Q390MF TMCP Steel Plate GB/T 1591 Supplier
What is Q390MF TMCP Steel Plate GB/T 1591?
Q390MF, also searched as GB/T 1591 Q390MF, Q390MF steel plate, Q390MF TMCP plate and Q390 MF, is the 390 MPa quality-grade-F grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 390 is the thin-plate minimum yield in MPa, M is the delivery letter, and F is the quality letter for Charpy impact at −60°C.
The M is the point of this page. A normalized certificate cannot be stamped MF. Grade E on the TMCP route is GB/T 1591 Q390ME, tested at −40°C. Grade D is GB/T 1591 Q390MD. Grade C is GB/T 1591 Q390MC. Grade B is GB/T 1591 Q390MB. The normalized −40°C sister is GB/T 1591 Q390NE. The 355 MPa TMCP sister at −60°C is GB/T 1591 Q355MF. The full family sits on GB/T 1591. Do not drop a 390 MPa drawing onto a 355 MPa plate, and do not upgrade it to GB/T 1591 Q420NE without a price check.
EN 10025 has no S390 letter and no −60°C quality letter. The closest higher TMCP comparison is EN 10025-4 S420ML, tested at −50°C. That is colder than S420M, but it is not an F twin. EN 10025-3 S420NL is normalized. On the US side, ASTM A572 Gr.55 is 55 ksi / 380 MPa, one step lower, and it is not an MF twin. JIS G3106 SM520C is the usual Japanese comparison. Dual mark only when both books are fully met. See EN 10025-4 and high strength low alloy plates.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q390MF from first-line structural mills that can actually run the TMCP schedule and hold −60°C impact, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 1591-2018 Q390MF | Confirmed |
| Other search names | Q390MF steel plate, Q390 MF, Q390MF TMCP | Covered |
| Delivery condition | Thermomechanical controlled process | Confirmed |
| Yield, ≤ 16 mm | 390 MPa min | Confirmed |
| Quality grade | F, impact at −60°C | Confirmed |
| Not this page | GB/T 1591 Q390ME | −40°C, not F |
| Not this page | Normalized GB/T 1591 Q390NE | Different condition |
| EN comparison | EN 10025-4 S420ML is −50°C | Not a twin |
| US comparison | ASTM A572 Gr.55 is 380 MPa | Not a twin |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q390ND, GB/T 1591 Q355MF and ASTM A572 Gr.55.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q390. Product analysis, when ordered, follows GB/T 222. Q390MF is a microalloyed HSLA plate. Grade F is the tightest cleanliness letter on this family, because the impact test is at −60°C. Phosphorus and sulfur are tighter than grade E. Mills may add Nb, V or Ti. The certificate shows the elements actually used. TMCP chemistry is often leaner than a normalized heat of the same yield, because the rolling schedule does part of the grain refinement.
Heat Analysis and Product Analysis — GB/T 1591 Q390MF, TMCP
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.18 | 0.20 |
| Silicon (Si), max | 0.50 | 0.55 |
| Manganese (Mn), max | 1.70 | 1.80 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.015 |
| Niobium (Nb), max | 0.07 | 0.08 |
| Vanadium (V), max | 0.20 | 0.22 |
| Titanium (Ti), max | 0.20 | 0.21 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Nickel (Ni), max | 0.70 | 0.75 |
| Copper (Cu), max | 0.40 | 0.45 |
| Molybdenum (Mo), max | 0.10 | 0.11 |
| Nitrogen (N), max | 0.015 | 0.017 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than normalized GB/T 1591 Q390NE. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as quenched-and-tempered GB/T 16270 Q460E. A warmer 355 MPa file is GB/T 1591 Q355C, not this grade.
Mechanical Properties
Buyers search Q390MF mechanical properties, Q390MF yield strength, GB/T 1591 Q390MF tensile and Q390MF impact −60°C.
Tensile and impact — GB/T 1591 Q390MF, TMCP
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 16 mm | 390 MPa | 490–650 MPa | 20% | −60°C, grade F |
| > 16–40 mm | 380 MPa | 490–650 MPa | 20% | −60°C, grade F |
| > 40–63 mm | 360 MPa | 490–650 MPa | 19% | −60°C, grade F |
| > 63–80 mm | 350 MPa | 490–650 MPa | 19% | −60°C, grade F |
| > 80–100 mm | 340 MPa | 490–650 MPa | 19% | −60°C, grade F |
Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 27 J to 34 J minimum at −60°C, depending on the ordered edition and thickness. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it. Not every TMCP heat will hold F on thick plate. SHH STEEL confirms the thickness before promising the letter.
Yield steps down with thickness. A 390 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 390 MPa is about 56.5 ksi. ASTM A572 Gr.55 is 55 ksi and is not this book. Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the F letter.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| GB/T 1591 Q390NE | GB/T 1591-2018 | Normalized | 390 MPa | −40°C | Different process |
| GB/T 1591 Q390ME | GB/T 1591-2018 | TMCP | 390 MPa | −40°C | Warmer M sister |
| Q390MF | GB/T 1591-2018 | TMCP | 390 MPa | −60°C | This page |
| GB/T 1591 Q355MF | GB/T 1591-2018 | TMCP | 355 MPa | −60°C | Lower yield |
| GB/T 1591 Q420NE | GB/T 1591-2018 | Normalized | 420 MPa | −40°C | Higher yield |
| EN 10025-4 S420ML | EN 10025-4 | TMCP | 420 MPa | −50°C | Closest, not a twin |
| EN 10025-3 S420NL | EN 10025-3 | Normalized | 420 MPa | −50°C | Different process |
| ASTM A572 Gr.55 | ASTM A572 | As rolled | 380 MPa | Different | Lower yield |
A warmer TMCP file is GB/T 1591 Q390MD. A 460 MPa file is GB/T 1591 Q460E.
Equivalent Material Grades
There is no official one-to-one substitute for Q390MF. What buyers compare is a 390 MPa TMCP plate tested at −60°C.
EN 10025 has no S390. EN 10025-4 S420ML is the closest higher TMCP comparison, but it stops at −50°C. EN 10025-4 S420M is only −20°C. EN 10025-3 S420NL is normalized. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A572 Gr.55 is 55 ksi / 380 MPa. ASTM A572 Gr.50 is 50 ksi and is one step lower. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM520C is the usual comparison. SHH STEEL will not stamp EN 10025-4 S420ML or ASTM A572 Gr.55 on a Q390MF certificate unless the purchase order names both books and both tables are met.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q390MF | China | GB/T 1591-2018 | Name on this page |
| GB/T 1591 Q390ME | China | GB/T 1591-2018 | TMCP, −40°C |
| GB/T 1591 Q390NE | China | GB/T 1591-2018 | Normalized, −40°C |
| GB/T 1591 Q355MF | China | GB/T 1591-2018 | 355 MPa, −60°C |
| GB/T 1591 Q420E | China | GB/T 1591-2018 | 420 MPa, hot rolled |
| EN 10025-4 S420ML | Europe | EN 10025-4 | TMCP, −50°C, not a twin |
| ASTM A572 Gr.55 | USA | ASTM A572 | 55 ksi, lower yield |
| JIS G3106 SM520C | Japan | JIS G3106 | Usual Japanese comparison |
Structural Service
Buyers pick Q390MF when a bridge, building member or welded fabrication wants about 390 MPa yield, a TMCP condition, and impact at −60°C. Search phrases such as Q390MF steel plate and GB/T 1591 Q390MF all point here. The family index is GB/T 1591.
It is the wrong plate when the drawing says normalized. That work is GB/T 1591 Q390NE if −40°C is enough. It is the wrong plate for a −40°C file. That work is GB/T 1591 Q390ME. It is the wrong plate for a −20°C file. That work is GB/T 1591 Q390MD, and the normalized sister is GB/T 1591 Q390ND. It is the wrong plate for a 0°C file. That work is GB/T 1591 Q390MC. It is the wrong plate for a 355 MPa file. That work is GB/T 1591 Q355MF or GB/T 1591 Q355E. It is the wrong plate for a 420 MPa file. That work is GB/T 1591 Q420NE or GB/T 1591 Q420ND. It is the wrong plate for a 460 MPa file. That work is GB/T 1591 Q460NC or GB/T 1591 Q460NE. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.
SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade F, and the M condition at 390 MPa.
Weldability
Q390MF is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q390MF. Carbon equivalent on the M route is often lower than normalized GB/T 1591 Q390NE, which helps the root pass, but the TMCP microstructure still needs a qualified procedure. A procedure qualified only at −40°C may miss the −60°C coupon.
Typical consumables are matching 55–60 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 is a useful strength reference after chemistry and the −60°C coupon are checked. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.
The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q390MF procedure on GB/T 1591 Q355MB without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q460ND either.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q390MF is thermomechanical controlled process. The plate is not normalized as GB/T 1591 Q390NE.
TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q390MF as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.
The certificate lists GB/T 1591 Q390MF, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and −60°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-4 S420ML is available only when both books are fully met. S420ML does not cover −60°C by itself.
Dimensions
Usual supply range from SHH STEEL for Q390MF steel plate:
- Thickness: commonly 8 mm – 50 mm, heavier plate to 60 mm by mill confirmation
- Width: 1500 mm – 3000 mm, wider by enquiry
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.
Tolerances
Dimensional limits for Q390MF follow GB/T 709 unless the purchase order names EN 10029 or another table.
Typical thickness tolerance idea for Q390MF plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 15 | −0.3 | +0.8 |
| 15 – 25 | −0.4 | +0.9 |
| 25 – 40 | −0.5 | +1.1 |
| 40 – 60 | −0.6 | +1.3 |
Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q390MF unless the order says so.
Supplementary Requirements
Q390MF already defines 390 MPa yield, TMCP delivery and −60°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 1591 Q390MF. Do not write only Q390, and do not write Q390NE if the mill must stamp M and F. The family page is GB/T 1591.
Impact. Grade F is −60°C. Write a higher energy if the owner requires it. Do not expect this result from GB/T 1591 Q390ME.
Delivery condition. Write thermomechanical controlled process. Write GB/T 1591 Q390NE if normalized and −40°C are enough.
EN or US comparison. Write EN 10025-4 S420ML or ASTM A572 Gr.55 only if dual mark is required and both tables are met. S420ML is −50°C, not −60°C.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Identification. Heat number, Q390MF, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Arctic and cold-region bridges | Q390MF webs and flanges from SHH STEEL |
| Outdoor structures | Q390MF columns and base plates tested at −60°C |
| Construction machinery | Q390MF frames where the drawing names M and −60°C |
| General fabrication | Q390MF gussets and connection plates |
| Comparison vs EN 10025-4 | Q390MF next to EN 10025-4 S420ML |
| Comparison vs ASTM A572 | Q390MF next to ASTM A572 Gr.55 |
| Lower yield option | GB/T 1591 Q355ME when 355 MPa is enough |
Q390MF is the plate for a 390 MPa TMCP file tested at −60°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A 460 MPa normalized file is GB/T 1591 Q460ND.
Supply Capability
SHH STEEL sources Q390MF from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when an F heat is in yard; standard TMCP with −60°C test about 35–50 days; 3.2 inspection about 45–55 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q390MF that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule and test at −60°C, so the M and the F are both on the certificate.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard MF heat about 35–50 days, 3.2 inspection about 45–55 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 1591 Q390MF, keep the TMCP route, and do not ship GB/T 1591 Q390NE or GB/T 1591 Q390ME as MF. We will not drop the M to save a cooling cycle, and we will not change F to E to save a cold test. If the drawing only needs −40°C, we will move the inquiry to Q390ME. If the drawing needs 420 MPa, we will move it to GB/T 1591 Q420NC or GB/T 1591 Q420NB.
FAQ
-
What is Q390MF steel plate?
- Q390MF in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 390 MPa minimum yield on thin plate and Charpy impact at −60°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q390MF the same as Q390ME?
- No. Both are TMCP. Q390ME is tested at −40°C. Q390MF is tested at −60°C.
-
Is Q390MF the same as Q390NE?
- No. Q390NE is normalized and tested at −40°C. Q390MF is TMCP and tested at −60°C.
-
Is Q390MF the same as Q355MF?
- No. Both are TMCP and both are tested at −60°C. Q355MF is 355 MPa. Q390MF is 390 MPa.
-
What is the European equivalent of Q390MF?
- There is no official twin. EN 10025-4 S420ML is the closest higher TMCP comparison, and it is tested at −50°C, not −60°C. Dual mark only when both books are fully met.
-
What is the US equivalent of Q390MF?
- There is no official ASTM twin. ASTM A572 Grade 55 is 55 ksi / 380 MPa, slightly lower, and it does not carry an MF letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
-
What thickness can SHH STEEL supply?
- Common supply is 8 mm to 50 mm. Plate to 60 mm is confirmed with the mill before order. Yield on plate over 16 mm is lower than the 390 MPa thin-plate number.
Conclusion
Q390MF steel plate to GB/T 1591 is 390 MPa TMCP structural plate with impact at −60°C. It is not normalized GB/T 1591 Q390NE and not −40°C GB/T 1591 Q390ME. EN 10025 has no S390. EN 10025-4 S420ML is a higher TMCP comparison tested at −50°C. ASTM A572 Grade 55 is 380 MPa and is not a substitute. Whether the inquiry says Q390MF, GB/T 1591 Q390MF or Q390MF TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q390MF chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q390MF Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition and the F letter. The grade family is listed on GB/T 1591.
Contact SHH STEEL for mill rolling, −60°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.
Q390MF, Q390MF steel plate, GB/T 1591 Q390MF, Q390MF TMCP, Q390MF supplier, SHH STEEL