GB/T 14976 07Cr18Ni11Nb Seamless Stainless Steel Pipe
What is GB/T 14976 07Cr18Ni11Nb Seamless Stainless Steel Pipe
GB/T 14976 covers seamless stainless pipe for fluid service — cold-drawn or hot-finished — with hydrostatic proof and optional Annex A cryogenic or Annex B oxygen extras. Inside that standard, 07Cr18Ni11Nb is filed as austenitic. GB/T 14976 07Cr18Ni11Nb is ordered when Chinese hot-fluid specs need Nb stabilisation and a carbon floor in one seamless mark.
From pierce/extrude/draw through marking and bundle protection, SHH STEEL can produce GB/T 14976 07Cr18Ni11Nb for the sizes and tests on your RFQ. Application sketch: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 07Cr18Ni11Nb before production starts. Size practice for 07Cr18Ni11Nb remains W-H for heavy hot-service walls; density 8.03 for weight calcs.
On the floor people shorten marks; in QA they must not. 07Cr18Ni11Nb under GB/T 14976 carries specific Table 2 windows and Table 3 floors that a loose “347H” note will not enforce. Caution: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 07Cr18Ni11Nb so informal alias language cannot reopen the carbon or molybdenum window after melt. Application context for 07Cr18Ni11Nb stays hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Cryogenic Annex A and oxygen Annex B sit in 14976’s special-requirements clause; still match the alloy to the medium. For 07Cr18Ni11Nb, that means: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. Nearby marks: 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10, 07Cr17Ni12Mo2. Document the medium, design temperature, and weld map beside the 07Cr18Ni11Nb line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for 07Cr18Ni11Nb remains W-H for heavy hot-service walls; density 8.03 for weight calcs.
Inside this GB/T 14976 series, compare GB/T 14976 06Cr18Ni11Nb, GB/T 14976 07Cr19Ni11Ti, GB/T 14976 07Cr19Ni10, GB/T 14976 07Cr17Ni12Mo2. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP347H.
For 07Cr18Ni11Nb dual-form buying, the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 07Cr18Ni11Nb. See also the GB/T 4237 hub for related plate designations. Quote 07Cr18Ni11Nb pipe and plate under separate line items.
Chemical Composition of GB/T 14976 07Cr18Ni11Nb
For 07Cr18Ni11Nb, the melt ticket has to show Table 2 compliance — C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 9.00–12.00, Cr 17.00–19.00, Nb 8C–1.10. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters.
Where Mo, Cu, Ti, Nb, Al or N appear, they are intentional levers for 07Cr18Ni11Nb, not optional marketing. Confirm them on the MTC line-by-line. Role: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 07Cr18Ni11Nb before the order is acknowledged. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters.
| Grade | C | Si | Mn | P | S | Ni | Cr | Nb |
|---|---|---|---|---|---|---|---|---|
| 07Cr18Ni11Nb | 0.04–0.10 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 9.00–12.00 | 17.00–19.00 | 8C–1.10 |
Mechanical Properties of GB/T 14976 07Cr18Ni11Nb
Do not confuse Table 3 pipe tensile floors with plate or tube standards that share the 347H / UNS S34779 alias. For 07Cr18Ni11Nb under 14976 expect Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%, verified per heat/lot rules. Tensile sampling follows the batch rules for the ordered test unit of 07Cr18Ni11Nb, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 07Cr18Ni11Nb | 520 | 205 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 07Cr18Ni11Nb. Heat treatment (Table 1): cold-drawn ≥1100 °C; hot-finished ≥1050 °C; water or rapid cool. Density 8.03 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 07Cr18Ni11Nb
SHH STEEL can produce 07Cr18Ni11Nb as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 07Cr18Ni11Nb; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Application context for 07Cr18Ni11Nb stays hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Cold-drawn austenitic 07Cr18Ni11Nb may ship cold-worked only by written agreement (6.3.3) with negotiated bend and tensile rules — silence means heat-treated delivery. Heat treatment: cold-drawn ≥1100 °C; hot-finished ≥1050 °C; water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.
Hydrostatic testing is mandatory; ultrasonic or eddy-current may replace hydro per 7.3.3 when agreed. Manufacture stays seamless-only. Size: W-H for heavy hot-service walls; density 8.03 for weight calcs. Hydrostatic pressure or NDT class for 07Cr18Ni11Nb is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. This paragraph is locked to 07Cr18Ni11Nb duty: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines.
Dimensions and Tolerances for GB/T 14976 07Cr18Ni11Nb
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 07Cr18Ni11Nb. Duty: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. Tolerance class (PA/PC) follows the precision ordered for 07Cr18Ni11Nb, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 07Cr18Ni11Nb: 347H-class fillers; protect Nb and carbon balance in the joint.
Ovality and wall unevenness, when ordered, stay within 80% of the respective OD and wall tolerances. Size reminder: W-H for heavy hot-service walls; density 8.03 for weight calcs. Fixed lengths and multiple cut lengths for 07Cr18Ni11Nb are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 07Cr18Ni11Nb duty: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines.
Equivalent Grades for GB/T 14976 07Cr18Ni11Nb
Lock 07Cr18Ni11Nb on the PO when the datasheet owner wants GB/T 14976 seamless stainless fluid-transport pipe. Commercial talk as 347H / UNS S34779 is fine in emails; mill paperwork must still show GB/T 14976 07Cr18Ni11Nb. Application framing: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 07Cr18Ni11Nb | Governing pipe grade for this page |
| Commercial / UNS (body only) | 347H / UNS S34779 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
When the service outgrows 07Cr18Ni11Nb, move to a sister rather than stretching the alias: GB/T 14976 06Cr18Ni11Nb, GB/T 14976 07Cr19Ni11Ti, GB/T 14976 07Cr19Ni10, GB/T 14976 07Cr17Ni12Mo2. Apps context: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry. Full list under GB/T 14976. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (07Cr18Ni11Nb).
Heat Treatment and Delivery Condition for GB/T 14976 07Cr18Ni11Nb
Hot-finished austenitic seamless may use in-line rapid cool inside the Table 1 band under 6.3.2 unless the purchaser forbids it. Confirm for 07Cr18Ni11Nb. Band: cold-drawn ≥1100 °C; hot-finished ≥1050 °C; water or rapid cool. Recorded furnace charts for 07Cr18Ni11Nb should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 07Cr18Ni11Nb caution visible here: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route.
Grain-size or inclusion testing under 7.8.3 applies only when ordered — state any extra metallographic demand on the PO for 07Cr18Ni11Nb. Field heat treatment of 07Cr18Ni11Nb after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 07Cr18Ni11Nb: 347H-class fillers; protect Nb and carbon balance in the joint.
Corrosion Resistance of GB/T 14976 07Cr18Ni11Nb
Medium, temperature, crevice geometry and weld condition decide whether 07Cr18Ni11Nb is enough. Summary: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters. Escalate via sisters 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10, 07Cr17Ni12Mo2 when coupons fail. Coupon orientation, weld condition, and surface finish for 07Cr18Ni11Nb belong in the corrosion test order so annex results can be compared to the installed spool honestly. Application context for 07Cr18Ni11Nb stays hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 07Cr18Ni11Nb. Corrosion framing: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 07Cr18Ni11Nb rather than relying on wall thickness alone. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters.
Applications of GB/T 14976 07Cr18Ni11Nb Seamless Pipe
From utility rooms to process racks, 07Cr18Ni11Nb shows up wherever Chinese fluid specs want austenitic seamless behaviour. Use list: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry. Spool fabricators should copy 07Cr18Ni11Nb onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 07Cr18Ni11Nb duty: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines.
If the only reason for 07Cr18Ni11Nb is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route. Commissioning teams benefit when the as-built dossier repeats 07Cr18Ni11Nb beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 07Cr18Ni11Nb stays hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Weldability of GB/T 14976 07Cr18Ni11Nb
Automatic mill welding is outside GB/T 14976; manual and automatic field welds must still respect 07Cr18Ni11Nb chemistry. Guidance: 347H-class fillers; protect Nb and carbon balance in the joint. Procedure qualification for 07Cr18Ni11Nb should use the same product form and wall class as production, including the seamless finish that will ship. Application context for 07Cr18Ni11Nb stays hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 07Cr18Ni11Nb are procedure items, not afterthoughts. Guidance: 347H-class fillers; protect Nb and carbon balance in the joint. Consumable lot control and shielding-gas notes for 07Cr18Ni11Nb stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 07Cr18Ni11Nb: 347H-class fillers; protect Nb and carbon balance in the joint.
Surface Finishes for GB/T 14976 07Cr18Ni11Nb
07Cr18Ni11Nb under GB/T 14976 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (07Cr18Ni11Nb).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
When 07Cr18Ni11Nb ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Inspection and Testing for GB/T 14976 07Cr18Ni11Nb
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GB/T 14976 for 07Cr18Ni11Nb. Sampling plans for 07Cr18Ni11Nb keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 07Cr18Ni11Nb caution visible here: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route.
Dimensional inspection against Table 4/5 tolerances closes the lot. Failures retest per GB/T 2102 — they are not silently shipped. Role: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. Non-conforming 07Cr18Ni11Nb lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 07Cr18Ni11Nb remains W-H for heavy hot-service walls; density 8.03 for weight calcs.
Packaging and Shipping for GB/T 14976 07Cr18Ni11Nb
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 07Cr18Ni11Nb stays visible on outer tags. Oxygen Annex B adds oil-free packing language when invoked. Bundle tickets for 07Cr18Ni11Nb repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 07Cr18Ni11Nb remains W-H for heavy hot-service walls; density 8.03 for weight calcs.
Container loading plans should keep heavy walls from crushing thin-wall 07Cr18Ni11Nb layers. Desiccant and wrap choices for 07Cr18Ni11Nb follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 07Cr18Ni11Nb: 347H-class fillers; protect Nb and carbon balance in the joint Desiccant and wrap choices for 07Cr18Ni11Nb follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Use-case reminder for 07Cr18Ni11Nb: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 07Cr18Ni11Nb. Claims handling for 07Cr18Ni11Nb starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 07Cr18Ni11Nb stays hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 07Cr18Ni11Nb as a governed product grade, not a marketing synonym for 347H / UNS S34779. Role: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. SHH STEEL can produce and supply 07Cr18Ni11Nb against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 07Cr18Ni11Nb enquiry sizes and document packs are already exercised on prior Chinese-spec orders. Use: hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry. Ask for a written acknowledgement that names 07Cr18Ni11Nb, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 07Cr18Ni11Nb to that written scope.
Supply Capability
Capability framing for 07Cr18Ni11Nb: Chinese-spec seamless fluid pipe, W-C/W-H manufacture, documented heats. Caution remains: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 07Cr18Ni11Nb when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 07Cr18Ni11Nb (S34779) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 07Cr18Ni11Nb change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. SHH STEEL can supply alternate walls and precision classes for 07Cr18Ni11Nb once the design pressure and corrosion allowance are clear.
Repeat orders for 07Cr18Ni11Nb go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. SHH STEEL can produce trial lengths of 07Cr18Ni11Nb for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of 07Cr18Ni11Nb for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside 07Cr18Ni11Nb: Nb stabilisation plus carbon floor for hot duty; aqueous chloride process still may want Mo sisters.
FAQ
-
What is GB/T 14976 07Cr18Ni11Nb seamless stainless steel pipe used for?
- GB/T 14976 07Cr18Ni11Nb is seamless stainless pipe for fluid transport — hot process headers, heat-recovery fluid piping, and high-temperature transfer written to 347H-class chemistry. Role summary: controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. It is a Chinese product standard grade (S34779), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 07Cr18Ni11Nb seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr18Ni11Nb when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 07Cr18Ni11Nb?
- 07Cr18Ni11Nb is delivered solution annealed under GB/T 14976. Table 1 reference: cold-drawn ≥1100 °C; hot-finished ≥1050 °C; water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 07Cr18Ni11Nb so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 07Cr18Ni11Nb compare with sister grades 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10?
- 07Cr18Ni11Nb is filed as austenitic. Typical sisters on the same RFQ are 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10. Design caution: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 07Cr18Ni11Nb?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 347H / UNS S34779 the same as ordering 07Cr18Ni11Nb?
- No. 347H / UNS S34779 is a commercial / UNS cross-walk for body text (unified S34779). The purchase order should lock GB/T 14976 and 07Cr18Ni11Nb so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 07Cr18Ni11Nb?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr18Ni11Nb within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-H for heavy hot-service walls; density 8.03 for weight calcs. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 07Cr18Ni11Nb be welded on site?
- Shop guidance: 347H-class fillers; protect Nb and carbon balance in the joint. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route
-
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr18Ni11Nb?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: IGC exempt under 7.5; cold-drawn HT ≥1100 °C vs hot-finished ≥1050 °C — match certificate to manufacture route Sister pointers: 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 07Cr18Ni11Nb with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 07Cr18Ni11Nb does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 07Cr18Ni11Nb so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 07Cr18Ni11Nb?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr18Ni11Nb when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 07Cr18Ni11Nb is seamless stainless steel pipe for fluid transport — controlled-carbon Nb-stabilised austenitic seamless pipe for elevated-temperature fluid lines. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr18Ni11Nb, 07Cr19Ni11Ti, 07Cr19Ni10. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.