon structural plate with 690 MPa minimum yield on thin plate and Charpy impact at 0°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q690C the same as Q620C?
- No. Both are QT plate tested at 0°C. Q690C yields at 690 MPa. Q620C yields at 620 MPa.
-
What is the US equivalent of Q690C?
- The nearest comparison is ASTM A514, 100 ksi / 690 MPa QT plate. The books are not identical. A572 Grade 65 and A656 Grade 80 are lower. SHH STEEL does not dual-mark A514 unless both books are met.
-
Is Q690C the same as S690Q?
- They are the usual comparison pair: both are about 690 MPa QT plate tested at 0°C. Dual mark only when both books are fully met. S690QL is colder and closer to Q690E.
-
What thickness can SHH STEEL supply?
- Common rolling is 8 mm to 80 mm. Plate to 100 mm is quoted by enquiry. Yield on plate over 50 mm is lower than the 690 MPa thin-plate number.
-
Can SHH STEEL ship Q690C to the USA, Europe or the Middle East?
- Yes. SHH STEEL quotes FOB Shanghai and CIF to US West, US Gulf, Rotterdam, Jebel Ali, Singapore and other major ports.
-
What is the delivery time for Q690C?
- x-stock about 5–7 days when plate is in yard. Standard QT rolling about 35–45 days. 3.2 inspection about 45–60 days.
-
Can SHH STEEL issue EN 10204 3.2 for Q690C?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS or the inspector named on the order.
Conclusion
Q690C QT carbon steel plate to GB/T 16270 is 690 MPa quenched-and-tempered structural plate with impact at 0°C. The nearest US comparison is ASTM A514, which matches the 100 ksi yield but is not a silent substitute. Whether the inquiry says Q690C, GB/T 16270 Q690C, Q690C QT plate or Q690C carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q690C chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q690C QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.
Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.
Q690C, Q690C steel plate, GB/T 16270 Q690C, Q690C QT plate, Q690C carbon steel plate, Q690C supplier, SHH STEEL