GB/T 14976 06Cr13Al Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 06Cr13Al Seamless Stainless Steel Pipe

GB/T 14976 06Cr13Al seamless stainless steel pipe (405 / UNS S40500-class, S11348), ferritic, Table 2 cast analysis, Rm min 415 MPa / Rp0.2 min 205 MPa, annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr13Al (S11348 / 405 / UNS S40500-class — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr13Al Seamless Stainless Steel Pipe

GB/T 14976-2025 is the Chinese national standard for seamless stainless steel pipes for fluid transport — replacing the 2012 edition and folding in prior LNG and oxygen-line tube GBs. Grade 06Cr13Al (unified number S11348) sits in the ferritic set of Table 1. GB/T 14976 06Cr13Al is ordered when the Chinese fluid spec wants aluminium in the 12Cr ferritic melt, not a hope that 06Cr13 will oxidise the same way.

SHH STEEL can produce and supply GB/T 14976 06Cr13Al as seamless W-C or W-H pipe across the enquiry OD×wall band, heat-treated per Table 1, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and Table 3 tensile results. Duty focus: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Shop language may still say “405 pipe,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 14976 and 06Cr13Al so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies.

Scope discipline: 06Cr13Al is seamless fluid-transport pipe under GB/T 14976, not a boiler tube under GB/T 13296 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 06Cr13, 10Cr15, 10Cr17, 022Cr17NbTi. Role reminder: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Inside this GB/T 14976 series, compare GB/T 14976 06Cr13, GB/T 14976 10Cr15, GB/T 14976 10Cr17, GB/T 14976 022Cr17NbTi. Hub: GB/T 14976.

When 06Cr13Al pipe sits beside plate on the same BOM, link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 4237 06Cr13Al so purchasing does not treat one product form as the other. Keep 06Cr13Al acceptance text on the governing pipe/tube standard.

Chemical Composition of GB/T 14976 06Cr13Al

Cast analysis for GB/T 14976 06Cr13Al follows Table 2. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤1.00, P ≤0.035, S ≤0.030, Ni ≤0.60, Cr 11.50–14.50, Al 0.10–0.30. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 405 / UNS S40500-class; unified number S11348. Corrosion thread: aluminium aids oxidation resistance in mild heat-facing fluid duties; aqueous chlorides remain limited.

Chemical limits for 06Cr13Al under GB/T 14976-2025 appear in the table underneath. Source priority is the 2025 Table 2 extract. If your client specification cites a 2012 footnote, send it before the heat is melted — phosphorus and several grade rows changed. Duty thread: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Grade C Si Mn P S Ni Cr Al
06Cr13Al ≤0.08 ≤1.00 ≤1.00 ≤0.035 ≤0.030 ≤0.60 11.50–14.50 0.10–0.30

Mechanical Properties of GB/T 14976 06Cr13Al

Ambient tensile floors for 06Cr13Al come from GB/T 14976 Table 3: Rm min 415 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 20% / transverse min 18%. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr13Al 415 205 20 18

Ambient values from GB/T 14976-2025 Table 3 for 06Cr13Al. Heat treatment (Table 1): 780–830 °C air or slow cool. Density 7.75 kg/dm³. Delivery: annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr13Al

For 06Cr13Al, the mill path is pierce/extrude/draw — never ERW or automatic-arc under GB/T 14976. Delivery is heat-treated and pickled unless overall ground/bored or bright protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Seamless W-C and W-H options remain available for 06Cr13Al; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Corrosion framing beside 06Cr13Al: aluminium aids oxidation resistance in mild heat-facing fluid duties; aqueous chlorides remain limited.

Ferritic heats follow Table 1 anneal bands with air or slow cool as listed — not austenitic solution practice. Do not copy 06Cr19Ni10 furnace charts onto ferritic marks. Heat-treatment reference for 06Cr13Al: 780–830 °C air or slow cool. Pickling follows unless bright heat treatment or overall machining leaves a scale-free surface. Duty thread: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 06Cr13Al: anneal 780–830 °C; mid-bore OD×wall common. Hydrostatic pressure or NDT class for 06Cr13Al is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Weld-shop note tied to 06Cr13Al: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review.

Dimensions and Tolerances for GB/T 14976 06Cr13Al

SHH STEEL aligns nominal OD (or ID), wall, length tolerance, and precision class (PA ordinary / PC higher) for 06Cr13Al before the mill slot is locked. Dimensions follow GB/T 17395 unless otherwise agreed. Size hint: anneal 780–830 °C; mid-bore OD×wall common. Tolerance class (PA/PC) follows the precision ordered for 06Cr13Al, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 06Cr13Al caution visible here: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against GB/T 2102 so pickled finishes are not iron-stained in transit. Duty thread: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13. Fixed lengths and multiple cut lengths for 06Cr13Al are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr13Al duty: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Equivalent Grades for GB/T 14976 06Cr13Al

Under GB/T 14976, 06Cr13Al is the governing seamless stainless fluid-transport pipe designation on this page. Commercial shorthand such as 405 / UNS S40500-class helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GB/T 14976 06Cr13Al line. ASTM A312 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.

System Designation Notes
GB/T 14976 06Cr13Al Governing pipe grade for this page
Commercial / UNS (body only) 405 / UNS S40500-class (unified S11348) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 06Cr13Al, move to a sister rather than stretching the alias: GB/T 14976 06Cr13, GB/T 14976 10Cr15, GB/T 14976 10Cr17, GB/T 14976 022Cr17NbTi. Apps context: heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry. Full list under GB/T 14976. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (06Cr13Al).

Heat Treatment and Delivery Condition for GB/T 14976 06Cr13Al

06Cr13Al is delivered annealed under GB/T 14976. Table 1 reference: 780–830 °C air or slow cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review. Recorded furnace charts for 06Cr13Al should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 06Cr13Al: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review.

Cooling type matters — austenitics need rapid cool after solution treatment; ferritic/martensitic anneal practice follows the air or slow-cool notes in Table 1. Duty thread: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13. Density 7.75 kg/dm³ for weight calcs. Field heat treatment of 06Cr13Al after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr13Al: aluminium aids oxidation resistance in mild heat-facing fluid duties; aqueous chlorides remain limited.

Corrosion Resistance of GB/T 14976 06Cr13Al

Corrosion behaviour of GB/T 14976 06Cr13Al tracks its ferritic balance: aluminium aids oxidation resistance in mild heat-facing fluid duties; aqueous chlorides remain limited. IGC clause 7.5 targets austenitic marks; for ferritic 06Cr13Al, corrosion testing follows the duty file rather than automatic method E. Design caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 06Cr13Al is filed as ferritic. Caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr13Al rather than relying on wall thickness alone. Application context for 06Cr13Al stays heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry.

Applications of GB/T 14976 06Cr13Al Seamless Pipe

Applications of GB/T 14976 06Cr13Al seamless pipe centre on heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry. Role summary: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry. Duty thread: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Weldability of GB/T 14976 06Cr13Al

06Cr13Al ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 06Cr13Al should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 06Cr13Al remains anneal 780–830 °C; mid-bore OD×wall common.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — ferritic — not a single shop habit. Caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies. Consumable lot control and shielding-gas notes for 06Cr13Al stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 06Cr13Al duty: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Surface Finishes for GB/T 14976 06Cr13Al

Typical GB/T 14976 supply for 06Cr13Al is a clean pickle after the required heat treatment, with bright anneal reserved for scale-free OD/ID appearance and ground/polished finishes reserved for written roughness targets. Use case colour: heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry. Free-iron control starts at the finishing bay, not at commissioning.

Finish Typical supply Order note
Annealed and pickled Standard pipe mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; inspect before polish on ferritic stock
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

When 06Cr13Al ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry.

Inspection and Testing for GB/T 14976 06Cr13Al

Inspection for GB/T 14976 06Cr13Al covers cast analysis, tensile tests, hydrostatic test (or replacing UT/ET), dimensions, appearance, and flattening/bend/flare when ordered. IGC clause 7.5 targets austenitic marks; for ferritic 06Cr13Al, corrosion testing follows the duty file rather than automatic method E. Documents follow GB/T 2102 / purchaser-specified EN 10204 styles. Sampling plans for 06Cr13Al keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 06Cr13Al: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review.

Marking includes 06Cr13Al, manufacturer, and other mandatory GB/T 2102 data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry. Non-conforming 06Cr13Al lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr13Al: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review.

Packaging and Shipping for GB/T 14976 06Cr13Al

Packaging for 06Cr13Al uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 06Cr13Al repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 06Cr13Al: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies. Desiccant and wrap choices for 06Cr13Al follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 06Cr13Al caution visible here: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies.

Shipping documents list GB/T 14976, 06Cr13Al, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13. Claims handling for 06Cr13Al starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 06Cr13Al: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 06Cr13Al with the seamless route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless capacity covering W-C and W-H for this mark. Duty focus: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13.

Technical sales can map 06Cr13Al against sisters 06Cr13, 10Cr15, 10Cr17, 022Cr17NbTi and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 06Cr13Al, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr13Al to that written scope.

Supply Capability

SHH STEEL can produce and supply GB/T 14976 06Cr13Al across enquiry-oriented OD × wall bands, in seamless W-C or W-H routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr13Al when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr13Al (S11348)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes: enquiry band typically aligns with GB/T 17395 OD×wall practice, with PA or PC precision as ordered. For 06Cr13Al, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: anneal 780–830 °C; mid-bore OD×wall common. SHH STEEL can supply alternate walls and PA/PC classes for 06Cr13Al once design pressure and corrosion allowance are clear. Corrosion framing beside 06Cr13Al: aluminium aids oxidation resistance in mild heat-facing fluid duties; aqueous chlorides remain limited.

Cut lengths, bevels, special NDT, IGC, and Annex A/B extras add lead time — call them early. Sisters often quoted alongside: 06Cr13, 10Cr15, 10Cr17, 022Cr17NbTi. Email the size list to start. SHH STEEL can produce trial lengths of 06Cr13Al for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr13Al seamless stainless steel pipe used for?
GB/T 14976 06Cr13Al is seamless stainless pipe for fluid transport — heat-adjacent mild fluid lines, utility water, and Chinese ferritic BOMs that call 405-class chemistry. Role summary: Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13. It is a Chinese product standard grade (S11348), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr13Al seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr13Al when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr13Al?
06Cr13Al is delivered annealed under GB/T 14976. Table 1 reference: 780–830 °C air or slow cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr13Al so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr13Al compare with sister grades 06Cr13, 10Cr15, 10Cr17?
06Cr13Al is filed as ferritic. Typical sisters on the same RFQ are 06Cr13, 10Cr15, 10Cr17. Design caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr13Al?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 405 / UNS S40500-class the same as ordering 06Cr13Al?
No. 405 / UNS S40500-class is a commercial / UNS cross-walk for body text (unified S11348). The purchase order should lock GB/T 14976 and 06Cr13Al so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr13Al?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr13Al within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: anneal 780–830 °C; mid-bore OD×wall common. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr13Al be welded on site?
Shop guidance: 405-class fillers; low heat input; avoid austenitic fillers that create mismatched joints without review. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr13Al?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: Al 0.10–0.30% is intentional — do not substitute plain 06Cr13; ferritic weld practice still applies Sister pointers: 06Cr13, 10Cr15, 10Cr17. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr13Al with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr13Al does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr13Al so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr13Al?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr13Al when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr13Al is seamless stainless steel pipe for fluid transport — Al-bearing 12Cr ferritic seamless pipe for mild fluid service needing improved scaling resistance versus plain 06Cr13. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr13, 10Cr15, 10Cr17. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X