GB/T 14976 06Cr19Ni10N Seamless Stainless Steel Pipe
What is GB/T 14976 06Cr19Ni10N Seamless Stainless Steel Pipe
GB/T 14976 covers seamless stainless pipe for fluid service — cold-drawn or hot-finished — with hydrostatic proof and optional Annex A cryogenic or Annex B oxygen extras. Inside that standard, 06Cr19Ni10N is filed as austenitic. If the stress calculation outgrew 06Cr19Ni10 but the medium still does not justify molybdenum, GB/T 14976 06Cr19Ni10N is the governed Chinese answer.
From pierce/extrude/draw through marking and bundle protection, SHH STEEL can produce GB/T 14976 06Cr19Ni10N for the sizes and tests on your RFQ. Application sketch: elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr19Ni10N before production starts. Corrosion framing beside 06Cr19Ni10N: aqueous behaviour tracks 06Cr19Ni10; nitrogen is for strength, not PREN marketing.
On the floor people shorten marks; in QA they must not. 06Cr19Ni10N under GB/T 14976 carries specific Table 2 windows and Table 3 floors that a loose “304N” note will not enforce. Caution: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates.
Cryogenic Annex A and oxygen Annex B sit in 14976’s special-requirements clause; still match the alloy to the medium. For 06Cr19Ni10N, that means: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. Nearby marks: 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N, 06Cr19Ni9NbN. Document the medium, design temperature, and weld map beside the 06Cr19Ni10N line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for 06Cr19Ni10N stays elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N.
Inside this GB/T 14976 series, compare 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N, 06Cr19Ni9NbN. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): A312 TP304.
Chemical Composition of GB/T 14976 06Cr19Ni10N
For 06Cr19Ni10N, the melt ticket has to show Table 2 compliance — C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00, N 0.10–0.16. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: aqueous behaviour tracks 06Cr19Ni10; nitrogen is for strength, not PREN marketing.
Where Mo, Cu, Ti, Nb, Al or N appear, they are intentional levers for 06Cr19Ni10N, not optional marketing. Confirm them on the MTC line-by-line. Role: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr19Ni10N before the order is acknowledged. Application context for 06Cr19Ni10N stays elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N.
| Grade | C | Si | Mn | P | S | Ni | Cr | N |
|---|---|---|---|---|---|---|---|---|
| 06Cr19Ni10N | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 8.00–11.00 | 18.00–20.00 | 0.10–0.16 |
Mechanical Properties of GB/T 14976 06Cr19Ni10N
Do not confuse Table 3 pipe tensile floors with plate or tube standards that share the 304N / UNS S30458 alias. For 06Cr19Ni10N under 14976 expect Rm min 550 MPa, Rp0.2 min 275 MPa, elongation longitudinal min 35% / transverse min 30%, verified per heat/lot rules. Tensile sampling follows the batch rules for the ordered test unit of 06Cr19Ni10N, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Application context for 06Cr19Ni10N stays elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 06Cr19Ni10N | 550 | 275 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 06Cr19Ni10N. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.93 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 06Cr19Ni10N
Seamless is not optional wording for 06Cr19Ni10N: clause 6.2 limits manufacture to W-C or W-H seamless routes. Pick W-C when OD precision and surface finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 14976 line item. Seamless W-C and W-H options remain available for 06Cr19Ni10N; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Keep the 06Cr19Ni10N caution visible here: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates.
Cold-drawn austenitic 06Cr19Ni10N may ship cold-worked only by written agreement (6.3.3) with negotiated bend and tensile rules — silence means heat-treated delivery. Heat treatment: 1010–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.
Hydrostatic testing is mandatory; ultrasonic or eddy-current may replace hydro per 7.3.3 when agreed. Manufacture stays seamless-only. Size: W-H or W-C per wall; mid-to-large OD under GB/T 17395 with PA/PC tolerance as ordered. Hydrostatic pressure or NDT class for 06Cr19Ni10N is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 06Cr19Ni10N caution visible here: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates.
Dimensions and Tolerances for GB/T 14976 06Cr19Ni10N
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 06Cr19Ni10N. Duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. Tolerance class (PA/PC) follows the precision ordered for 06Cr19Ni10N, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10.
Ovality and wall unevenness, when ordered, stay within 80% of the respective OD and wall tolerances. Size reminder: W-H or W-C per wall; mid-to-large OD under GB/T 17395 with PA/PC tolerance as ordered. Fixed lengths and multiple cut lengths for 06Cr19Ni10N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10.
Equivalent Grades for GB/T 14976 06Cr19Ni10N
Cross-references help sourcing 06Cr19Ni10N, but they do not replace the GB/T 14976 grade line on the enquiry. Family framing here is austenitic; delivery practice from the crib is “solution annealed”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (06Cr19Ni10N).
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 06Cr19Ni10N | Governing pipe grade for this page |
| Commercial / UNS (body only) | 304N / UNS S30458 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Sister pages worth reading beside 06Cr19Ni10N: 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N, 06Cr19Ni9NbN. Duty locked here: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. Any EN or ASTM designation above is a starting point for comparison, not a substitute grade on the GB/T 14976 certificate. Series hub: GB/T 14976.
Heat Treatment and Delivery Condition for GB/T 14976 06Cr19Ni10N
Hot-finished austenitic seamless may use in-line rapid cool inside the Table 1 band under 6.3.2 unless the purchaser forbids it. Confirm for 06Cr19Ni10N. Band: 1010–1150 °C, water or rapid cool. Recorded furnace charts for 06Cr19Ni10N should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 06Cr19Ni10N: 308/308L fillers with LN-aware procedures; control heat input when carbon sits mid-window.
Grain-size or inclusion testing under 7.8.3 applies only when ordered — state any extra metallographic demand on the PO for 06Cr19Ni10N. Field heat treatment of 06Cr19Ni10N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 06Cr19Ni10N: 308/308L fillers with LN-aware procedures; control heat input when carbon sits mid-window.
Corrosion Resistance of GB/T 14976 06Cr19Ni10N
Medium, temperature, crevice geometry and weld condition decide whether 06Cr19Ni10N is enough. Summary: aqueous behaviour tracks 06Cr19Ni10; nitrogen is for strength, not PREN marketing. Escalate via sisters 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N, 06Cr19Ni9NbN when coupons fail. Coupon orientation, weld condition, and surface finish for 06Cr19Ni10N belong in the corrosion test order so annex results can be compared to the installed spool honestly. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 06Cr19Ni10N. Corrosion framing: aqueous behaviour tracks 06Cr19Ni10; nitrogen is for strength, not PREN marketing. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr19Ni10N rather than relying on wall thickness alone. Size practice for 06Cr19Ni10N remains W-H or W-C per wall; mid-to-large OD under GB/T 17395 with PA/PC tolerance as ordered.
Applications of GB/T 14976 06Cr19Ni10N Seamless Pipe
From utility rooms to process racks, 06Cr19Ni10N shows up wherever Chinese fluid specs want austenitic seamless behaviour. Use list: elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N. Spool fabricators should copy 06Cr19Ni10N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 06Cr19Ni10N caution visible here: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates.
If the only reason for 06Cr19Ni10N is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates. Commissioning teams benefit when the as-built dossier repeats 06Cr19Ni10N beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 06Cr19Ni10N: aqueous behaviour tracks 06Cr19Ni10; nitrogen is for strength, not PREN marketing.
Weldability of GB/T 14976 06Cr19Ni10N
Automatic mill welding is outside GB/T 14976; manual and automatic field welds must still respect 06Cr19Ni10N chemistry. Guidance: 308/308L fillers with LN-aware procedures; control heat input when carbon sits mid-window. Procedure qualification for 06Cr19Ni10N should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr19Ni10N caution visible here: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 06Cr19Ni10N are procedure items, not afterthoughts. Guidance: 308/308L fillers with LN-aware procedures; control heat input when carbon sits mid-window. Consumable lot control and shielding-gas notes for 06Cr19Ni10N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10.
Surface Finishes for GB/T 14976 06Cr19Ni10N
Surface condition for 06Cr19Ni10N is part of the pipe identity under GB/T 14976. Order annealed/pickled as default HX or process supply, then add bright anneal or polish only with OD/ID scope named. Keep caution visible: higher proof stress does not cancel the 0. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (06Cr19Ni10N).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
SHH STEEL sequences pickle, optional passivation, and any agreed polish for 06Cr19Ni10N after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long pipe life in the field. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (06Cr19Ni10N).
Inspection and Testing for GB/T 14976 06Cr19Ni10N
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GB/T 14976 for 06Cr19Ni10N. Sampling plans for 06Cr19Ni10N keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 06Cr19Ni10N remains W-H or W-C per wall; mid-to-large OD under GB/T 17395 with PA/PC tolerance as ordered.
Dimensional inspection against Table 4/5 tolerances closes the lot. Failures retest per GB/T 2102 — they are not silently shipped. Role: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. Non-conforming 06Cr19Ni10N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 06Cr19Ni10N duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10.
Packaging and Shipping for GB/T 14976 06Cr19Ni10N
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 06Cr19Ni10N stays visible on outer tags. Oxygen Annex B adds oil-free packing language when invoked. Bundle tickets for 06Cr19Ni10N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 06Cr19Ni10N stays elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N.
Container loading plans should keep heavy walls from crushing thin-wall 06Cr19Ni10N layers. Desiccant and wrap choices for 06Cr19Ni10N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 06Cr19Ni10N stays elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 06Cr19Ni10N. Claims handling for 06Cr19Ni10N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr19Ni10N remains W-H or W-C per wall; mid-to-large OD under GB/T 17395 with PA/PC tolerance as ordered.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 06Cr19Ni10N as a governed product grade, not a marketing synonym for 304N / UNS S30458. Role: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. SHH STEEL can produce and supply 06Cr19Ni10N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 06Cr19Ni10N enquiry sizes and document packs are already exercised on prior Chinese-spec orders. Use: elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N. Ask for a written acknowledgement that names 06Cr19Ni10N, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr19Ni10N to that written scope.
Supply Capability
Capability framing for 06Cr19Ni10N: Chinese-spec seamless fluid pipe, W-C/W-H manufacture, documented heats. Caution remains: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr19Ni10N when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 06Cr19Ni10N (S30458) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 06Cr19Ni10N change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. SHH STEEL can supply alternate walls and precision classes for 06Cr19Ni10N once the design pressure and corrosion allowance are clear.
Repeat orders for 06Cr19Ni10N go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. SHH STEEL can produce trial lengths of 06Cr19Ni10N for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GB/T 14976 06Cr19Ni10N seamless stainless steel pipe used for?
- GB/T 14976 06Cr19Ni10N is seamless stainless pipe for fluid transport — elevated design-pressure utility and process headers, rack piping with thinner walls chasing weight, and Chinese fluid BOMs that call 304N. Role summary: nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. It is a Chinese product standard grade (S30458), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 06Cr19Ni10N seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr19Ni10N when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 06Cr19Ni10N?
- 06Cr19Ni10N is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr19Ni10N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr19Ni10N compare with sister grades 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N?
- 06Cr19Ni10N is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N. Design caution: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr19Ni10N?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 304N / UNS S30458 the same as ordering 06Cr19Ni10N?
- No. 304N / UNS S30458 is a commercial / UNS cross-walk for body text (unified S30458). The purchase order should lock GB/T 14976 and 06Cr19Ni10N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 06Cr19Ni10N?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr19Ni10N within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-H or W-C per wall; mid-to-large OD under GB/T 17395 with PA/PC tolerance as ordered. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 06Cr19Ni10N be welded on site?
- Shop guidance: 308/308L fillers with LN-aware procedures; control heat input when carbon sits mid-window. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr19Ni10N?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: higher proof stress does not cancel the 0.08% carbon sensitisation caution on corrosive as-welded joints — consider 022Cr19Ni10N when welding dominates Sister pointers: 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 06Cr19Ni10N with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr19Ni10N does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr19Ni10N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 06Cr19Ni10N?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr19Ni10N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 06Cr19Ni10N is seamless stainless steel pipe for fluid transport — nitrogen-strengthened standard-carbon 18-8 seamless pipe for fluid lines that need higher proof stress than 06Cr19Ni10. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni10, 022Cr19Ni10N, 06Cr17Ni12Mo2N. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.