GB/T 1591 Q390ME thermomechanically rolled high-strength low-alloy structural steel plate, 390 MPa yield, −40 °C impact, SHH STEEL

Q390ME TMCP Steel Plate GB/T 1591 Supplier

GB/T 1591 Q390ME is thermomechanical controlled process plate with 390 MPa minimum yield and −40°C impact. SHH STEEL supplies Q390ME plate mill-direct for bridges, cold-region frames and outdoor fabrication that names the M condition. This is not normalized Q390NE.
Keywords
Q390ME, Q390ME steel plate, GB/T 1591 Q390ME, Q390ME TMCP, Q390ME supplier, EN 10025-4 S420ML, ASTM A572 Gr.55, Q390NE, Q390MD
Equivalent Grades:
GB/T 1591 Q390ME / ASTM A572 Gr 55 / EN 10025-4 S355ML (-40℃) / GB Q390E — Material Specification: GB/T 1591 — Delivery: TMCP; -40℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q390ME TMCP Steel Plate GB/T 1591?

Q390ME, also searched as GB/T 1591 Q390ME, Q390ME steel plate, Q390ME TMCP plate and Q390 ME, is the 390 MPa quality-grade-E grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 390 is the thin-plate minimum yield in MPa, M is the delivery letter, and E is the quality letter for Charpy impact at −40°C.

The M is the point of this page. Normalized GB/T 1591 Q390NE has an N. A normalized certificate cannot be stamped ME. Grade B on the TMCP route is GB/T 1591 Q390MB. Grade C is GB/T 1591 Q390MC. Grade D is GB/T 1591 Q390MD. The 355 MPa TMCP sister at the same temperature is GB/T 1591 Q355ME. The full family sits on GB/T 1591. Do not drop a 390 MPa drawing onto a 355 MPa plate, and do not upgrade it to GB/T 1591 Q420NE without a price check.

EN 10025 has no S390 letter. The closest higher TMCP comparison is EN 10025-4 S420ML, tested colder than −20°C. EN 10025-4 S420M is only −20°C. EN 10025-3 S420NL is normalized. On the US side, ASTM A572 Gr.55 is 55 ksi / 380 MPa, one step lower, and it is not an ME twin. JIS G3106 SM520C is the usual Japanese comparison. Dual mark only when both books are fully met. See EN 10025-4 and high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q390ME from first-line structural mills that can actually run the TMCP schedule and hold −40°C impact, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q390ME Confirmed
Other search names Q390ME steel plate, Q390 ME, Q390ME TMCP Covered
Delivery condition Thermomechanical controlled process Confirmed
Yield, ≤ 16 mm 390 MPa min Confirmed
Quality grade E, impact at −40°C Confirmed
Not this page Normalized GB/T 1591 Q390NE Different condition
Warmer TMCP sister GB/T 1591 Q390MD −20°C
EN comparison EN 10025-4 S420ML is higher Not a swap
US comparison ASTM A572 Gr.55 is 380 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q390ND, GB/T 1591 Q355ME and ASTM A572 Gr.55.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q390. Product analysis, when ordered, follows GB/T 222. Q390ME is a microalloyed HSLA plate. Grade E is the tightest cleanliness letter on this TMCP family, because the impact test is at −40°C. Mills may add Nb, V or Ti. The certificate shows the elements actually used. TMCP chemistry is often leaner than a normalized heat of the same yield, because the rolling schedule does part of the grain refinement.

Heat Analysis and Product Analysis — GB/T 1591 Q390ME, TMCP

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.50 0.55
Manganese (Mn), max 1.70 1.80
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.020 0.025
Niobium (Nb), max 0.07 0.08
Vanadium (V), max 0.20 0.22
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.30 0.35
Nickel (Ni), max 0.50 0.55
Copper (Cu), max 0.40 0.45
Molybdenum (Mo), max 0.10 0.11
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than normalized GB/T 1591 Q390NE. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as quenched-and-tempered GB/T 16270 Q460E. A 355 MPa file is GB/T 1591 Q355E, not this grade.

Mechanical Properties

Buyers search Q390ME mechanical properties, Q390ME yield strength, GB/T 1591 Q390ME tensile and Q390ME impact −40°C.

Tensile and impact — GB/T 1591 Q390ME, TMCP

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 390 MPa 490–650 MPa 20% −40°C, grade E
> 16–40 mm 380 MPa 490–650 MPa 20% −40°C, grade E
> 40–63 mm 360 MPa 490–650 MPa 19% −40°C, grade E
> 63–80 mm 350 MPa 490–650 MPa 19% −40°C, grade E
> 80–100 mm 340 MPa 490–650 MPa 19% −40°C, grade E
> 100–150 mm 330 MPa 470–620 MPa 18% −40°C, grade E

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 27 J to 34 J minimum at −40°C, depending on the ordered edition and thickness. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it. Not every TMCP heat will hold E on very thick plate. SHH STEEL confirms the thickness before promising the letter.

Yield steps down with thickness. A 390 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 390 MPa is about 56.5 ksi. ASTM A572 Gr.55 is 55 ksi and is not this book. Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the E letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 1591 Q390NE GB/T 1591-2018 Normalized 390 MPa −40°C Different process
GB/T 1591 Q390MD GB/T 1591-2018 TMCP 390 MPa −20°C Warmer M sister
Q390ME GB/T 1591-2018 TMCP 390 MPa −40°C This page
GB/T 1591 Q355ME GB/T 1591-2018 TMCP 355 MPa −40°C Lower yield
GB/T 1591 Q420NE GB/T 1591-2018 Normalized 420 MPa −40°C Higher yield
EN 10025-4 S420ML EN 10025-4 TMCP 420 MPa −50°C Higher comparison
EN 10025-3 S420NL EN 10025-3 Normalized 420 MPa −50°C Different process
ASTM A572 Gr.55 ASTM A572 As rolled 380 MPa Different Lower yield

A warmer hot-rolled file is GB/T 1591 Q355B. A 460 MPa file is GB/T 1591 Q460E.

Equivalent Material Grades

There is no official one-to-one substitute for Q390ME. What buyers compare is a 390 MPa TMCP plate tested at −40°C.

EN 10025 has no S390. EN 10025-4 S420ML is the higher TMCP comparison and is tested colder. EN 10025-4 S420M is only −20°C. EN 10025-3 S420NL is normalized. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A572 Gr.55 is 55 ksi / 380 MPa. ASTM A572 Gr.50 is 50 ksi and is one step lower. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM520C is the usual comparison. SHH STEEL will not stamp EN 10025-4 S420ML or ASTM A572 Gr.55 on a Q390ME certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q390ME China GB/T 1591-2018 Name on this page
GB/T 1591 Q390NE China GB/T 1591-2018 Normalized, not this page
GB/T 1591 Q390MD China GB/T 1591-2018 TMCP, −20°C
GB/T 1591 Q355ME China GB/T 1591-2018 355 MPa, TMCP
GB/T 1591 Q420E China GB/T 1591-2018 420 MPa, hot rolled
EN 10025-4 S420ML Europe EN 10025-4 Higher TMCP comparison
ASTM A572 Gr.55 USA ASTM A572 55 ksi, lower yield
JIS G3106 SM520C Japan JIS G3106 Usual Japanese comparison

Structural Service

Buyers pick Q390ME when a bridge, building member or welded fabrication wants about 390 MPa yield, a TMCP condition, and impact at −40°C. Search phrases such as Q390ME steel plate and GB/T 1591 Q390ME all point here. The family index is GB/T 1591.

It is the wrong plate when the drawing says normalized. That work is GB/T 1591 Q390NE. It is the wrong plate for a −20°C file. That work is GB/T 1591 Q390MD, and the normalized sister is GB/T 1591 Q390ND. It is the wrong plate for a 0°C file. That work is GB/T 1591 Q390MC. It is the wrong plate for a +20°C file. That work is GB/T 1591 Q390MB. It is the wrong plate for a 355 MPa file. That work is GB/T 1591 Q355ME or GB/T 1591 Q355E. It is the wrong plate for a 420 MPa file. That work is GB/T 1591 Q420NE or GB/T 1591 Q420D. It is the wrong plate for a 460 MPa file. That work is GB/T 1591 Q460NC or GB/T 1591 Q460NE. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade E, and the M condition at 390 MPa.

Weldability

Q390ME is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q390ME. Carbon equivalent on the M route is often lower than normalized GB/T 1591 Q390NE, which helps the root pass, but the TMCP microstructure still needs a qualified procedure. A procedure qualified only at −20°C may miss the −40°C coupon.

Typical consumables are matching 55–60 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 is a useful strength reference after chemistry and the −40°C coupon are checked. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q390ME procedure on GB/T 1591 Q355MB without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q460ND either.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q390ME is thermomechanical controlled process. The plate is not normalized as GB/T 1591 Q390NE.

TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q390ME as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.

The certificate lists GB/T 1591 Q390ME, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-4 S420ML is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q390ME steel plate:

  • Thickness: commonly 8 mm – 60 mm, heavier plate to 80 mm by mill confirmation
  • Width: 1500 mm – 3000 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q390ME follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q390ME plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 60 −0.6 +1.3
60 – 80 −0.7 +1.5

Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q390ME unless the order says so.

Supplementary Requirements

Q390ME already defines 390 MPa yield, TMCP delivery and −40°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q390ME. Do not write only Q390, and do not write Q390NE if the mill must stamp M. The family page is GB/T 1591.

Impact. Grade E is −40°C. Write a higher energy if the owner requires it. Do not expect this result from GB/T 1591 Q390MD.

Delivery condition. Write thermomechanical controlled process. Write GB/T 1591 Q390NE if normalized is required.

EN or US comparison. Write EN 10025-4 S420ML or ASTM A572 Gr.55 only if dual mark is required and both tables are met. Do not treat EN 10025-4 S420M as a −40°C grade.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q390ME, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Cold-region bridges Q390ME webs and flanges from SHH STEEL
Outdoor structures Q390ME columns and base plates tested at −40°C
Construction machinery Q390ME frames where the drawing names M and −40°C
General fabrication Q390ME gussets and connection plates
Comparison vs EN 10025-4 Q390ME next to EN 10025-4 S420ML
Comparison vs ASTM A572 Q390ME next to ASTM A572 Gr.55
Lower yield option GB/T 1591 Q355MF when 355 MPa and −60°C are the file

Q390ME is the plate for a 390 MPa TMCP file tested at −40°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A 460 MPa normalized file is GB/T 1591 Q460ND.

Supply Capability

SHH STEEL sources Q390ME from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm, 60 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an E heat is in yard; standard TMCP with −40°C test about 30–45 days; 3.2 inspection about 40–50 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q390ME that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule and test at −40°C, so the M and the E are both on the certificate.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard ME heat about 30–45 days, 3.2 inspection about 40–50 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q390ME, keep the TMCP route, and do not ship GB/T 1591 Q390NE or GB/T 1591 Q390MD as ME. We will not drop the M to save a cooling cycle, and we will not change E to D to save a cold test. If the drawing only needs −20°C, we will move the inquiry to Q390MD. If the drawing needs 420 MPa, we will move it to GB/T 1591 Q420NC or GB/T 1591 Q420ND.

FAQ

What is Q390ME steel plate?
Q390ME in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 390 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q390ME the same as Q390NE?
No. Both yield at 390 MPa and both are tested at −40°C. Q390NE is normalized. Q390ME is TMCP.
Is Q390ME the same as Q390MD?
No. Both are TMCP. Q390MD is tested at −20°C. Q390ME is tested at −40°C.
Is Q390ME the same as Q355ME?
No. Both are TMCP and both are tested at −40°C. Q355ME is 355 MPa. Q390ME is 390 MPa.
What is the European equivalent of Q390ME?
There is no S390 in EN 10025. EN 10025-4 S420ML is the higher TMCP comparison and is tested colder than −20°C. EN 10025-4 S420M is only −20°C. Dual mark only when both books are fully met.
What is the US equivalent of Q390ME?
There is no official ASTM twin. ASTM A572 Grade 55 is 55 ksi / 380 MPa, slightly lower, and it does not carry an ME letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
What thickness can SHH STEEL supply?
Common supply is 8 mm to 60 mm. Plate to 80 mm is confirmed with the mill before order. Yield on plate over 16 mm is lower than the 390 MPa thin-plate number.

Conclusion

Q390ME steel plate to GB/T 1591 is 390 MPa TMCP structural plate with impact at −40°C. It is not normalized GB/T 1591 Q390NE. EN 10025 has no S390. EN 10025-4 S420ML is a higher TMCP comparison. ASTM A572 Grade 55 is 380 MPa and is not a substitute. Whether the inquiry says Q390ME, GB/T 1591 Q390ME or Q390ME TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q390ME chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q390ME Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition. The grade family is listed on GB/T 1591.

Contact SHH STEEL for mill rolling, −40°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.

Q390ME, Q390ME steel plate, GB/T 1591 Q390ME, Q390ME TMCP, Q390ME supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X