GB/T 14976 06Cr18Ni11Nb Seamless Stainless Steel Pipe
What is GB/T 14976 06Cr18Ni11Nb Seamless Stainless Steel Pipe
Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 06Cr18Ni11Nb is the Table 2/3 Chinese grade name for this austenitic chemistry (S34778). GB/T 14976 06Cr18Ni11Nb is the Chinese 347 seamless fluid mark — Nb on the melt, not a hope that 06Cr18Ni11Ti paperwork will be accepted.
Mill path for 06Cr18Ni11Nb: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs.
Body text may mention 347 / UNS S34778 (unified S34778) for cross-reference, but the H1 and order line stay on 06Cr18Ni11Nb. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review.
Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10, 06Cr17Ni12Mo2Ti before stretching surface finish or wall alone. Duty thread: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium. Document the medium, design temperature, and weld map beside the 06Cr18Ni11Nb line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to 06Cr18Ni11Nb: 347 fillers; control heat input to protect Nb carbides.
Inside this GB/T 14976 series, compare GB/T 14976 07Cr18Ni11Nb, GB/T 14976 06Cr18Ni11Ti, GB/T 14976 022Cr19Ni10, GB/T 14976 06Cr17Ni12Mo2Ti. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP347.
Chemical Composition of GB/T 14976 06Cr18Ni11Nb
Table 2 sets the melt limits for 06Cr18Ni11Nb. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 9.00–12.00, Cr 17.00–19.00, Nb 10C–1.10. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 347 / UNS S34778. Every ladle analysis for 06Cr18Ni11Nb is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Application context for 06Cr18Ni11Nb stays chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs.
The composition table below is the cast window SHH STEEL quotes against for 06Cr18Ni11Nb. Edition framing is GB/T 14976-2025. Use thread: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr18Ni11Nb before the order is acknowledged. This paragraph is locked to 06Cr18Ni11Nb duty: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium.
| Grade | C | Si | Mn | P | S | Ni | Cr | Nb |
|---|---|---|---|---|---|---|---|---|
| 06Cr18Ni11Nb | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 9.00–12.00 | 17.00–19.00 | 10C–1.10 |
Mechanical Properties of GB/T 14976 06Cr18Ni11Nb
Table 3 mechanical acceptance for 06Cr18Ni11Nb: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 06Cr18Ni11Nb. Tensile sampling follows the batch rules for the ordered test unit of 06Cr18Ni11Nb, and retests follow GB/T 2102 when a result sits under the Table 3 floor. This paragraph is locked to 06Cr18Ni11Nb duty: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 06Cr18Ni11Nb | 520 | 205 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 06Cr18Ni11Nb. Heat treatment (Table 1): 920–1150 °C, water or rapid cool. Density 8.03 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 06Cr18Ni11Nb
For 06Cr18Ni11Nb, the mill path is pierce/extrude/draw — never ERW or automatic-arc under GB/T 14976. Delivery is heat-treated and pickled unless overall ground/bored or bright protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Seamless W-C and W-H options remain available for 06Cr18Ni11Nb; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Weld-shop note tied to 06Cr18Ni11Nb: 347 fillers; control heat input to protect Nb carbides.
After forming, 06Cr18Ni11Nb receives Table 1 treatment — 920–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs.
Marking carries the grade 06Cr18Ni11Nb, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1. Weld thread for fabricator joints: 347 fillers; control heat input to protect Nb carbides. Hydrostatic pressure or NDT class for 06Cr18Ni11Nb is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for 06Cr18Ni11Nb remains W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1.
Dimensions and Tolerances for GB/T 14976 06Cr18Ni11Nb
Dimensional order lines for 06Cr18Ni11Nb should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. Tolerance class (PA/PC) follows the precision ordered for 06Cr18Ni11Nb, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 06Cr18Ni11Nb: Nb stabilisation resists weld decay similarly to Ti grades; chloride ranking remains Mo-free austenitic.
OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review. Fixed lengths and multiple cut lengths for 06Cr18Ni11Nb are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr18Ni11Nb duty: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium.
Equivalent Grades for GB/T 14976 06Cr18Ni11Nb
Under GB/T 14976, 06Cr18Ni11Nb is the governing seamless stainless fluid-transport pipe designation on this page. Commercial shorthand such as 347 / UNS S34778 helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GB/T 14976 06Cr18Ni11Nb line. ASTM A312 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 06Cr18Ni11Nb | Governing pipe grade for this page |
| Commercial / UNS (body only) | 347 / UNS S34778 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 347 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare GB/T 14976 07Cr18Ni11Nb, GB/T 14976 06Cr18Ni11Ti, GB/T 14976 022Cr19Ni10, GB/T 14976 06Cr17Ni12Mo2Ti before swapping marks for medium or temperature. Confirm chemistry windows on the 06Cr18Ni11Nb MTC before dual-cert claims. Hub: GB/T 14976. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr18Ni11Nb).
For 06Cr18Ni11Nb, vertical navigation stays form-specific — tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 4237 06Cr18Ni11Nb. Do not stretch a 06Cr18Ni11Nb pipe certificate onto plate.
Heat Treatment and Delivery Condition for GB/T 14976 06Cr18Ni11Nb
Mill heat treatment for 06Cr18Ni11Nb: 920–1150 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 06Cr18Ni11Nb should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 06Cr18Ni11Nb: 347 fillers; control heat input to protect Nb carbides.
Certificate wording for 06Cr18Ni11Nb should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. Field heat treatment of 06Cr18Ni11Nb after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr18Ni11Nb: Nb stabilisation resists weld decay similarly to Ti grades; chloride ranking remains Mo-free austenitic.
Corrosion Resistance of GB/T 14976 06Cr18Ni11Nb
Nb stabilisation resists weld decay similarly to Ti grades; chloride ranking remains Mo-free austenitic Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni11Nb unless the mark is one of the four carbon-floor exemptions.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 06Cr18Ni11Nb honestly against 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10, 06Cr17Ni12Mo2Ti. Role: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr18Ni11Nb rather than relying on wall thickness alone. Size practice for 06Cr18Ni11Nb remains W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1.
Applications of GB/T 14976 06Cr18Ni11Nb Seamless Pipe
Typical BOM language pairs GB/T 14976 06Cr18Ni11Nb with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. Spool fabricators should copy 06Cr18Ni11Nb onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 06Cr18Ni11Nb remains W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1.
Spell 06Cr18Ni11Nb on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10, 06Cr17Ni12Mo2Ti. Commissioning teams benefit when the as-built dossier repeats 06Cr18Ni11Nb beside heat numbers, linking isometric revisions to the same mill certificates. Keep the 06Cr18Ni11Nb caution visible here: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review.
Weldability of GB/T 14976 06Cr18Ni11Nb
Weldability of 06Cr18Ni11Nb follows austenitic practice. Filler/shop note: 347 fillers; control heat input to protect Nb carbides. Caution: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review. Procedure qualification for 06Cr18Ni11Nb should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr18Ni11Nb caution visible here: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review.
For corrosive as-welded duty on 06Cr18Ni11Nb, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 347 fillers; control heat input to protect Nb carbides. Consumable lot control and shielding-gas notes for 06Cr18Ni11Nb stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 06Cr18Ni11Nb remains W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1.
Surface Finishes for GB/T 14976 06Cr18Ni11Nb
Iron-free handling after pickle matters for 06Cr18Ni11Nb — carbon-steel strapping stains show up later as rust blooms on finished pipe. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Apps: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Reject grinding burns, embedded free iron, and unrepaired undercut on 06Cr18Ni11Nb before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GB/T 14976 for this austenitic mark. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 06Cr18Ni11Nb.
Inspection and Testing for GB/T 14976 06Cr18Ni11Nb
SHH STEEL reports the tests actually performed for 06Cr18Ni11Nb — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review. Sampling plans for 06Cr18Ni11Nb keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 06Cr18Ni11Nb duty: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium.
NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1. Non-conforming 06Cr18Ni11Nb lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 06Cr18Ni11Nb remains W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1.
Packaging and Shipping for GB/T 14976 06Cr18Ni11Nb
Export packing for GB/T 14976 06Cr18Ni11Nb is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium. Bundle tickets for 06Cr18Ni11Nb repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 06Cr18Ni11Nb caution visible here: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 06Cr18Ni11Nb. Desiccant and wrap choices for 06Cr18Ni11Nb follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 06Cr18Ni11Nb caution visible here: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review.
Photographic packing records are available on request for project QA files on 06Cr18Ni11Nb. Claims handling for 06Cr18Ni11Nb starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 06Cr18Ni11Nb duty: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium.
Why Choose SHH STEEL
Buyers choose SHH STEEL for 06Cr18Ni11Nb because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. SHH STEEL can produce and supply 06Cr18Ni11Nb against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 06Cr18Ni11Nb cleanly. Ask for a written acknowledgement that names 06Cr18Ni11Nb, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr18Ni11Nb to that written scope.
Supply Capability
Supply capability for 06Cr18Ni11Nb covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr18Ni11Nb when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 06Cr18Ni11Nb (S34778) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes for 06Cr18Ni11Nb: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1. SHH STEEL can supply alternate walls and precision classes for 06Cr18Ni11Nb once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 06Cr18Ni11Nb supply scope when the PO says so. Use: chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. SHH STEEL can produce trial lengths of 06Cr18Ni11Nb for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GB/T 14976 06Cr18Ni11Nb seamless stainless steel pipe used for?
- GB/T 14976 06Cr18Ni11Nb is seamless stainless pipe for fluid transport — chemical transfer, heat-exchange fluid loops, and process lines where 347-class Nb stabilisation is specified on Chinese BOMs. Role summary: Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium. It is a Chinese product standard grade (S34778), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 06Cr18Ni11Nb seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr18Ni11Nb when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 06Cr18Ni11Nb?
- 06Cr18Ni11Nb is delivered solution annealed under GB/T 14976. Table 1 reference: 920–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr18Ni11Nb so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr18Ni11Nb compare with sister grades 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10?
- 06Cr18Ni11Nb is filed as austenitic. Typical sisters on the same RFQ are 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10. Design caution: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr18Ni11Nb?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 347 / UNS S34778 the same as ordering 06Cr18Ni11Nb?
- No. 347 / UNS S34778 is a commercial / UNS cross-walk for body text (unified S34778). The purchase order should lock GB/T 14976 and 06Cr18Ni11Nb so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 06Cr18Ni11Nb?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr18Ni11Nb within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-C or W-H; density 8.03 kg/dm³ on theoretical weight calcs per Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 06Cr18Ni11Nb be welded on site?
- Shop guidance: 347 fillers; control heat input to protect Nb carbides. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr18Ni11Nb?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Nb window is 10C–1.10 — verify Nb on the MTC; do not substitute Ti grades without engineer review Sister pointers: 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 06Cr18Ni11Nb with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr18Ni11Nb does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr18Ni11Nb so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 06Cr18Ni11Nb?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr18Ni11Nb when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 06Cr18Ni11Nb is seamless stainless steel pipe for fluid transport — Nb-stabilised 18-8 austenitic seamless pipe for welded fluid service preferring niobium over titanium. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 07Cr18Ni11Nb, 06Cr18Ni11Ti, 022Cr19Ni10. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.